Post by granolaboy » May 30 2015 6:47pm

So I finally have some time to do something with the stuff I ordered from OSN Power.

What I got:

8 x AMP20M1HD-A A123 20Ah cells
1 x OSN-Assembly kit
1 x BMS-L4S100100-480 4S 100A 100A BMS
1 x CHA-1210 Lifepo4 12V 10A charger

I'm going to build myself a 4s2p (12v 40ah) booster battery for my scooter. With my current 13s Li-ion battery at 54.6 volts fully charged plus the booster battery at 14.4v fully charged, I'll be sitting at 69v fully charged. I'm pretty happy with how the math worked out on that. :lol:

Anyway

First off, they sent me a 36v 10a LifePO4 charger by mistake. They basically said to keep it and sent me another 12v one. That's pretty cool if you ask me. I now have this charger to sell if anyone wants it.

Here's what they look like:

Image


Yep. Wrinles. Short tabs. Some were even bent a little. Not a chance these are grade A cells.


Image
Image
Image
Image


Oh well, they'll do for me I guess. So I went over to the dollar store and got some dinner placemats to use as spacer material, and started putting it together:


Image


I figured to do the 4s2p, I'll connect them in parallel groups and then use some copper plate to make the serial connections after.


Image
Image


The BMS they sent me is actually 2 boards:


Image
Image


I assume that they both need to be hooked up. Seems odd to me tho...not that I know anything about BMS boards.
2010 EVT 168 @ 69v

User avatar
Takemehome   1 kW

1 kW
Posts: 312
Joined: Sep 30 2008 11:40pm
Location: Montreal, Qc, Canada

Re: My 4s2p A123 Amp20 Battery Build

Post by Takemehome » May 30 2015 10:53pm

Just a reminder:
Many 48V. controlers have 63V. rated caps.
Don't dream your life, live your dream.

Don't buy anything before visiting http://ebikes.ca

Justin, Thank you.

whatever   100 kW

100 kW
Posts: 1126
Joined: Jun 03 2010 2:16am

Re: My 4s2p A123 Amp20 Battery Build

Post by whatever » May 31 2015 3:12am

dont forget to compress the cells

999zip999   100 GW

100 GW
Posts: 8433
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: My 4s2p A123 Amp20 Battery Build

Post by 999zip999 » May 31 2015 1:18pm

I would put them all in parallel and charge them to 3.6v first.

User avatar
granolaboy   100 W

100 W
Posts: 273
Joined: Nov 09 2011 5:02pm
Location: Skidegate, BC, Canada

Re: My 4s2p A123 Amp20 Battery Build

Post by granolaboy » May 31 2015 6:47pm

999zip999 wrote:I would put them all in parallel and charge them to 3.6v first.
without compression? They are all sitting at roughly 3.3v right now. My plan is to assemble the pack when it is at this voltage, with stiff end plates, so that when it charges the cells will expand and become nice and compressed.
2010 EVT 168 @ 69v

999zip999   100 GW

100 GW
Posts: 8433
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: My 4s2p A123 Amp20 Battery Build

Post by 999zip999 » Jun 02 2015 1:58pm

There is a big range of capacity in 3.3 and in 3.4v at the 3.5 number and up the lower and lower capacity and will race higher voltage very fast. So all the numbers have a different meaning. Like it will charge from 2.8v to 3.0 pretty fast then start filling up. The sweet spot of A123 lifepo4 cells. Of course this is my opinion.
The reason for pre charging to 3.6 or as I like to 3.5v then build the pack. Now it's not all on the bms to balance a new pack. Those poor little resistors bleeding down a 20ah cell for balancing.
Last edited by 999zip999 on Jun 02 2015 10:17pm, edited 1 time in total.

User avatar
granolaboy   100 W

100 W
Posts: 273
Joined: Nov 09 2011 5:02pm
Location: Skidegate, BC, Canada

Re: My 4s2p A123 Amp20 Battery Build

Post by granolaboy » Jun 02 2015 5:29pm

Ahh...I hear yah...that makes sense.

I assembled it all at 3.3v, and I just threw it on the ImaxB6 and balance charged it for the first time. I was expecting a lot more expansion of the cells, actually...they didn't seem to expand much at all. All cells at 3.60v. This is after building the "box" and stuff...

I have a bunch more pics to post. Still waiting for the copper plate, and busy as heck, so posts will be infrequent.
2010 EVT 168 @ 69v

User avatar
granolaboy   100 W

100 W
Posts: 273
Joined: Nov 09 2011 5:02pm
Location: Skidegate, BC, Canada

Re: My 4s2p A123 Amp20 Battery Build

Post by granolaboy » Sep 30 2015 7:59pm

Finally have some time to post pics and finish this thread.

So I needed some end plates that were good and stiff to put compression on the cells. Metal seemed too heavy to me, so I went down to the dollar store and got a cutting board. It's about 3/8" thick, really REALLY stiff, and much lighter than metal.

Image
Image

Then to see what kind of expansion I'd get once fully charged, I wrapped it as tight as I could with some duct tape:

Image

It seemed pretty darn tight to me, and duct tape is pretty strong, so I just glue-gunned some sides and a bottom on it:

Image
Image

Then duct-taped the hell out of it:

Image

Then charged it up:

Image

Starting cell voltages:

Image

Ending cell voltages:

Image

The cells didn't seem to expand at all, so now I'm worried that duct tape isn't going to provide enough compression on the cells.

I discharged the cells to storage, and decided to go with a better solution.
Last edited by granolaboy on Sep 30 2015 9:18pm, edited 1 time in total.
2010 EVT 168 @ 69v

User avatar
granolaboy   100 W

100 W
Posts: 273
Joined: Nov 09 2011 5:02pm
Location: Skidegate, BC, Canada

Re: My 4s2p A123 Amp20 Battery Build

Post by granolaboy » Sep 30 2015 8:05pm

So screw duct tape, I'm using metal banding for compression.

I took a file and notched the end plates so the bands had a place to sit and not slide around.

Image
Image

Crank those suckers down tight:

Image
Image

Glue on the sides and bottom again:

Image

And copious amounts of duct-tape:

Image
Image
Image
2010 EVT 168 @ 69v

User avatar
granolaboy   100 W

100 W
Posts: 273
Joined: Nov 09 2011 5:02pm
Location: Skidegate, BC, Canada

Re: My 4s2p A123 Amp20 Battery Build

Post by granolaboy » Sep 30 2015 8:09pm

I didn't like wires making the series connections, so I got some 2mm thick copper plate and made my own bus bars.

I just cut them out with a jigsaw, and used my desk grinder to smooth the edges and round off the corners.

I used 3 of the original bars to make a jig to drill the holes:

Image

Much better:

Image
2010 EVT 168 @ 69v

User avatar
granolaboy   100 W

100 W
Posts: 273
Joined: Nov 09 2011 5:02pm
Location: Skidegate, BC, Canada

Re: My 4s2p A123 Amp20 Battery Build

Post by granolaboy » Sep 30 2015 8:48pm

Now I got to wire this thing up to the BMS.

First I did the ends to connect to the battery. I split the 6awg silicone wire I'm using into two, then used 10awg ring terminals on each end. Then I heat-shrunk it up. Should make a decent connection.

Image
Image
Image
2010 EVT 168 @ 69v

User avatar
granolaboy   100 W

100 W
Posts: 273
Joined: Nov 09 2011 5:02pm
Location: Skidegate, BC, Canada

Re: My 4s2p A123 Amp20 Battery Build

Post by granolaboy » Sep 30 2015 9:00pm

So the way the battery is going into the trunk under my seat means mounting the BMS on the side makes the nicest fit.

Image

Then I took the 6awg silicone wire, and split it into 4 wires. Each of the pads on the BMS has 4 holes in it, so I figure I'll use all of them for each connection.

Image
Image

A whole ton of soldering and an Anderson SB-50 later, we have this mess. Note this BMS uses the same connections for both charge/discharge.

Image
Image
Image
Image

And here it is in my scooter all hooked up:

Image
Image

I'll post another thread where I go through all the headaches of getting this battery to fit into my scooter, and the simple mod to my EVT scooter to wire it in. This thread is just the battery build.

I will say the results are fantastic. Everything fits perfectly, and the power increase is awesome.
2010 EVT 168 @ 69v

miro13car   1 MW

1 MW
Posts: 1542
Joined: Mar 26 2007 1:30pm
Location: Calgary, Canada

Re: My 4s2p A123 Amp20 Battery Build

Post by miro13car » Oct 02 2015 11:29am

Where did you got this BMS from.?


Really able to handle 100A?

User avatar
granolaboy   100 W

100 W
Posts: 273
Joined: Nov 09 2011 5:02pm
Location: Skidegate, BC, Canada

Re: My 4s2p A123 Amp20 Battery Build

Post by granolaboy » Oct 02 2015 6:17pm

I got everything from OSN Power

This is the BMS:

http://www.osnpower.com/pddetaildate/pr ... 05563.html

Says it does 100A continuous, and over-current protection kicks in at 220A +- 30A.

I have to say, the over-charge protection voltage at 3.9v is totally useless for a LiFePO4 cell....how about 3.65?

If anyone knows how to mod this, please let me know, because 3.9v is WAAAAY too high. What were they thinking?
2010 EVT 168 @ 69v

RobertC   1 W

1 W
Posts: 54
Joined: Jun 14 2015 7:46am
Location: Hanoi, Viet Nam

Re: My 4s2p A123 Amp20 Battery Build

Post by RobertC » Oct 13 2015 11:39pm

OSN does not list prices.. What was your cost per cell?

User avatar
granolaboy   100 W

100 W
Posts: 273
Joined: Nov 09 2011 5:02pm
Location: Skidegate, BC, Canada

Re: My 4s2p A123 Amp20 Battery Build

Post by granolaboy » Oct 21 2015 3:35pm

I paid $20 USD per cell when I ordered for AMP20M1HD-A.

BMS-L4S100100-480 was $75. Assembly kit was $40. CHA-1210 charger (12v 10A) was $40. All USD.

And I might as well mention that they accidentally sent me a 36v charger, and they just told me to keep it and sent me another one. Pretty cool if you ask me. I sold the 36v charger to someone on ES.
2010 EVT 168 @ 69v

sendler2112   10 kW

10 kW
Posts: 978
Joined: Dec 07 2012 6:14am
Location: Syracuse, NY USA

Re: My 4s2p A123 Amp20 Battery Build

Post by sendler2112 » Oct 21 2015 4:43pm

How did you end up paying them?

User avatar
granolaboy   100 W

100 W
Posts: 273
Joined: Nov 09 2011 5:02pm
Location: Skidegate, BC, Canada

Re: My 4s2p A123 Amp20 Battery Build

Post by granolaboy » Oct 21 2015 6:21pm

paypal
2010 EVT 168 @ 69v

RobertC   1 W

1 W
Posts: 54
Joined: Jun 14 2015 7:46am
Location: Hanoi, Viet Nam

Re: My 4s2p A123 Amp20 Battery Build

Post by RobertC » Oct 21 2015 8:12pm

WOW! Super deal. I was under the impression that A123 was premium and premium price, cheapest I saw was maybe $30 each up to $70 for "real a123".

You are doing a Lead Acid conversion, right? so these should be lighter and higher power.

Did it change the balance and handling of the bike? Hopefully in a good way?

Are you driving it yet?

sendler2112   10 kW

10 kW
Posts: 978
Joined: Dec 07 2012 6:14am
Location: Syracuse, NY USA

Re: My 4s2p A123 Amp20 Battery Build

Post by sendler2112 » Oct 22 2015 9:34am

granolaboy wrote:paypal
Good to know they will take paypal if asked. OSN Power has initially only offered me wire transfer or Western Union.

999zip999   100 GW

100 GW
Posts: 8433
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: My 4s2p A123 Amp20 Battery Build

Post by 999zip999 » Oct 22 2015 10:17am

This cells are from a recall and probably cut out of a pack. This could be the reason for the short tabs. Don't get the ones with the repaired tabs. These are great cell with long life so can have a long shelf life if storage voltage above 2.8v or better 3.3v but who knows if they put a low cell on the charger before sale ? Plus they must be 5yrs old or more can be a gamble. My 24s pack has 735 cycles and stay well balanced bulk charging @ 16 amp and 40amp discharge.
3.9v hvc is nuts they are best at 3.5v that's full. It's like when filling your car and the nozzle cuts off and you pull the trigger 2 or 3 times or more till the gasoline spits out the top.

I was hoping to hear othet input about your 8ga 4way pos pig tail for the bms.

lettersize   10 mW

10 mW
Posts: 32
Joined: Oct 26 2015 9:14am

Re: My 4s2p A123 Amp20 Battery Build

Post by lettersize » Oct 26 2015 7:06pm

Thanks for the photos! Learning a lot!

lettersize   10 mW

10 mW
Posts: 32
Joined: Oct 26 2015 9:14am

Re: My 4s2p A123 Amp20 Battery Build

Post by lettersize » Nov 09 2015 7:03am

Any update on the pack? How is performance so far?

User avatar
granolaboy   100 W

100 W
Posts: 273
Joined: Nov 09 2011 5:02pm
Location: Skidegate, BC, Canada

Re: My 4s2p A123 Amp20 Battery Build

Post by granolaboy » Jan 12 2018 12:21am

Was pointing this thread to a friend building a battery, and thought I might as well post the battery is still in use, and still functioning perfectly. I've probably put over 6000km on it.

The main battery that came with the bike is feeling a bit weak though...I think I'll probably have to replace it next summer if I want to still make it to town and back on a single charge.
2010 EVT 168 @ 69v

999zip999   100 GW

100 GW
Posts: 8433
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: My 4s2p A123 Amp20 Battery Build

Post by 999zip999 » May 11 2018 6:42pm

Do you charge them separately. Do you think the A123 pack take some of the amp Spike out of your demand and less on the 13s pack ?

Post Reply