Lithium Batteries Shipping Rules Discussions
Re: Lithium Batteries Shipping Rules Discussions
Not sure if this is the best place to put it, but in any case, I recently got a quote to send batteries from Australia to the east coast of the USA. I had an enquiry about a 5 kWh battery build, which I'm happy to do, but shipping it to Baltimore was going to cost AUD$1766.
This was for a 1 cubic metre allowance in a loose container load. So it wouldn't matter if it was 5 kWh or 50 kWh.
Still, it makes battery movements far more expensive than I'd hoped.
This was for a 1 cubic metre allowance in a loose container load. So it wouldn't matter if it was 5 kWh or 50 kWh.
Still, it makes battery movements far more expensive than I'd hoped.
Voltron Evo - Electric Superbike
Voltron - the dual Agni powered smoke machine
My Lithium powered E-Max scooter
My stolen e-bike
I build great batteries!
If you think electric bikes are slow, build a faster one and we'll see you next year.
Voltron - the dual Agni powered smoke machine
My Lithium powered E-Max scooter
My stolen e-bike

I build great batteries!
If you think electric bikes are slow, build a faster one and we'll see you next year.
Re: Lithium Batteries Shipping Rules Discussions
hallo guys,
I have read lot of topis and post about selling and sending the cells, but the price thing were to high for used cell so I writening this post becouse I am able to get brand new cells for you with really good prices from EU. Now I have 18650 2500mAh 3C and LG18650F1. I am now building 22s39p from 2500mAh and 22s20p from samsung30Q. And I am also wondering if I sbould use fused on positive side or just hard spot welded with nikl plate? how much experiance do you have pack with fuses? I see that it look nice and more safe but it is really needed. Has anyone alredy seen breaked fuse becouse of cell damage?
thank you
I have read lot of topis and post about selling and sending the cells, but the price thing were to high for used cell so I writening this post becouse I am able to get brand new cells for you with really good prices from EU. Now I have 18650 2500mAh 3C and LG18650F1. I am now building 22s39p from 2500mAh and 22s20p from samsung30Q. And I am also wondering if I sbould use fused on positive side or just hard spot welded with nikl plate? how much experiance do you have pack with fuses? I see that it look nice and more safe but it is really needed. Has anyone alredy seen breaked fuse becouse of cell damage?
thank you
-
- Posts: 7
- Joined: Dec 17 2016 11:41pm
Re: Lithium Batteries Shipping Rules Discussions
Humorously we've had several Dell laptop batteries (The thin, lipo type) start to swell. Dell wanted them back and said to just toss them in the mail.
Fought that baby all the way up. I talked with my IT guy and told him point blank not to ship it unless Dell sent the proper packaging, otherwise we'd get spanked with a massive fine.
I wish I could've gotten that call documented. That's the BS you deal with. At least most of my shipping guys know the right approach.
Fought that baby all the way up. I talked with my IT guy and told him point blank not to ship it unless Dell sent the proper packaging, otherwise we'd get spanked with a massive fine.
I wish I could've gotten that call documented. That's the BS you deal with. At least most of my shipping guys know the right approach.
Re: Lithium Batteries Shipping Rules Discussions
So I bought a couple battery packs from a Horrid Ebay seller (Southtownpowersupply) and they arrived damaged. Seller shipped each battery pack in a USPS Medium Flat rate box and used 4.... YES 4 bubble mailers as packing material. I now have a Ebay claim in for damaged items received and from what I can see (Legally) I can't even ship these back without a special shipping account. These are 200x 18650 packs in a 72c 20s 10p configuration which is well over the UPS and Fedex Limits for normal shipping.
- spinningmagnets 100 GW
- Posts: 11994
- Joined: Dec 21 2007 10:27pm
- Location: Ft Riley, NE Kansas
Re: Lithium Batteries Shipping Rules Discussions
Upgraded rules for shipping Lithium batteries in cargo bays of aircraft. I assume phones and laptops in the possession of the passengers (=/< 100-WH?) is still under the older rules...
Main point seems to be any allowable quantity of lithium in of a cargo-plane cargo-bay must be at or under the specified watt-hours and shall be charged to 30% for maximum safety.
No more lithium shipped in cargo-bay of "passenger" aircraft.
https://www.phmsa.dot.gov/news/us-trans ... provisions
Main point seems to be any allowable quantity of lithium in of a cargo-plane cargo-bay must be at or under the specified watt-hours and shall be charged to 30% for maximum safety.
No more lithium shipped in cargo-bay of "passenger" aircraft.
https://www.phmsa.dot.gov/news/us-trans ... provisions
Re: Lithium Batteries Shipping Rules Discussions
Has someone find a way to send batteries to USA from Europe? Even by sea.. I don't know the company.. appreciate any help.
Vector Typhoon v2.0 e-bike 10kWt - http://endless-sphere.com/forums/viewtopic.php?t=61259
Our web site: http://www.vectorebike.com
Our web site: http://www.vectorebike.com
Re: Lithium Batteries Shipping Rules Discussions
If someone find a way to send battery from Europe to USA , by sea or by air, for 20kg under 200usd. I will give this person a 100$
price valid worldwide for 7 days from now. Don't have time to write to logistics companies

Vector Typhoon v2.0 e-bike 10kWt - http://endless-sphere.com/forums/viewtopic.php?t=61259
Our web site: http://www.vectorebike.com
Our web site: http://www.vectorebike.com
Re: Lithium Batteries Shipping Rules Discussions
In 2019, the shipping label requirements changed for batteries.
I found a remarkably good interactive guide to the labeling requirements:
https://hazmateam.com/uploads/2019LITHI ... 182019.pdf
But if you've got old labels, they're not good for much anymore - you can't ship lithium with the old Class 9 Hazmat label, and the medium battery shipment labels have changed as well.
I found a remarkably good interactive guide to the labeling requirements:
https://hazmateam.com/uploads/2019LITHI ... 182019.pdf
But if you've got old labels, they're not good for much anymore - you can't ship lithium with the old Class 9 Hazmat label, and the medium battery shipment labels have changed as well.
Battery packs, Sunkko Welders, and more. http://syonyk.blogspot.com/
-
- Posts: 11516
- Joined: Aug 03 2010 10:33pm
- Location: Sydney ..(Hilly part !) .. Australia/ Down under !
Re: Lithium Batteries Shipping Rules Discussions
It seems Apple Mac book pro batteries are highly suspect and those laptops are banned from check in luggage on some airlines (Virgin)
Is there a known problem with them ?
Is there a known problem with them ?
This forum owes its existence to Justin of ebikes.ca
- amberwolf 100 GW
- Posts: 32148
- Joined: Aug 17 2009 6:43am
- Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
- Contact:
Re: Lithium Batteries Shipping Rules Discussions
Apparently some recalls.
https://www.google.com/search?q=Apple+M ... +batteries
https://www.google.com/search?q=Apple+M ... +batteries
If you found this advice helpful, supporting contributions are accepted here.
"if it ain't broke, improve it till it is"----Dog-Hauler Cargo eTrike SB Cruiser----The HI-Lebowski: a Lebowski SMD brain running a zombified Honda IMA Inverter: a HOW-TO guide----Cargo eBike CrazyBike2----General Blog
"if it ain't broke, improve it till it is"----Dog-Hauler Cargo eTrike SB Cruiser----The HI-Lebowski: a Lebowski SMD brain running a zombified Honda IMA Inverter: a HOW-TO guide----Cargo eBike CrazyBike2----General Blog
-
- Posts: 11
- Joined: Aug 17 2019 2:25am
Re: Lithium Batteries Shipping Rules Discussions
Does anyone have any information regarding the situation shipping in a container via sea ?
Yes it takes a lot of cells to make this workout but if one could get the required number of cells together, how difficult is it to ship via container shipping on a ship?
Yes it takes a lot of cells to make this workout but if one could get the required number of cells together, how difficult is it to ship via container shipping on a ship?
Re: Lithium Batteries Shipping Rules Discussions
Yes, I am also interested in practice vs theory. Theoretically I know about all those hazmat and UN9473958375289356345893465 regulations, but how does it look in real life when you ship by sea, where the requirements are not that strict.
I have managed to ship my ebike on a pallet with my other goods to USA and didn't declare that there were 180 cells in it.
I also know that in Europe nobody will bother to check the contents of the package that LEAVES by sea, but what happens upon ARRIVAL to the US?
If CBP discovers batteries it will not imposed any taxes because the value is low, that's for sure, but if the batteries were shipped without those UNwhatever stickers, do they impound them? If the package is insured, do I get my money back from the post office? Do they just issue a warning that that package was improperly transported and let it go?
I think that CBP is responsible for taxing stuff and protecting borders from banned goods. Batteries are NOT BANNED, they just need special stickers and packaging... So what actually happens at the US border? I would hate to order 300-400 batteries and lose thousands of $$$
I have managed to ship my ebike on a pallet with my other goods to USA and didn't declare that there were 180 cells in it.
I also know that in Europe nobody will bother to check the contents of the package that LEAVES by sea, but what happens upon ARRIVAL to the US?
If CBP discovers batteries it will not imposed any taxes because the value is low, that's for sure, but if the batteries were shipped without those UNwhatever stickers, do they impound them? If the package is insured, do I get my money back from the post office? Do they just issue a warning that that package was improperly transported and let it go?
I think that CBP is responsible for taxing stuff and protecting borders from banned goods. Batteries are NOT BANNED, they just need special stickers and packaging... So what actually happens at the US border? I would hate to order 300-400 batteries and lose thousands of $$$
Re: Lithium Batteries Shipping Rules Discussions
My understanding is you abide by the law or risk prosecution meaning fines and jail time. I would not expect a warning or mere confiscation.
Re: Lithium Batteries Shipping Rules Discussions
Well, not necessarily. I am the recipient of the package so how can I be responsible for the sender not putting a sticker on the box?
Re: Lithium Batteries Shipping Rules Discussions
The sender is the one who ships the package and is responsible for following the law and rules. The recipient has no control over that.
I am stating my opinions based on trying to ship Lithium batteries a few years ago. I just gave up and only sold them to people able to pick up, cash and carry. On the other hand, I've bought quite a few, big and small, from reputable dealers who appear to always abide by the law and regulations.
Re: Lithium Batteries Shipping Rules Discussions
OKI, but what happens in practice when batteries are inspected by anybody at the border or later? Do they arrive to the recipient?
My problem is very simple. I can buy really good batteries from a person in Europe. I know the guy, he is a geek, sells only perfect stuff but, as a nerd, he doesn't care about all those post office paperwork. He is just willing to pack them in plastic bubble wrap, spray poly foam in the box, put the batteries and let it swell. So he can really secure them well but will not do any paperwork other than insuring at the post office and sending.
Or maybe there is no paperwork involved and you just need to buy a 'batteries inside' sticker and that's it?
My problem is very simple. I can buy really good batteries from a person in Europe. I know the guy, he is a geek, sells only perfect stuff but, as a nerd, he doesn't care about all those post office paperwork. He is just willing to pack them in plastic bubble wrap, spray poly foam in the box, put the batteries and let it swell. So he can really secure them well but will not do any paperwork other than insuring at the post office and sending.
Or maybe there is no paperwork involved and you just need to buy a 'batteries inside' sticker and that's it?
Re: Lithium Batteries Shipping Rules Discussions
Hi they added new rules next year(:
It be harder to post
No small shops will do this now
https://dgtraining.com/new-lithium-batt ... st-report/
Good luck
It be harder to post
No small shops will do this now
https://dgtraining.com/new-lithium-batt ... st-report/