Post by mkp007 » Nov 05 2016 12:41am

Below is an idea for cell-to-strip-to-fuse-to-cable connection. The cells are rated to 10A peak discharge. My peak load will pull about 8A. The cells feed into the nickel strip of some thickness t and width w. The nickel strip then sandwiches a blade from a 50A blade-type low voltage fuse. A similar connection is on the other blade. Nickel strip is then wrapped around the cable and soldered. Insulation is placed between the fuse and battery terminal. This is all pressed flat for low pack depth. The back side is a similar connection except no fuse.

Image


Here is a link fuses that are about $0.70/ea. http://www.ebay.com/itm/New-10pc-MAXI-M ... 1875028161

I haven't worked with nickel sheet. Hoping it does not fracture when folded.

mkp
Mark

User avatar
mkp007   100 mW

100 mW
Posts: 48
Joined: Oct 28 2016 2:17pm
Location: San Diego, CA
Contact:

Re: Common pack design mistakes, how to avoid?

Post by mkp007 » Nov 05 2016 12:11pm

mistercrash wrote:How much current can be carried by that strip of material joining the groups of four cells?
From a rough calc, 10mm x 0.2mm nickel strip will have a voltage drop of about 1.5% for 16A and 5 inches of length. I am having a hard time sourcing this size strip without it being plated steel? Any thoughts on Ni plated steel vs all-nickel strips? Steel is 2.4x more resistant than Ni and Ni is 4x more resistant than Cu. More resistance = larger voltage drop = lost energy to heat. Also, I don't like the idea of plating as it could fail :!: .

eTrike wrote:...You might consider using a fuse holder instead of spot welding the strips....
Thanks eTrike. It is hard to find fuse a holder that doesn't add significant bulk to the sub-pack. I like the idea of spot welding and soldering to the blades for a more permanent connection.

I am concerned about the labor involved in fabricating all the strip/fuse sub-assemblies. But at least they are all the same and repeated 100's of times. So there's that. :|
Mark

User avatar
Matador   10 kW

10 kW
Posts: 941
Joined: Jun 29 2016 10:00pm

Re: Common pack design mistakes, how to avoid?

Post by Matador » Nov 05 2016 4:39pm

I would avoid plated steel. Too much resistance means lots of loss in heat and big voltage sag. The steel could turn red hot and melt at too high currents.
We have an example of the possible complications here : https://endless-sphere.com/forums/viewt ... 0#p1234386

For pure Nickel strips see my post here : https://endless-sphere.com/forums/viewt ... 5#p1214787

But in summary

Let's say your strips are 10 mm width by 0.2 mm thickness
It means your strips have a cross sectionnal area of 0.000002 m2

Now let's say you want to use 10 cm long strips... you can calculate the resistance of each strip...
Now let's compare it for different metals, using resistivity tables from here : https://en.wikipedia.org/wiki/Electrica ... nductivity

1. COPPER STRIPS (10mm width x 0.2mm thick x 10 cm lenght)
Resitivity of Copper is 1.68 x 10^-8 Ohm.m
So the resistance of a 10 cm lenght is : [1.68×10−8 Ohms.m] x [0.1m] / [0.000002 m2] = 0.00088 Ohms or 0.88 milliOhms
Since dP (heat loss) = R x I^2,
At 5 amps, 0.02 W of heat will be generated by just one 10 cm strip.
At 10 amps, 0.09 W of heat will be generated by just one 10 cm strip.
At 20 amps, 0.35 W of heat will be generated by just one 10 cm strip.
At 30 amps, 0.79 W of heat will be generated by just one 10 cm strip.

At 40 amps, 1.41 W of heat will be generated by just one 10 cm strip.
At 50 amps, 2.20 W of heat will be generated by just one 10 cm strip.
At 100 amps, 8.80 W of heat will be generated by just one 10 cm strip.
If I assume that a 1W CONSTANT heat loss PER STRIP is the max loss I can tolerate, I could go for up to 33.7 amps (SUSTAINED) with Copper of those dimension specs.
If I assume that a 5W PEAK heat loss PER STRIP is the max I can tolarate, I could go for up to 75.4 amps (PEAK) with Copper of those dimension specs.

2. NICKEL STRIPS (10mm width x 0.2mm thick x 10 cm lenght)
Resitivity of Nickel is 6.99 x 10^-8 Ohm.m
So the resistance of a 10 cm lenght is : [6.99×10−8 Ohms.m] x [0.1m] / [0.000002 m2] = 0.00349 Ohms or 3.49 milliOhms
--> 4 times more resistance than pure copper = 4 times more heat power loss than with copper (dP = R x I^2)
Since dP (heat loss) = R x I^2,
At 5 amps, 0.09 W of heat will be generated by just one 10 cm strip.
At 10 amps, 0.35 W of heat will be generated by just one 10 cm strip.
At 20 amps, 1.40 W of heat will be generated by just one 10 cm strip.
At 30 amps, 3.14 W of heat will be generated by just one 10 cm strip.
At 40 amps, 5.58 W of heat will be generated by just one 10 cm strip.
At 50 amps, 8.72 W of heat will be generated by just one 10 cm strip.
At 100 amps, 34.9 W of heat will be generated by just one 10 cm strip.
If I assume that a 1W CONSTANT heat loss PER STRIP is the max loss I can tolerate, I could go for up to 16.9 amps (SUSTAINED) with Nickel of those dimension specs.
If I assume that a 5W PEAK heat loss PER STRIP is the max I can tolarate, I could go for up to 37.8 amps (PEAK) with Nickel of those dimension specs (0.2 mm thick, 10 mm wide !)

3. CARBON-STEEL STRIPS (10mm width x 0.2mm thick x 10 cm lenght)
Resitivity of Carbon-Steel is 1.43 x 10^-7 Ohm.m
So the resistance of a 10 cm lenght is : [1.43×10−7 Ohms.m] x [0.1m] / [0.000002 m2] = 0.00715 Ohms or 7.15 milliOhms
--> 8 times more resistance than pure copper = 8 times more heat power loss than with copper (dP = R x I^2)
Since dP (heat loss) = R x I^2,
At 5 amps, 0.18 W of heat will be generated by just one 10 cm strip.
At 10 amps, 0.72 W of heat will be generated by just one 10 cm strip.
At 20 amps, 2.86 W of heat will be generated by just one 10 cm strip.
At 30 amps, 6.43 W of heat will be generated by just one 10 cm strip.
At 40 amps, 11.4 W of heat will be generated by just one 10 cm strip.
At 50 amps, 17.9 W of heat will be generated by just one 10 cm strip.
At 100 amps, 71.5 W of heat will be generated by just one 10 cm strip.
If I assume that a 1W CONSTANT heat loss PER STRIP is the max loss I can tolerate, I could go for up to 11.8 amps (SUSTAINED) with Carbon-Steel of those dimension specs.
If I assume that a 5W PEAK heat loss PER STRIP is the max I can tolarate, I could go for up to 26.4 amps (PEAK) with Carbon-Steel of those dimension specs.


4 . STAINLESS-STEEL STRIPS (10mm width x 0.2mm thick x 10 cm lenght)
Resitivity of Stainless-Steel is 6.90 x 10^-7 Ohm.m
So the resistance of a 10 cm lenght is : [6.90×10−7 Ohms.m] x [0.1m] / [0.000002 m2] = 0.0345 Ohms or 34.5 milliOhms
Since dP (heat loss) = R x I^2,
At 5 amps, 0.86 W of heat will be generated by just one 10 cm strip.
At 10 amps, 3.45 W of heat will be generated by just one 10 cm strip.
At 20 amps, 13.8 W of heat will be generated by just one 10 cm strip.
At 30 amps, 31.1 W of heat will be generated by just one 10 cm strip.
At 40 amps, 55.2 W of heat will be generated by just one 10 cm strip.
At 50 amps, 86.2 W of heat will be generated by just one 10 cm strip.
At 100 amps, 345 W of heat will be generated by just one 10 cm strip (IT WILL MELT FOR SURE !!!)
If I assume that a 1W CONSTANT heat loss PER STRIP is the max loss I can tolerate, I could go for up to 5.4 amps (SUSTAINED) with Stainless-Steel of those dimension specs.
If I assume that a 10W PEAK heat loss PER STRIP is the max I can tolarate, I could go for up to 17.0 amps (PEAK) with Stainless-Steel of those dimension specs.

So of course, nickel plated steel in not the same as bare steel.... You could make calculation accounting for the plating thickness to calculate the nickel cross sectionnal area to add to the steel core surface area.... But keep in mind plating is usually very very thin, somewhere between 5 and 50 microns of thickness... So the nickel plating is kind of non significant...

I would definitly avoid nickel plated steel.
Heck I'm even trying to stay away from bare nickel.
I'd rather go for nickel plated copper. See my post here : https://endless-sphere.com/forums/viewt ... 5#p1235640
Why ? Copper is a great conductor... But over time it oxidizes.... So resistance increase in contact points. Solution ?
Nickel really does not oxidises that much, but is a bit less conductive..
So Nickel-plated Copper core is the best of both worlds in my opinion.

Just my two-cents
Last edited by Matador on Nov 26 2016 10:57am, edited 6 times in total.

User avatar
Matador   10 kW

10 kW
Posts: 941
Joined: Jun 29 2016 10:00pm

Re: Common pack design mistakes, how to avoid?

Post by Matador » Nov 05 2016 8:54pm

Just as a side note... You might have noticed from the Wikipedia's resistivity table that Gold is not as good a conductor as Copper.
Why do we use it in Hi-Fidelity stereo equipement then ???
Why are most high quality Hi-Fi cable terminals/connectors Gold-plated ?

We know that Nickel oxidises a lot less than Copper ; almost no significant oxidation.
But if you heat up Copper past certain temperatures, I oxides crazy fast in contact with the oxygen from the air. And that resulting layer of copper-oxide is not good at conducting electricity.

Gold, on the other hand, does not oxidise at all (it's a very noble metal), so gold-plated connectors make for very reliable connection in Hi-Fi equipement.
The thing is gold is way too expensive. So the Nickel-plating of Copper is good enough for my own purpose... Gold plated Silver would probably be great !
Trust me, if I could use supraconductors, I would !

After all, the battery is THE single most important part of an eBike in my opinion.
Last edited by Matador on Nov 06 2016 4:32pm, edited 2 times in total.

Voltron   10 MW

10 MW
Posts: 2248
Joined: May 02 2013 4:53pm
Location: Santa Barbara CA

Re: Common pack design mistakes, how to avoid?

Post by Voltron » Nov 06 2016 10:16am

Re the drawing... I'm not sure I'm understanding it. Does the negative of the next group that isn't shown hook to that wire? And if so then why is it going off two directions like the start of a paralleling setup?
And if there is a fuse on the series connect, wouldn't it kill the whole series string when it went? I thought part of the benefit of putting up with the multiple connections of an 18650 pack was if one or two in a parallel group gets weak the whole series doesn't suffer as much because of the redundancy?

Also, how is the current sharing going to be with the 4p groups? Are the two center cells going to be seeing more current?

Not to badger you with questions, they;re just popping to mind right now... the last one was what kind of a system only sees 8 amp peaks. It would seem like even a low power set up would see more than that in bursts?

User avatar
mkp007   100 mW

100 mW
Posts: 48
Joined: Oct 28 2016 2:17pm
Location: San Diego, CA
Contact:

Re: Common pack design mistakes, how to avoid?

Post by mkp007 » Nov 06 2016 11:58am

Voltron wrote:Re the drawing... I'm not sure I'm understanding it. Does the negative of the next group that isn't shown hook to that wire? And if so then why is it going off two directions like the start of a paralleling setup? ....... It would seem like even a low power set up would see more than that in bursts?
'

The drawing shows a sub-group within the "sub-pack" illustrated near the bottom of page 2.

https://endless-sphere.com/forums/viewt ... 5#p1237927

The sub-pack is 1Sx36P. There is 9 rows of 4 cells. The drawing just shows only one of those rows. So the total "planned" peak current capability is 8A x 36 = 288A which is why the 300A is shown in the 4 gauge cable.

The reason to do it this way is because of space constraints. I have to fit 11 of the sub-packs in series in a triangular shape. There will actually be two stacks of these for a total of 22Sx36P (792cells). 90V and 288A will certainly move some things. and that is only 1/6th of the overall total.

So, the benefit of doing it this way is the cell-to-cell connections are all parallel and the sub-pack-to-sub-pack are all series. The current draw on each cell is very uniform I think.
Mark

User avatar
mkp007   100 mW

100 mW
Posts: 48
Joined: Oct 28 2016 2:17pm
Location: San Diego, CA
Contact:

Re: Common pack design mistakes, how to avoid?

Post by mkp007 » Nov 06 2016 12:51pm

Matador wrote:I would avoid plated steel. Too much resistance means lots of loss in heat and big voltage sag....

...I'd rather go for nickel plated copper.......So Nickel-plated Copper core is the best of both worlds in my opinion.
Thanks Matador. That was my thought too. I did find a rather inexpensive source for 0.2mm Nickel foil.

https://www.aliexpress.com/item/99-99-h ... 81711.html

I think shearing to the width needed (10mm, 12mm, etc.) is the way to go. I think a paper cutter would do the trick.

I like the idea of Ni plated copper foil. I used to work for a composites company and we made plated waveguides. Adding a Ni strike over copper was common. But that was fresh copper in a bath-to-bath process. If you take copper foil, I think you would need to do an acid etch first to remove any corrosion to make sure the Ni remains adhered to the copper.

I'm actually a little surprised that Ni plated copper foil isn't readily available and Ni plated steel is. Cost of Cu vs Ni foil is about 1/20th (ref. McMaster-Carr) so Ni plated copper would likely be less than Ni foil. There is a good plating facility near my shop. Maybe I'll bring a couple copper sheets over to them to see what they can do.

Is 0.25mm copper foil difficult to spot weld using the lower cost spot welders?
Mark

User avatar
Matador   10 kW

10 kW
Posts: 941
Joined: Jun 29 2016 10:00pm

Re: Common pack design mistakes, how to avoid?

Post by Matador » Nov 06 2016 2:59pm

mkp007 wrote: Thanks Matador. That was my thought too. I did find a rather inexpensive source for 0.2mm Nickel foil.
https://www.aliexpress.com/item/99-99-h ... 81711.html
I think shearing to the width needed (10mm, 12mm, etc.) is the way to go. I think a paper cutter would do the trick.
Nickel foil is a good idea...

But wow ! 138.88 USD (and there's the shipping fees too) is actually kind of expensive in my opinion, isn't it ?
I mean 0.2 mm (thick) x 200 mm (width) x 1500 mm (long) is actually 60 cubic-centimeter in volume... That's 60 mL volume of metal... Nickel has a density of 8.908 g/mL, meaning that the 60 mL translate to 534.5 grams of Nickel.
So at 138.88 USD/534.5 grams of Nickel, you pay 0.26 USD per gram of Nickel.
In Canada, Nickel coins made between 1955 and 1981 where 99.9% pure nickel... They cost only 5 cents and are 4.54 grams weight (https://en.wikipedia.org/wiki/Nickel_(Canadian_coin)), Now thats just 0.01 $ per gram (and CAD is worth less than USD).
So more than 26 times what it's worth in raw material. I understand you pay premium for the sheet shape formation of the material.... But personally I'd prefer copper sheets for less money AND better conductivity.
mkp007 wrote:I like the idea of Ni plated copper foil. I used to work for a composites company and we made plated waveguides. Adding a Ni strike over copper was common. But that was fresh copper in a bath-to-bath process. If you take copper foil, I think you would need to do an acid etch first to remove any corrosion to make sure the Ni remains adhered to the copper.

I'm actually a little surprised that Ni plated copper foil isn't readily available
and Ni plated steel is. Cost of Cu vs Ni foil is about 1/20th (ref. McMaster-Carr) so Ni plated copper would likely be less than Ni foil. There is a good plating facility near my shop. Maybe I'll bring a couple copper sheets over to them to see what they can do.
I'm also very surprised that they don't sell Nickel-plated Copper... I have good hopes that it will become available on the market once people realise that that's what we really need for our batteries. Once people become sensibilized to this resistance issue, they won't be satisfied with bare nickel (strips or sheets). They will require Nickel-plated Copper as a gold-standard of quality. Then as the demand grows, the offer will follow... And the Nickel-Plated COPPER sheets or strips will become widely and readily available to the wide market.

You're right about the Acid Etch... I managed to Nickel-Plate Copper on small scale with good results, just using 99.9% made Nickel-coins (see here for photos : https://endless-sphere.com/forums/viewt ... 5#p1235640). I didn't have any strong acid like hydrochloric acid to do the etch (so I sanded smooth my copper pieces with different grits up to 2000 grit wet sanding before plating).

mkp007 wrote: Is 0.25mm copper foil difficult to spot weld using the lower cost spot welders?
I have no clue... I have no experience with spot welding.... My battery build prototype is solderless... (se here : https://endless-sphere.com/forums/viewt ... 0#p1213147)
But I'd love to know if somebody on this forum has experience with Copper spot-welding.

I'm currently playing with and planning to rewire a MOT (Microwave oven-transformer)... Maybe I'll turn it into a spot-welder :mrgreen:
But for now I just pulled out the old secondary (2350 Volts AC) and repainted the ferrous core in black... Looks cool :
Attachments
IMG_0541[1].JPG
IMG_0541[1].JPG (231.28 KiB) Viewed 3205 times
Last edited by Matador on Nov 06 2016 4:45pm, edited 5 times in total.

cwah   10 GW

10 GW
Posts: 4214
Joined: Jul 24 2011 5:42am
Location: Between paris and london

Re: Common pack design mistakes, how to avoid?

Post by cwah » Nov 06 2016 3:48pm

subscribe
Help me find my stolen electric brompton: http://bit.ly/1a0vbBC and Bosch Sinus B3 http://bit.ly/1eV0WQz

User avatar
Matador   10 kW

10 kW
Posts: 941
Joined: Jun 29 2016 10:00pm

Re: Common pack design mistakes, how to avoid?

Post by Matador » Nov 06 2016 4:49pm

Found this video on copper tab spot-welding :
https://www.youtube.com/watch?v=jcXInB3YMBA
https://www.youtube.com/watch?v=NaqqfzFaM7w
0.007" copper thickness is equivalent to 0.18 mm thickness...
Not bad !

The welder seem kinda different than the cheap chinese spot welders though.
Last edited by Matador on Nov 06 2016 5:57pm, edited 1 time in total.

User avatar
Matador   10 kW

10 kW
Posts: 941
Joined: Jun 29 2016 10:00pm

Re: Common pack design mistakes, how to avoid?

Post by Matador » Nov 06 2016 5:50pm

I just googled a bit "why copper is difficult to spot weld"...(look here : http://cr4.globalspec.com/thread/7404/c ... ot-welding)

I mean of course people thought of Copper instead of Nickel waaay long before me. I doesn't take a PhD to figure out that Copper is 4 times more conductive than pure Nickel.
But people seem not to use copper much on this forum. Nickel seems more user-friendly than Copper... Why ???
That made me suspect that copper was not soo easy to spotweld, hence, people chose the next best thing : Nickel...

Seem like since copper has such a low resistance (which we want !), it make it harder to spot-weld.
Why ? To produce a good weld, you have to have a certain quantity of power dissipation in the form of heat.
But since copper has such a low resistance, you need to have more current to make the weld, or more voltage. (P = R x I^2... or P = V x I)

I'm crazy enough that I would want to weld 2 mm thick bussbars to my 18650s. I might as well find an alternative to spot-welding.
Copper is cheap... I bought 50 feets of 1/4 inch outer diameter copper pipe that I flattened. It cost me 40$ CAD. It gave me bussbars of around 10 mm width per 1.8 mm thick once flattened (I calculated a cross sectional area of 17.6 mm2, equivalent to 5 AWG gauge !)

Anyways, I'm pretty sure there are ways to spot-weld copper as we can see on the youtube video previously posted.
Last edited by Matador on Nov 06 2016 8:48pm, edited 1 time in total.

Hillhater   100 GW

100 GW
Posts: 10980
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: Common pack design mistakes, how to avoid?

Post by Hillhater » Nov 06 2016 5:59pm

Matador wrote: 0.007" copper thickness is equivalent to 0.18 mm thickness....
:?: :?: :?:
This forum owes its existence to Justin of ebikes.ca

User avatar
Matador   10 kW

10 kW
Posts: 941
Joined: Jun 29 2016 10:00pm

Re: Common pack design mistakes, how to avoid?

Post by Matador » Nov 06 2016 6:10pm

Hillhater wrote:
Matador wrote: 0.007" copper thickness is equivalent to 0.18 mm thickness....
:?: :?: :?:
Yes. 1 inch is 25.4 millimeters.
So 0.007 inch is 0.1778 mm, rounded off to 0.18 mm Right ?

User avatar
mkp007   100 mW

100 mW
Posts: 48
Joined: Oct 28 2016 2:17pm
Location: San Diego, CA
Contact:

Re: Common pack design mistakes, how to avoid?

Post by mkp007 » Nov 06 2016 7:48pm

I created a new thread for spot welding copper foil to 18650 style cells. Let's come up with a better way.

https://endless-sphere.com/forums/viewt ... 14&t=84680

Matador, thanks for your contributions!
Mark

Hillhater   100 GW

100 GW
Posts: 10980
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: Common pack design mistakes, how to avoid?

Post by Hillhater » Nov 06 2016 9:58pm

One point which seems to have been forgotten is the rule of Keeping welds clear of the center of the -ve base of the can.
Some of the manufacturers data sheets are very clear on this and even give dimentions of where not to put the welds to avoid sensitive internal areas.
This has been repeated on these forums previously.

[moderator edit to pics which provides an example of the point made here]

Image

Image
This forum owes its existence to Justin of ebikes.ca

User avatar
Allex   1 GW

1 GW
Posts: 3258
Joined: Dec 05 2011 8:46am
Location: Stockholm, Sweden

Re: Common pack design mistakes, how to avoid?

Post by Allex » Nov 08 2016 3:23am

Welding 2mm on to the cells do require som special equipment.

Here is a 0,3mm nickel compared to the negative cap och a 18650 cell. click on the link and you also will see why you should not spot weld in the middle of the can, just like Hillhater stated
https://endless-sphere.com/forums/viewt ... 5#p1011357
Image

User avatar
Overclocker   10 kW

10 kW
Posts: 689
Joined: Mar 17 2014 5:48am
Location: Philippines

Re: Common pack design mistakes, how to avoid?

Post by Overclocker » Nov 08 2016 7:54am

Hillhater wrote:One point which seems to have been forgotten is the rule of Keeping welds clear of the center of the -ve base of the can.
Some of the manufacturers data sheets are very clear on this and even give dimentions of where not to put the welds to avoid sensitive internal areas.
This has been repeated on these forums previously.

Image

Image

so i try to weld at the outside edges of the nickel

Skrzypas   10 W

10 W
Posts: 65
Joined: Jun 16 2014 3:08pm
Location: Warsaw, Poland

Re: Common pack design mistakes, how to avoid?

Post by Skrzypas » Nov 09 2016 4:25am

Well it's a news for me. I hope I didn't do many welds in the middle of cells in my pack.

LewTwo   100 kW

100 kW
Posts: 1057
Joined: Apr 08 2014 4:46pm
Location: Houston, Texas
Contact:

Re: Common pack design mistakes, how to avoid?

Post by LewTwo » Nov 10 2016 2:13pm

I 'peeked' inside my Luna Cycle Shark battery pack. It was suggested that I link the pictures to this thread so ...
Image
Image
Image
The full thread is here https://endless-sphere.com/forums/viewt ... &e=1239761
The more I learn the more obvious the immensity of my ignorance becomes.
Weight Wennie E-Bike https://endless-sphere.com/forums/viewt ... 3#p1173723
Shaft Drive Grocery Getter https://endless-sphere.com/forums/viewt ... =6&t=90718
...and thanks to Justin!

User avatar
mkp007   100 mW

100 mW
Posts: 48
Joined: Oct 28 2016 2:17pm
Location: San Diego, CA
Contact:

Re: Common pack design mistakes, how to avoid?

Post by mkp007 » Nov 10 2016 2:57pm

LewTwo wrote:I 'peeked' inside my Luna Cycle Shark battery pack. It was suggested that I link the pictures to this thread so ...
Image
The full thread is here https://endless-sphere.com/forums/viewt ... &e=1239761
Are those copper strips? I take it that is corrosion. Is that + terminal protection absorbing moisture? Maybe water is collecting at the bottom of your container?
Mark

Lectric Cycles   1 µW

1 µW
Posts: 3
Joined: Apr 06 2015 10:28am

Re: Common pack design mistakes, how to avoid?

Post by Lectric Cycles » Nov 11 2016 3:11pm

This a good example of a similar slim case configuration with solid construction
our_battry_5.jpg
our_battry_5.jpg (64.86 KiB) Viewed 4502 times

User avatar
tomjasz   10 GW

10 GW
Posts: 4245
Joined: Mar 29 2014 1:45pm
Location: Out riding, MN USA
Contact:

Re: Common pack design mistakes, how to avoid?

Post by tomjasz » Nov 11 2016 4:52pm

Nice battery! I'm excited about the wave of cased batteries coming with plastic mount separators. Also watch for the innovations coming from EM3ev. We can still get the budget hot glued Batts for low prices, but I predict these better built batteries, while more expensive, will have longer service lives. AND DO come with better warranties.
Thanks Justin_le we're here thanks to you. All the best to the mods for their tireless work keeping it on an even keel.

LewTwo   100 kW

100 kW
Posts: 1057
Joined: Apr 08 2014 4:46pm
Location: Houston, Texas
Contact:

Re: Common pack design mistakes, how to avoid?

Post by LewTwo » Nov 11 2016 4:56pm

mkp007 wrote:Are those copper strips? I take it that is corrosion. Is that + terminal protection absorbing moisture? Maybe water is collecting at the bottom of your container?
They appear to be nickle. No that is a solder spot. I believe they may have tinned that spot for the balance lead but wound up soldering it further to the left.
The more I learn the more obvious the immensity of my ignorance becomes.
Weight Wennie E-Bike https://endless-sphere.com/forums/viewt ... 3#p1173723
Shaft Drive Grocery Getter https://endless-sphere.com/forums/viewt ... =6&t=90718
...and thanks to Justin!

User avatar
spinningmagnets   100 GW

100 GW
Posts: 11675
Joined: Dec 21 2007 10:27pm
Location: Ft Riley, NE Kansas

Re: Common pack design mistakes, how to avoid?

Post by spinningmagnets » Nov 11 2016 5:21pm

When it comes to electrical conductivity, aluminum and zinc are both similar or better than nickel, and also much cheaper than nickel. I am persuaded that using 0.20mm thick nickel strips to form the paralleled sub-groups is reasonable, but for the thicker high-current series bus-bars, it seems to me that copper is easy and cheap to use there, but I'm told bare copper experiences corrosion (perhaps worse near the salt air of the beaches, but even in the desert, shiney copper turns brown with oxidation)

How about series bus bars made from thick copper and thinly plated by aluminum or zinc?

Micah Toll is selling a battery pack custom build-kit where he supplies the paralleled sub-groups with nickel strips and spot welds. The home pack-builder solders the series connections, with no fear of heat damage to the individual cells...

User avatar
Relanium   10 W

10 W
Posts: 95
Joined: Nov 25 2012 12:38pm
Location: Slovenia, EU

Re: Common pack design mistakes, how to avoid?

Post by Relanium » Nov 11 2016 7:12pm

There's a spray paint of zinc/zinc-aluminum for corosion protection (when welding up exhausts), maybe that would work.