Post by Punx0r » Mar 17 2017 3:44am

Similar setup I knocked together from a cheap "1200W" DC-DC boost converter from ebay:

http://www.ebay.co.uk/itm/1200W-DC-DC-B ... SwZQRYbiCL

12-60V input, 12-83V output. Claims 20A input rating.

It's running at 74V 4A to slightly under-charge an 18S li-ion pack (BMS is limited to <5A charge current).

PSU is a cheapo 48V Meanwell clone. Volt/ammeter is another cheapo ebay unit and powered by its own tiny 230VAC-5VDC PSU.

Case is a generic equipment case with a handle added to the top.
20170316_212516.jpg
20170316_212516.jpg (174.7 KiB) Viewed 3790 times
20170316_213152.jpg
20170316_213152.jpg (95.41 KiB) Viewed 3790 times
20170316_213136.jpg
20170316_213136.jpg (84.58 KiB) Viewed 3790 times

User avatar
Matador   100 kW

100 kW
Posts: 1046
Joined: Jun 29 2016 10:00pm

Re: Bulk charging using a digital DC-DC boost module

Post by Matador » Mar 30 2017 11:50am

Overclocker wrote:
well it arrived ridiculously fast from china! it worked fine at the default 20v / 5a. when i upped the voltage to around 60v it stopped working and fried my PSU :evil:

upon closer inspection it uses a schottky diode that's only rated 45v! this is a module that's supposed to go up to 120v! i guess that's why it failed at the higher voltages, but then again i'm no switch-mode expert

here's a simplified diagram of a boost converter
Upon inspection, mine has a STMicroelectronics Branded "STPS20150" Schottky Rectifier : It has an IXYS Branded "IXFH150N17T" POWER MOSFET (175V V, 150 A, <12 mΩ) :
IXYS brand IXFH150N17T POWER MOSFET.pdf
(157.73 KiB) Downloaded 103 times
I got it from ebay seller "joytownoline" : http://www.ebay.co.uk/itm/BST-900W-DC-D ... 2213076941
Should be good to go up to 120V DC no problems.

In case anybody is looking for it...

Ming He BST900W MANUAL :
BST900W Boost Converter Manual.pdf
(217.42 KiB) Downloaded 257 times
Matador

whereswally606   100 kW

100 kW
Posts: 1155
Joined: Jun 19 2011 2:11pm
Location: Cheshire, UK

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by whereswally606 » May 01 2017 4:16am

So for a while I've been worrying about the lack of protection from small persons fingers on these bst400 dcdc s. I created an enclosure which channels the air over the heat sink and allows the user to get to the buttons and see the digital display. It's a bit crude and moving the interface panel to the side via two ribbon cables or on higher riser pins. Will post us photos later but I'm confident it is a lot safer than it was and much better protected.
bstboxtopview.png
bstboxtopview.png (44.75 KiB) Viewed 3715 times
so this is printed upside down.
bstbox.png
bstbox.png (66.53 KiB) Viewed 3715 times
Here you can see the slot to guide the air from the fan along the heatsink.

There are two pilot holes for the fan which need to be drifted a touch to line up with those in the heatsink but its close enough. everything else fits like a glove.

I may want to add another hole to hide the fan power wires too. Also mk2 might have allow the user panel to be flush with the case with printed buttons to further help from spills from above. Best off not actually drinking your brew while/near your charging .
Distributing "Lebowski" FOC Controller PCB (Through hole) since 2016
Moped: Emax 110s 2009

markz   100 GW

100 GW
Posts: 12205
Joined: Jan 09 2014 11:38pm

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by markz » Jun 10 2017 10:46pm

Meanwell Clone's
Are they sold on ebay?
What is the search term I use?

Want to do something similar.

User avatar
Overclocker   10 kW

10 kW
Posts: 740
Joined: Mar 17 2014 5:48am
Location: Philippines

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by Overclocker » Jun 11 2017 12:41am

markz wrote:Meanwell Clone's
Are they sold on ebay?
What is the search term I use?

Want to do something similar.

viewtopic.php?f=14&t=82731&start=25

on page 2 are pix of this Smun meanwell clone. true clones have indentations on the aluminum case where the power transistors sit on. and have 99% identical PCB layout and mechanical design

you'll also find PSU's w/ flat sides (no indentation). they're not true clones. totally different PCB. often with some corners cut i.e. missing the AC input filtering stage and 220/110v switch

User avatar
Overclocker   10 kW

10 kW
Posts: 740
Joined: Mar 17 2014 5:48am
Location: Philippines

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by Overclocker » Jun 11 2017 12:50am

Image

just an update i built another PMS this time w/ a 48V Smun PSU to charge my 63v nominal batt pack. also printed out a cheat sheet

the reason for this is that the BST900W isn't very efficient at boosting 36v to 71.4v max

User avatar
Overclocker   10 kW

10 kW
Posts: 740
Joined: Mar 17 2014 5:48am
Location: Philippines

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by Overclocker » Jun 15 2017 1:21pm

Image

just an update to using 48v PSU. i think the BST900W somehow got damaged from the higher input voltage. behaving strangely. it's showing 0.52A with NO LOAD. this isn't normal behavior

cerberpeter   10 mW

10 mW
Posts: 26
Joined: Nov 20 2016 11:56pm
Location: Newark-on-Trent, UK

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by cerberpeter » Jun 17 2017 6:55pm

Has anyone tried connecting 2 boost converters in parallel? I'm trying to do that with the 1200w modules from ebay, but the result is that always one of the modules is taking all the amps, no matter how I set the pots. I'm running them on constant current (battery is not charged and therefore the set voltage is not yet reached)
Any idea how to avoid that? Maybe adding a diode somewhere on the trace?

User avatar
amberwolf   100 GW

100 GW
Posts: 32238
Joined: Aug 17 2009 6:43am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by amberwolf » Jun 18 2017 12:59am

Well, you could put a diode in series with each supply's positive output to the load, so the cathodes of the diodes are connected to the load, and the anode of one diode is on one supply's positive, and the anode of the other diode is on the other supply's positive.

That would isolate the outputs of the supplies from each other, but I don't know exactly what effects it would have on their monitoring capabilities (if any).

You'd want to measure the voltage drop across the diodes and then add that much to each supply's voltage, though.

Punx0r   100 GW

100 GW
Posts: 5513
Joined: May 03 2012 8:16am
Location: England

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by Punx0r » Jun 19 2017 3:06am

cerberpeter wrote:Has anyone tried connecting 2 boost converters in parallel? I'm trying to do that with the 1200w modules from ebay, but the result is that always one of the modules is taking all the amps, no matter how I set the pots
This was my experience with some lower-power ("800" I think) units as well. Even though I'd seen it written that they could be paralleled.

markz   100 GW

100 GW
Posts: 12205
Joined: Jan 09 2014 11:38pm

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by markz » Jun 19 2017 5:05pm

Paralleling is harder to do, obviously, because they werent meant to be paralleled, obviously.
Just thinking about that in regards to the Meanwell PSU's, because them MW's are specifically designed to share the current for certain models of MW's. Perhpas in this case the circtuitry does not accomodate paralleling, and maybe the impedence is off and the lower one takes it all. Maybe impedence is the wrong term to use, but over all resistance perhaps. Because you are changing the OVERALL circuit when you parallel two units.

cerberpeter   10 mW

10 mW
Posts: 26
Joined: Nov 20 2016 11:56pm
Location: Newark-on-Trent, UK

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by cerberpeter » Jun 22 2017 8:30pm

Adding diodes didn't help unfortunately. They are acting the same way.
At first glance it looks fairly simple task, but in reality it isn't :(
It would've been great if we can parallel these boost converters, as this would make super cheap high power (fast) charger for our larger batteries.


pp.. I think I realize what is happening. The current shunt is placed on the negative side and the current there is always split equally through both of the boards, because the resistance path is almost identical. So no matter which board is boosting the voltage and pushing current through it's inductor, the current flow on the negative always splits between the 2 current shunts and makes them think they work the same when they are set to do that.
So I wonder if I try to brake the paths for reference voltage from the shunt and place shunt on the positive site, connecting its 2 ends where the reference voltage should go might make it work? :|

markz   100 GW

100 GW
Posts: 12205
Joined: Jan 09 2014 11:38pm

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by markz » Jul 04 2017 8:58pm

This is all over my head, but the basic concept is to use a cheap SMUN switching psu and then a dc-dc buck converter. Makes sense, efficiency is the concern as I read the thread.

What do I need to do to get 41.5V (10S) and 25A or higher charge doing the DCDC thang?

There are SMUN psu's that are 24V 25A/33A/50A @ $75/$151/$193(CAD) would have to split my pack in half and parallel.
I currently already have three Meanwell HRP-300-24 rated at 21.6V-28.8V and 15A, I use two in series for 10S at 15A.

Nice note to add - I got a shit ton of Dell 12V 62A psu's laying around. So DCDC looks like the way to go.

***Maybe I gotta start my own thread in Battery.

Punx0r   100 GW

100 GW
Posts: 5513
Joined: May 03 2012 8:16am
Location: England

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by Punx0r » Jul 05 2017 4:23am

The DC-DC converter acts as a voltage & current limiter, allowing you to use any old PSU as a power source (not a current-limited on or one with exactly the right voltage).

You aren't going to do 41.5V @ 25A though with the common parts from ebay.

The largest common dc-dc boost converters are 1200W max (if you'd dare run anywhere close to a China rating lol). It's also limited to 20A max current, but this is INPUT current. So if you're using a 12V PSU then you'll get only 12 x 20A = 240W before it burns up.

You want a PSU voltage that's as close to your desired output voltage for best efficiency. So I'd be looking at a 36V PSU. That's still only going to give you 36V x 20A = 720W input. Output would be 720W / 41.5V = 17.3A x 0.9 (approx. efficiency) = ~15A at best.

tostino   10 kW

10 kW
Posts: 970
Joined: Mar 24 2008 4:12pm
Location: New Port Richey, FL

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by tostino » Jul 05 2017 8:27pm

I decided to use this setup for charging my 18s 32ah multistar pack. I ordered 2x of both of the models listed in this thread so I could test things out.

I already blew one of the BST-900's somehow, I had it at maybe 600w, hit the voltage up slightly, and it blew the fuse, and took out the fet and diode with it.

On the bright side, I ordered some higher quality fets, they max out at 100v, but are much lower resistance: https://www.infineon.com/dgdl/irfp4468p ... 2c73472019 and diodes: https://www.onsemi.com/pub/Collateral/MBR20100CT-D.PDF

I'll attempt to repair the blown one, and upgrade the others after a bit more testing.

Also have an Eltek Flatpack2 (1800w) coming in in the next couple days, which should power these without issue.

I beefed up the traces on these boards, because they were pretty damn sad. Here are some pics: https://goo.gl/photos/N6Jqa1UxCX9CGwxWA

markz   100 GW

100 GW
Posts: 12205
Joined: Jan 09 2014 11:38pm

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by markz » Jul 05 2017 8:35pm

So 3 Dells 12Vx3=36V and 62A is 2232W, and the one dcdc I found puts out 30A. Yeah I need $pecial gear.
MW SE models or something. Then that current limiter board.

User avatar
parabellum   10 MW

10 MW
Posts: 2086
Joined: Nov 19 2010 9:55am
Location: Dominican Republic, north.

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by parabellum » Jul 05 2017 11:54pm

I have one from Drok. It worked nicely at 15A12v In to 24V out for hours, but blew up the IRFP4568 (150V fet by specs) at 9A 36V in and 120V out in under 1 minute. It overheated apparently, with additional fan blowing on the sink.
Is it a bad idea 3x+ multiplication or just a counterfeit Fet?

User avatar
Matador   100 kW

100 kW
Posts: 1046
Joined: Jun 29 2016 10:00pm

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by Matador » Jul 08 2017 9:18pm

Quote I have from Doctorbass in a Personal Messages when we talking about the BST900 :

ORIGINAL QUOTE IN FRENCH :
"Wow, bon achats :wink: Fait gaffe pour le BST900 quand tu le branche. met toi une diode en serie avec l'entrée si tu peux, au moins 30A car l'entrée est sensible aux spark qui font des poiontes de courant élevé et momentané quand les condensateur d'entrée se rechargent."

ENGLISH TRANSLATION :

"Great buy :wink: Be carefull with the BST900 when you plug/connect it. Make sure to put in a diode in series with the input if you can, at least 30A value because the input is sensitive to spark that stems from transient current surges when the input condensers get charged up."

I havent burned up my BST900 yet (still sits in it's box)... What do you think ? Could that solve the issues I see you guy experiencing ?

tostino   10 kW

10 kW
Posts: 970
Joined: Mar 24 2008 4:12pm
Location: New Port Richey, FL

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by tostino » Jul 12 2017 7:11am

Well i've been using my BST-900 with my meanwell s-350-27 for the past couple weeks with everything working fine.

I just got my Eltek Flatpack2 in, and I made a makeshift wiring harness to plug into it using some flattened bullet connectors and epoxy. Plugged that bad boy in and it worked first try. Putting out a stable 53.6v.

I plugged it into the BST-900, and it's powering it perfectly to charge my packs. The extra 20v on the flatpack2 compared to the meanwell really helps to not heat up the BST-900 when charging an 18s pack. I am not pushing it past 6a until I have my replacement fets in so i'm able to fix it if it does blow. I believe that once I replace the fet and diode with the better ones I ordered, I should be able to push this to ~1000w boosting from 53v to 75v. We'll see though, that's what testing is for.

Pictures: https://goo.gl/photos/N6Jqa1UxCX9CGwxWA

User avatar
parabellum   10 MW

10 MW
Posts: 2086
Joined: Nov 19 2010 9:55am
Location: Dominican Republic, north.

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by parabellum » Jul 12 2017 10:12am

tostino wrote: I believe that once I replace the fet and diode with the better ones I ordered, I should be able to push this to ~1000w boosting from 53v to 75v. We'll see though, that's what testing is for.
What Fet and diode did you order?

tostino   10 kW

10 kW
Posts: 970
Joined: Mar 24 2008 4:12pm
Location: New Port Richey, FL

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by tostino » Jul 12 2017 10:16am

parabellum wrote:
tostino wrote: I believe that once I replace the fet and diode with the better ones I ordered, I should be able to push this to ~1000w boosting from 53v to 75v. We'll see though, that's what testing is for.
What Fet and diode did you order?
Here is what I got:
tostino wrote:On the bright side, I ordered some higher quality fets, they max out at 100v, but are much lower resistance: https://www.infineon.com/dgdl/irfp4468p ... 2c73472019 and diodes: https://www.onsemi.com/pub/Collateral/MBR20100CT-D.PDF

User avatar
parabellum   10 MW

10 MW
Posts: 2086
Joined: Nov 19 2010 9:55am
Location: Dominican Republic, north.

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by parabellum » Jul 12 2017 10:38am

Thanks.

whereswally606   100 kW

100 kW
Posts: 1155
Joined: Jun 19 2011 2:11pm
Location: Cheshire, UK

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by whereswally606 » Jul 12 2017 11:49am

I've been using mine with and esp120 54.6v power supply. And can get a full 15a at 58.4v

16x3.65v for lifepo4.
I only charge like this when I can be near and manually terminate the charge. It is handy for a quick charge and not far off the 18a that the 60ah 0.3c batteries can take.

Sent from my ALE-L02 using Tapatalk
Distributing "Lebowski" FOC Controller PCB (Through hole) since 2016
Moped: Emax 110s 2009

markz   100 GW

100 GW
Posts: 12205
Joined: Jan 09 2014 11:38pm

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by markz » Jul 12 2017 2:30pm

15A @ ~60V is very very good.

I am not doing dcdc but I can charge two seperate batteries @ 15A and ~60V out of the same 110V outlet pulling 12A or so. Using 4 MW HRP-300-24's, all in I am at $50+$170 so $220cad plus I got a spare MW so 5 total for $270cad.

With your setup, I am sure it was much cheaper.

whereswally606   100 kW

100 kW
Posts: 1155
Joined: Jun 19 2011 2:11pm
Location: Cheshire, UK

Re: Bulk charging via digital DC-DC boost Minghe BST-900W

Post by whereswally606 » Jul 13 2017 4:27am

Esp120 was £50 off Sacko here on ES

Sent from my ALE-L02 using Tapatalk
Distributing "Lebowski" FOC Controller PCB (Through hole) since 2016