Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by ridethelightning » Aug 24 2015 5:42pm

subscribe

User avatar
Allex   1 GW

1 GW
Posts: 3257
Joined: Dec 05 2011 8:46am
Location: Stockholm, Sweden

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by Allex » Aug 26 2015 7:14am

+1

jumpjack   100 W

100 W
Posts: 195
Joined: Apr 11 2011 6:16am

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by jumpjack » Sep 14 2015 5:23am

I read in datasheet that these "amazing" new 30Q cells have just 250 cycles.... at 60% capacity, but even just 120 cycles at 80% capacity, a more usual percentage value.
So, why are they "amazing"?!?

User avatar
ridethelightning   1 MW

1 MW
Posts: 1870
Joined: Jul 21 2013 9:48pm

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by ridethelightning » Sep 14 2015 5:38am

I would expect that statement is only relevent with regard to the maximum discharge rate, of something like 25A/cell?

which particular data sheet are you referring to, have you got a link there please?

User avatar
riba2233   1 MW

1 MW
Posts: 1848
Joined: Jun 30 2013 10:23am
Location: Croatia

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by riba2233 » Sep 14 2015 1:51pm

jumpjack wrote:I read in datasheet that these "amazing" new 30Q cells have just 250 cycles.... at 60% capacity, but even just 120 cycles at 80% capacity, a more usual percentage value.
So, why are they "amazing"?!?

This is in worst/extreme conditions, not relevant for EV users.
My electric moped: http://www.evalbum.com/4966

My electric car: http://www.evalbum.com/5364

jumpjack   100 W

100 W
Posts: 195
Joined: Apr 11 2011 6:16am

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by jumpjack » Sep 14 2015 2:26pm

ridethelightning wrote:I would expect that statement is only relevent with regard to the maximum discharge rate, of something like 25A/cell?

which particular data sheet are you referring to, have you got a link there please?
First post in this same thread
https://endless-sphere.com/forums/viewt ... 6#p1033978

User avatar
Allex   1 GW

1 GW
Posts: 3257
Joined: Dec 05 2011 8:46am
Location: Stockholm, Sweden

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by Allex » Sep 21 2015 6:57pm

Okashira, do you have som updates on Cycle test of 30Q?

okashira   10 kW

10 kW
Posts: 957
Joined: Nov 17 2014 6:45pm
Location: Houston, TX

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by okashira » Sep 22 2015 12:26am

Allex wrote:Okashira, do you have som updates on Cycle test of 30Q?
I will get to it as soon as I can. I have alot of data that I have not went through, maybe 100-200 more cycles. Have not been cycling for the past month or so. I will resume it again when I have time.
"Peace out - I'm done."
-- Bernhard Riemann, 1859

edisonmotors.net
Tesla Model S 18650 cells - like new - and custom packs from Tesla cells for sale. Any shape Any power Any capacity.
PM me or search my threads.

Nathan   10 W

10 W
Posts: 76
Joined: Sep 21 2015 6:01am

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by Nathan » Sep 23 2015 5:54am

this 30Q 15a cell came out a few months ago ? and the 35E 10amp cell, when will the next 35Q cell be out ? a 3.5 amp 15 amp continuous cell well be awesome.

User avatar
Allex   1 GW

1 GW
Posts: 3257
Joined: Dec 05 2011 8:46am
Location: Stockholm, Sweden

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by Allex » Sep 25 2015 7:19am

So this one is NMC. How about calendar life compared to NCA, NCA should at least hold 5-8 years right?

"The dirty secret: manganese in NCM cells will always dissolve into the electrolyte. You can slow the process with surface treatments but it is always happening. NCA cells will capacity fade to 70-80% and then stabilize with very gradual loss thereafter."
https://endless-sphere.com/forums/viewt ... 0&p=829540

70-80 of fade but what is the time frame?

User avatar
ridethelightning   1 MW

1 MW
Posts: 1870
Joined: Jul 21 2013 9:48pm

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by ridethelightning » Sep 25 2015 7:46am

gulp! :shock:

well,by the time iv waited for my new pack to get too old to use, i guesse there will be 10ah 18650 on the market :lol:

User avatar
riba2233   1 MW

1 MW
Posts: 1848
Joined: Jun 30 2013 10:23am
Location: Croatia

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by riba2233 » Sep 25 2015 5:02pm

I'm pretty sure that 30Q is NCA cell. NMC should last at least 7 years, and NCA over 10, maybe 15. That's if you don't kill the cell in some other way, of course.
My electric moped: http://www.evalbum.com/4966

My electric car: http://www.evalbum.com/5364

User avatar
Allex   1 GW

1 GW
Posts: 3257
Joined: Dec 05 2011 8:46am
Location: Stockholm, Sweden

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by Allex » Sep 25 2015 5:44pm


User avatar
ridethelightning   1 MW

1 MW
Posts: 1870
Joined: Jul 21 2013 9:48pm

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by ridethelightning » Sep 25 2015 6:26pm

it says on the dampfakkus tat the 20R and 25R are nmc also...
http://dampfakkus.de/akkutest.php?id=490

so either they have got it wrong or many people are thinking these cells are NCA but actually are not.

okashira   10 kW

10 kW
Posts: 957
Joined: Nov 17 2014 6:45pm
Location: Houston, TX

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by okashira » Sep 25 2015 7:15pm

They are all NCA
"Peace out - I'm done."
-- Bernhard Riemann, 1859

edisonmotors.net
Tesla Model S 18650 cells - like new - and custom packs from Tesla cells for sale. Any shape Any power Any capacity.
PM me or search my threads.

User avatar
riba2233   1 MW

1 MW
Posts: 1848
Joined: Jun 30 2013 10:23am
Location: Croatia

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by riba2233 » Sep 26 2015 10:10am

Yep, dampfakkus has wrong info on his site. They are NCA. Also, I think that all cells marked with INR are NCA, and those marked With ICR are either NMC or just Co.
My electric moped: http://www.evalbum.com/4966

My electric car: http://www.evalbum.com/5364

User avatar
bigbore   10 kW

10 kW
Posts: 531
Joined: Sep 25 2009 7:43am
Location: Italy

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by bigbore » Nov 12 2015 2:56pm

I'm doing same research to see if is possible to substitute a 5S 10Ah LiPo battery with a lighter 18650 battery pack.
I need to build a battery pack with 18650 cells capable of delivering 80A continuous and I would like to have a 4P config so each cell would deliver 20A cont.
I've been reading a lot of data and it seems to me that Samsung 30Q and LG HG2 could be the right cells with the lower voltage sag at 20A.
My conclusions are based on the following graph. Is not too much 86°C at the end of the discharge for a 18650 cell?

Image
Image
Image

Sony VTC5A could be a good cell also? What do you think?

User avatar
Allex   1 GW

1 GW
Posts: 3257
Joined: Dec 05 2011 8:46am
Location: Stockholm, Sweden

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by Allex » Nov 12 2015 4:04pm

20A cont. per cell is very demanding even for 30q or vtc. If you are okay with reaching end of life at 200cycles, then go for it. 86C will of course kill it rapidly. I would not recommend going above 45C if you want to prolong their life.

Hillhater   100 GW

100 GW
Posts: 10816
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by Hillhater » Nov 12 2015 4:07pm

How long do you expect this pack to last ?...weeks, months , years ?
20 amp/cell continuous discharge will kill those cells fast !.
This forum owes its existence to Justin of ebikes.ca

User avatar
cycborg   1 kW

1 kW
Posts: 470
Joined: Jul 05 2014 4:45pm
Location: Boston metro, US

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by cycborg » Nov 12 2015 6:26pm

What do you mean by "continuous"? A minute or two? A 3 Ah cell at 20 A discharges in 9 minutes. 20 A all the time means really short rides and fairly short battery life. But a minute at a time with adequate rest in between might not cause too much heating. Still, I'd go with a couple more p's unless you plan on upgrading your pack every year or two anyway.

User avatar
bigbore   10 kW

10 kW
Posts: 531
Joined: Sep 25 2009 7:43am
Location: Italy

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by bigbore » Nov 13 2015 11:29am

cycborg wrote:What do you mean by "continuous"? A minute or two? A 3 Ah cell at 20 A discharges in 9 minutes. 20 A all the time means really short rides and fairly short battery life.
That's what I mean. The battery would be made for my RC FE Offshore that has run time from 5,5 minutes to 12 minutes depending on the water conditions. I've been using a 5S2P 10Ah LiPo and I think they will not last 200 cycles anyway so I think I could try to build a 18650 battery just to see what these high drain 18650 are capable of.
A cool feature could be the battery water cooling that I've thought to implement.
The price I've to pay for the LiPos is in the range of 137-150€. Now I start looking for a good price for 30 cells of the type LG HG2 or Sam. 30Q

Hillhater   100 GW

100 GW
Posts: 10816
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by Hillhater » Nov 13 2015 3:48pm

Have you compared 18650 voltage sag to some decent RC Lipos ?
I suspect you will be losing some voltage on a like for like pack.
This forum owes its existence to Justin of ebikes.ca

bellfador   10 mW

10 mW
Posts: 30
Joined: Aug 05 2015 2:17am

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by bellfador » Nov 13 2015 4:11pm

VTC5A has low DC Internal Resistance but lipo has less (approximately 10 mOhm/Ah).

Image

okashira   10 kW

10 kW
Posts: 957
Joined: Nov 17 2014 6:45pm
Location: Houston, TX

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by okashira » Nov 13 2015 4:54pm

bellfador wrote:VTC5A has low DC Internal Resistance but lipo has less (approximately 10 mOhm/Ah).

Image
Not really helpful to compare /Ah

How about /kg or /m^3
"Peace out - I'm done."
-- Bernhard Riemann, 1859

edisonmotors.net
Tesla Model S 18650 cells - like new - and custom packs from Tesla cells for sale. Any shape Any power Any capacity.
PM me or search my threads.

bellfador   10 mW

10 mW
Posts: 30
Joined: Aug 05 2015 2:17am

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by bellfador » Nov 13 2015 11:43pm

Easy calcs... 3S 1300 mAh turnigy nano 25-50C weight 139g, or 46.3g per cell. Dc internal resistence will be approximaly 7.7 mOhm or 166 mOhm /g and 37 mOhm/Wh. VTC5A have 377 mOhm /g and 152 mOhm/ Wh. Soon I will make a test on some lipo and I can tell with sure.