RC Lipo pack inspection, series/parallel charging, and lifespan/safety tips
-
- Posts: 585
- Joined: May 31 2015 3:45pm
- Location: Sydney Australia, Me: 70kg/154lb. 350w, 22kg ex battery, 24 speed axial mid-drive Bofeili MTB.
Re: RC Lipo series charging tutorial
Ha. You thought you were rid of me.
I am not quite there?
discussion on lipo all seems about hardcore fussing about with RC sub paks that have to be laboriously and meticulously charged and balanced. Its not for those who have a life. Perhaps i have been misled. Hi drain also has limited appeal for ebikes, as per the goldenmotors link below.
I didnt know lipo came in pouch cell form.
i wasnt aware, & nobody explained, & i got the impression, nobody used
further, the chinese seem to make it a major puzzle finding out what exactly is in a pak; wrong/ambiguous terms (lipo/polymer/li-ion,cannister/pouch/bms/c-rate,,...???), vague, ...
eg.:
http://gebattery.en.alibaba.com/product ... _cell.html
"Product Description:
Dimensions: 8.7*150*180mm
Nominal capacity:20Ah
Nominal voltage:3.7V
Operation Voltage:(Charge)3.9V,(Discharge)2.5V
Charging ways:Constant-current/constant voltage
Max Charge Current:≤1CA
Max Discharge Current:(Constant Current)≤100A,(Impulse Current):≤400A
Standard Charge/Discharge Current:0.3 CA
Cycle Life:( 80DOD%)≥500Times
Operating Temperature:(Charge)0°C~45°C, (Discharge)-25°C~60°C
Self-discharge Rate:≤3%(Monthly)
Weight:less than 400g"
i like general rules of thumb, so the above means; a 36v 20ah, 5c (am happy with 2-3c, but 5c is good so its not straining) discharge using 10 x 3.7v nominal?? cells at 400g ea. for a total of 4kg for 20ah, or ~100amp (3.6kw) burst.
AND BMS
that is pretty awesome.
500 cycles - meh. hang the expense, tho i hear these numbers are optimistic.
A similar lipo pouch cell
http://gebattery.en.alibaba.com/product ... _3_7V.html
an example of a similar finished product:
http://www.alibaba.com/product-detail/F ... 0.0.Wfi9uF
So, is this as convenient as a bottle battery - is recharge as safe and simple? Whats the catch?
seeking wisdom on this. pls help?
incidentally, gary salo of goldenmotor expresses similar views to mine about lifepo4, but better:
http://www.goldenmotor.ca/news/184/LiFe ... M-ION.html
NB, yes, a 12x cell 36v lifepo4 is heavier than a 10 cell lipo 36v pak, but they are a very steady 38.4v vs 37v diminishing?.
OTH
am thinking, if the 15ah lifepo4 is too big and heavy, maybe its my estimate is the problem. Get a sturdy lifepo4, but smaller.
an hour and a half is all i want to be in the saddle, and am thinking 250w ph average use, a generous allowance w/o no pedaling on my mid-drive, - 25-30kph, with 500w on tap if needed.
10ah lifepo4 does that at a liveable ~3.5kg, tho 12ah (~4.2kg) seems sound for some wiggle room as it ages.
Pouch brands seem a well kept secret by pak makers. What gives? Ought one be wary?
all the fakes and lies of 18650s seem absent in the pouch world.
i have heard of crap quality tabs to work on, but not poor function or fraud or mislableing?
any advice?
ta in advance
I am not quite there?
discussion on lipo all seems about hardcore fussing about with RC sub paks that have to be laboriously and meticulously charged and balanced. Its not for those who have a life. Perhaps i have been misled. Hi drain also has limited appeal for ebikes, as per the goldenmotors link below.
I didnt know lipo came in pouch cell form.
i wasnt aware, & nobody explained, & i got the impression, nobody used
further, the chinese seem to make it a major puzzle finding out what exactly is in a pak; wrong/ambiguous terms (lipo/polymer/li-ion,cannister/pouch/bms/c-rate,,...???), vague, ...
eg.:
http://gebattery.en.alibaba.com/product ... _cell.html
"Product Description:
Dimensions: 8.7*150*180mm
Nominal capacity:20Ah
Nominal voltage:3.7V
Operation Voltage:(Charge)3.9V,(Discharge)2.5V
Charging ways:Constant-current/constant voltage
Max Charge Current:≤1CA
Max Discharge Current:(Constant Current)≤100A,(Impulse Current):≤400A
Standard Charge/Discharge Current:0.3 CA
Cycle Life:( 80DOD%)≥500Times
Operating Temperature:(Charge)0°C~45°C, (Discharge)-25°C~60°C
Self-discharge Rate:≤3%(Monthly)
Weight:less than 400g"
i like general rules of thumb, so the above means; a 36v 20ah, 5c (am happy with 2-3c, but 5c is good so its not straining) discharge using 10 x 3.7v nominal?? cells at 400g ea. for a total of 4kg for 20ah, or ~100amp (3.6kw) burst.
AND BMS
that is pretty awesome.
500 cycles - meh. hang the expense, tho i hear these numbers are optimistic.
A similar lipo pouch cell
http://gebattery.en.alibaba.com/product ... _3_7V.html
an example of a similar finished product:
http://www.alibaba.com/product-detail/F ... 0.0.Wfi9uF
So, is this as convenient as a bottle battery - is recharge as safe and simple? Whats the catch?
seeking wisdom on this. pls help?
incidentally, gary salo of goldenmotor expresses similar views to mine about lifepo4, but better:
http://www.goldenmotor.ca/news/184/LiFe ... M-ION.html
NB, yes, a 12x cell 36v lifepo4 is heavier than a 10 cell lipo 36v pak, but they are a very steady 38.4v vs 37v diminishing?.
OTH
am thinking, if the 15ah lifepo4 is too big and heavy, maybe its my estimate is the problem. Get a sturdy lifepo4, but smaller.
an hour and a half is all i want to be in the saddle, and am thinking 250w ph average use, a generous allowance w/o no pedaling on my mid-drive, - 25-30kph, with 500w on tap if needed.
10ah lifepo4 does that at a liveable ~3.5kg, tho 12ah (~4.2kg) seems sound for some wiggle room as it ages.
Pouch brands seem a well kept secret by pak makers. What gives? Ought one be wary?
all the fakes and lies of 18650s seem absent in the pouch world.
i have heard of crap quality tabs to work on, but not poor function or fraud or mislableing?
any advice?
ta in advance
Re: RC Lipo series charging tutorial
Don't know if i am right here
I want to make a 12s 90ah pack out 3x ( 2x30ah) tattu lippo's. How can i balanced charge this as a complete pack......what do I need
What kind of charger and balancer?
Thx


What kind of charger and balancer?
Thx
Re: RC Lipo series charging tutorial
Theres only 2 ways to do it.bionicon wrote:Don't know if i am right hereI want to make a 12s 90ah pack out 3x ( 2x30ah) tattu lippo's. How can i balanced charge this as a complete pack......what do I need
![]()
What kind of charger and balancer?
Thx
1. get a BMS that works for 12s... this makes it easy as the OEM stuff, just feed it a bulk charge.
2. split the pack balance leads into 8s groups or less. You can then monitor everything with RC vehicle tools... you can still bulk charge, but keep an eye on the balance and run it through an RC balancer when needed.
to do #1 you need a BMS and a bulk charger.
to do #2, you need a RC balance charger... but to bulk charge you need a bulk charger and some cheap cellogs or other cell monitor. They're a couple bucks and they let you see the voltages as it charges.
Warning:This post is being read via light, a substance known to the state of California to cause cancer.
Re: RC Lipo series charging tutorial
easy..
Buy a nice high quality 6s charger, use it to weed out the funky packs ( guaranteed you will get shipped at least 1 ), then bulk charge the pack for 99% of it's life. Charge to 4.15v average, discharge to 3.6v average ( or whatever the lowest common denominator is for all packs once you've created the graphs ).
With a little monitoring here and there, you can get away with this.. you just want to cut off the top 5-10% and bottom 5-10% of the pack's capacity. As long as the packs in question remain balanced over lots of cycles, this works.
If they don't remain balanced, you can always break apart the pack and do a balance on the 6S charger when needed.
12S BMS would certainly be a lot nicer though. If you can find one with the appropriate amperage output, that doesn't drain cell #1 and kill your battery early, and has the right voltage cutoffs etc.
Buy a nice high quality 6s charger, use it to weed out the funky packs ( guaranteed you will get shipped at least 1 ), then bulk charge the pack for 99% of it's life. Charge to 4.15v average, discharge to 3.6v average ( or whatever the lowest common denominator is for all packs once you've created the graphs ).
With a little monitoring here and there, you can get away with this.. you just want to cut off the top 5-10% and bottom 5-10% of the pack's capacity. As long as the packs in question remain balanced over lots of cycles, this works.
If they don't remain balanced, you can always break apart the pack and do a balance on the 6S charger when needed.
12S BMS would certainly be a lot nicer though. If you can find one with the appropriate amperage output, that doesn't drain cell #1 and kill your battery early, and has the right voltage cutoffs etc.
"Love and compassion are necessities, not luxuries. Without them, humanity cannot survive." - Dalai Lama
My first major build: 1.6kW 8T MAC motor on a Trek 4500 MTB.
Monster MTB: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: Heavy duty Cannondale semi recumbent - under construction.
Blue Dream: Maxaraya FS semi recumbent and high efficiency mid-drive - under construction.
My first major build: 1.6kW 8T MAC motor on a Trek 4500 MTB.
Monster MTB: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: Heavy duty Cannondale semi recumbent - under construction.
Blue Dream: Maxaraya FS semi recumbent and high efficiency mid-drive - under construction.
Re: RC Lipo series charging tutorial
....euh did a quick search and did not found a 12s bms that has a continue discharge of 350 amps. My battery's are 3X2 30000mah with 25C continue ...so 90X 25 =2250 AMPS continue!(tell me if i am wrong)
So can I use the bms just to charge the pack? And to discharge disconnect the bms?
So can I use the bms just to charge the pack? And to discharge disconnect the bms?
Re: RC Lipo series charging tutorial
You don't even have to disconnect the bms to bypass it for discharge. Just use a separate main ground wire for the discharge and leave the bms connected all the time if you want to. But yes, you could just unplug the bms if you designed it that way.
Need Advice? https://endless-sphere.com/forums/viewt ... =3&t=66302
Mongoose 26" Ledge 2.1 mtb bike $99, yescomusa.com 48V 1000W rear hub kit $200, Hua Tong 72V 40A controller $35, 10ah 24s lipo $217=~43mph, range=45 miles @ 20mph. 25K miles and still going strong.
Huffy Fortress 3.0 with MXUS 3000 4T motor, 24s lipo, 96V 60A controller. Total cost with extras <$700. Top speed ~50mph
My videos https://www.youtube.com/channel/UC0KW4U ... _G2wQhptMg
Mongoose 26" Ledge 2.1 mtb bike $99, yescomusa.com 48V 1000W rear hub kit $200, Hua Tong 72V 40A controller $35, 10ah 24s lipo $217=~43mph, range=45 miles @ 20mph. 25K miles and still going strong.
Huffy Fortress 3.0 with MXUS 3000 4T motor, 24s lipo, 96V 60A controller. Total cost with extras <$700. Top speed ~50mph
My videos https://www.youtube.com/channel/UC0KW4U ... _G2wQhptMg
Re: RC Lipo series charging tutorial
If you do that, the BMS will not cut off when a cell goes too low though.
Which is one of the main things you wire up a BMS for, ya know.
Which is one of the main things you wire up a BMS for, ya know.

"Love and compassion are necessities, not luxuries. Without them, humanity cannot survive." - Dalai Lama
My first major build: 1.6kW 8T MAC motor on a Trek 4500 MTB.
Monster MTB: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: Heavy duty Cannondale semi recumbent - under construction.
Blue Dream: Maxaraya FS semi recumbent and high efficiency mid-drive - under construction.
My first major build: 1.6kW 8T MAC motor on a Trek 4500 MTB.
Monster MTB: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: Heavy duty Cannondale semi recumbent - under construction.
Blue Dream: Maxaraya FS semi recumbent and high efficiency mid-drive - under construction.
Re: RC Lipo series charging tutorial
and if i will use regenerative braking.....wihout bms? Will that work?
Re: RC Lipo series charging tutorial
of course.bionicon wrote:and if i will use regenerative braking.....wihout bms? Will that work?
Just dont fully charge it at the top of the mountain and regen brake the entire way down.
Warning:This post is being read via light, a substance known to the state of California to cause cancer.
Re: RC Lipo series charging tutorial
MrDude_1 wrote:of course.bionicon wrote:and if i will use regenerative braking.....wihout bms? Will that work?
Just dont fully charge it at the top of the mountain and regen brake the entire way down.

-
- Posts: 2
- Joined: Dec 23 2016 9:34pm
Re: RC Lipo series charging tutorial
Hi, I'm planning my first ebike. I have a 26 in steel frame bike and I'm thinking of a 350-500w front hub. My commute is a flat 5 miles. I have years of flying rc planes with lipos. These batteries from hk seem like a good fit:
https://hobbyking.com/en_us/multistar-h ... -pack.html
Huge capacity, light weight and a screaming deal. They are 10C, which is really low compared to my airplane lipos, but at 10Ah should be capable of 100 amps. The bike load should be more like 10 amps or only 1C, right?
https://hobbyking.com/en_us/multistar-h ... -pack.html
Huge capacity, light weight and a screaming deal. They are 10C, which is really low compared to my airplane lipos, but at 10Ah should be capable of 100 amps. The bike load should be more like 10 amps or only 1C, right?
Re: RC Lipo series charging tutorial
3qty of those series wired for 12S1P would be a nice voltage for majority 48V systems. 500W @ 48V would be about 10A, plenty of headroom for those packs.Dylancoffin wrote:Hi, I'm planning my first ebike. I have a 26 in steel frame bike and I'm thinking of a 350-500w front hub. My commute is a flat 5 miles. I have years of flying rc planes with lipos. These batteries from hk seem like a good fit:
https://hobbyking.com/en_us/multistar-h ... -pack.html
Huge capacity, light weight and a screaming deal. They are 10C, which is really low compared to my airplane lipos, but at 10Ah should be capable of 100 amps. The bike load should be more like 10 amps or only 1C, right?
$/Wh is a very good deal although you may have to install different connectors or hardwired to series them. Have you checked prices on 6S packs? if similar price that would require one less series connection.
Talent must not be wasted.... Those who have talent must hug it, embrace it, nurture it and share it lest it be taken away from you as fast as it was loaned to you.
- Frank Sinatra
- Frank Sinatra
-
- Posts: 2
- Joined: Dec 23 2016 9:34pm
Re: RC Lipo series charging tutorial
Thanks Ykick. The 4s 10 Ah are $37 and the 6S are $90. I don't know why the 4S are so cheap. Maybe they made a bunch. My experience with Turnegy batteries has been problem free, although I've never used these 10C packs. I like the XT connectors. It would be easy to make up a series connector.
Re: RC Lipo series charging tutorial
Pricing is just one of those HK mysteries. When they wanna move stuff they price it to move.
I believe these 10C packs are intended for AP multi-rotors? Slow and steady with long flight times but well within modest eBike needs.
I like XT’s and use them for all my aircraft but for series wiring packs 4mm Bullets have spoiled me. I’ve been using 4S Turnigy Hardcase with bullets for several years on my bikes. That was before these MS (multi star) packs became more prevalent.
I believe these 10C packs are intended for AP multi-rotors? Slow and steady with long flight times but well within modest eBike needs.
I like XT’s and use them for all my aircraft but for series wiring packs 4mm Bullets have spoiled me. I’ve been using 4S Turnigy Hardcase with bullets for several years on my bikes. That was before these MS (multi star) packs became more prevalent.
Talent must not be wasted.... Those who have talent must hug it, embrace it, nurture it and share it lest it be taken away from you as fast as it was loaned to you.
- Frank Sinatra
- Frank Sinatra
Re: RC Lipo series charging tutorial
I was measuring internal resistance in some packs I just bought. I believe that's measured in micro-ohms?
One cell was showing 3x the resistance of all other cells. I remeasured, and it's consistently off. I'm getting .001 in the other 63 cells, but .003 in that one cell.
Is that measurement meaningful enough that I should use that pack for "utility purposes" or spare cells, is it something I should be returning as faulty, or is it truly no big deal at all?
One cell was showing 3x the resistance of all other cells. I remeasured, and it's consistently off. I'm getting .001 in the other 63 cells, but .003 in that one cell.
Is that measurement meaningful enough that I should use that pack for "utility purposes" or spare cells, is it something I should be returning as faulty, or is it truly no big deal at all?
Re: RC Lipo series charging tutorial
The 4s hardcase are so cheap because HUGE numbers of RC racers buy them. The non-hardpack ones are the same, except for the shrinkwrap instead of the case.. so the huge volume lets them be cheaper.Dylancoffin wrote:Thanks Ykick. The 4s 10 Ah are $37 and the 6S are $90. I don't know why the 4S are so cheap. Maybe they made a bunch. My experience with Turnegy batteries has been problem free, although I've never used these 10C packs. I like the XT connectors. It would be easy to make up a series connector.
Warning:This post is being read via light, a substance known to the state of California to cause cancer.
Re: RC Lipo series charging tutorial
So what charger out there now does 14S Lipo packs and balances at the same time?
Re: RC Lipo series charging tutorial
thunder power, adapttoCobraJet wrote:So what charger out there now does 14S Lipo packs and balances at the same time?
Re: RC Lipo series charging tutorial
Please school me on why I can charge my 4S lipos more after they have been balanced charged to "Full"
45a charger charging 6x turnigy 4S 5000mah 25C batteries in parallel.(30ah total charging them at .5C) Charger completes says they are full. But if I hit stop and start again they will take another 3-4000ah. Is this normal? An issue with my charger?
Charger:EV-Peak C6 High Power LiPo/LiHV DC Battery Charger (6S/45A/1140W
Full build thread: viewtopic.php?f=34&t=91687

45a charger charging 6x turnigy 4S 5000mah 25C batteries in parallel.(30ah total charging them at .5C) Charger completes says they are full. But if I hit stop and start again they will take another 3-4000ah. Is this normal? An issue with my charger?
Charger:EV-Peak C6 High Power LiPo/LiHV DC Battery Charger (6S/45A/1140W
Full build thread: viewtopic.php?f=34&t=91687

Re: RC Lipo series charging tutorial
What's the difference in resting voltage for the whole pack between balanced and full?
Maybe 'balanced' means something else to your charger than 'full'.
Important to know these things so that things don't go
on you.
Maybe 'balanced' means something else to your charger than 'full'.
Important to know these things so that things don't go



"Love and compassion are necessities, not luxuries. Without them, humanity cannot survive." - Dalai Lama
My first major build: 1.6kW 8T MAC motor on a Trek 4500 MTB.
Monster MTB: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: Heavy duty Cannondale semi recumbent - under construction.
Blue Dream: Maxaraya FS semi recumbent and high efficiency mid-drive - under construction.
My first major build: 1.6kW 8T MAC motor on a Trek 4500 MTB.
Monster MTB: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: Heavy duty Cannondale semi recumbent - under construction.
Blue Dream: Maxaraya FS semi recumbent and high efficiency mid-drive - under construction.
Re: RC Lipo pack inspection, series/parallel charging, and lifespan/safety tips
My neighbor bought some Lipo off eBay. They won’t charge and in balance mode they show 1.3xV per cell 3s1p.
Trash battery?
Trash battery?
Thanks Justin_le we're here thanks to you. All the best to the mods for their tireless work keeping it on an even keel.
- amberwolf 100 GW
- Posts: 32148
- Joined: Aug 17 2009 6:43am
- Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
- Contact:
Re: RC Lipo pack inspection, series/parallel charging, and lifespan/safety tips
Below 2v I wouldn't use them, myself.
If you found this advice helpful, supporting contributions are accepted here.
"if it ain't broke, improve it till it is"----Dog-Hauler Cargo eTrike SB Cruiser----The HI-Lebowski: a Lebowski SMD brain running a zombified Honda IMA Inverter: a HOW-TO guide----Cargo eBike CrazyBike2----General Blog
"if it ain't broke, improve it till it is"----Dog-Hauler Cargo eTrike SB Cruiser----The HI-Lebowski: a Lebowski SMD brain running a zombified Honda IMA Inverter: a HOW-TO guide----Cargo eBike CrazyBike2----General Blog
Re: RC Lipo pack inspection, series/parallel charging, and lifespan/safety tips
Thanks. That’s what I thought I learned here but have zero experience. I wanted to hear a repeat of what I surmised was the best advice. A shame. The fella paid more than double the hobbyking price on eBay, and made modifications before ever testing/metering the packs. A sad lesson.
Thanks for confirming.
Thanks Justin_le we're here thanks to you. All the best to the mods for their tireless work keeping it on an even keel.