I ordered.15mm thickx8mmwx1kg roll of PURE nickel welding strip... I received EXACTLY what I ordered.. what more can you ask...price, excellent...$45.00 us plus shipping..he also has other sizes ... email... tob.gavin@tobmachine.com
Got this 11.11 discount day 48$ + Free shipping, tested and was pure.
https://www.aliexpress.com/item/0-15-7mm-pure-nickel-strip-0-15mm-thickness-7mm-width/1316380630.html
be carefull.. I ordered from an alliexpress seller\Alisha\ about 2months ago.. ad looks the same.. pure nikel athe start of thr message which then says pure nickel plate... I ordered.15mmtx8mmwx1kg PURE NICKEL..... i received .3mmtx4mmwx 1kg of nickel plated STEEL.. neither the seller nor aliexpress offered refund or exchange... there are a lot of ads on aliexpress that read similar they never say nickel plated steel,just pure nickel plate
Store name E-bike Lithium Battery adding a little trust. They should know what they are selling.
See feedback messages, people report there that they tested and nickel was pure, including me.