Post by DrkAngel » Oct 08 2013 10:27pm

It seems that, with no doubt, lowering charge-float voltage will prolong capacity and lifespan of Li-ion cells.
Image
Multiple sources estimate a doubling of usable cycles from a .10V reduction in peak charge.
In some cases this is a mere 10% capacity reduction in preliminary capacity.
But soon, the capacity in the lower charge voltage cells exceeds the capacity of the higher voltage cells.

More info - Determining Optimal Charge Voltage

LiFePO4 types are much more difficult to quantify due to their charge-discharge process.
Last edited by DrkAngel on Oct 09 2013 7:56am, edited 1 time in total.
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - December 2019

EBike Toolbox - Bargains! $

Endless Sphere Wiki - Lost?

powersupply   100 W

100 W
Posts: 215
Joined: Apr 14 2013 8:04am
Location: Santa Monica

Re: Homemade Battery Packs

Post by powersupply » Oct 08 2013 11:19pm

Mine are hardcase packs (LiPo) but I'm looking into LiFePos.

Got a setback with my SmartBMS, seems it is not as smart as built.

ricklearned   100 mW

100 mW
Posts: 36
Joined: Feb 07 2012 8:10pm
Location: Hermosa Beach California USA

Re: Homemade Battery Packs

Post by ricklearned » Oct 08 2013 11:36pm

DrkAngel wrote:It seems that, with no doubt, lowering charge-float voltage will prolong capacity and lifespan of Li-ion cells.
................
LiFePO4 types are much more difficult to quantify due to their charge-discharge process.
I charge my LiFePO4's to 3.4 volts. The extra amphours I would get by going to 3.65 is not worth the decreased cycle life.

1KW   1 kW

1 kW
Posts: 341
Joined: Jul 24 2013 10:23am

Re: Homemade Battery Packs

Post by 1KW » Oct 09 2013 6:20pm

I was thinking about going makita packs..since I can get a 18s8p delivered for 260.00. However have to sort through everything and ect. However they are also 5C cells!

Could the same pack be put together with laptop cells for cheaper? What model laptops should the batterys be coming from? Any higher discharge cells that come in lots from recent laptops? 2012+

User avatar
DrkAngel   100 GW

100 GW
Posts: 5277
Joined: Dec 15 2010 11:14am
Location: Upstate-Western-Southern Tier NY. USA

Re: Homemade Battery Packs

Post by DrkAngel » Oct 10 2013 9:34am

Great price for Makita cells, dependent on condition ... if you need the C rate.

Laptop cells, in the 2600mAh range are cheaper and more plentiful.
I have seen few "actual" higher capacity cells, forgeries, mislabeled, abound, especially in "replacement" packs.
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - December 2019

EBike Toolbox - Bargains! $

Endless Sphere Wiki - Lost?

1KW   1 kW

1 kW
Posts: 341
Joined: Jul 24 2013 10:23am

Re: Homemade Battery Packs

Post by 1KW » Oct 10 2013 10:10am

ok great, I only need about 30 amp max discharge, as Im going to go for a little higher voltage..around 72v.

What model packs should I look for however? I want to match the cells vs getting 10 different types of cells.


Will be built in 3 6s packs and balanced charged with bc charger.

User avatar
DrkAngel   100 GW

100 GW
Posts: 5277
Joined: Dec 15 2010 11:14am
Location: Upstate-Western-Southern Tier NY. USA

Finding Laptop cells for recycling?

Post by DrkAngel » Oct 10 2013 10:55am

1KW wrote:ok great, I only need about 30 amp max discharge, as Im going to go for a little higher voltage..around 72v.

What model packs should I look for however? I want to match the cells vs getting 10 different types of cells.


Will be built in 3 6s packs and balanced charged with bc charger.
At 30A max, you want a minimum of 30Ah, (12p = 31.2Ah - 2600mAh cells)), more is better!

I highly recommend cells of same capacity and brand!

"Lot laptop batteries -new" search on ebay might be your best bet.
Local recycling centers?
Large companies often replace quantities of laptop packs annually, "ask da boss"?
Craigs list?

After finding cells, refer to - Cell Testing and Selection
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - December 2019

EBike Toolbox - Bargains! $

Endless Sphere Wiki - Lost?

User avatar
DrkAngel   100 GW

100 GW
Posts: 5277
Joined: Dec 15 2010 11:14am
Location: Upstate-Western-Southern Tier NY. USA

Charge vs Float voltage

Post by DrkAngel » Oct 14 2013 7:43am

In regard to charging cells, there is a difference between "charge" and "float" voltage.

"Float" voltage involves applying the desired resultant voltage. This provides an initial high amperage charge rate that reduces till desired pack voltage is attained. Amperage reduces to an ultimate .0 Amps. The disadvantage is a prolonged, minute "topping" charge. This method is used in charging using a variable power supply, such as the venerable MeanWell, adjusting the resultant voltage then waiting till pack nears set voltage.

"Charge voltage", by contrast, typically refers to the speedier method of charging cells by supplying a higher voltage to cells and disconnecting voltage when amperage reduces to a predetermined amount. Charge voltage is higher than the desired resultant voltage. This method requires a "smart charger" that stops charging at an estimated higher voltage, as amperage drops to a certain level. The purpose is to attain a final voltage by estimating the voltage and amperage necessary to acquire the desired resultant voltage after charge stopped. The advantage is a much quicker "topping" voltage.

Hypothetically, a battery could be fully charged at a 1C amperage rate in 1 hour. However, this would involve hazardous voltages, a 4.2V rated cell might require a 4.5V charge voltage. This could be extremely damaging and dangerous. Typically, "charge voltage" is limited to 4.25-4.3V and regulated by multiple cutoffs.

"Smart" chargers often "cycle" applying charge voltage, then stopping, waiting, and measuring the retained voltage, then reapplying charge etc. There are

Personally, after determining optimal charge voltages, I might charge at 4.2V per cell but manually stop charge when amperage reduces to <1amp. Reduced amp estimated as point to attain a 4.1V, or other desired voltage, final "float" voltage.
Last edited by DrkAngel on Oct 14 2013 8:24am, edited 1 time in total.
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - December 2019

EBike Toolbox - Bargains! $

Endless Sphere Wiki - Lost?

User avatar
GCinDC   10 GW

10 GW
Posts: 4245
Joined: Jan 23 2009 11:19am
Location: Washington, DC

Re: Homemade Battery Packs

Post by GCinDC » Oct 14 2013 8:01am

fwiw, termination current seems to matter too, from here.
the author wrote:Battery charge voltage and current

In my charger reviews I often comment on a high termination current, and says that the battery will not be fully charged, but I do not specify more precise what that means.
In this test here I have taken a battery and charged it with many different charge settings and then measured the capacity and energy in the battery. All the measurements was done on automated equipment, i.e. voltage, current and timing was exactly the same in each test, except the charger termination setting. For the test I have used a fairly new AW18650-26 cell.

The charger started at 1.3 ampere and followed a perfect CC/CV curve until the specified limits.
After charging the battery rested for one hour.
The discharge was done at 1 ampere and stopped when the battery was down to 2.8 volt.

In the table the green line is what a typical hobby charger will do at the 1A LiPo setting.
Image


Plotting the voltage after 60 minute versus capacity shows a very good correlation:
Image
As can be seen from the table, both the termination current and termination voltage is very significant to get the most energy from the cell. The downside to filling the cell completely is lifetime, a cell with a high resting voltage will wear down a lot faster and this will happen even if it is not used.
Youtube channel, 2013 Highlights vid. Ebike Nerdcast.
Giant DH Comp: 20s lipo (11.6Ah), hs3540, Adaptto Mini-E, 900W BMSBattery charger.
GT I-Drive (sold), 20s lipo, 9C, 72V 45A 12FET.

powersupply   100 W

100 W
Posts: 215
Joined: Apr 14 2013 8:04am
Location: Santa Monica

Re: Homemade Battery Packs

Post by powersupply » Oct 17 2013 5:47am

But what if a BMS is used?
The charger could (should?) be a "dumb" charger, with no CC or CV in that situation, right?
Because the BMS takes control of everything?

I can get "or" able power supplies roughly 56V/5A for $20 (for 13s LiPo pack).

Would be perfect for me as I can add more power supplies at some point if 5A charging feels too slow.

But they are just simple power supplies, no CC/CV.
Would those work for a BMS?

Thanks!

User avatar
DrkAngel   100 GW

100 GW
Posts: 5277
Joined: Dec 15 2010 11:14am
Location: Upstate-Western-Southern Tier NY. USA

Re: Homemade Battery Packs

Post by DrkAngel » Oct 17 2013 8:59am

powersupply wrote:But what if a BMS is used?
The charger could (should?) be a "dumb" charger, with no CC or CV in that situation, right?
Because the BMS takes control of everything?

I can get "or" able power supplies roughly 56V/5A for $20 (for 13s LiPo pack).

Would be perfect for me as I can add more power supplies at some point if 5A charging feels too slow.

But they are just simple power supplies, no CC/CV.
Would those work for a BMS?

Thanks!
Very much depends on the BMS!
Some seem worse than useless, while others control every segment of the charge-discharge process.

I use a bulk (dumb) charger because I want the capability of adjusting the final voltage.
Effectively, I can "program" the Ah capacity vs longevity of the battery pack.

Manufactures tend to recommend a maximum of a .8C charge rate.
I try to not exceed .5C charge, or continuous discharge, for my recycled laptop cells.

Non-adjustable chargers can have their voltage trimmed by running through one or more diodes.
Voltage drop can be between .3V - .7V per diode.
Smart charger might require a return voltage which the diodes block.
A small wattage resister bypassing the diodes might resolve this malfunction.
I extended my charger cord with an additional cord, connected with a Deans (T) plug.
Double T plug, inserts (modules) can be built and placed in line for various "adjustments".
Last edited by DrkAngel on May 03 2014 9:34am, edited 2 times in total.
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - December 2019

EBike Toolbox - Bargains! $

Endless Sphere Wiki - Lost?

powersupply   100 W

100 W
Posts: 215
Joined: Apr 14 2013 8:04am
Location: Santa Monica

Re: Homemade Battery Packs

Post by powersupply » Oct 17 2013 9:10am

It is for the SmartBMS unit.
The charger would be mounted onto my scooter and the charging rate would be 0.25C over 4 hours.

It is a simple power supply:
XL275-AC Series 275-Watt AC to DC_PS-5649.pdf
charger
(1.27 MiB) Downloaded 183 times
Thanks!!

User avatar
DrkAngel   100 GW

100 GW
Posts: 5277
Joined: Dec 15 2010 11:14am
Location: Upstate-Western-Southern Tier NY. USA

Re: Homemade Battery Packs

Post by DrkAngel » Oct 17 2013 10:06am

powersupply wrote:It is for the SmartBMS unit.
The charger would be mounted onto my scooter and the charging rate would be 0.25C over 4 hours.

It is a simple power supply:
XL275-AC Series 275-Watt AC to DC_PS-5649.pdf
Thanks!!
Make sure to add a cooling fan.
12V voltage supplied.
54VDC 5.2A & 56V 4.9A SWITCHING POWER SUPPLYs - $16.95
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - December 2019

EBike Toolbox - Bargains! $

Endless Sphere Wiki - Lost?

powersupply   100 W

100 W
Posts: 215
Joined: Apr 14 2013 8:04am
Location: Santa Monica

Re: Homemade Battery Packs

Post by powersupply » Oct 17 2013 10:57am

Yes, fan of course, plus some casing against splatter etc.

The 275W is the unit I was aiming at.
The 280W cannot be adjusted unfortunately, love its isolated 12V though.

In the comments (of the 280W) somebody writes that it is not easy to modify the voltage, but no details on how.

So yould that 275W power supply work in my cenario?

Thanks!

User avatar
DrkAngel   100 GW

100 GW
Posts: 5277
Joined: Dec 15 2010 11:14am
Location: Upstate-Western-Southern Tier NY. USA

Modified Voltage Perimeters!

Post by DrkAngel » Oct 20 2013 11:23am

My 29.6V 31.2A (8s12p) Sanyo 18650 cells seem to have suffered an early demise.
After barely 1000 miles, pack is deteriorating quickly.

Cells began as an 6s16p (22.2V 41.6Ah) stuffed into an eZip RMB shell.
See -22.2V Battery Woes

Image
While initial tests provide 60 miles @16+mph and ...
"41.6Ah pack (4.20 - 3.71V per cell discharge) accepted 32.86Ah recharge, at an estimated 80-85% DOD, for a ~38-41Ah capacity!
So cells appear to be of excellent capacity condition."
... I felt performance "... inadequate".
Initially I considered converting pack to 12s8p (44.4V 20.8Ah) but decided on a more utilitarian 8s12p (29.6 31.2Ah).
After initial excellent speed and range, recharge Ah began reducing with nearly every cycle.
I blame my own ignorance!
Initially I discharged to near 3.6V and charged to 4.20V, using my mAh/100thV Discharge Capacity Map as my guide.
Image
Unfortunetly, of fortunetly, I developed a method of capacity mapping using charge mAh/200thV.

This method precisely quantifies the amount of electricity to raise pack voltage between steps of voltage.
Results were enlightening!
Image
It seems discharging below 3.72V is needlessly damaging!
Further, all experts agree, lowering peak charge voltage greatly increases capacity and cycle life!
A 1/10V reduction in charge voltage will double usable life!

As indicated by the graph, the last capacity bulge ends at 4.05V.
Keeping voltages between 3.72V and 4.05V should increase usable life to 300%!
This from an initial loss of usable Ah of a measured 18%.

Well, this is merely a prelude to my next project using my best Sanyo 18650 cells.
9s12p (33.3 31.2Ah) will squeeze into an eZip RMB pack.
I have 108+ saved (best bleed down) cells.
Bleed down test revised to maintained above 4.05V after 6 months - my last bulk charge of candidate cells.
But I intend on retesting all my Sanyo cells with my Bulk Capacity Test, 60 cells at a time.
All cells will be discharged rated from 4.10V to 3.7V.

33.3V pack will work on my 36V controller Winter eZip and my universal controller eZip LS.
I intend on keeping a spare oem geared wheel-motor combo, ready for quick swap for high torque 20mph legality from 33.3V.

I have to keep my upgeared eZips for my 25.9V Lipo packs.
7s12p is the best I can squeeze into the RMB pack.
Last build gave adequate performance for 5000+ miles. (Still use it for quick trips around town - 6500+ miles)
Charge Capacity mapping indicates a 50% increase in usable life by reducing charge to 4.15V, with a miniscule loss of capacity!

Test was run twice to confirm odd capacity bulge between 4.10-4.15V.
Image
Alternatively, reducing charge voltage below 4.05V increases usable life +300% ... but with a 25%+ loss of capacity.
25.9V 26Ah Lipo pack reduced to to ~18Ah usable ... might be worth it for 6 years of daily use - vs 2 years.
Best of all ... I can use a 2nd battery in the rack for longer trips ...
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - December 2019

EBike Toolbox - Bargains! $

Endless Sphere Wiki - Lost?

Teh Stork   1 kW

1 kW
Posts: 461
Joined: May 25 2011 8:02am

Re: Homemade Battery Packs

Post by Teh Stork » Oct 20 2013 6:43pm

Keep in mind that running a 1C pack at 1C isn't going to net you very long lifetime, regardless of float voltage.
2013 VW E-UP!
Kona mtb: Cromotor, Kelly KEB, ~6kW peak, 1,4kWh 90V battery 29E cells, 38 kg

User avatar
DrkAngel   100 GW

100 GW
Posts: 5277
Joined: Dec 15 2010 11:14am
Location: Upstate-Western-Southern Tier NY. USA

Re: Homemade Battery Packs

Post by DrkAngel » Oct 21 2013 5:37am

Teh Stork wrote:Keep in mind that running a 1C pack at 1C isn't going to net you very long lifetime, regardless of float voltage.
Of course ... with laptop cells, I recommend a maximum surge of 1C, with a continuous drain of .5C or less.
For the eZips with 30-35A controllers-450w motor, I've always recommended a 30Ah+ pack.

The exception is my laptop recycled Lipo builds.
Unfortunately, the eZip oem battery pack can fit a mere 25.92Ah at 25.9V.
But even with full throttle starts I've never blown the 30A fuse I installed ...

Deep discharges ...
High float voltage ...
High discharge rates ...
High charge rates ...
Anything that produces heat, is damaging!

Also, interesting to consider ...
As capacity decreases, charge and discharge rates should be likewise reduced.
In other words, the C rate should be based on actual capacity rather than original rated capacity.
This is why batteries begin to deteriorate at an accelerated rate.
If retasked to low drain applications, while cells are still of reasonably capacity, they might enjoy a fruitful ... retirement ...

Power backup-emergency power - with inverter
Lights, many power tools etc., run well on 120V DC
A camp florescent or LED lantern
Part of a laarrge pack for mobility scooter or trike
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - December 2019

EBike Toolbox - Bargains! $

Endless Sphere Wiki - Lost?

User avatar
DrkAngel   100 GW

100 GW
Posts: 5277
Joined: Dec 15 2010 11:14am
Location: Upstate-Western-Southern Tier NY. USA

Re: Homemade Battery Packs

Post by DrkAngel » Nov 03 2013 12:00pm

Building 2 packs for Winter
For the first time I will be building 9s 33.3V packs.
I have 2 eZips with compatible controllers.
1st 2008 Moutain Trailz converted to 36V controller and rigged for winter, studded tires etc.
2nd is my 2009 Trailz LS which is 22.2V - 37V+ capable.
Packs will be as large as possible to offset cold effects.

Lipo - recycled laptop cells
I plan on using a minimum of 21 6-packs of 2160mAh cells.
9s14p for 11.1V 30.24Ah = 1.007kWh
I'm hoping to stuff into a 6 pack insulated cooler.
Ideally, pack will be mounted between suspension fork and handlebars and run wire back to controller.
Capacity mapping indicates optimal voltages above 3.75V and about 4.15V peak charge.
(My previous build using these brand cells, at 4.20V charge, provided 2 years - 5000+ miles of acceptable use.)
However, I intend on limiting charge to 4.05V, although this neglects a large capacity bulge, it will, reputably, more than double the usable life. (Will take several years to confirm!)

Image

Li-ion - 18650 recycled laptop cells
Careful planning will allow me to squeeze 9s12p into an oem eZip RMB battery shell.
9s12p = 108 2600mAh cells = 33.3V 31.2Ah = 1.038kWh.

About 8 months ago I bulk charged my entire supply of cells and used the B rated cells for my 22.2V and 29.6V builds.
Longevity was disappointing, so peak charge voltage will be lowered to prolong useful lifespan.
Optimal charge voltage, for these Sanyo cells looks to be 4.05V.
I just checked the residual voltage on the remaining cells and selected 150+ that, after setting for 8 months, still retain 4.05V or higher.
1. I will equalize all cells to 4.10V.
2. I will use my bulk capacity test method to rate all cells.
3. Best 108 cells will be selected and arranged into 9 banks of equal mAh capacity.
Capacity mapping recommends limiting charge to 4.05V and discharge to above 3.7V.
Hopefully limiting these voltages will greatly prolong usable life.
I will be able to compare directly with this years previous builds, (same batch Sanyo cells).

Image

Standardizing at 4.05V per cell will allow 1 charger for the Winter.
1 MeanWell S-350-48 modified to bulk charge at 36.35V 9.5A. (< .3C charging rate recommended ... by me.)
(I never found a bargain price for 36V S series MeanWell)
MeanWell S-350-48 mods will be documented on the ES Wiki.

S-150-XX mods are well documented or being updated in stages.
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - December 2019

EBike Toolbox - Bargains! $

Endless Sphere Wiki - Lost?

User avatar
Toorbough ULL-Zeveigh   100 MW

100 MW
Posts: 2566
Joined: Feb 09 2007 3:02am
Location: Marlboro

Re: Homemade Battery Packs

Post by Toorbough ULL-Zeveigh » Nov 03 2013 1:52pm

DrkAngel wrote:Will take several years to confirm!
no it won't.
calendar life doesn't change.
Kick down the barricades Listen what the kids say.
From time to time people change their minds But the Frock is here to stay.
I've seen it all from the bottom to the top Everywhere I go the kids wanna Frock.
Around the world or around the block Everywhere I go the kids wanna Frock.

User avatar
DrkAngel   100 GW

100 GW
Posts: 5277
Joined: Dec 15 2010 11:14am
Location: Upstate-Western-Southern Tier NY. USA

Re: Homemade Battery Packs

Post by DrkAngel » Nov 03 2013 2:50pm

Recycled Lipo charged to 4.20V per cell, were previously documented at 2 year 6000 mile usability.
Multiple reputable sources insist that lowering charge voltage from 4.20V to 4.10V will double the number of usable cycles ... at a mere 10% capacity sacrifice.
Lowering voltage to 4.05V should increase usable cycles to 250-300%.
Usable capacity from the 4.05V might exceed the usable capacity of the 4.20V pack before the 1st year of use ends.
Previous 2 year usable life might extend into 5-6 years and previous 6000 mile total might exceed 12-15 thousand miles.

Since my previous charges were typically partial, rather than full depth, my use shouldn't suffer at all.
Instead of the previous ~500 cycles, ~1500 seems viable.

These cells vary in age, but even some dated 2004 still measured at better than 90% of oem rated capacity!
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - December 2019

EBike Toolbox - Bargains! $

Endless Sphere Wiki - Lost?

IBScootn   100 W

100 W
Posts: 212
Joined: Jan 30 2012 11:47pm
Location: Colorado, USA

Re: Homemade Battery Packs

Post by IBScootn » Nov 03 2013 6:45pm

Bump
Motorcycles:
ZEV T7100, 84V, 60AH, 65+mph; Mods: TNC throttle, windshield, Cycle Analyst , Cell Log , and custom charger
Kymco GT300i - for long rides through the Rocky Mountains
Big EV Grin. :)

e-beach   1 GW

1 GW
Posts: 3215
Joined: Jan 10 2012 9:48pm
Location: Any Los Angeles area beach I am at. Or Santa Monica or possibly the south bay beaches.

Re: Homemade Battery Packs

Post by e-beach » Nov 03 2013 8:34pm

A question on your experience with recycled 18650 batteries...

I recently bought 49 dell laptop battery packs in 2 lots. One lot was 27 packs and the other 22 packs. The total price was just under $70 USA for all the packs.

I have yet to fully count the total number of batteries but it's about 325 used 18650's. Mostly Samsung 2.600 amp hour cells but also Sony's LG's and others I have yet to identify.

Right now, I have them separated into 3 groups.
A: Those that are above 3.25 volts,
B: Those that are 3.24 to 2 volts
C: and those that are 1.99 to zero volts.....I have about 113 of these.

At this point my question is what should I do with the 113or so that are 1.99 to 0 volts. They may be the dangerous ones and I am wondering if they are worth trying to revive with a slow charge to see if any are salvageable.

From your experience is it worth trying to salvage low voltage cells?

Thanks!

:D
Favorite Quote: "This is L.A., sugar. There is no 'over the top." --- Chris Erskine

Current build: Liahona w/ cheap front suspension and suspension seat post. Yescomusa 36v 800w generic front hub motor. 15ah Headway triangle mounted pack. Tronsung 30 amp,

Previous Build:1992 Trek Antelope 800 - Bone Crusher (no suspension) - Yescomusa 800 watt 36 volt front wheel kit. Don't do it! Get suspension!!!

User avatar
DrkAngel   100 GW

100 GW
Posts: 5277
Joined: Dec 15 2010 11:14am
Location: Upstate-Western-Southern Tier NY. USA

Re: Homemade Battery Packs

Post by DrkAngel » Nov 04 2013 2:28am

e-beach wrote:A question on your experience with recycled 18650 batteries...


At this point my question is what should I do with the 113or so that are 1.99 to 0 volts. They may be the dangerous ones and I am wondering if they are worth trying to revive with a slow charge to see if any are salvageable.

From your experience is it worth trying to salvage low voltage cells?

Thanks!

:D
Want to play it safe?
Apply a 3.5V charge (or lower, 3.25V?) to each cell.
Cell voltage will climb to that point very quickly ... or it won't.

Check for heat during charge.
Check for voltage loss or heat a few minutes after charge removed (self-discharge)
Eliminate any that fail.

If cells retain fair voltage after 1 hour, save for full charge and test.

Method should eliminate "unsafe" cells.
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - December 2019

EBike Toolbox - Bargains! $

Endless Sphere Wiki - Lost?

User avatar
Toorbough ULL-Zeveigh   100 MW

100 MW
Posts: 2566
Joined: Feb 09 2007 3:02am
Location: Marlboro

Re: Homemade Battery Packs

Post by Toorbough ULL-Zeveigh » Nov 04 2013 3:50am

DrkAngel wrote:some dated 2004 still measured at better than 90% of oem rated capacity!
define 'some'!

some people live past a hundred!
what does that tell you about your chances?!!
DrkAngel wrote:Previous 2 year usable life might extend into 5-6 years and previous 6000 mile total might exceed 12-15 thousand miles.
increase cycle life, yes!
calendar life, no!

Battery performance deteriorates over time whether the battery is used or not. This is known as "calendar fade". Performance allso deteriorates with usage and this is known as "cycle fade"
http://www.mpoweruk.com/life.htm

After one year on the shelf, a LiFePO4 cell typically has approximately the same energy density as a LiCoO2 Li-ion cell, because of LFP's slower decline of energy density. Thereafter, LiFePO4 likely has a higher density.
http://en.wikipedia.org/wiki/Lithium_ir ... te_battery
Attachments
MSA-calendar.pdf
!!!!!!!!!!!!!1!
(219.42 KiB) Downloaded 165 times
Kick down the barricades Listen what the kids say.
From time to time people change their minds But the Frock is here to stay.
I've seen it all from the bottom to the top Everywhere I go the kids wanna Frock.
Around the world or around the block Everywhere I go the kids wanna Frock.

cwah   10 GW

10 GW
Posts: 4214
Joined: Jul 24 2011 5:42am
Location: Between paris and london

Re: Homemade Battery Packs

Post by cwah » Nov 04 2013 4:38am

What's the difference between a float voltage and open voltage?
Help me find my stolen electric brompton: http://bit.ly/1a0vbBC and Bosch Sinus B3 http://bit.ly/1eV0WQz

Post Reply