Found a good Li-Ion cylindrical cell pack capacity remaining v resting voltage table from an E-bike pack rebuilder.
Use the Volts Per Cell column data times number of cells in-Series to apply the table data to larger and smaller Series packs.
It might be just a bit conservative - a good thing, as it shows the cell empty at 3.0 vrs most manufacturers using a 2.5 Volts discharge cutoff.
Use the Volts Per Cell column data times number of cells in-Series to apply the table data to larger and smaller Series packs.
It might be just a bit conservative - a good thing, as it shows the cell empty at 3.0 vrs most manufacturers using a 2.5 Volts discharge cutoff.