Is a little rust normal for nickel strip in salt water

Batteries, Chargers, and Battery Management Systems.
Post Reply
pbert   100 mW

100 mW
Posts: 36
Joined: May 08 2019 11:08pm

Is a little rust normal for nickel strip in salt water

Post by pbert » Dec 07 2020 9:26pm

[img][img]I purchased some pure nickel strip from ali express. I cut a small portion and scratched the surface of the strip in order to epose the center of the strip and then placed it in salt water for 48h. Ther eis a small amount of rust as can be seen in the pics. Is this normal or does this mean that the strips are not pure nickel ?
Thanks.

pbert   100 mW

100 mW
Posts: 36
Joined: May 08 2019 11:08pm

Re: Is a little rust normal for nickel strip in salt water

Post by pbert » Dec 07 2020 9:29pm

Also im unable to attach a picture ... ive tried jpg and png format. What are valid picture formats ?

Thanks.

pbert   100 mW

100 mW
Posts: 36
Joined: May 08 2019 11:08pm

Re: Is a little rust normal for nickel strip in salt water

Post by pbert » Dec 07 2020 10:17pm

Ok, i renamed the file to jpeg extension and seems to work now.
Attachments
nstrip1.jpeg
nstrip1.jpeg (90.56 KiB) Viewed 352 times

User avatar
Chalo   100 GW

100 GW
Posts: 8352
Joined: Apr 29 2009 11:29pm
Location: Austin, Texas

Re: Is a little rust normal for nickel strip in salt water

Post by Chalo » Dec 07 2020 11:09pm

Nickel doesn't rust. Red means steel.
This is to express my gratitude to Justin of Grin Technologies for his extraordinary measures to save this forum for the benefit of all.

kansas   10 mW

10 mW
Posts: 27
Joined: Nov 05 2018 7:58pm

Re: Is a little rust normal for nickel strip in salt water

Post by kansas » Dec 08 2020 9:51am

Check it with a magnet.

999zip999   100 GW

100 GW
Posts: 9934
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: Is a little rust normal for nickel strip in salt water

Post by 999zip999 » Dec 08 2020 10:19am

do you have a link so you can check it out and see how they wrote it cuz I was reading this one and they call it nickel steel. ? Hard to trust and know what you're getting.

pbert   100 mW

100 mW
Posts: 36
Joined: May 08 2019 11:08pm

Re: Is a little rust normal for nickel strip in salt water

Post by pbert » Dec 08 2020 2:43pm

Hi, here is the link to the product :

https://www.aliexpress.com/item/4000060 ... 4c4dMCFMtj

It does not mention steel anywhere, just Nickel strip.

I tested with a magnet and it is magnetic ....

Ill keep searching for true nickel strip on aliexpress.

Thanks.

User avatar
spinningmagnets   100 GW

100 GW
Posts: 11869
Joined: Dec 21 2007 10:27pm
Location: Ft Riley, NE Kansas

Re: Is a little rust normal for nickel strip in salt water

Post by spinningmagnets » Dec 08 2020 3:15pm

First, check out the copper/nickel sandwich discussion.

User avatar
Chalo   100 GW

100 GW
Posts: 8352
Joined: Apr 29 2009 11:29pm
Location: Austin, Texas

Re: Is a little rust normal for nickel strip in salt water

Post by Chalo » Dec 08 2020 4:30pm

kansas wrote:
Dec 08 2020 9:51am
Check it with a magnet.
Pure nickel is ferromagnetic. Less so than steel.
This is to express my gratitude to Justin of Grin Technologies for his extraordinary measures to save this forum for the benefit of all.

pbert   100 mW

100 mW
Posts: 36
Joined: May 08 2019 11:08pm

Re: Is a little rust normal for nickel strip in salt water

Post by pbert » Dec 08 2020 10:01pm

spinningmagnets wrote:
Dec 08 2020 3:15pm
First, check out the copper/nickel sandwich discussion.
spinningmagnets thanks for pointing me towards the nickel / copper sandwhich thread. I read through it and it looks like i might give this solution a try. I had actually ordered some copper from aliexpress and never got around to experimenting with it so now i have a reason. Is there any way to know if the copper is pure copper or mixed with another material ?

Thanks.

kdog   10 kW

10 kW
Posts: 694
Joined: Feb 02 2014 9:22pm
Location: hobart, tasmania

Re: Is a little rust normal for nickel strip in salt water

Post by kdog » Dec 09 2020 7:54am

I've often had a little rust colour (exactly like in your pic) with pure nickel. I think if you have old gal pipes some dissolved iron precipitates out causing the colour, usually rubs off showing bright nickel inderneatg. The rust you get with nickel plated steel is very obviously part of the metal and inhabits the scratch.
Magnet test is useless.

User avatar
spinningmagnets   100 GW

100 GW
Posts: 11869
Joined: Dec 21 2007 10:27pm
Location: Ft Riley, NE Kansas

Re: Is a little rust normal for nickel strip in salt water

Post by spinningmagnets » Dec 09 2020 8:10am

I dont know if theres a purity test for copper that would be easy for DIY garage builders. Even if there is some admixture from a cheap copper recycler, just check the resistance in ohms with a multimeter.

The reading wouldnt have to be precise. As long as it's very high conductivity and very low resistance, its miles ahead of using pure nickel. Check a longish section of your copper, and then check the same length on a section of copper wire that you are certain is pure copper.

The IACS conductivity of nickel is around 24/100, and pure copper is 100/100, four times better.

If you got ahold of some dirty recycled copper that was only 98% copper, you are still doing great. Steel is roughly 5/100, which is horrible.

pbert   100 mW

100 mW
Posts: 36
Joined: May 08 2019 11:08pm

Re: Is a little rust normal for nickel strip in salt water

Post by pbert » Dec 10 2020 9:50am

I tried verifying the resistance of the nickel strip vs the copper but my ohm meter is not precise enough, the smallest resistance measurement is at 200 ohm level.

Post Reply