Post by kiwipete » Mar 30 2014 6:50pm

I looking to make one of these no solder/weld battery packs using some Sony US18650VTC4's which I have ordered and are on the way and have been looking around for the bits to make it.

I have problems sourcing the Poron urethane blanket. (I'm in New Zealand). Would neoprene rubber strip work as a substitute?

snath   100 W

100 W
Posts: 126
Joined: Jan 04 2010 6:01pm
Location: Colorado, USA

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by snath » Mar 30 2014 8:19pm

I'm not sure. This is the place where I got mine and they have a pretty good informative section on foams here:
http://www.mcmaster.com/#poron-urethane-foam/=rbq659

This is the stuff that I got from them:
http://www.mcmaster.com/#poron-urethane-foam/=rbq610

Part Number 86375K132

Good luck.

Gregb   100 W

100 W
Posts: 185
Joined: Apr 28 2010 6:59pm
Location: Canberra Australia

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by Gregb » Mar 30 2014 8:51pm

kiwipete wrote:I looking to make one of these no solder/weld battery packs using some Sony US18650VTC4's which I have ordered and are on the way and have been looking around for the bits to make it.

I have problems sourcing the Poron urethane blanket. (I'm in New Zealand). Would neoprene rubber strip work as a substitute?
I haven't tried it but I think the closed cell foem used in building footings would work. It comes in rolls. try you nearest builder supplier to have a look at it. You have Bunnings over there? they sell it.

User avatar
liveforphysics   100 GW

100 GW
Posts: 14134
Joined: Oct 29 2008 1:48am
Location: Santa Cruz, CA, USA

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by liveforphysics » Mar 30 2014 9:16pm

One would be best off not guessing with a foam they think will or will not have safe levels of compression-set.


Get the relevant compression-set % data. Ensure you crush it by more than that amount if you want it to keep your cells connected long-term.

It is not hard to do this, but you can't ensure your success by going of hunches or assumptions on materials choice, or it could result in fire.

It is 100% impossible to squeeze a chunk of foam between your fingers and know ANYTHING related to it's compression-set behavior will be after it's been in squeezed in your battery for a few months.

Simply checking material property datasheets are really the difference between a long-lasting great pack and a potential home fire, spend the effort to use proper materials.
Each carcinogen vapor exposure includes a dice roll for cancer.

Each mutagen vapor exposure includes a dice roll for reproductive genetic defects in your children.

Each engine start sprays them into a shared atmosphere which includes beings not offered an opportunity to consent accepting these cancer experiences and defective genetics life experiences.

Every post is a free gift to the collective of minds composing the living bleeding edge of LEV development on our spaceship.

kiwipete   100 mW

100 mW
Posts: 45
Joined: Nov 13 2013 9:40pm

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by kiwipete » Mar 31 2014 4:51pm

liveforphysics wrote:One would be best off not guessing with a foam they think will or will not have safe levels of compression-set.
Get the relevant compression-set % data. Ensure you crush it by more than that amount if you want it to keep your cells connected long-term.
Simply checking material property datasheets are really the difference between a long-lasting great pack and a potential home fire, spend the effort to use proper materials.
I totally agree with you lfp, but none of the NZ based suppliers have any data sheets listing compression set on their websites, and the ones I contacted via phone were unable to provide solid info re compression set either.

I have considered buying the same stuff that 'snath' used and contacted McMaster-Carr via email about purchasing some and shipping to New Zealand. Their reply was quick but extremely unhelpful:

"Due to the complexity of U.S. export regulations, McMaster-Carr accepts international orders only from our established customers. This decision also applies to orders shipping within the United States, because it is based on the final destination of the items. We will not provide a quotation or accept your orders."

So much for that...

The foam itself is not that expensive ($6.60 for a 12" x 12" sheet) and I imagine that if it was folded or cut to fit a big size envelope, mailing it would not be too horrendous either.So if there is a kind ES (US based) member who is willing to help out here, please PM me. I'll pay all costs upfront (Paypal would be easiest).

User avatar
Bronko   1 W

1 W
Posts: 61
Joined: Jul 16 2012 12:06pm
Location: Austin Tx

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by Bronko » Mar 31 2014 6:18pm

Masterful job sir. Is there any advantage for using the multi pin connector instead of say an XLR for the charge connector?

snath   100 W

100 W
Posts: 126
Joined: Jan 04 2010 6:01pm
Location: Colorado, USA

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by snath » Mar 31 2014 6:35pm

Bronko wrote: Is there any advantage for using the multi pin connector instead of say an XLR for the charge connector?
I use 11 of the pins on the DB 15 connector to hook up to a mating DB to JST XH connector that goes to the Balance port on my charger. I suppose you could use an XLR-type connector but I'm not sure if you can get one with enough pins. I'm about 100% sure it wouldn't fit in the space that a DB connector takes up. Finally, the DB 15 is what I had on hand :)

User avatar
Bronko   1 W

1 W
Posts: 61
Joined: Jul 16 2012 12:06pm
Location: Austin Tx

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by Bronko » Apr 06 2014 11:08am

I agree that a video time lapse on this build would be awesome.

snath   100 W

100 W
Posts: 126
Joined: Jan 04 2010 6:01pm
Location: Colorado, USA

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by snath » Apr 06 2014 8:30pm

Bronko wrote:I agree that a video time lapse on this build would be awesome.
I'm pretty much a "technological Luddite" when it comes to that sort of thing. But if you look at the pictures, it's all there. Once you make the die block to make the dimples and fit them up to the spacer blocks, it becomes easier to visualize.

snath   100 W

100 W
Posts: 126
Joined: Jan 04 2010 6:01pm
Location: Colorado, USA

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by snath » Apr 06 2014 8:33pm

snath wrote:
Bronko wrote:I agree that a video time lapse on this build would be awesome.
I'm pretty much a "technological Luddite" when it comes to that sort of thing. But if you look at the pictures, it's all there. Once you make the die block to make the dimples and fit them up to the spacer blocks, it becomes easier to visualize.
I'm about to make a couple of 10s4p packs so Ill try to throw up a few more pictures of the steps/process. Is there anything in particular(steps/process) that you are interested in?

User avatar
liveforphysics   100 GW

100 GW
Posts: 14134
Joined: Oct 29 2008 1:48am
Location: Santa Cruz, CA, USA

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by liveforphysics » Apr 07 2014 12:23am

kiwipete wrote:
liveforphysics wrote:One would be best off not guessing with a foam they think will or will not have safe levels of compression-set.
Get the relevant compression-set % data. Ensure you crush it by more than that amount if you want it to keep your cells connected long-term.
Simply checking material property datasheets are really the difference between a long-lasting great pack and a potential home fire, spend the effort to use proper materials.
I totally agree with you lfp, but none of the NZ based suppliers have any data sheets listing compression set on their websites, and the ones I contacted via phone were unable to provide solid info re compression set either.

I have considered buying the same stuff that 'snath' used and contacted McMaster-Carr via email about purchasing some and shipping to New Zealand. Their reply was quick but extremely unhelpful:

"Due to the complexity of U.S. export regulations, McMaster-Carr accepts international orders only from our established customers. This decision also applies to orders shipping within the United States, because it is based on the final destination of the items. We will not provide a quotation or accept your orders."

So much for that...

The foam itself is not that expensive ($6.60 for a 12" x 12" sheet) and I imagine that if it was folded or cut to fit a big size envelope, mailing it would not be too horrendous either.So if there is a kind ES (US based) member who is willing to help out here, please PM me. I'll pay all costs upfront (Paypal would be easiest).


Ebay or whatever you have to get proper material for the foam. This battery is so tolerant of substitutions on all other materials, but the foam must be right for success.
Each carcinogen vapor exposure includes a dice roll for cancer.

Each mutagen vapor exposure includes a dice roll for reproductive genetic defects in your children.

Each engine start sprays them into a shared atmosphere which includes beings not offered an opportunity to consent accepting these cancer experiences and defective genetics life experiences.

Every post is a free gift to the collective of minds composing the living bleeding edge of LEV development on our spaceship.

kiwipete   100 mW

100 mW
Posts: 45
Joined: Nov 13 2013 9:40pm

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by kiwipete » Apr 07 2014 1:06am

liveforphysics wrote: Ebay or whatever you have to get proper material for the foam. This battery is so tolerant of substitutions on all other materials, but the foam must be right for success.
I found out since then that the NZ Post office has a service for cases like this. You get the company to send it to an NZ Post run office/warehouse in the US and they then onsend it to NZ.

Shipping cost are pretty painful ($5 (US) from McMaster Carr to Portland OR and then NZD$31.50 to go to NZ), but at least I can get the right stuff. Now just waiting for the batteries..

Pat Eaton   10 W

10 W
Posts: 65
Joined: Aug 31 2009 9:12pm
Location: Abbotsford, British Columbia

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by Pat Eaton » Apr 07 2014 7:51pm

How much of a contact patch do you expect between the bus and battery?

I am experimenting with forming bus bars with the required dimples. I drilled a hole in some steel and have been using a steel rod with a rounded end (hammered) to create the dimples.

I have been able to make them all the same depth, but the shape is not always consistent.

Thanks for any reply.

Dark Knight   100 W

100 W
Posts: 166
Joined: May 10 2013 1:13am
Location: Perth, Western Australia

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by Dark Knight » Apr 07 2014 8:44pm

Was looking for a way to make a small 4s4p battery out of 18650 cells (small I know) - this solution is perfect - thanks so much <pats Snath on the back>.
As always, continue to be amazed by the ingenuity and innovation of the ES members...it seems whenever I encounter a problem, there is already a multitude of solutions to hand!
Now, time to see if I can source most of the materials (or appropriate substitutes) locally...don't worry LFP, I'll ensure the right compression material is used!

User avatar
liveforphysics   100 GW

100 GW
Posts: 14134
Joined: Oct 29 2008 1:48am
Location: Santa Cruz, CA, USA

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by liveforphysics » Apr 07 2014 9:15pm

Pat Eaton wrote:How much of a contact patch do you expect between the bus and battery?

I am experimenting with forming bus bars with the required dimples. I drilled a hole in some steel and have been using a steel rod with a rounded end (hammered) to create the dimples.

I have been able to make them all the same depth, but the shape is not always consistent.

Thanks for any reply.

I suppose to answer that one would need to know the expected current delivery capabilities of the cell you're running in short circuit.

If you just want a rule of thumb though, I would try to target at least a 4mm^2 flat contact area.

Does anyone want to make the compound #70 silicone gel polymer and graphene dielectric grease? I doubt too many people would want to spend the few hundred bucks to make the lowest quantity batch. I am personally interested in testing the stuff out because I've heard talk of some seemingly impossible contact resistance numbers. I would assume 1-2mg/cell would be enough if you design your cell contact dimple well and get it decently flat with a fine-stone or something. I have the equipment to blend up a batch if I bought the raw materials. and transfer it into perhaps 0.5cc-1cc syringes with blunt needle tips for applying if anyone would be interested. It would obviously be at least >100x the cost per unit of volume of any non-nano-conductor based dielectric grease, but since so little could do so many cells, it would be perhaps a few cents per cell to potentially get conductivity I've heard claimed as better than many welding processes.
Each carcinogen vapor exposure includes a dice roll for cancer.

Each mutagen vapor exposure includes a dice roll for reproductive genetic defects in your children.

Each engine start sprays them into a shared atmosphere which includes beings not offered an opportunity to consent accepting these cancer experiences and defective genetics life experiences.

Every post is a free gift to the collective of minds composing the living bleeding edge of LEV development on our spaceship.

snath   100 W

100 W
Posts: 126
Joined: Jan 04 2010 6:01pm
Location: Colorado, USA

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by snath » Apr 07 2014 9:35pm

Pat Eaton wrote:How much of a contact patch do you expect between the bus and battery?

I am experimenting with forming bus bars with the required dimples. I drilled a hole in some steel and have been using a steel rod with a rounded end (hammered) to create the dimples.

I have been able to make them all the same depth, but the shape is not always consistent.

Thanks for any reply.
If you will take a look at my dimpling punch, you'll notice that it is flat on the end; resulting in flat dimples. I made it out of a 3/16 high speed tool bit and barely knocked off the corner to keep it from cutting the copper. The resulting dimple is about 17 sq mm.

Pat Eaton   10 W

10 W
Posts: 65
Joined: Aug 31 2009 9:12pm
Location: Abbotsford, British Columbia

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by Pat Eaton » Apr 07 2014 9:44pm

Thanks Snath, I have a better understanding of the jig you made.

snath   100 W

100 W
Posts: 126
Joined: Jan 04 2010 6:01pm
Location: Colorado, USA

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by snath » Apr 07 2014 9:48pm

liveforphysics wrote:
Pat Eaton wrote:How much of a contact patch do you expect between the bus and battery?

I am experimenting with forming bus bars with the required dimples. I drilled a hole in some steel and have been using a steel rod with a rounded end (hammered) to create the dimples.

I have been able to make them all the same depth, but the shape is not always consistent.

Thanks for any reply.

I suppose to answer that one would need to know the expected current delivery capabilities of the cell you're running in short circuit.

If you just want a rule of thumb though, I would try to target at least a 4mm^2 flat contact area.

Does anyone want to make the compound #70 silicone gel polymer and graphene dielectric grease? I doubt too many people would want to spend the few hundred bucks to make the lowest quantity batch. I am personally interested in testing the stuff out because I've heard talk of some seemingly impossible contact resistance numbers. I would assume 1-2mg/cell would be enough if you design your cell contact dimple well and get it decently flat with a fine-stone or something. I have the equipment to blend up a batch if I bought the raw materials. and transfer it into perhaps 0.5cc-1cc syringes with blunt needle tips for applying if anyone would be interested. It would obviously be at least >100x the cost per unit of volume of any non-nano-conductor based dielectric grease, but since so little could do so many cells, it would be perhaps a few cents per cell to potentially get conductivity I've heard claimed as better than many welding processes.
I just bought some grease used in automotive electrical service from Big Moose but I would be willing to participate in a batch of the super dielectric grease in the interest of refining this pack building method.

I don't think these dimples need much flattening after they are punched especially if one doesn't cold-work the copper too much with excessive flexing. The copper is flat when it leaves the dimpling block and, if still soft, the dimples are readily pushed flat against the cells by the compressed urethane.

flathill   100 kW

100 kW
Posts: 1273
Joined: Jul 06 2010 9:26pm

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by flathill » Apr 07 2014 10:55pm

Silicone grease isnt recommend if the contact pressure is low but maybe with graphene who knows

Cant wait for vapor desposited graphene on all our electrical contacts including cell terminals but for now



Gold plate the busbar and ur done for now. Anything is better than raw copper for contacts if u care about contact resistance rather than thermal

But how much would you guys pay per gold plated ncr18650pd cell?

User avatar
liveforphysics   100 GW

100 GW
Posts: 14134
Joined: Oct 29 2008 1:48am
Location: Santa Cruz, CA, USA

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by liveforphysics » Apr 07 2014 11:31pm

flathill wrote:Silicone grease isnt recommend if the contact pressure is low but maybe with graphene who knows

Cant wait for vapor desposited graphene on all our electrical contacts including cell terminals but for now



Gold plate the busbar and ur done for now. Anything is better than raw copper for contacts if u care about contact resistance rather than thermal

But how much would you guys pay per gold plated ncr18650pd cell?

I've got a plasma metal sputtering machine in my garage and a gold foil target. :-) I'm not sold on gold over clean copper or silver though, but I agree gold tends to stay clean longest. If cleaned before coated in compound #70, copper can stay pretty nice if you keep it dry.
Each carcinogen vapor exposure includes a dice roll for cancer.

Each mutagen vapor exposure includes a dice roll for reproductive genetic defects in your children.

Each engine start sprays them into a shared atmosphere which includes beings not offered an opportunity to consent accepting these cancer experiences and defective genetics life experiences.

Every post is a free gift to the collective of minds composing the living bleeding edge of LEV development on our spaceship.

snath   100 W

100 W
Posts: 126
Joined: Jan 04 2010 6:01pm
Location: Colorado, USA

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by snath » Apr 07 2014 11:46pm

flathill wrote:Silicone grease isnt recommend if the contact pressure is low but maybe with graphene who knows

Cant wait for vapor desposited graphene on all our electrical contacts including cell terminals but for now



Gold plate the busbar and ur done for now. Anything is better than raw copper for contacts if u care about contact resistance rather than thermal

But how much would you guys pay per gold plated ncr18650pd cell?
Maybe one of these? http://www.caswellplating.com/plug-n-pl ... d-kit.html

I use one for plating silver on to copper findings for flame worked glass pieces my wife makes. It works pretty well but the plating thickness is pretty thin and would probably rub off over time in a pack. Some type of compound would probably work better.

flathill   100 kW

100 kW
Posts: 1273
Joined: Jul 06 2010 9:26pm

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by flathill » Apr 08 2014 12:21am

standard copper nickel coating results an order of magnitude less
contact resistance than clean uncoated 99.99 pure oxgen free copper

if i remember correct

gold porosity is inversely proportional to the thickness for small range starting from zero

or is it the reverse

gold plating would need to be relatively thick to be optimal but even a thin layer would make a huge diff

Gregb   100 W

100 W
Posts: 185
Joined: Apr 28 2010 6:59pm
Location: Canberra Australia

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by Gregb » Apr 08 2014 7:50pm

kiwipete wrote:
liveforphysics wrote: Ebay or whatever you have to get proper material for the foam. This battery is so tolerant of substitutions on all other materials, but the foam must be right for success.
I found out since then that the NZ Post office has a service for cases like this. You get the company to send it to an NZ Post run office/warehouse in the US and they then onsend it to NZ.

Shipping cost are pretty painful ($5 (US) from McMaster Carr to Portland OR and then NZD$31.50 to go to NZ), but at least I can get the right stuff. Now just waiting for the batteries..
Have you had a look at "shipito"?? thsy are a forwarding agency I have used for amazon things. You can choose what service / price they use to send it on. I can't see NZ being any different to Oz.

Pat Eaton   10 W

10 W
Posts: 65
Joined: Aug 31 2009 9:12pm
Location: Abbotsford, British Columbia

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by Pat Eaton » Apr 08 2014 8:18pm

Where will I find the copper for the bus bars? 0.010 is pretty thin. The pieces I have currently (pun intended) are .020.

opz.EST   10 µW

10 µW
Posts: 6
Joined: Oct 14 2009 4:38am

Re: Another No Solder/Weld 18650 Build (Updated 03/09/2014)

Post by opz.EST » Apr 17 2014 6:12am

Awesome idea, great build!
Here is my 2 cents in the picture...
HAND DIMPLING.jpg
Waiting for spacers 12s8p but cannot buy closedcell compressing foam... Can someone send me stripes for my battery in envelope? I am in EU. PM