Dear forum friends,

As the topic say I'm get sick off the BMS problems that shutdown the battery!!!!!

Is there some kind of information or book where I can learn about bms's??
I'm not a electronic guy but want and need to learn solving problems.

Where Can I find it?


I'm not the only one with this problem???

Joost

User avatar
Matador   10 kW

10 kW
Posts: 890
Joined: Jun 29 2016 10:00pm

Re: BMS's i get sick of it too understand what the problem i

Post by Matador » Mar 31 2017 1:03pm

My guess is one of your battery string might not be well balanced. Maybe one string is way below average cell voltage. So when that weak group hits LVC it triggers down the whole BMS to shut down in order to protect the battery from over-discharging some cells. That's my guess but maybe more details as to how it happens may help in the diagnosis process.

Joost   1 W

1 W
Posts: 54
Joined: Mar 31 2014 12:53pm

Re: BMS's i get sick of it too understand what the problem i

Post by Joost » Apr 02 2017 5:18am

Thank you for your answer.

The battery pack holds 2x 13s8p li-ion cells.
Every part has its own BMS. Too charge the battery pack I connected both BMS on one charge input.
The problem came after I charged every group on both parts. After finishing it I took a drive around 15Km. Then I hook it on the charger 54,4V 2A. It starts charging without problems.
The next day I disconnected it and want too make a test drive. I could drive 1Km and shuts down.

With your suggestion in mind i think it is a balancing issue.
On YouTube is saws a video about bottom balancing.

Are here people who have experienced with bottom balancing?

999zip999   100 GW

100 GW
Posts: 8933
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: BMS's i get sick of it too understand what the problem i

Post by 999zip999 » Apr 02 2017 11:54am

You start by knowing the state of charge your battery. So write on paper the voltage of each cell like this.
1. 3.85v
2. 3.99v
3. 4.02v


13. Xxx volt
This is where to start. Post here.

Joost   1 W

1 W
Posts: 54
Joined: Mar 31 2014 12:53pm

Re: BMS's i get sick of it too understand what the problem i

Post by Joost » Apr 11 2017 12:06am

The problem is unbalanced cells. Li-ion charged at 4,2v

User avatar
neptronix   100 GW

100 GW
Posts: 13968
Joined: Jun 15 2010 5:56pm
Location: California refugee living in Utah, USA
Contact:

Re: BMS's i get sick of it too understand what the problem i

Post by neptronix » Apr 11 2017 3:08am

Much like a car, it's hard to fix a problem without knowing what could cause it.
A properly designed BMS will shut down pack output when one cell has hit too high or too low a voltage.

A pack that cannot handle the load will cut off early.

What are your per cell measurements when the pack has shut down, and how far does the voltage drop between the time you have the throttle at 0% and the bike is at full load ( IE climbing a hill or accelerating ) ?
Efficiency is everything :bolt:

My first major build: 1.6kW 8T MAC motor on a Trek 4500.
The new all-arounder: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: 20" eZee on a Cannondale Semi Recumbent.
Whipper-snapper: ? on a lightweight BikeE Semi Recumbent

User avatar
amberwolf   100 GW

100 GW
Posts: 27554
Joined: Aug 17 2009 6:43am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: BMS's i get sick of it too understand what the problem i

Post by amberwolf » Apr 11 2017 3:36am

Joost wrote:The problem is unbalanced cells.
If you already know the problem is unbalanced cells, then you should fix that, because the BMS is just doing it's job of protecting the cells against overdischarge or overcharge.

Either let the BMS balance the cells or manually do so, then check under a load (acceleration or hill climbing, or simulated load (see "load tester" in various threads around ES, including things like "heater coils", lights, etc).


Then replace the cells that wont' stay balanced, or that sag more than others under that load.

That will fix the problem of cutting out under load.


For more understanding about the problem you are having, look around at the dozens (hundreds?) of battery troubleshooting threads.

User avatar
Ykick   100 GW

100 GW
Posts: 5558
Joined: Nov 26 2009 6:10pm
Location: San Diego, California

Re: BMS's i get sick of it too understand what the problem i

Post by Ykick » Apr 11 2017 8:44am

Folks who wanna learn more about these sorts of battery systems often find RC planes, heli’s, cars, boats a great way to have fun while learning key basic fundamentals.

I’d find a model type you might like then outfit with RC balance charger and Lipo packs. Dig in and have fun while you get an education about manually managing series cell groups. Aided with a little equipment you become the BMS which is the best way IMO to learn how BMS are supposed to work...
Talent must not be wasted.... Those who have talent must hug it, embrace it, nurture it and share it lest it be taken away from you as fast as it was loaned to you.

- Frank Sinatra

User avatar
neptronix   100 GW

100 GW
Posts: 13968
Joined: Jun 15 2010 5:56pm
Location: California refugee living in Utah, USA
Contact:

Re: BMS's i get sick of it too understand what the problem i

Post by neptronix » Apr 11 2017 10:37am

No kidding. Watching the cells do their thing on an iCharger 1010b+ using logview on my PC taught me half of what i know about batteries. Simply an amazing teaching tool.

A BMS is basically the opposite. It's a circuit board with some wires coming out of it that tells you nothing about what decisions it's making or why it's making them.
Efficiency is everything :bolt:

My first major build: 1.6kW 8T MAC motor on a Trek 4500.
The new all-arounder: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: 20" eZee on a Cannondale Semi Recumbent.
Whipper-snapper: ? on a lightweight BikeE Semi Recumbent

User avatar
neptronix   100 GW

100 GW
Posts: 13968
Joined: Jun 15 2010 5:56pm
Location: California refugee living in Utah, USA
Contact:

Re: BMS's i get sick of it too understand what the problem i

Post by neptronix » Apr 11 2017 10:40am

neptronix wrote:No kidding. Watching the cells do their thing on an iCharger 1010b+ using logview on my PC taught me half of what i know about batteries. Simply an amazing teaching tool.

A BMS is basically the opposite. It's a circuit board with some wires coming out of it that tells you nothing about what decisions it's making or why it's making them.
At least getting some measurements of voltage sag and amp hours delivered from a turnigy watt meter or equivalent device is a start on figuring out what the hell is going on with a BMSed battery.
Efficiency is everything :bolt:

My first major build: 1.6kW 8T MAC motor on a Trek 4500.
The new all-arounder: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: 20" eZee on a Cannondale Semi Recumbent.
Whipper-snapper: ? on a lightweight BikeE Semi Recumbent

k-harvey   100 W

100 W
Posts: 265
Joined: Aug 05 2011 4:47pm
Location: New Zealand

Re: BMS's i get sick of it too understand what the problem i

Post by k-harvey » Apr 15 2017 7:05pm

My first troubles with lithium batteries were BMS being the cheapest was only for low current & needed a higher current BMS . I've replaced heaps because of this.

Joost   1 W

1 W
Posts: 54
Joined: Mar 31 2014 12:53pm

Re: BMS's i get sick of it too understand what the problem i

Post by Joost » Apr 22 2017 12:31am

Hello again,

After many tries too read and write too the smart BMS with many different dongles I bought the expansive smartBMS own sub O2Micro i2c dongle.

I tried:

RUSB3410
Pikkit icd 2
Profilic 23xx
Ftdi rs232
Rfduino

Nothing worked. All of the dongles has not the good vid id. Is there a way to manipulate drivers under Windows too fake the cowboy oz890 program?

Joost   1 W

1 W
Posts: 54
Joined: Mar 31 2014 12:53pm

Re: BMS's i get sick of it too understand what the problem i

Post by Joost » Apr 28 2017 2:28am

Solved!!!

It's the Smart BMS.... I have another one but I'm scared too use it. I don't want to loose another one.....

Post Reply