Guys,
I know the recommended LVC here is 3,5V, so batt will bump up to 3,65V resting voltage.
Could it be that this just doesn't hold through for this particular cell?
I did a discharge from full to 3,5V on a brand new genuine 18650GA, only got 2292mAh out of it, instead of the rated 3450mAh.
I found some tests of this cell, with discharge curves. Even at 10A discharge, the cliff only appears at 3V.
What LVC would you guys recommend for this cell, based on this graph?