Multistar High Capacity 6S 16000mAh

Batteries, Chargers, and Battery Management Systems.
Post Reply
User avatar
Emoto   10 kW

10 kW
Posts: 544
Joined: Jun 13 2011 9:31am
Location: Australia

Multistar High Capacity 6S 16000mAh

Post by Emoto » Sep 04 2014 11:25am

This is big MAH :shock: not having to parallel multiple pacs means cleaner wiring lets hope for a higher c rante in the future.
http://www.hobbyking.com/hobbyking/stor ... ouse_.html
Attachments
61510(2).jpg
61510(2).jpg (136.94 KiB) Viewed 11935 times

User avatar
RLT   10 kW

10 kW
Posts: 683
Joined: Oct 02 2007 6:47pm
Location: Ruidoso, NM; USA
Contact:

Re: Multistar High Capacity 6S 16000mAh

Post by RLT » Sep 04 2014 1:38pm

Interesting.
The highest AH they offer on the US site is 10, and they are backordered
I might be tempted to try (4X) 5S, if they had them, or maybe even (5X) 4S.

User avatar
teslanv   100 MW

100 MW
Posts: 2680
Joined: Nov 03 2013 8:42pm
Location: Bellevue, WA - USA
Contact:

Re: Multistar High Capacity 6S 16000mAh

Post by teslanv » Sep 04 2014 1:44pm

Pricing not bad, either. That's only $0.366 per watt-hour !!!
DD Hubs, Batteries, Controllers & Custom Ebikes.
http://westcoastelectrics.com
West Coast Electric Cycles
Bellevue, WA
USA

Punx0r   100 GW

100 GW
Posts: 5513
Joined: May 03 2012 8:16am
Location: England

Re: Multistar High Capacity 6S 16000mAh

Post by Punx0r » Sep 04 2014 2:05pm

Interesting.

Looking at the pattern in the heatshrink it looks like a bunch of paralleled cells inside the pack, but hopefully they are at least somewhat matched when assembled. That would offer an advantage over parallel separate packs.

User avatar
dogman dan   100 GW

100 GW
Posts: 35740
Joined: May 17 2008 12:53pm
Location: Las Cruces New Mexico USA

Re: Multistar High Capacity 6S 16000mAh

Post by dogman dan » Sep 04 2014 4:15pm

Or, the beauty of the 4s pack, is only 4 pouches if you have to chuck one.

User avatar
Russell   10 MW

10 MW
Posts: 2014
Joined: Nov 22 2008 3:08pm
Location: State of Wisconsin, USA

Re: Multistar High Capacity 6S 16000mAh

Post by Russell » Sep 04 2014 4:23pm

Emoto wrote:This is big MAH :shock: not having to parallel multiple pacs means cleaner wiring lets hope for a higher c rante in the future.
http://www.hobbyking.com/hobbyking/stor ... ouse_.html

Already out of supply and on backorder :(

-R
Jeep Comanche Trekking Bike w/YOUE geared motor, 42 lbs + 15 lb rear trunk bag w/12S 16Ah LiPo battery, tools, etc., 21A controller, 700 x 40C tires. 27 MPH.


My other E-Bikes: Nashbar Steel Flatbar

User avatar
teslanv   100 MW

100 MW
Posts: 2680
Joined: Nov 03 2013 8:42pm
Location: Bellevue, WA - USA
Contact:

Re: Multistar High Capacity 6S 16000mAh

Post by teslanv » Sep 04 2014 4:37pm

dogman wrote:Or, the beauty of the 4s pack, is only 4 pouches if you have to chuck one.
Great point, Dogman. I just nuked a 4S pack last night. Was a "dammit" moment for me, but with a 6S 16Ah pack, it would be an "Oh, F@#*!? Moment. :wink:
DD Hubs, Batteries, Controllers & Custom Ebikes.
http://westcoastelectrics.com
West Coast Electric Cycles
Bellevue, WA
USA

User avatar
dogman dan   100 GW

100 GW
Posts: 35740
Joined: May 17 2008 12:53pm
Location: Las Cruces New Mexico USA

Re: Multistar High Capacity 6S 16000mAh

Post by dogman dan » Sep 05 2014 5:37am

Mostly I was just thinking of the probability of one pouch puffing right out of the box.

It's a dilemma, less wiring would be nice, but only if they do a better QC before assembly.

I've often wished you could buy a 2s 4p pack. that would be 8 cells per pack, 7 to get 14s 20 ah. You'd cut off the 3 pin balance plugs and replace with two 8 pin plugs.

If one went bad, you would be tossing the same number of cells of two 4s packs.

babyhughie   100 W

100 W
Posts: 116
Joined: Feb 04 2014 4:21am
Location: Michigan, Metro Detroit

Multistar High Capacity 6S 16000mAh

Post by babyhughie » Sep 08 2014 3:32am

These packs are badass I will be holding out n waiting until they get stock in... 18s1p for 16ah makes me happy :-). The only thing I don't like is the XT-90 connectors.. Is it possible to series connect them without adapters? I am not familiar with the XT-90 connectors they look kind of funky..

User avatar
neptronix   100 GW

100 GW
Posts: 14320
Joined: Jun 15 2010 5:56pm
Location: California refugee living in Utah, USA
Contact:

Re: Multistar High Capacity 6S 16000mAh

Post by neptronix » Sep 08 2014 3:53am

icecube57 had great results with the 10AH packs. I'm crossing my fingers that these will get stocked in the USA warehouse.

You could make an average sized ebike pack by just hooking up a series harness.. i'm droolin'
"Love and compassion are necessities, not luxuries. Without them, humanity cannot survive." - Dalai Lama

My first major build: 1.6kW 8T MAC motor on a Trek 4500.
The new all-arounder: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: 20" eZee on a Cannondale Semi Recumbent.
Whipper-snapper: ? on a lightweight BikeE Semi Recumbent

User avatar
neptronix   100 GW

100 GW
Posts: 14320
Joined: Jun 15 2010 5:56pm
Location: California refugee living in Utah, USA
Contact:

Re: Multistar High Capacity 6S 16000mAh

Post by neptronix » Sep 08 2014 4:02am

If you calculated these based on whrs/kg with a 3.8v nominal voltage, they'd come out to 190whrs/kg.
Just a hair below the 10AH packs, which may mean that there's extra weight from cell interconnections or whatnot.

Dude, a 12S 16AH pack comes in at 8.5lbs.
"Love and compassion are necessities, not luxuries. Without them, humanity cannot survive." - Dalai Lama

My first major build: 1.6kW 8T MAC motor on a Trek 4500.
The new all-arounder: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: 20" eZee on a Cannondale Semi Recumbent.
Whipper-snapper: ? on a lightweight BikeE Semi Recumbent

nechaus   1 MW

1 MW
Posts: 1875
Joined: Oct 11 2011 7:41pm
Location: Brisbane > AUSTRALIA

Re: Multistar High Capacity 6S 16000mAh

Post by nechaus » Sep 08 2014 6:24am

dammit hobbyking take my damm money, i need 16 ah cells

Hillhater   100 GW

100 GW
Posts: 11159
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: Multistar High Capacity 6S 16000mAh

Post by Hillhater » Sep 08 2014 5:52pm

nechaus wrote:dammit hobbyking take my damm money, i need 16 ah cells
...but they are only 8 Ahr cells ! .....arranged 6s, 2p into the pack :wink:
This forum owes its existence to Justin of ebikes.ca

nechaus   1 MW

1 MW
Posts: 1875
Joined: Oct 11 2011 7:41pm
Location: Brisbane > AUSTRALIA

Re: Multistar High Capacity 6S 16000mAh

Post by nechaus » Sep 08 2014 5:59pm

ooooooooooooooh
bugger that then, I have about 80 of the 8000mah cell


looking at that top pic, looks like you can see heaps of cells inside..


User avatar
neptronix   100 GW

100 GW
Posts: 14320
Joined: Jun 15 2010 5:56pm
Location: California refugee living in Utah, USA
Contact:

Re: Multistar High Capacity 6S 16000mAh

Post by neptronix » Sep 09 2014 1:34pm

Wow, another company selling the same high density cell. I wonder if they come out of the same factory, or shit just gets copied so fast in China...
"Love and compassion are necessities, not luxuries. Without them, humanity cannot survive." - Dalai Lama

My first major build: 1.6kW 8T MAC motor on a Trek 4500.
The new all-arounder: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: 20" eZee on a Cannondale Semi Recumbent.
Whipper-snapper: ? on a lightweight BikeE Semi Recumbent

Hillhater   100 GW

100 GW
Posts: 11159
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: Multistar High Capacity 6S 16000mAh

Post by Hillhater » Sep 09 2014 6:08pm

neptronix wrote:Wow, another company selling the same high density cell. I wonder if they come out of the same factory, or shit just gets copied so fast in China...
That pack states 6S, 1P, and actually looks to only have 6 cells, 15 - 30 C and $300 !!
.......so it's not the same as the Multistar .
This forum owes its existence to Justin of ebikes.ca

botz244   10 W

10 W
Posts: 89
Joined: Oct 06 2011 2:13am

Re: Multistar High Capacity 6S 16000mAh

Post by botz244 » Sep 10 2014 4:50am

in down for 6 packs for 18s2p -32 ah oh ya for 2200.00 no problem. for 25 lbs heck ya

User avatar
Emoto   10 kW

10 kW
Posts: 544
Joined: Jun 13 2011 9:31am
Location: Australia

Re: Multistar High Capacity 6S 16000mAh

Post by Emoto » Sep 10 2014 10:08am

Punx0r wrote:Interesting.

Looking at the pattern in the heatshrink it looks like a bunch of paralleled cells inside the pack, but hopefully they are at least somewhat matched when assembled. That would offer an advantage over parallel separate packs.
Well spotted Punx0r but we wont know for sure until someone gets some.
neptronix wrote:icecube57 had great results with the 10AH packs. I'm crossing my fingers that these will get stocked in the USA warehouse.

You could make an average sized ebike pack by just hooking up a series harness.. i'm droolin'

These have landed in aus now ill guess the states is next :D the other thing is far less balance leads dangling around so a safer pack.

User avatar
ambroseliao   100 kW

100 kW
Posts: 1221
Joined: Apr 27 2009 3:34pm
Location: Washington, DC, USA area
Contact:

Re: Multistar High Capacity 6S 16000mAh

Post by ambroseliao » Sep 10 2014 11:40am

Not to change the subject, but I just spotted this 6S 22000mAh LiPO battery on alibaba...

http://www.alibaba.com/product-detail/c ... 87073.html
Attachments
cendao_high_capacity_lipo_battery_22_2v.jpg
cendao_high_capacity_lipo_battery_22_2v.jpg (159.77 KiB) Viewed 11420 times
http://www.ebikes.ca/ is the best!

TidalForce M-750X, Tidalforce S-750 with Crystalyte HS3540, 1x TF iO-X Cruiser. E+ 1000W hybrid bike. ebikes.ca DrainBrain & Cycle Analyst meters. GoPro HD Hero2 camera. Bosch Fat Packs, 37V 10Ah LiPO pack. Turnigy Multistar batteries
My blog: http://ebikerider.blogspot.com
Remember LiFEPo4 HVC is 3.65V and LVC is 2.7V

User avatar
TheBeastie   10 MW

10 MW
Posts: 2078
Joined: Jul 28 2012 12:31am
Location: Melbourne Australia

Re: Multistar High Capacity 6S 16000mAh

Post by TheBeastie » Sep 10 2014 12:23pm

ambroseliao wrote:Not to change the subject, but I just spotted this 6S 22000mAh LiPO battery on alibaba...
When I try to evaluate dubious battery backs especially Zippy packs I prefer to go by weight then their stated Ah, going by weight that pack does seem like a somewhat real deal as its 2.5kilos in weight! Thats a chunky battery!
Speed Kills Range, 10mph = 46 miles range, 20mph = 20 miles, 30mph = 8 miles rangehttps://goo.gl/1JNL53
Over Charging Kills ur battery bit.ly/1hzWKl4
Consider PAS as your only throttle https://goo.gl/Kg1F8F
Fuel-Cell is the ultimate battery coupled with 4th-gen Nuclear
https://goo.gl/TcKtHs https://goo.gl/ZhFFot https://goo.gl/gfa215
10 Square Miles of solar panels = 0.12GW average power! https://goo.gl/Ub1S39

User avatar
neptronix   100 GW

100 GW
Posts: 14320
Joined: Jun 15 2010 5:56pm
Location: California refugee living in Utah, USA
Contact:

Re: Multistar High Capacity 6S 16000mAh

Post by neptronix » Sep 10 2014 12:35pm

TheBeastie wrote:When I try to evaluate dubious battery backs especially Zippy packs I prefer to go by weight then their stated Ah, going by weight that pack does seem like a somewhat real deal as its 2.5kilos in weight! Thats a chunky battery!
That's a bad way of figuring energy density, because it varies widely across batteries.

Let's do some math for that pack.

22ah x 3.8v nominal x 6 cells = 501.6 watt hours.
501.6 watt hours / 2.518kg = 199 whrs/kg.

If that pack really has that capacity, that's right up there with high end panasonic 18650's, in terms of energy density per weight. But this is some random brand - they could easily be bullshitting us.

Typical 20C lipo, by those same calculations, is 149whrs/kg. Lead acid batteries are something stupid like 33whrs/kg.
"Love and compassion are necessities, not luxuries. Without them, humanity cannot survive." - Dalai Lama

My first major build: 1.6kW 8T MAC motor on a Trek 4500.
The new all-arounder: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: 20" eZee on a Cannondale Semi Recumbent.
Whipper-snapper: ? on a lightweight BikeE Semi Recumbent

toniovelo   10 W

10 W
Posts: 91
Joined: May 30 2013 12:15pm

Re: Multistar High Capacity 6S 16000mAh

Post by toniovelo » Sep 18 2014 6:19am

Not new review about this big lipo Multistar? The C discharge is true or a bit less? Thanks.

User avatar
TheBeastie   10 MW

10 MW
Posts: 2078
Joined: Jul 28 2012 12:31am
Location: Melbourne Australia

Re: Multistar High Capacity 6S 16000mAh

Post by TheBeastie » Sep 18 2014 6:47am

neptronix wrote:
TheBeastie wrote:When I try to evaluate dubious battery backs especially Zippy packs I prefer to go by weight then their stated Ah, going by weight that pack does seem like a somewhat real deal as its 2.5kilos in weight! Thats a chunky battery!
That's a bad way of figuring energy density, because it varies widely across batteries.

Let's do some math for that pack.

22ah x 3.8v nominal x 6 cells = 501.6 watt hours.
501.6 watt hours / 2.518kg = 199 whrs/kg.

If that pack really has that capacity, that's right up there with high end panasonic 18650's, in terms of energy density per weight. But this is some random brand - they could easily be bullshitting us.

Typical 20C lipo, by those same calculations, is 149whrs/kg. Lead acid batteries are something stupid like 33whrs/kg.
Yeah I meant its the real deal in a very loose was as in its actually 2.5kilos of battery nothing more. When I evaluate zippy I still only go by weight though, buts its the only packs I look at it that way.
Also when looking at things this way is the most important final sum is of Wh/Kg per $
So actually in summary what I meant to actually say is I like to try and evaluate battery by kg/$ for a dubious battery pack like in buying fruit, raw lithium per dollar!
Speed Kills Range, 10mph = 46 miles range, 20mph = 20 miles, 30mph = 8 miles rangehttps://goo.gl/1JNL53
Over Charging Kills ur battery bit.ly/1hzWKl4
Consider PAS as your only throttle https://goo.gl/Kg1F8F
Fuel-Cell is the ultimate battery coupled with 4th-gen Nuclear
https://goo.gl/TcKtHs https://goo.gl/ZhFFot https://goo.gl/gfa215
10 Square Miles of solar panels = 0.12GW average power! https://goo.gl/Ub1S39

melodious   100 kW

100 kW
Posts: 1157
Joined: Aug 26 2011 8:57am
Location: East Coast, U.S.A.

Re: Multistar High Capacity 6S 16000mAh

Post by melodious » Sep 18 2014 8:29am

I need to see if these big capacity bricks are sized right for my skateboard. Once they hit the USA sites, I'll grab 1-2 (if the dimensions are appropriate for my build) and buzz around with confidence that I will have enough watt hours to accomplish my goals. :mrgreen:
Surly Ogre rigid 29er, rear 10T MAC @ 50V 25AH & 40A: 30mph road/gravel/hill machine
42" dual diagonal Eskateboard @6s & 90mm wheels
Next: eMTB @10-12s & 8"-12" pneumatic wheels; Got Strapped? d-(',')z