Hi,

The individual cells are 15AH, which are rated conservatively by GM at 7.8C. They are welded together in 3P 45AH groups, which are welded into 6S and 12S modules. That is a substantial disadvantage because it makes it very difficult to reconfigure the packs.
VoltBlades2.jpg
VoltBlades2.jpg (105.47 KiB) Viewed 18948 times
It looks like the plates on the end might be used to compress the modules?

The module dimensions are 11" high and 9.5" wide. The Volt packs have 7 modules with 12 groups (~48v ) that are 9.2" long and 2 modules with 6 groups (~24v) that are 4.6" long.

There is a thread on the DiyEv car forum with quite a bit of info (prices paid range from $2000 + $150 shipping to $1,3xx picked up locally):
http://www.diyelectriccar.com/forums/sh ... 93101.html
Including some information on separating cell groups and individual cells:
http://www.diyelectriccar.com/forums/sh ... tcount=108
To do the individual cells, get a 26" x 1.75/2.25 bicycle tube. Cut off 1" slices like rubberbands. Put these on all cell welds to insulate.

Get Channellock PN 748, which are long reach cutters:
https://www.channellock.com/product.aspx?zpid=407

Start at one end, and SNIP/SNIP/SNIP/SNIP ... Pull cells out bottom.Pop-rivet cells together with .032/.064 thick .375 wide and 1.75" long copper strips on the outside for support. This will pass at least as much current as the 3 small OEM welds.

However... If you are not careful, you could cut the tabs too short. AND you cannot do 3P 1S this way.
http://www.diyelectriccar.com/forums/sh ... tcount=118
Well, with the right tools, you can take out the cells "as welded" in 3P 1S. It is actually easier than taking out the individual cells and safer. Weight per cell is 1153.0g / 3 with the copper tab left on. There is room to separate the plates for air cooling.
Image
Image
Yabert's tests of Volt packs on the DiyEv car forum suggest a high C rate, 15+ C!:
http://www.diyelectriccar.com/forums/sh ... 09698.html

In this video I show the EV drive drain from a 2013 Chevy Volt that was removed from a wreck with only 7,000 miles. The traction pack is disassembled down to the individual 24V and 48V modules.
Design West Volt Teardown:

Slides from the Design West youtube video can be downloaded here:
https://docs.google.com/file/d/0BwHvhEb ... edit?pli=1

A pdf with a little more info is here (GM rates the cells at 7.8C):
http://endless-sphere.com/forums/downlo ... ?id=142558

ES thread using a Volt pack in a Solectria Force:
http://endless-sphere.com/forums/viewto ... 25#p920925
yopappamon wrote:$1,400 plus $360 freight. Still over a grand cheaper than new lead.
Last edited by MitchJi on Aug 15 2014 1:15pm, edited 15 times in total.
Best Wishes!

Mitch


The best quality batteries and lowest priced batteries for DIY EV's are tier 1 OEM Quality Cells from salvaged (wrecked) EV packs. Three examples are Chevy Volt and Nissan Leaf and Tesla Model 3 packs.

Nissan Leaf Module specs are here
Chevy Volt Pack Info - Salvage 16kwh Packs Under $2k here

User avatar
MitchJi   1 GW

1 GW
Posts: 3204
Joined: Jun 02 2008 8:09pm
Location: Marin County California

Re: Chevy Volt Pack Info - 16kwh Under $2k

Post by MitchJi » Aug 15 2014 10:42am

Volt packs are easy to find now for $1,500-$2k :mrgreen:. There are about 50 now on car-part.com.
http://www.car-part.com/

I searched by distance from my zip code. I found one for $1,771, with a six month warranty 90 miles away:
VoltCarPartScreenShot.jpg
VoltCarPartScreenShot.jpg (123.07 KiB) Viewed 16528 times
Image

Image

Image
Last edited by MitchJi on Sep 06 2015 6:21pm, edited 2 times in total.
Best Wishes!

Mitch


The best quality batteries and lowest priced batteries for DIY EV's are tier 1 OEM Quality Cells from salvaged (wrecked) EV packs. Three examples are Chevy Volt and Nissan Leaf and Tesla Model 3 packs.

Nissan Leaf Module specs are here
Chevy Volt Pack Info - Salvage 16kwh Packs Under $2k here

User avatar
Monstarr   100 W

100 W
Posts: 220
Joined: Apr 12 2011 4:56am
Location: The Netherlands

Re: Chevy Volt Pack Info - 16kwh Under $2k UNCOMPLETED

Post by Monstarr » Aug 15 2014 10:52am

??

what do u mean?

User avatar
MitchJi   1 GW

1 GW
Posts: 3204
Joined: Jun 02 2008 8:09pm
Location: Marin County California

Re: Chevy Volt Pack Info - Salvage 16kwh Packs Under $2k

Post by MitchJi » Sep 06 2015 6:09pm

bump
Best Wishes!

Mitch


The best quality batteries and lowest priced batteries for DIY EV's are tier 1 OEM Quality Cells from salvaged (wrecked) EV packs. Three examples are Chevy Volt and Nissan Leaf and Tesla Model 3 packs.

Nissan Leaf Module specs are here
Chevy Volt Pack Info - Salvage 16kwh Packs Under $2k here

Hillhater   100 GW

100 GW
Posts: 11517
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: Chevy Volt Pack Info - Salvage 16kwh Packs Under $2k

Post by Hillhater » Sep 06 2015 11:58pm

MitchJi wrote:bump
.??? Why. .?? :?:
This forum owes its existence to Justin of ebikes.ca

User avatar
MitchJi   1 GW

1 GW
Posts: 3204
Joined: Jun 02 2008 8:09pm
Location: Marin County California

Re: Chevy Volt Pack Info - Salvage 16kwh Packs Under $2k

Post by MitchJi » Sep 07 2015 7:39pm

Hillhater wrote:
MitchJi wrote:bump
.??? Why. .?? :?:
I posted this purchase information:
Volt packs are easy to find now for $1,500-$2k :mrgreen:. There are about 50 now on car-part.com.
http://www.car-part.com/

I searched by distance from my zip code. I found one for $1,771, with a six month warranty 90 miles away:
Best Wishes!

Mitch


The best quality batteries and lowest priced batteries for DIY EV's are tier 1 OEM Quality Cells from salvaged (wrecked) EV packs. Three examples are Chevy Volt and Nissan Leaf and Tesla Model 3 packs.

Nissan Leaf Module specs are here
Chevy Volt Pack Info - Salvage 16kwh Packs Under $2k here

lettersize   10 mW

10 mW
Posts: 32
Joined: Oct 26 2015 9:14am

Re: Chevy Volt Pack Info - Salvage 16kwh Packs Under $2k

Post by lettersize » Oct 26 2015 5:37pm

MitchJi, you've mentioned that cells are welded into 6S and 12S modules making it very difficult to reconfigure the packs.
But can the 48v module be reconfigured to 24v module? The Chevy Volt pack has 2x 24v/45Ah modules and 7x 48v/45Ah modules.
I wonder if i can turn 48v/45Ah module in 24v/90ah module.

User avatar
MitchJi   1 GW

1 GW
Posts: 3204
Joined: Jun 02 2008 8:09pm
Location: Marin County California

Re: Chevy Volt Pack Info - Salvage 16kwh Packs Under $2k

Post by MitchJi » Oct 30 2015 10:34am

lettersize wrote:MitchJi, you've mentioned that cells are welded into 6S and 12S modules making it very difficult to reconfigure the packs.
But can the 48v module be reconfigured to 24v module? The Chevy Volt pack has 2x 24v/45Ah modules and 7x 48v/45Ah modules.
I wonder if i can turn 48v/45Ah module in 24v/90ah module.
Check the DIY Ev threads in my op.
Best Wishes!

Mitch


The best quality batteries and lowest priced batteries for DIY EV's are tier 1 OEM Quality Cells from salvaged (wrecked) EV packs. Three examples are Chevy Volt and Nissan Leaf and Tesla Model 3 packs.

Nissan Leaf Module specs are here
Chevy Volt Pack Info - Salvage 16kwh Packs Under $2k here

baltimorebiker   10 mW

10 mW
Posts: 20
Joined: Feb 24 2015 12:30pm
Location: Baltimore, USA

Re: Chevy Volt Pack Info - Salvage 16kwh Packs Under $2k

Post by baltimorebiker » Sep 13 2016 5:14pm

Hi Forum People,

I just thought it would be relevant for me to post that I have been using a 2 kwhr 44v chevy volt module paired to a leaf bike 48v 1500w motor. Used tp 1430c charger. I did not use a BMS.It has been rock solid for the last year. Tons of power, tons of capacity. Just really heavy (45 lb battery and 20 lb motor)

I had a top speed of about 42 mph on flat ground using 1800 watts. I was able to go bike from Baltimore to Washington DC without pedaling (I actually can't pedal because I removed the chain) with lots of battery left over.

I'd be willing to answer any questions.
yescom 48V 1000w kit
sunthing 15 ah battery, which tested at 10 ah

1500w leaf bike motor
12s 45 ah 2000 whr chevy volt module

Harold in CR   1 MW

1 MW
Posts: 1663
Joined: Feb 01 2010 7:19pm
Location: Costa Rica

Re: Chevy Volt Pack Info - Salvage 16kwh Packs Under $2k

Post by Harold in CR » Sep 13 2016 6:29pm

I buy these and sell off part of them, so I can afford to get what I need at a decent price, because I can't afford to buy and keep a whole pack.

Actually, getting ready to go to Florida and build some parts and will buy another pack and offer modules for those guys that don't need a complete Volt battery.

I'm presently modding a dirt bike to a leaning reverse tadpole and will install a 28S Volt pack in it, with lots of room for groceries, controllers, charger, etc.

Also, going to convert most of our house to Volt battery, because of terrible Power Co. service and cost per Kwh.
Thanks to Justin, the forum is open source and NON-commercialized.

redilast   1 kW

1 kW
Posts: 317
Joined: Apr 14 2016 12:47am

Re: Chevy Volt Pack Info - Salvage 16kwh Packs Under $2k

Post by redilast » Sep 15 2016 4:24am

What kind of BMS and or Chargers are people using with these monster packs? These would be great for off grid energy storage for about the same price as golf cart flooded batteries...

mark.curry3   100 W

100 W
Posts: 103
Joined: Nov 20 2014 2:52pm
Location: Tampa, fl

Re: Chevy Volt Pack Info - Salvage 16kwh Packs Under $2k

Post by mark.curry3 » Oct 11 2016 3:24pm

These posts about the chevy volt batteries have me thinking about how too use them in my 60V 1000w e-scooter. I found a 88v pack for around $900 and am trying to see if it could be configured to use with my bike. The size may be an issue but I have not been able to find dimensions. i assume they can be installed sideways or upside down like lifepo4. I also need to know if the standard lifepo4 charger would work. If the size is workable, there is a possibility that I could move to a 72v bike if that would work better.. Any guidance would be appreciated,

User avatar
liveforphysics   100 GW

100 GW
Posts: 14143
Joined: Oct 29 2008 1:48am
Location: Long Beach, CA, USA

Re: Chevy Volt Pack Info - Salvage 16kwh Packs Under $2k

Post by liveforphysics » Oct 11 2016 5:46pm

baltimorebiker wrote:Hi Forum People,

I just thought it would be relevant for me to post that I have been using a 2 kwhr 44v chevy volt module paired to a leaf bike 48v 1500w motor. Used tp 1430c charger. I did not use a BMS.It has been rock solid for the last year. Tons of power, tons of capacity. Just really heavy (45 lb battery and 20 lb motor)

I had a top speed of about 42 mph on flat ground using 1800 watts. I was able to go bike from Baltimore to Washington DC without pedaling (I actually can't pedal because I removed the chain) with lots of battery left over.

I'd be willing to answer any questions.
Sounds like a nice capacity/voltage pack. What's the weight?
Each carcinogen vapor exposure includes a dice roll for cancer.

Each mutagen vapor exposure includes a dice roll for reproductive genetic defects in your children.

Each engine start sprays them into a shared atmosphere which includes beings not offered an opportunity to consent accepting these cancer experiences and defective genetics life experiences.

Every post is a free gift to the collective of minds composing the living bleeding edge of LEV development on our spaceship.

User avatar
Monstarr   100 W

100 W
Posts: 220
Joined: Apr 12 2011 4:56am
Location: The Netherlands

Re: Chevy Volt Pack Info - Salvage 16kwh Packs Under $2k

Post by Monstarr » Oct 27 2016 7:31am

liveforphysics wrote:
baltimorebiker wrote:Hi Forum People,

I just thought it would be relevant for me to post that I have been using a 2 kwhr 44v chevy volt module paired to a leaf bike 48v 1500w motor. Used tp 1430c charger. I did not use a BMS.It has been rock solid for the last year. Tons of power, tons of capacity. Just really heavy (45 lb battery and 20 lb motor)

I had a top speed of about 42 mph on flat ground using 1800 watts. I was able to go bike from Baltimore to Washington DC without pedaling (I actually can't pedal because I removed the chain) with lots of battery left over.

I'd be willing to answer any questions.
Sounds like a nice capacity/voltage pack. What's the weight?
:D

User avatar
Monstarr   100 W

100 W
Posts: 220
Joined: Apr 12 2011 4:56am
Location: The Netherlands

Re: Chevy Volt Pack Info - Salvage 16kwh Packs Under $2k

Post by Monstarr » Oct 27 2016 7:46am

baltimorebiker wrote:Hi Forum People,

I just thought it would be relevant for me to post that I have been using a 2 kwhr 44v chevy volt module paired to a leaf bike 48v 1500w motor. Used tp 1430c charger. I did not use a BMS.It has been rock solid for the last year. Tons of power, tons of capacity. Just really heavy (45 lb battery and 20 lb motor)

I had a top speed of about 42 mph on flat ground using 1800 watts. I was able to go bike from Baltimore to Washington DC without pedaling (I actually can't pedal because I removed the chain) with lots of battery left over.

I'd be willing to answer any questions.
I have done the same on a Novox C10 electric moped/scooter with hubmotor. Refitted the 12s3p pack with compression bands from parcel packingband machine I have at my work. I then fully covered it with protective tape and carry it around in a low priced bag I bought from Hobbyking (Turnigy Heavy Duty Large Carry Bag). Fits nicely.

Image

eddieboy   1 µW

1 µW
Posts: 2
Joined: Feb 18 2019 5:58pm

Re: Chevy Volt Pack Info - Salvage 16kwh Packs Under $2k

Post by eddieboy » Feb 18 2019 6:06pm

Well, with the right tools, you can take out the cells "as welded" in 3P 1S. It is actually easier than taking out the individual cells and safer. Weight per cell is 1153.0g / 3 with the copper tab left on. There is room to separate the plates for air cooling.
Image
Image

What are the necessary tools to take out the cells "as welded"?

User avatar
MitchJi   1 GW

1 GW
Posts: 3204
Joined: Jun 02 2008 8:09pm
Location: Marin County California

Re: Chevy Volt Pack Info - Salvage 16kwh Packs Under $2k

Post by MitchJi » Feb 19 2019 5:35pm

eddieboy wrote:
Feb 18 2019 6:06pm
Well, with the right tools, you can take out the cells "as welded" in 3P 1S. It is actually easier than taking out the individual cells and safer. Weight per cell is 1153.0g / 3 with the copper tab left on. There is room to separate the plates for air cooling.
Image
Image

What are the necessary tools to take out the cells "as welded"?
I don’t remember how it’s done. Check the article on the diyev forum that i posted the quote from in my op.

At this point in time I’d compare them with Tesla M3 modules. The Tesla M3 packs are starting to be available for excellent prices.
Best Wishes!

Mitch


The best quality batteries and lowest priced batteries for DIY EV's are tier 1 OEM Quality Cells from salvaged (wrecked) EV packs. Three examples are Chevy Volt and Nissan Leaf and Tesla Model 3 packs.

Nissan Leaf Module specs are here
Chevy Volt Pack Info - Salvage 16kwh Packs Under $2k here