999zip999   100 GW

100 GW
Posts: 9862
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: Common pack design mistakes, how to avoid?

Post by 999zip999 » Nov 20 2016 7:42pm

Solder between copper and aluminum with silver solder. Good luck. First flex. Hundreds of so called silver solder .
About temps
Silver. 1575 melt temp
85% silver solder's 1450
80% 1400
75% 1350
70% 1285
That silver solder ? It's for Jeweler Or something with some % of silver and ? Anyway at that temp it's brazing.

LewTwo   100 kW

100 kW
Posts: 1057
Joined: Apr 08 2014 4:46pm
Location: Houston, Texas
Contact:

Re: Common pack design mistakes, how to avoid?

Post by LewTwo » Nov 21 2016 3:13pm

The conductivity/resistancee is between copper and aluminum.
The alloy can be silver soldered.
The more I learn the more obvious the immensity of my ignorance becomes.
Weight Wennie E-Bike https://endless-sphere.com/forums/viewt ... 3#p1173723
Shaft Drive Grocery Getter https://endless-sphere.com/forums/viewt ... =6&t=90718
...and thanks to Justin!

User avatar
spinningmagnets   100 GW

100 GW
Posts: 11824
Joined: Dec 21 2007 10:27pm
Location: Ft Riley, NE Kansas

Re: Common pack design mistakes, how to avoid?

Post by spinningmagnets » Nov 22 2016 1:58am

Agniusm is using nickel-plated copper

https://endless-sphere.com/forums/viewt ... 0#p1164028

And there was one example shown of tin-plating of copper:

https://endless-sphere.com/forums/viewt ... 5#p1148497

The builder using tin-plating expressed disappointment at the finish of the parts, but I suspect they would work fine. I would not expect tin-plated parts to be shiny or pretty. Also, I would only want enough tin thickness to prevent corrosion from exposure to air and humidity.

edit: I just went back and re-read some of the posts. I now feel that copper is the way to go. Maybe even for the paralleling strips. Pure nickel strips are used by industry, but almost all of those are low-amp packs. Nickel-plated copper may be the premium option of choice in the near future, but...there are many affordable ways to apply some type of corrosion protection to copper strips, either before or after the cell connections.

I had been looking at purchasing spot-welded paralleled sub-groups, and then soldering the thick copper bars to make the series connections. That way I don't ever need to buy a spot-welder. And then I realized one of my issues with spot-welding is that any store-bought or DIY spot-welder I was considering had a variable amps in order to allow it to adjust to making a consistent weld on a variety of thicknesses of nickel strips. Rther than try to save a few pennies by using the thinnest nickel that would barely be acceptable, why not just set up for the thickest commonly available? 0.20mm seems to be common here, especially if there is a series connection between every two cells. a 20A cell only has to provide current a short distance through the nickel strip to get to the closest copper bar (of course, the copper would be sized thicker than needed). The series bar might even act as a heat sink for the current peaks in the nickel, but...the nickel would still act as a bottle-neck (un-necessary resistance)

Copper is now (and is likely to continue to be) readily available and cheap. Spot-welding copper is being explored in another thread, and I believe that is the future, because the builders who are interested in a DIY pack, are almost all also interested in high current.

In the DIY capacitive discharge (CD) spot-welder thread, there was a link to a video about taking a large transformer from a scrap microwave oven, and rewinding one end (as shown, it was MUCH easier than I imagined it would be), literally two wraps of thick cable. Since copper is so cheap, we can choose a thickness of copper sheet that is thicker than needed, and then adjust the windings on the transformer to perform good welds on that thickness, no adjustability would be needed after that.

https://www.youtube.com/watch?annotatio ... 5pGN6pqkyY

But even beyond a simple caveman transformer spot-welder, agniusm made his laser-cut copper plates that perform the function of paralleling and also series out of copper foil that was thick enough for the series connection. Of course that means that the parallel connections were from copper that was way thicker than needed, but again...copper is cheap. If someone was insistent that they wanted a thinner copper on the cell-tips (perhaps for contact area flexibility?) then it is easy to double-up on the thickness around the series connections, in the same way that we have seen controller traces beefed up.

vicens   100 W

100 W
Posts: 106
Joined: Aug 27 2015 3:08am
Location: Barcelona. Spain.

Re: Common pack design mistakes, how to avoid?

Post by vicens » Nov 30 2016 8:52pm

I need help.

I'm making a 38S22P battery for my vectrix.

I've soldered some nikel strips. In groups of 11.

I have read that it is much better to weld the strips of nickel in series. And then solder the parallels.

How bad is it to solder the cells in series on top of the parallels?
like in the picture.

Image

I have half soldiers and the other half without welding.

Those who do not have soldiers could stay that way. Without the 11-cell connection strips. like in the picture.

Image

For the connection of positive and negative I have thought this.

Put a strip of nikel out of the cells.

Image

Solder a copper wire with tin. To the nikel strip that is out of the cells.

Image

Solder the positive battery cable to the mitat of the nikel strip.

Image

Is there another better way to connect the positive cable?

User avatar
fechter   100 GW

100 GW
Posts: 15098
Joined: Dec 31 2006 3:23pm
Location: California Bay Area, USA

Re: Common pack design mistakes, how to avoid?

Post by fechter » Nov 30 2016 11:24pm

You could just have nickel series strips go past the end of the cells a way, then fold them over the copper wire, then solder. If the copper is extra thick, the voltage drop across it will be minimal and you don't need a fancy arrangement of feeders.

See how I did it here: https://endless-sphere.com/forums/viewt ... 14&t=79324

I don't like soldering directly over the end of a cell as the heat could still damage it. Between cells and you could melt the insulation. I built one pack with soldered series connections but I kept the connections away from the centers of the cells and watched the insulation carefully. It worked out OK. Welding everything is really the best.

Remember, except for the end cells, the parallel connections between cells normally don't carry any current, or at least not much, so they can be very thin. Each cell should ideally have its own series connection to the next cell. For most 18650 cells, one strip is probably enough. The criss cross pattern would actually provide you parallel connection as well and has some redundancy, so not bad but does use more nickel.

A simpler, but maybe a bit more expensive approach would be to just cut out a large nickel sheet to cover all the cell ends in a single piece. Then just weld away. You'd need some way to locate the centers of each cell (like denting the sheet slightly).
"One test is worth a thousand opinions"

User avatar
multifrag   100 W

100 W
Posts: 130
Joined: Feb 19 2016 5:44am
Location: London, UK

Re: Common pack design mistakes, how to avoid?

Post by multifrag » Dec 10 2016 4:20pm

Any criticism on welding layout? It's 14S4P battery. Panasonic GA(10A) cells and set for 25-30A output. 6-7.5A for each cell.
Attachments
Battery.jpg

User avatar
fechter   100 GW

100 GW
Posts: 15098
Joined: Dec 31 2006 3:23pm
Location: California Bay Area, USA

Re: Common pack design mistakes, how to avoid?

Post by fechter » Dec 10 2016 4:40pm

The layout looks OK, but 30A though a pair of nickel strips might be too much. You could use multiple layers of nickel (like maybe 3) to get the resistance down or possibly just solder some copper over the top of a single strip.
"One test is worth a thousand opinions"

kdog   10 kW

10 kW
Posts: 694
Joined: Feb 02 2014 9:22pm
Location: hobart, tasmania

Re: Common pack design mistakes, how to avoid?

Post by kdog » Dec 10 2016 5:09pm

Don't pull the power out of one single point- undoes all your work. I like to solder/weld multiple smaller copper wires/strips on to the nickel (say 2-3 in your case ) in different spots and bring them out to the main lead.

User avatar
madin88   1 GW

1 GW
Posts: 3099
Joined: May 27 2013 2:02am
Location: Austria

Re: Common pack design mistakes, how to avoid?

Post by madin88 » Dec 11 2016 6:31am

thats what i do for better protection against a short between the groups when i arrange the cells in honeycomb shape:

Image

Image

here a few pics of how i weld my packs:

Image

Image

Image

for a well balanced current flow through every single cell i do this:

Image

Image

last but not least the shell made plastic brackets and fiberglass sheets, fuse and connectors (with antispark function):

Image

Image

Image
Last edited by madin88 on Dec 11 2016 7:00am, edited 2 times in total.
- 10kW belt drive with Neumotor 8057: [url]viewtopic.php?
- KTM Hardtail Pedelec / eZee V2 6T / 27,5" / Kelly KBSX @ 1,5kW / Torque PAS / CA-V3 / 13s4p Sanyo GA in Shark case

User avatar
madin88   1 GW

1 GW
Posts: 3099
Joined: May 27 2013 2:02am
Location: Austria

Re: Common pack design mistakes, how to avoid?

Post by madin88 » Dec 11 2016 6:46am

Building packs like this is very time consuming, but with the additional protection against a short and the balanced current flow through every single cell, lifetime should be ahead compared to cheap made stuff.
Equal current flow is one of the most impartant things for a well balanced pack. If not done right, it could be that in one group of parallel cells, one cell sees for instance 10A and another 15A due to big differences in resistance. I think i must not explain that aging and wear on the cells than is not similar anymore, and sooner or later the pack will drift apart.
- 10kW belt drive with Neumotor 8057: [url]viewtopic.php?
- KTM Hardtail Pedelec / eZee V2 6T / 27,5" / Kelly KBSX @ 1,5kW / Torque PAS / CA-V3 / 13s4p Sanyo GA in Shark case

User avatar
madin88   1 GW

1 GW
Posts: 3099
Joined: May 27 2013 2:02am
Location: Austria

Re: Common pack design mistakes, how to avoid?

Post by madin88 » Dec 11 2016 7:04am

this could happen if the series sheets are to small dimensioned (or to high-ohmic) for the current flow
the pack was wrapped with foam so heat flow to outside was not good. you can see the black areas where the foam has melted and stick to the sheets.
it is ONLY 3p of low current cells (15A controller)

Image
- 10kW belt drive with Neumotor 8057: [url]viewtopic.php?
- KTM Hardtail Pedelec / eZee V2 6T / 27,5" / Kelly KBSX @ 1,5kW / Torque PAS / CA-V3 / 13s4p Sanyo GA in Shark case

User avatar
Allex   1 GW

1 GW
Posts: 3272
Joined: Dec 05 2011 8:46am
Location: Stockholm, Sweden

Re: Common pack design mistakes, how to avoid?

Post by Allex » Dec 11 2016 7:56am

Thats some battery porn there, amazing!
Do you unload the stress on the standing cells on the pottom of the pack in some way? It cannot be good if the positive side of the cell is subjected to vibration and its own weght during the ride. We have an insulator between negative and postive on the battery can so it is best to leave it alone and not stress it. So some type of battery holder is also a very good tool to use.

User avatar
madin88   1 GW

1 GW
Posts: 3099
Joined: May 27 2013 2:02am
Location: Austria

Re: Common pack design mistakes, how to avoid?

Post by madin88 » Dec 11 2016 1:28pm

Allex wrote:Thats some battery porn there, amazing!
thanks mate :)
i build my packs in view of an owner and not in view of a company. that may say all.
Do you unload the stress on the standing cells on the pottom of the pack in some way? It cannot be good if the positive side of the cell is subjected to vibration and its own weght during the ride. We have an insulator between negative and postive on the battery can so it is best to leave it alone and not stress it. So some type of battery holder is also a very good tool to use.
you are talking about the insualtion between + and - inside the cell, right? honestly, i never have thought about that..
It looks like the can is very stiff at this area and i believe it would need quite high abuse to deform the roundness.
Yes, it would not be good if the shape would always varie a tiny little bit under the own weight, or when subjected to vibrations.
This probabaly could destroy the sealing and the insulation.

On the batteries i build, i normally stick plastic angles to the outer edges by using plenty of glue. thats special glue which stays flexible. between the angles on tehe large surfaces, i glue fiber glass plates.
The side, where all the wires are soldered and routed, i put wood profiles underneath the plastic angles - mainly for getting a constant gap and seating for the plastic angles.

I don't know what may happen if i need to disasemble one of that batteries one day, but it might well be that when removing the plates, the welded sheets could come off from the cells. Furtunately there was no need to do this yet :)
- 10kW belt drive with Neumotor 8057: [url]viewtopic.php?
- KTM Hardtail Pedelec / eZee V2 6T / 27,5" / Kelly KBSX @ 1,5kW / Torque PAS / CA-V3 / 13s4p Sanyo GA in Shark case

litespeed   100 kW

100 kW
Posts: 1438
Joined: Aug 11 2010 4:42pm
Location: O’Fallon, Missouri

Re: Common pack design mistakes, how to avoid?

Post by litespeed » Dec 11 2016 1:56pm

Maddin88,

That is some excellent well thought out battery builds.....as I said before, that is why I copied your design for my build.

Are you still using .2 nickel?

Have you given any thought to using copper or brass on future battery builds to lower the resistance further? Have you tried to weld either with your DN5 (10?) that you have?

Tom
I'm married so you know I'm no stranger to pain!

Voltron   100 MW

100 MW
Posts: 2969
Joined: May 02 2013 4:53pm
Location: Santa Barbara CA

Re: Common pack design mistakes, how to avoid?

Post by Voltron » Dec 11 2016 7:29pm

So after learning a lot from this thread, I'm going to have to guess this is not ideal current share...

It looks OK from one side (except for the broken off balance wire!)... Three strips for each 6p group, but then only one strip to join the oddball end cluster.
KIMG0110-640x360.JPG
KIMG0110-640x360.JPG (84.38 KiB) Viewed 3265 times

But the other side all the series connects are just one nickel strip? (Oh yeah, and the other broken off balance wire.)
KIMG0112-640x360.JPG
KIMG0112-640x360.JPG (84.73 KiB) Viewed 3265 times

Should this be a pack that comes on a $5400US turnkey bike?

Voltron   100 MW

100 MW
Posts: 2969
Joined: May 02 2013 4:53pm
Location: Santa Barbara CA

Re: Common pack design mistakes, how to avoid?

Post by Voltron » Dec 11 2016 9:30pm

Lots of welds right in the center of the negatives too :(

User avatar
fechter   100 GW

100 GW
Posts: 15098
Joined: Dec 31 2006 3:23pm
Location: California Bay Area, USA

Re: Common pack design mistakes, how to avoid?

Post by fechter » Dec 11 2016 10:21pm

Voltron wrote:So after learning a lot from this thread, I'm going to have to guess this is not ideal current share...

It looks OK from one side (except for the broken off balance wire!)... Three strips for each 6p group, but then only one strip to join the oddball end cluster.
But the other side all the series connects are just one nickel strip? (Oh yeah, and the other broken off balance wire.)

Should this be a pack that comes on a $5400US turnkey bike?
Thanks for sharing the imbalanced sharing. Yes, how not to build a pack. But it was less labor to build it that way and I guess it must have worked for a while. At really low currents, the layout is less critical. If this was running at 10A or less, it might be justifiable.
"One test is worth a thousand opinions"

Voltron   100 MW

100 MW
Posts: 2969
Joined: May 02 2013 4:53pm
Location: Santa Barbara CA

Re: Common pack design mistakes, how to avoid?

Post by Voltron » Dec 12 2016 12:33am

Luckily the balance wires broke off and shut the system down before the cells died... I'm planning on cutting it up and reconfiguring it with more series connections.

It was hooked to a big Clyte DD hub in a 26 inch wheel on an 80 pound bike.

(Just to be clear, I didn't have any part in making that pack or choosing what to run it on :D )

User avatar
Allex   1 GW

1 GW
Posts: 3272
Joined: Dec 05 2011 8:46am
Location: Stockholm, Sweden

Re: Common pack design mistakes, how to avoid?

Post by Allex » Dec 12 2016 3:04am

madin88 wrote: you are talking about the insulation between + and - inside the cell, right?
Yeah, the button top itself, I don't think we should neglect this detail.

atol77   10 µW

10 µW
Posts: 5
Joined: Jan 07 2017 5:43pm

Re: Common pack design mistakes, how to avoid?

Post by atol77 » Jan 27 2017 10:37am

Hello,

What is this on the picture ??
Image

Thanks

User avatar
madin88   1 GW

1 GW
Posts: 3099
Joined: May 27 2013 2:02am
Location: Austria

Re: Common pack design mistakes, how to avoid?

Post by madin88 » Jan 27 2017 10:45am

atol77 wrote:Hello,

What is this on the picture ??

Thanks
this is a mini-anl fuse (here 2x 100A one upon the other so 200A)
- 10kW belt drive with Neumotor 8057: [url]viewtopic.php?
- KTM Hardtail Pedelec / eZee V2 6T / 27,5" / Kelly KBSX @ 1,5kW / Torque PAS / CA-V3 / 13s4p Sanyo GA in Shark case

User avatar
skeetab5780   10 MW

10 MW
Posts: 2432
Joined: Jun 15 2009 10:58pm
Location: MA
Contact:

Re: Common pack design mistakes, how to avoid?

Post by skeetab5780 » Jan 27 2017 11:21am

madin88 wrote:
atol77 wrote:Hello,

What is this on the picture ??

Thanks
this is a mini-anl fuse (here 2x 100A one upon the other so 200A)
Those are common in car stereo systems for protection of the positive wire going to the amplifier from the battery. You can typically buy them at Walmart for $5

kundvagn   1 mW

1 mW
Posts: 15
Joined: Jul 07 2015 2:41pm
Location: Skåne, Sweden

Re: Common pack design mistakes, how to avoid?

Post by kundvagn » Feb 04 2017 7:44am

Hi all,

I'm currently in the process of building a battery pack for my FUTR Beta.

My plan it to have 7 smaller 8P subpacks, connected in series.

3S+3S+3S+3S+4S+2S+2S for a total of 20S and 8P (160 cells)

The cells I chosen is Samsung 30Qs with a max continuos current of 15A (8P x 15A=120A)
I will use 8AWG wires with XT150 connectors. And 10mm x 0,15mm nickelstrips for welding (Double or triple?)

The sub packs will have the cells arranged in a honey comp pattern using the brackets seen on the attached image and heat resistant double-sided tape to keep them in place.
subpack_small.jpg
Subpack prototype before going with 8P instead.
I havent seen any other battery builds made this way. And maybe there is good reason for that. I just havent found one yet. ;)

For me there a couple of reasons I like build it this way.
- Smaller subpacks is easier to troubleshoot, and a temporary fix is to remove a misbehaving subpack. And the cells will be easier to get out.
- The Adaptto BMS has a limit of 4S per BMS module. So it will make my life easier when connecting the subpacks to BMS.
- It easier to get the more cells in to the frame and still have a good current flow within every subpack.

I like the design myself, but as I'm new to this and I feel I'm about to make a mistake. For example will the total pack performance suffer from all the extra wiring (high interna resistance) between the subpacks?

But I havent started welding yet, so please stop me before I do something stupid. And maybe help someone else so they wont make the same misstake. :)
FUTR Beta / Leaf 35mm / Adaptto Midi-E / 22s6p 30q

litespeed   100 kW

100 kW
Posts: 1438
Joined: Aug 11 2010 4:42pm
Location: O’Fallon, Missouri

Re: Common pack design mistakes, how to avoid?

Post by litespeed » Feb 04 2017 1:34pm

You will actually want to do 4s modules instead of 3s for wiring simplicity. You would have to make a special harness to convert your 3s balance taps to 4s which would require way to many connections. My pack I built before having a MaxE was 3 separate 8s15p and when I went to a MaxE I hade to make a generally straight forward 8s to 2--4s balance wire adaptor.

Yours would be really confusing in my opinion but could be done.

23mm wide strips work great. They cover the positive and negative to make the series and parallel connections. Much cleaner and less connections. This also allows for more current draw. I used .2 mm for mine. I welded a 23mm strip on the end cells and then folded it over so it had the same current carrying capabilities.

Since I've had to replace a couple cells I'd tell you to not use tape. My next pack I'll glue the parallel cells together in a row but only the nickel (or brass or copper if I figure out how to weld that!) will hold the parallel groups together. Then tightly foam and tape the whole pack together. Then heat shrink. That will make maintenance if needed so much easier. It's always the cell in the middle that goes out....ask me how I know?

Have fun with it.

Tom
Attachments
IMG_0573.JPG
I'm married so you know I'm no stranger to pain!

Valld   10 mW

10 mW
Posts: 23
Joined: Dec 06 2016 8:03am

Leady Solar Busbar Wire 6mm X0.2mm

Post by Valld » Feb 06 2017 1:31am

Maybe not the best thread to discuss spot welder strips material, please move to the appropriate place if you think it doesn't belong here.... Looking for different metal strips I found this :

https://www.aliexpress.com/store/produc ... 0.0.h8KLPr

What do you guys think about it as an alternative to pure nickel strips? It is a strip with a good dimensions (6 x 0.2 mm) pure copper core with solder coating. Do you think it will weld good to battery tabs and carry better current than nickel strip? Or I'm talking non sense :D It's price is also very good, much cheaper than the nickel. Would the 6 pence welder be able to weld this?