I’m using 20S9P battery with 45A from recycled laptop 18650 cell. It work well during testing until my controller was dead short.
When the controller is dead short, it doesn’t trip the 100A main circuit breaker, but it killed my 45A bms along with burned 3 of the cell fuse. I’m replacing the bms and also replace the cell fuse. My question is; do I need to add a fuse from the main battery (before the contactor)? I’m thinking about using a dc 60amp glass fuse. My plan is also to add another 20S12P with separate bms. Can the fuse protect the bms?
Thank you for your help.
Cell fuse with battery pack fuse
Re: Cell fuse with battery pack fuse
link to the cell fuse please
Re: Cell fuse with battery pack fuse
Usually not. Fuses take a definite period of time to blow and that is usually a lot longer than the time it takes the bms to die. Just get a bigger bms. Don't know why you have a 100amp CB on a 45a bms, that won't protect bms. If you have a CB rated at the peak load of the bms then maybe it would but that might cause you issues of it inadvertent tripping, right when you crank the throttle to nip in front of a truck
Also when a switch/fuse suddenly pops open the voltage spine alone can kill the bms. I'd get a bms that can handle well above the controllers rating and if you want it protected, an adequate cb. Bear in mind they all have different ways of tripping.

-
- Posts: 85
- Joined: Oct 23 2020 8:19pm
Re: Cell fuse with battery pack fuse
Thank you for your reply. The reason I choose 45a bms is because my 20S9P battery is build from recycled laptop battery. So I think the max amp drain of the battery is about 36A.kdog wrote: ↑Nov 02 2020 4:53amUsually not. Fuses take a definite period of time to blow and that is usually a lot longer than the time it takes the bms to die. Just get a bigger bms. Don't know why you have a 100amp CB on a 45a bms, that won't protect bms. If you have a CB rated at the peak load of the bms then maybe it would but that might cause you issues of it inadvertent tripping, right when you crank the throttle to nip in front of a truckAlso when a switch/fuse suddenly pops open the voltage spine alone can kill the bms. I'd get a bms that can handle well above the controllers rating and if you want it protected, an adequate cb. Bear in mind they all have different ways of tripping.
I’m replace the mosfets of the bms so that it use 2 mosfet in parallel in the same position
-
- Posts: 85
- Joined: Oct 23 2020 8:19pm