In my theoretical battery pack, the 8mm wide flat copper bars cross the 10mm wide nickel strips, so the contact area for 20A is 80 Sq mm.

This current needs to travel through 6mm length of 10mm wide pure nickel strip (0.20mm thickness) to get from the center of the cell tip, to the edge of the nickel-plated copper series bars.

Just a side-note, I found bare solid copper wire in 8-ga for 500-ft roll at $150, so...$0.34 per foot, which can be compressed into bar stock. Which is $0.04 per inch/25mm

1/16th inch thick (copper bar-stock/plate) is 0.065" thick, which is 1.6mm thick. that looks to be a fruitful hunting ground, since cutting it into strips of 8mm wide X 1.6mm thick is somewhere around 12.8mm squared in cross-section, equal to somewhere around 6.5-ga

edit, found 0.032 thick (1/32nd", 0.8mm) X .375" wide (9.5mm) copper bar stock, for 5-cents per inch/ per 25mm of length, so...0.8mm x 9.5mm = 7.6mm/squared in area cross-section, equal to 8.5-ga solid copper wire. https://www.etsy.com/listing/231678857/ ... -in-x-36-x
30mm long [1.2 inch] x (3 per P=group X 14S = 42 plus 6 for end caps ) roughly 60 inches? so a 14s / 6P pack would take $3 worth of bare copper bar for series connections equal to 8.5-ga (70A continuous?)

Here is same price, but narrower at 0.25-inch wide (6.3mm), and at 0.32-inch/ 0.8mm thick, its equal to 5mm squared / 10-ga (good for 50A continuous?)

Home DIY of the nickel-plating is always an option, but how to get a factory to make a thin nickel-plate? And at what price?

In the pic below, I just grabbed a pic from ES, and then drew-in two copper flat bars (for the series connection) where I would make the series connections (possibly nickel-plated and then soldered onto the nickel paralleling strips. The two red arrows point to how this builder only made the series connection with a single nickel strip of the same material and thickness as the paralleling strips:
BatteryBusBars.jpg
BatteryBusBars.jpg (104.88 KiB) Viewed 4234 times
These are high-current cells, so those single-path nickel series strips were being asked to handle 80A peaks...

User avatar
Matador   100 kW

100 kW
Posts: 1036
Joined: Jun 29 2016 10:00pm

Re: Common pack design mistakes, how to avoid?

Post by Matador » Nov 13 2016 8:56pm

spinningmagnets wrote:I have recently been impressed by the PF cell, when used at 10A peaks. Imagine someone spot-welds six cells in-line, we solder thick copper flat bars in between every 2-cell group to make the series connection. Three series-bars connections from one 6-cell paralleled sub-group to the next. Copper is cheap, so we make them thicker than necessary. The distance from the center of one cell to the next is 20-ish mm, so each cells' 10A-worth of peak current only has to travel 10mm to reach a series connection.

Only 0.35 milliOhms according to this chart (0.20mm thick nickel strips flowing current a distance of one centimeter): viewtopic.php?f=14&t=84412&start=50#p1238471

10A X six paralleled cells is 60A peaks, which is what I am aiming for in an initial prototype. Of course the 30Q cell costs a little more, but at a rated 15A per cell, 6P would be 90A?
You can also make the calculation from my more complete table here (for future reference) https://endless-sphere.com/forums/viewt ... 5#p1240322

Look under the "10 mm width" row--> then under the " 0.2 mm thick sub-row --> then cross check under the "Nickel" column.... You'll see that the value resistance value (printed in red) is 35.0 mOhm/meter (multiply that buy 0.01 m (that is 1 cm)). So for 1 cm of lenght, the resistance is exactly 0.35 mOhms (R = 35.0 mOhm/meter x 0.01 meter = 0.35 mOhm).

See picture below for how to read the table :
resistance value per meter 10x0.2 Nickel.jpg
Just thought I'd make a usefull chart for resistances too, not just the "subjective" amapacities...

User avatar
Matador   100 kW

100 kW
Posts: 1036
Joined: Jun 29 2016 10:00pm

Re: Common pack design mistakes, how to avoid?

Post by Matador » Nov 13 2016 9:10pm

spinningmagnets wrote:In my theoretical battery pack, the 8mm wide flat copper bars cross the 10mm wide nickel strips, so the contact area for 20A is 80 Sq mm.
Home DIY of the nickel-plating is always an option, but how to get a factory to make a thin nickel-plate? And at what price?
Well I don't know what they will charge you, but plating 5 to 30 microns thickness of nickel does not require a whole lot of Nickel metal from the electrode... and at aroung 5 USD per pound of metal Nickel, you can make a hell of a big electrode. A pound of nickel goes a looooooooooooooonnnnng way for plating copper.

Then you need Nickel ammonium sulfate hexahydrate((NH4)2Ni(SO4)2 . 6 H2O) cristals to make a nickel ion electrolyte solution (just dissolve the cristals in distilled water until the solution is saturated) ... One you have the electolyte solution, you can pretty much use it infinitly (as nickel ions are constantly self resplenished by the bare nickel metal electrode which make new Ni2+ ions into solution)...

The most expensive part of plating by a company is clearly for the labor, rather than for the equipement, chemicals and electricity bills.
Last edited by Matador on Nov 17 2016 7:54am, edited 1 time in total.

Hillhater   100 GW

100 GW
Posts: 11069
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: Common pack design mistakes, how to avoid?

Post by Hillhater » Nov 13 2016 11:05pm

Plating is cool but why wouldnt you simply spray the finished assembled pack with one of the protective coatings used for electrical equipment and motors etc,..like Scotch 1601/1602. ?http://solutions.3m.co.uk/wps/portal/3M ... ng-sprays/
That would prevent corrosion and add insulation also.
This forum owes its existence to Justin of ebikes.ca

User avatar
Matador   100 kW

100 kW
Posts: 1036
Joined: Jun 29 2016 10:00pm

Re: Common pack design mistakes, how to avoid?

Post by Matador » Nov 14 2016 7:38am

Hillhater wrote:Plating is cool but why wouldnt you simply spray the finished assembled pack with one of the protective coatings used for electrical equipment and motors etc,..like Scotch 1601/1602. ?http://solutions.3m.co.uk/wps/portal/3M ... ng-sprays/
That would prevent corrosion and add insulation also.
Good point !

User avatar
madin88   1 GW

1 GW
Posts: 3075
Joined: May 27 2013 2:02am
Location: Austria

Re: Common pack design mistakes, how to avoid?

Post by madin88 » Nov 14 2016 2:04pm

Surface area is also important for current handling. A nickel sheet which is equivalent to lets say 1mm² copper can carry much higher current, because it will not overheat due to the much larger surface area.
The nickel or steel sheets are welded to the cells, this means the cells will soak up most of the heat which is produced by the resistance of the welding sheets.

talking about "the connection between the cells will add ..% to the total resistance of the battery" would make sense.

IMO it is not about absolutely BEST conductivity, because if the cross section is large enough, the nickel sheets will not add much to total resistance of the entire battery.
IMPORTANT is the equal current flow through all cells. Here is where most mistakes are made. This is the most important thing, not as for example 0,2 or 0,5% lower total resistnace.
- 10kW belt drive with Neumotor 8057: [url]viewtopic.php?
- KTM Hardtail Pedelec / eZee V2 6T / 27,5" / Kelly KBSX @ 1,5kW / Torque PAS / CA-V3 / 13s4p Sanyo GA in Shark case

User avatar
mkp007   100 mW

100 mW
Posts: 48
Joined: Oct 28 2016 2:17pm
Location: San Diego, CA
Contact:

Re: Common pack design mistakes, how to avoid?

Post by mkp007 » Nov 15 2016 10:35am

Hillhater wrote:Plating is cool but why wouldnt you simply spray the finished assembled pack with one of the protective coatings used for electrical equipment and motors etc,..like Scotch 1601/1602. ?http://solutions.3m.co.uk/wps/portal/3M ... ng-sprays/
That would prevent corrosion and add insulation also.
If you plate with nickel, it may make spot welding easier due the increased resistance. 2 for 1 hopefully (corrosion resistance + weldability).
Mark

User avatar
mkp007   100 mW

100 mW
Posts: 48
Joined: Oct 28 2016 2:17pm
Location: San Diego, CA
Contact:

Re: Common pack design mistakes, how to avoid?

Post by mkp007 » Nov 15 2016 10:43am

Matador wrote:
Hillhater wrote:I know you are using data from reference tables, but i am struggling to understand why a microscopic plating thickness of Nickle on the surface of a copper conductor would cause its Ampacity to be reduced by 13%...?? For sure , its Conductivity would not be affected. Can anyone explain ?
Good point, and honestly, I don't know the answer. I just took the derating factor of 0.87 from the reference I gave before as cash.
Maybe Nickel has less termal dissipation ability than copper. Maybe this is what reduces the ampacity rating...
I don't think the derating applies to our DC voltage application. That's more for AC high frequency stuff. DC current will go with area of the conductor and not more on the outside of it. You will notice that cables used for high frequency communication is bare copper for that reason. Plated copper is good for our application.
Maximum Frequency for 100% Skin Depth: This data is useful for high frequency AC engineering. When high frequency AC is conducted by a wire there is a tendency for the current to flow along the outside of the wire. This increases the effective resistance. The frequency listed in the table shows the frequency at which the calculated skin depth is equal to the radius of the wire, and is an indication that above this frequency you should start considering the skin effect when calculating the wire's resistance.
http://www.powerstream.com/Wire_Size.htm
Mark

User avatar
mxer   1 kW

1 kW
Posts: 350
Joined: May 15 2011 9:01am
Location: United Kindom

Re: Common pack design mistakes, how to avoid?

Post by mxer » Nov 16 2016 5:36pm

Thoughts on this pack?. Looks a work of art.

Image

Hillhater   100 GW

100 GW
Posts: 11069
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: Common pack design mistakes, how to avoid?

Post by Hillhater » Nov 16 2016 6:51pm

mkp007 wrote: If you plate with nickel, it may make spot welding easier due the increased resistance. 2 for 1 hopefully (corrosion resistance + weldability).
just how much would that resistance increase ??
i doubt the difference in resistance through a few microns of nickel at the interface , would be significant.
This forum owes its existence to Justin of ebikes.ca

User avatar
mistercrash   10 kW

10 kW
Posts: 960
Joined: Mar 09 2011 11:01am
Location: Guelph, Ontario, Canada eh!

Re: Common pack design mistakes, how to avoid?

Post by mistercrash » Nov 16 2016 8:35pm

mxer wrote:Thoughts on this pack?. Looks a work of art.

Image
16S7P if I see correctly. From the dimples at the spot welding points, it looks like 7 or 8mm X 0.15mm Nickle strips. The series connections connecting the P groups are irregular. I see some have up to 5 strips of Nickle making the series connection and others as low as just two strips. Let's say the 18650 cells are 3000mah and capable of a constant discharge of 3 amps per cell, times 7 is 21 amps. 5 strips of 8X0.15 Nickle could carry that load but anything lower is insufficient IMHO. And then there's the matter of this huge block of cells all held together by nothing more than the cell's heat shrink and the Nickle strips. Last, the pack is unfinished. What will carry the power out of the pack? The + and - terminations are not there. It looks like a battery I would have made 5 years ago when I started in the EV hobby.
Send $10 at paypal.me/Ray1964 and you will be in my thoughts and prayers.

Voltron   10 MW

10 MW
Posts: 2472
Joined: May 02 2013 4:53pm
Location: Santa Barbara CA

Re: Common pack design mistakes, how to avoid?

Post by Voltron » Nov 16 2016 10:02pm

As you said, it's obviously not done yet, but the least I count is three strips per series connection...

User avatar
mxer   1 kW

1 kW
Posts: 350
Joined: May 15 2011 9:01am
Location: United Kindom

Re: Common pack design mistakes, how to avoid?

Post by mxer » Nov 16 2016 10:28pm

Wow I've got alot more reading to do, I was going to follow this pack, back to the drawing board, thanks guys.

User avatar
parabellum   10 MW

10 MW
Posts: 2080
Joined: Nov 19 2010 9:55am
Location: Dominican Republic, north.

Re: Common pack design mistakes, how to avoid?

Post by parabellum » Nov 16 2016 10:46pm

Hillhater wrote:
mkp007 wrote: If you plate with nickel, it may make spot welding easier due the increased resistance. 2 for 1 hopefully (corrosion resistance + weldability).
just how much would that resistance increase ??
i doubt the difference in resistance through a few microns of nickel at the interface , would be significant.
Nickel is blown to dust at this point, do not count on it. Those microns just evaporise, just count cooper with some "surface protection" which is kind of questionable (I am doing that my self in hopes but, it just cracks and comes off in any strain scenario, like bending. I use electrolysis.)

User avatar
Matador   100 kW

100 kW
Posts: 1036
Joined: Jun 29 2016 10:00pm

Re: Common pack design mistakes, how to avoid?

Post by Matador » Nov 16 2016 11:03pm

parabellum wrote: it just cracks and comes off in any strain scenario, like bending. I use electrolysis.
What voltage do you use during that electroplating ?

I've had the best result at low voltages using ripple-less DC sources (either from 18650 or lower voltages from alcaline 1.5 volts cells). Some people on youtube say DC from walwarts doesnt give as good a result because of the ripple, while plating at a too high a voltage will give a smooth layer of plating, and it's more prone to flake off.
I haven't tried from walwarts or other external powersupplies, but I've experience that higher voltages give poor results. A lot of people suggest 1.5V or 3.0V. For my purpose, 3.7 volts worked fine.

https://www.youtube.com/watch?v=Q8Xo43sfLgY 8)
Last edited by Matador on Nov 17 2016 7:55am, edited 3 times in total.

User avatar
Matador   100 kW

100 kW
Posts: 1036
Joined: Jun 29 2016 10:00pm

Re: Common pack design mistakes, how to avoid?

Post by Matador » Nov 16 2016 11:11pm

parabellum wrote:Nickel is blown to dust at this point, do not count on it. Those microns just evaporise, just count cooper with some "surface protection" which is kind of questionable
Just to give you an idea those 0.1 mm nickel stips are actually just 100 microns thick.

Of course the plating can be just 3 or 5 microns if you don't plate for a long period of time, but if you're patient it's possible to plate 30 microns of Nickel over Copper with a low enough voltage (low voltage necessary for a smooth plating layer, especially for long periods of plating).

Check out Table 1 at page 9 of this "Nickel Plating Handbook" (very informative book btw). They do 50 microns nickel plating (50 microns) !
https://www.nickelinstitute.org/~/media ... 41015.ashx

This guy also says he gets best results with low voltage and using batteries as the DC electricity source for electroplating
https://www.youtube.com/watch?v=Q8Xo43sfLgY 8)
Last edited by Matador on Nov 17 2016 8:04am, edited 2 times in total.

User avatar
mistercrash   10 kW

10 kW
Posts: 960
Joined: Mar 09 2011 11:01am
Location: Guelph, Ontario, Canada eh!

Re: Common pack design mistakes, how to avoid?

Post by mistercrash » Nov 17 2016 6:20am

Voltron wrote:As you said, it's obviously not done yet, but the least I count is three strips per series connection...
Yes you are correct, I missed seeing that third little strip. Three or four is still not enough IMO unless it's for a very low power application.
Send $10 at paypal.me/Ray1964 and you will be in my thoughts and prayers.

User avatar
mkp007   100 mW

100 mW
Posts: 48
Joined: Oct 28 2016 2:17pm
Location: San Diego, CA
Contact:

Re: Common pack design mistakes, how to avoid?

Post by mkp007 » Nov 17 2016 1:03pm

parabellum wrote:
Hillhater wrote:
mkp007 wrote: If you plate with nickel, it may make spot welding easier due the increased resistance. 2 for 1 hopefully (corrosion resistance + weldability).
just how much would that resistance increase ??
i doubt the difference in resistance through a few microns of nickel at the interface , would be significant.
Nickel is blown to dust at this point, do not count on it. Those microns just evaporise, just count cooper with some "surface protection" which is kind of questionable (I am doing that my self in hopes but, it just cracks and comes off in any strain scenario, like bending. I use electrolysis.)
Vaporizing is good. As long as localized heat is being produced. It all comes down to localized heat.

As for the Ni flaking off, what was your surface prep technique? There are many ways to screw up plating and only one way to do it well. I recommend find a plating facility and have them do it for you. I believe the best prep is an acid etch, clean and dry in a non-humid environment and then plate.

Bending the copper strip after plating puts a lot of yield strain at that copper-nickel interface. I would not expect the plating to remain adhered in that situation. You must prevent bending the strip too much once plated.
Mark

User avatar
Matador   100 kW

100 kW
Posts: 1036
Joined: Jun 29 2016 10:00pm

Re: Common pack design mistakes, how to avoid?

Post by Matador » Nov 17 2016 3:38pm

mkp007 wrote:Vaporizing is good. As long as localized heat is being produced. It all comes down to localized heat.

As for the Ni flaking off, what was your surface prep technique? There are many ways to screw up plating and only one way to do it well. I recommend find a plating facility and have them do it for you. I believe the best prep is an acid etch, clean and dry in a non-humid environment and then plate.

Bending the copper strip after plating puts a lot of yield strain at that copper-nickel interface. I would not expect the plating to remain adhered in that situation. You must prevent bending the strip too much once plated.
I went getto here :lol: , plating in my appartment (Story and pics here : https://endless-sphere.com/forums/viewt ... 5#p1235640). My prep technic was sanding with sand paper to remove the oxide layer, 180 grit --> 320 grit, 600 grit (wet) --> 2000 grit (wet). Then used isopropyl alcool to remove any fingergrease, then plate in homemade Nickel acetate (for each 0.06 dm2 peace, I plated at 3.8 volts, current was around 10-15 mA, 12 hours of plating.... My nickel electrode was a nickel coin made of 99.9% Nickel (canadian coins between 1957 an 1981 I believe)...

I did not try to bend, but my stips are almost 1.8 mm thick (my build is bit unusual)

User avatar
parabellum   10 MW

10 MW
Posts: 2080
Joined: Nov 19 2010 9:55am
Location: Dominican Republic, north.

Re: Common pack design mistakes, how to avoid?

Post by parabellum » Nov 18 2016 2:03pm

Matador wrote:What voltage do you use during that electroplating ?
Voltage is not only factor. There is conductivity of the electrolyte, electrode to electrolyte contact surface and distance between electrode and work piece. I used plastic container with 2 electrodes in opposite corners and place 5 strips in between. Used adjustable buck converter from 12v supply, regulated to ~4.5V. Strips near the electrodes plate really quick, one in centre takes for ever, but they behave identically concerned to flacking.
mkp007 wrote: what was your surface prep technique?

Sanding with 400 sand paper. I did plating for corrosion protection in no weld pack, time will tell if it works.

User avatar
spinningmagnets   100 GW

100 GW
Posts: 11732
Joined: Dec 21 2007 10:27pm
Location: Ft Riley, NE Kansas

Re: Common pack design mistakes, how to avoid?

Post by spinningmagnets » Nov 20 2016 8:19am

From mkp007:
"Tin vs. Nickel - Nickel is not solderable, so any items that may need to be soldered to the bus bar wouldn’t stick to electroplated nickel. Forming, nickel is not as ductile as tin would be and therefore may crack under stress if bent. Tin is better than nickel as far as conductivity is concerned. Nickel can and will grow a heavy oxide that may prevent conductivity over time as the oxide is more difficult to break through than tin." (ref http://ppc1904.com/resources/faq)
Immediately, several posters pointed out that balance leads and even "thick copper wire" series connections have been soldered in the past, so solder works "well enough" connecting copper to nickel, BUT...my interest in posting this is that...nickel is expensive, and is slated to become MORE expensive as time goes on. Copper is cheap and works very well for parallel foil-strips, and also series current-bars. Corrosion over time is the issue of concern with copper, and tin is cheap. as far as resistance, we are only talking about a thin plating on a flat bar, that is bonded to the thick copper series-connection.

Lead-free solder is mostly tin, so...maybe if we "skin" copper series flat-bars with lead-free solder, we will have a useful style?
Lead-free solder melts at 220 to 300°C (depending on the formula)
The 60/40 alloy is one of the most common types of solder. The alloy contains 60 percent tin and 40 percent lead (tin is the first number in the label). The chemical symbols may also be included in the label such as "60Sn/40Pb" (tin is Sn and lead is Pb). The 60/40 solder has a melting point of approximately 360 degrees F and an electric soldering iron is used to melt and apply it. Flux-core 60/40 solder is a common choice for electronics work because it has a low melting point, it cools quickly and it "re-solidifies" quickly.

User avatar
Matador   100 kW

100 kW
Posts: 1036
Joined: Jun 29 2016 10:00pm

Re: Common pack design mistakes, how to avoid?

Post by Matador » Nov 20 2016 9:11am

spinningmagnets wrote:
"Tin is better than nickel as far as conductivity is concerned." (ref http://ppc1904.com/resources/faq)
Well it's strange that they say that !

According to wikipedia tables, Nickel is 1.5 times more conductive than Tin :
Nickel Conductivity (at 20°C) : 1.43×10^7 S/m
Tin Conductivity (at 20°C) : 9.17×10^6 S/m

Ref : https://en.wikipedia.org/wiki/Electrica ... nductivity

But besides conductivity (which is not so much of an issue since the bussbar core is Copper), I understand that tin has a lot of advantages : more ductile than nickel, electroplating can be avoided simply by applying a coat of Tin solder using flux.

User avatar
spinningmagnets   100 GW

100 GW
Posts: 11732
Joined: Dec 21 2007 10:27pm
Location: Ft Riley, NE Kansas

Re: Common pack design mistakes, how to avoid?

Post by spinningmagnets » Nov 20 2016 5:35pm

Thanks, I find so much conflicting info on the web.

If in fact "most of" the tin we find readily available (in low-lead solder) is slightly less conductive than "most of" the supposedly pure 0.20mm-thick nickel strips we buy from China, would a series connection copper flat-bar that is given a thin skin of high-tin solder conduct well enough (have reasonably low resistance) that its benefits will outweigh its drawbacks?

https://www.bluesea.com/resources/108
Perhaps the most interesting fact revealed by this chart is how low most copper alloy materials rank in relative conductivity. One might easily assume that alloys such as the brasses and bronzes, because they are mainly copper, are nearly as conductive as copper. This is not the case. The small percentages of tin, aluminum, nickel, zinc and phosphorus that make up these alloys degrade the electrical performance of the resulting alloy to a far greater percentage than their compositional percentage in the alloy.

One should not conclude from this, however, that brass should never be used in electrical applications. There are instances where the superior tensile and machining characteristics of brass make it a better choice than copper as long as the sectional areas are increased proportionately to achieve the conductivity that a copper part would have in the application. Size for size, however, copper is exceeded only by silver among the materials commonly used for electrical applications.
These guys rate conductivity as:

100__Copper
61___Aluminum
27___Zinc
22___Nickel
15___Tin
7____Lead

Common "lead free" solders have over a 95% of Tin in its composition, and the melting temperature is higher than older solders that are approximately half lead. Perhaps consider soldering the series flat bars onto the paralleling strips before they are spot-welded onto the cell ends? (using a jig to hold them in the exact shape needed?)

User avatar
mkp007   100 mW

100 mW
Posts: 48
Joined: Oct 28 2016 2:17pm
Location: San Diego, CA
Contact:

Multistar R/C Packs vs. 18650 Cells

Post by mkp007 » Nov 20 2016 6:23pm

'
This post may be of interest here: RC LiPo vs 18650 Cell High Power Packs https://endless-sphere.com/forums/viewt ... 14&t=84949

I don't want to derail this thread so please post comments there
Mark

LewTwo   100 kW

100 kW
Posts: 1057
Joined: Apr 08 2014 4:46pm
Location: Houston, Texas
Contact:

Re: Common pack design mistakes, how to avoid?

Post by LewTwo » Nov 20 2016 6:32pm

You folks might want to look at copper 95% zinc 5% alloy. It is commonly used as very thin sheets in arts and crafts. Also used in munitions (think full metal jacket). It has excellent corrosion resistance, conductivity betweel aluminum and copper and it can be soldered with silver solder.
The more I learn the more obvious the immensity of my ignorance becomes.
Weight Wennie E-Bike https://endless-sphere.com/forums/viewt ... 3#p1173723
Shaft Drive Grocery Getter https://endless-sphere.com/forums/viewt ... =6&t=90718
...and thanks to Justin!

Post Reply