Post by ThomasEekels » Aug 18 2019 1:35pm

Hi,
I have dismantled my Bosch 400 active line battery pack, as it was dead.
Finally, from the 40 batteries, 4 were still good, 4 were not so good and the remaining 32 were dead, zero volt or even minus 0.04.
It is a 40 battery pack, 10s2p

Is my assumption that also the BMS is faulty reasonable?

I want to replace all batteries and the BMS. The BMS is not the most expensive part I this renovation.

The Bosch BMS has not only 13 balance wires , it also has a 3wire to the bicycle connector, that I don't see on regular BMS boards.
From the 13 wires, 2 are short circuited and the rest are wired to the 10 plus and to one minus.

Can I buy any 11 wire BMS and forget abut the 3wire to the bicycle ?

advice is appreciated.
Thomas

Joachim   1 kW

1 kW
Posts: 435
Joined: Jul 30 2015 1:02pm
Contact:

Re: Battery pack revision for Bosch 400

Post by Joachim » Aug 18 2019 2:34pm

dont waste youre time and money...dead bosch battery: 99.9% the bms is also damaged and the bosch drive system
needs the signals from the bosch bms to wurk.

use Search: bosch battery

User avatar
neptronix   100 GW

100 GW
Posts: 15124
Joined: Jun 15 2010 5:56pm
Location: Utah, USA
Contact:

Re: Battery pack revision for Bosch 400

Post by neptronix » Aug 18 2019 2:35pm

Your Bosch has a special communication system between the battery and bike. Therefore, you need their BMS ( unless someone's hacked it! ). You're going to need to decide whether to stick with their parts, or dismantle their proprietary system and run a DIY setup to drive the bosch motor. Unless they'e also screwed you by not putting a 3 phase motor in the case.. :lol:
"Love and compassion are necessities, not luxuries. Without them, humanity cannot survive." - Dalai Lama

My first major build: 1.6kW 8T MAC motor on a Trek 4500 MTB.
Monster MTB: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: Heavy duty Cannondale semi recumbent - under construction.
Blue Dream: Maxaraya FS semi recumbent and high efficiency mid-drive - under construction.

ThomasEekels   10 mW

10 mW
Posts: 27
Joined: Aug 18 2019 12:33pm

Re: Battery pack revision for Bosch 400

Post by ThomasEekels » Aug 18 2019 3:37pm

Can I buy the original BMS somewhere ?
Has anyone bypassed the 3wire control to the bike ?

User avatar
flippy   10 MW

10 MW
Posts: 2206
Joined: Aug 12 2015 3:07pm

Re: Battery pack revision for Bosch 400

Post by flippy » Aug 18 2019 5:29pm

As soon as a single cell gets below 2v the bms commits suicide. You cant buy blanks because a unpowerd bosch bms means a dead bosch bms.

This is done to force you into the bosch ecosystem and dealership for maximizing profits. Its the apple of the ebike world.

Fun fact: the 300 and 400 powerpacks use the same cells, the bms just artificially caps the usable capacity on the 300 model.
Lithium beats liquid dinosaurs.

User avatar
neptronix   100 GW

100 GW
Posts: 15124
Joined: Jun 15 2010 5:56pm
Location: Utah, USA
Contact:

Re: Battery pack revision for Bosch 400

Post by neptronix » Aug 18 2019 5:48pm

I have a pack here with a suicided BMS and all cells above 3v. Sometimes the die because they feel like it!
"Love and compassion are necessities, not luxuries. Without them, humanity cannot survive." - Dalai Lama

My first major build: 1.6kW 8T MAC motor on a Trek 4500 MTB.
Monster MTB: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: Heavy duty Cannondale semi recumbent - under construction.
Blue Dream: Maxaraya FS semi recumbent and high efficiency mid-drive - under construction.

ThomasEekels   10 mW

10 mW
Posts: 27
Joined: Aug 18 2019 12:33pm

Re: Battery pack revision for Bosch 400

Post by ThomasEekels » Aug 19 2019 12:13pm

flippy wrote:
Aug 18 2019 5:29pm
As soon as a single cell gets below 2v the bms commits suicide. You cant buy blanks because a unpowerd bosch bms means a dead bosch bms.

This is done to force you into the bosch ecosystem and dealership for maximizing profits. Its the apple of the ebike world.

Fun fact: the 300 and 400 powerpacks use the same cells, the bms just artificially caps the usable capacity on the 300 model.
Well, that was expected. It's dead.
so either I get hold of a new Bosch BMS, or I hack the bike to discard of the 3wire control ?
I can charge the new built with any 10s bms, but the bike needs the Bosch I understand....

User avatar
flippy   10 MW

10 MW
Posts: 2206
Joined: Aug 12 2015 3:07pm

Re: Battery pack revision for Bosch 400

Post by flippy » Aug 19 2019 4:02pm

ThomasEekels wrote:
Aug 19 2019 12:13pm
so either I get hold of a new Bosch BMS, or I hack the bike to discard of the 3wire control ?
I can charge the new built with any 10s bms, but the bike needs the Bosch I understand....
1: good luck with that.
2: yes, welcome to the bosch ecosystem.

next time buy a bafang.
Lithium beats liquid dinosaurs.

User avatar
neptronix   100 GW

100 GW
Posts: 15124
Joined: Jun 15 2010 5:56pm
Location: Utah, USA
Contact:

Re: Battery pack revision for Bosch 400

Post by neptronix » Aug 19 2019 4:28pm

Option 3 is to bypass the proprietary stuff and free your bike like I mentioned.. IE run a new controller to the motor.
"Love and compassion are necessities, not luxuries. Without them, humanity cannot survive." - Dalai Lama

My first major build: 1.6kW 8T MAC motor on a Trek 4500 MTB.
Monster MTB: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: Heavy duty Cannondale semi recumbent - under construction.
Blue Dream: Maxaraya FS semi recumbent and high efficiency mid-drive - under construction.

User avatar
flippy   10 MW

10 MW
Posts: 2206
Joined: Aug 12 2015 3:07pm

Re: Battery pack revision for Bosch 400

Post by flippy » Aug 19 2019 5:58pm

neptronix wrote:
Aug 19 2019 4:28pm
Option 3 is to bypass the proprietary stuff and free your bike like I mentioned.. IE run a new controller to the motor.
and how would you do that? the controller is inside the motor. i got a bunch of detailed photo's of most used mid drives and apart from the bafang they all have the controller on the inside on a extremely custom pcb. only the bafang is universal.
Lithium beats liquid dinosaurs.

User avatar
neptronix   100 GW

100 GW
Posts: 15124
Joined: Jun 15 2010 5:56pm
Location: Utah, USA
Contact:

Re: Battery pack revision for Bosch 400

Post by neptronix » Aug 19 2019 6:59pm

flippy wrote:
Aug 19 2019 5:58pm
and how would you do that? the controller is inside the motor. i got a bunch of detailed photo's of most used mid drives and apart from the bafang they all have the controller on the inside on a extremely custom pcb. only the bafang is universal.
If it has 3 phases, there's a way to drive it.
Drill a hole in the drive and run phase wires out.

If you're lucky, it'll have hall sensors too. :)

Here's a guy who is driving it with a VESC ( some people have also played with other setups )
viewtopic.php?t=93831
"Love and compassion are necessities, not luxuries. Without them, humanity cannot survive." - Dalai Lama

My first major build: 1.6kW 8T MAC motor on a Trek 4500 MTB.
Monster MTB: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: Heavy duty Cannondale semi recumbent - under construction.
Blue Dream: Maxaraya FS semi recumbent and high efficiency mid-drive - under construction.

User avatar
flippy   10 MW

10 MW
Posts: 2206
Joined: Aug 12 2015 3:07pm

Re: Battery pack revision for Bosch 400

Post by flippy » Aug 19 2019 8:37pm

doing so would break the water seals, not something i recommend as the motor has zero protection for water or crap on the inside of the case.
the bafang is brilliant, all the electronics on the inside are driven by a potted box on the outside. its stupid easy to replace that controller.
and the bosch has a crank sensor, its useless without the magic sause from bosch and twitchy as hell if it is mounted even slighty wrong.
Lithium beats liquid dinosaurs.

User avatar
neptronix   100 GW

100 GW
Posts: 15124
Joined: Jun 15 2010 5:56pm
Location: Utah, USA
Contact:

Re: Battery pack revision for Bosch 400

Post by neptronix » Aug 19 2019 9:03pm

flippy wrote:
Aug 19 2019 8:37pm
doing so would break the water seals, not something i recommend as the motor has zero protection for water or crap on the inside of the case.
You might not even have to drill holes out of the case. There's likely some thickish power wires going to the unit. Those could be reused and sealed with RTV or something else.
"Love and compassion are necessities, not luxuries. Without them, humanity cannot survive." - Dalai Lama

My first major build: 1.6kW 8T MAC motor on a Trek 4500 MTB.
Monster MTB: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: Heavy duty Cannondale semi recumbent - under construction.
Blue Dream: Maxaraya FS semi recumbent and high efficiency mid-drive - under construction.

ThomasEekels   10 mW

10 mW
Posts: 27
Joined: Aug 18 2019 12:33pm

Re: Battery pack revision for Bosch 400

Post by ThomasEekels » Aug 20 2019 8:03am

Another out-of-he-box. idea.
If I can not get the original battery BMS, but rebuild the battery pack with ordinary 10S bms,
can I put the DIY pack parallel to an original Bosch pack ? Like charge it separately, but connect the decharge in parallel before the ride?
Just piggy bag both battery packs. The original pack will communicate with the bicycle, the 2nd pack will supply power in parallel...

is that feasible ?

User avatar
flippy   10 MW

10 MW
Posts: 2206
Joined: Aug 12 2015 3:07pm

Re: Battery pack revision for Bosch 400

Post by flippy » Aug 20 2019 9:04am

no, you cant because the bms is already dead.
neptronix wrote:
Aug 19 2019 9:03pm
You might not even have to drill holes out of the case. There's likely some thickish power wires going to the unit. Those could be reused and sealed with RTV or something else.
the connectors to the outside and its weather seals are on the controller board so that aint gonna work.
Lithium beats liquid dinosaurs.

Hillhater   100 GW

100 GW
Posts: 11425
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: Battery pack revision for Bosch 400

Post by Hillhater » Aug 20 2019 8:48pm

ThomasEekels wrote:
Aug 20 2019 8:03am
Another out-of-he-box. idea.
If I can not get the original battery BMS, but rebuild the battery pack with ordinary 10S bms,
can I put the DIY pack parallel to an original Bosch pack ? Like charge it separately, but connect the decharge in parallel before the ride?
Just piggy bag both battery packs. The original pack will communicate with the bicycle, the 2nd pack will supply power in parallel...

is that feasible ?
Sound like a strong possibility of killing the 2nd pack as well :roll:
This forum owes its existence to Justin of ebikes.ca

ThomasEekels   10 mW

10 mW
Posts: 27
Joined: Aug 18 2019 12:33pm

Re: Battery pack revision for Bosch 400

Post by ThomasEekels » Sep 01 2019 6:10am

flippy wrote:
Aug 20 2019 9:04am
no, you cant because the bms is already dead.

Maybe my question was not clear: I intended a new battery with good BMS. and put the rebuilt battery, (without BMS) in parrallel after charging.

User avatar
flippy   10 MW

10 MW
Posts: 2206
Joined: Aug 12 2015 3:07pm

Re: Battery pack revision for Bosch 400

Post by flippy » Sep 01 2019 8:20am

ThomasEekels wrote:
Sep 01 2019 6:10am
Maybe my question was not clear: I intended a new battery with good BMS. and put the rebuilt battery, (without BMS) in parrallel after charging.
you understand that as soon as you disconnect a single balance wire from the new bms it is also toast?

swapping boards will require one massive wire-dance if you want to keep all the wires connected to anything all the time.
Lithium beats liquid dinosaurs.

Post Reply