which solder to use and is this right?

Batteries, Chargers, and Battery Management Systems.
Post Reply
papasapien   10 mW

10 mW
Posts: 22
Joined: Nov 13 2020 2:09am

which solder to use and is this right?

Post by papasapien » Nov 21 2020 8:17pm

someone said i should use silver solder to connect my battery lead wires to the battery. what do you guys think? why not regular solder 60/40 or 63/37?

also does this look right for my battery? the way i have the end wires for best current flow? with the stitched together wires? is that okay right?
newbat.png
newbat.png (90.72 KiB) Viewed 325 times

goatman   100 MW

100 MW
Posts: 2656
Joined: Jun 23 2019 6:50pm
Location: Surrey, B.C.

Re: which solder to use and is this right?

Post by goatman » Nov 21 2020 10:23pm

i use 60/40, are you running 30amps

papasapien   10 mW

10 mW
Posts: 22
Joined: Nov 13 2020 2:09am

Re: which solder to use and is this right?

Post by papasapien » Nov 21 2020 10:37pm

the pack will have a max continuous discharge of 40 amps possible but my controller will only ever pull 35.

also what will the difference be if i use 63/37 vs 60/40? is that better recommended for electrical reasons or just solder preference?
thanks

goatman   100 MW

100 MW
Posts: 2656
Joined: Jun 23 2019 6:50pm
Location: Surrey, B.C.

Re: which solder to use and is this right?

Post by goatman » Nov 21 2020 10:51pm

60/40 melts quickly, 3 seconds with a 60 watt iron and the joint is done and the battery doesnt get hot but if youre spot welding the pack, solder first then spot weld the nickel strip to the battery. i tried 63/37 from a local store and didnt like it, it might have been when i was using a 40 watt iron and getting bad/cold joints, so i put it on the shelf and rode 30km to get the 60/40

goatman   100 MW

100 MW
Posts: 2656
Joined: Jun 23 2019 6:50pm
Location: Surrey, B.C.

Re: which solder to use and is this right?

Post by goatman » Nov 21 2020 10:56pm

and i melt Oatey No.95 lead free tinning flux on the battery/nickel strip first, let cool, then solder the wire to it

Balmorhea   1 MW

1 MW
Posts: 1575
Joined: Oct 01 2019 8:30pm
Location: Austin

Re: which solder to use and is this right?

Post by Balmorhea » Nov 21 2020 11:38pm

papasapien wrote:
Nov 21 2020 10:37pm
also what will the difference be if i use 63/37 vs 60/40? is that better recommended for electrical reasons or just solder preference?
No practical difference either way. The performance of the flux in the core will make more difference than the alloy.

Lead free? That's another matter, and something to steer clear of.
___________
Finish Reconstruction.

jonyjoe303   100 W

100 W
Posts: 167
Joined: Aug 31 2017 9:44pm

Re: which solder to use and is this right?

Post by jonyjoe303 » Nov 22 2020 2:43am

This is the brand I been using for years, its also 60/40 and 0.8mm is a good size, not too small or large. It works as good as the kester brand. I got 3 rolls always ready to go.
1 solder 6040.jpg
1 solder 6040.jpg (75.77 KiB) Viewed 285 times

goatman   100 MW

100 MW
Posts: 2656
Joined: Jun 23 2019 6:50pm
Location: Surrey, B.C.

Re: which solder to use and is this right?

Post by goatman » Nov 22 2020 8:13am

Balmorhea wrote:
Nov 21 2020 11:38pm
papasapien wrote:
Nov 21 2020 10:37pm
also what will the difference be if i use 63/37 vs 60/40? is that better recommended for electrical reasons or just solder preference?
No practical difference either way. The performance of the flux in the core will make more difference than the alloy.

Lead free? That's another matter, and something to steer clear of.
why stay free of lead-free tinning flux? been using it for 2 years with no battery issues and ive soldered up 5 packs using it

Balmorhea   1 MW

1 MW
Posts: 1575
Joined: Oct 01 2019 8:30pm
Location: Austin

Re: which solder to use and is this right?

Post by Balmorhea » Nov 22 2020 1:11pm

goatman wrote:
Nov 22 2020 8:13am
Balmorhea wrote:
Nov 21 2020 11:38pm
Lead free? That's another matter, and something to steer clear of.
why stay free of lead-free tinning flux? been using it for 2 years with no battery issues and ive soldered up 5 packs using it
I was talking about solder, not flux.

Lead free solders have higher melting points and poor wetting compared to traditional tin-lead electrical solder, in my observation. I use them for plumbing, but not for electric applications.
___________
Finish Reconstruction.

999zip999   100 GW

100 GW
Posts: 9934
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: which solder to use and is this right?

Post by 999zip999 » Nov 22 2020 2:10pm

What cells are you using brand and model number.