I had a couple of odd things happen with a smart BMS this week.
1. Cell voltages were all in the 3.5 to 3.7v range. There was no over current or low pack or cell voltage condition, but the P- mosfets shut off anyway. It was kind of weird. They turned off once and then right back on again. A minute later they did it again 3 times in rapid succession. I then stopped and tried the throttle once more, which worked for a second and then the BMS stayed off. checking the BMS status didn't show anything wrong.

2. Last night, same BMS, on the dashboard it was displaying LT and the P- mosfets were off. Since the BMS is on LIPO packs, I had the HVC recovery voltage set to 4.2 volts. No cell was above 4v. I then set HVC to 4.1 volts and the LT disappeared and the mosfets enabled.

This BMS has been working well for quite a while now.
XB-502: viewtopic.php?f=10&t=83302&p=1222730#p1222730

Currie scooter: viewtopic.php?f=35&t=83830&p=1227407#p1227407

Benjamin Franklin - "Any fool can criticize, condemn and complain and most fools do."

User avatar
trazor   100 W

100 W
Posts: 153
Joined: Jan 13 2015 10:48pm
Contact:

Re: bluetooth BMS?

Post by trazor » Nov 14 2018 2:46pm

Non important observation: the xiaoxiang app that connects to these BMS stole the logo from a more prominent project: https://hadoop.apache.org/ :lol: China shameless programmers. :roll:

User avatar
ElectricGod   100 MW

100 MW
Posts: 2851
Joined: Nov 01 2015 5:24pm
Location: 3 OH 3

Re: bluetooth BMS?

Post by ElectricGod » Nov 14 2018 6:26pm

trazor wrote:
Nov 14 2018 2:46pm
Non important observation: the xiaoxiang app that connects to these BMS stole the logo from a more prominent project: https://hadoop.apache.org/ :lol: China shameless programmers. :roll:
You never know...maybe inside those atmel 328 processors these BMS use is a subspace link into AWS.
XB-502: viewtopic.php?f=10&t=83302&p=1222730#p1222730

Currie scooter: viewtopic.php?f=35&t=83830&p=1227407#p1227407

Benjamin Franklin - "Any fool can criticize, condemn and complain and most fools do."

User avatar
trazor   100 W

100 W
Posts: 153
Joined: Jan 13 2015 10:48pm
Contact:

Re: bluetooth BMS?

Post by trazor » Nov 14 2018 6:54pm

ElectricGod wrote:
Nov 14 2018 6:26pm
trazor wrote:
Nov 14 2018 2:46pm
Non important observation: the xiaoxiang app that connects to these BMS stole the logo from a more prominent project: https://hadoop.apache.org/ :lol: China shameless programmers. :roll:
You never know...maybe inside those atmel 328 processors these BMS use is a subspace link into AWS.
Yeah, probably there is a bitcoin miner working at nights. That will explain last weird behaviour of your bms and the strange efficiency measurements :lol:

EbikeAus   100 W

100 W
Posts: 267
Joined: Feb 04 2018 5:58am

Re: bluetooth BMS?

Post by EbikeAus » Nov 14 2018 7:35pm

Just reporting that the app seems to connect perfectly fine with my new Samsung s9, seems to connect quicker than my old s5 :D
Choose LiFe 8)

May all your batteries be fully charged and perfectly balanced :P

User avatar
ElectricGod   100 MW

100 MW
Posts: 2851
Joined: Nov 01 2015 5:24pm
Location: 3 OH 3

Re: bluetooth BMS?

Post by ElectricGod » Nov 14 2018 11:20pm

EbikeAus wrote:
Nov 14 2018 7:35pm
Just reporting that the app seems to connect perfectly fine with my new Samsung s9, seems to connect quicker than my old s5 :D
THat's expected...faster phone.
XB-502: viewtopic.php?f=10&t=83302&p=1222730#p1222730

Currie scooter: viewtopic.php?f=35&t=83830&p=1227407#p1227407

Benjamin Franklin - "Any fool can criticize, condemn and complain and most fools do."

mario1122   1 µW

1 µW
Posts: 4
Joined: Aug 08 2015 10:09am

Re: bluetooth BMS?

Post by mario1122 » Nov 15 2018 9:04am

Here is an app to monitor/control multiple BMS devices in one battery pack:
https://mono.software/2018/11/15/multiple-bms-monitor/

User avatar
eee291   10 kW

10 kW
Posts: 996
Joined: Nov 05 2015 4:35pm
Location: Austria, Burgenland

Re: bluetooth BMS?

Post by eee291 » Nov 15 2018 11:57am

mario1122 wrote:
Nov 15 2018 9:04am
Here is an app to monitor/control multiple BMS devices in one battery pack:
https://mono.software/2018/11/15/multiple-bms-monitor/
Thanks for making this :thumb:
I'm sure I will need this someday.

A few different dashboard layouts would be cool, like raw values for battery current instead of an x10 multiplier.

User avatar
ElectricGod   100 MW

100 MW
Posts: 2851
Joined: Nov 01 2015 5:24pm
Location: 3 OH 3

Re: bluetooth BMS?

Post by ElectricGod » Nov 22 2018 11:32pm

mario1122 wrote:
Nov 15 2018 9:04am
Here is an app to monitor/control multiple BMS devices in one battery pack:
https://mono.software/2018/11/15/multiple-bms-monitor/
I finally got around to reading your thread on this app. Any chance you would be willing to make an APK? I do software development so I understood what you are doing here. BUT, lots of folks are not so inclined or are tech incapable. An APK would make using your app much easier for everyone.
XB-502: viewtopic.php?f=10&t=83302&p=1222730#p1222730

Currie scooter: viewtopic.php?f=35&t=83830&p=1227407#p1227407

Benjamin Franklin - "Any fool can criticize, condemn and complain and most fools do."

Alex07   100 W

100 W
Posts: 137
Joined: Jun 27 2016 4:00am

Re: bluetooth BMS?

Post by Alex07 » Nov 30 2018 3:47am

Hi i have the xiaoxing bms. Why does the bms sometimes pulse on cell overvoltage rappidly ? When near end of charge ? I.e it doesnt just stop at the end it pulses...

Also how to fix this? Is it a setting in bms or is the voltage in the charger too high ?

Does it stop chargeing only when one cell is high ? Or does it also stop if pack voltage is correct ?

Also for the open balance option. What does this open or close option mean ?

Is their any downside to always useing a static balance ? This is an old pack and charge balance is not good enough to keep it balance.

Does anyone get resistance readings as i dont ?

User avatar
izeman   10 GW

10 GW
Posts: 4929
Joined: Jun 21 2011 8:25am
Location: vienna, austria
Contact:

Re: bluetooth BMS?

Post by izeman » Nov 30 2018 3:51am

Alex, no offense, but have you tried reading the whole thread? Many ppl wrote down all their knowledge here for reference.
All but your first question are answered already. And i've never seen issue #1 happen with my BMS, sorry.

User avatar
eee291   10 kW

10 kW
Posts: 996
Joined: Nov 05 2015 4:35pm
Location: Austria, Burgenland

Re: bluetooth BMS?

Post by eee291 » Nov 30 2018 5:16am

I have experienced the Pulse thing.

It happens when you set overvolt cut-off to 4.2V and overvolt recovery to 4.18V or something like that.
So while charging your cell(s) reaches 4.2V and the BMS cuts off the charger, then the Cell voltage drops down to something like 4.17V and the BMS enables the charge again and that's how you get the pulsing effect.

The solution: Change the overvolt recovery voltage to some lower value like 4.15V or 4.1V

BotoXbz   10 W

10 W
Posts: 90
Joined: May 20 2018 7:00am

Re: bluetooth BMS?

Post by BotoXbz » Nov 30 2018 12:03pm

Btw. I wrote some open source firmware for the LLT bluetooth BMS to use it in a Xiaomi M365 scooter (scooter requires battery with proprietary communication protocol): https://github.com/BotoX/xiaomi-m365-compatible-bms
Might be of interest for some people here.

User avatar
tmho   100 W

100 W
Posts: 287
Joined: Jan 09 2011 3:25pm
Location: Richmond, BC, Canada

Re: bluetooth BMS?

Post by tmho » Dec 03 2018 11:38am

I recently bought one Bluetooth BMS from taobao.com. But the seller is not that helpful and so I need to get help from here.

Below are some photos of it.
IMG_1375a.jpg
Photo 1: my Bluetooth bms with heatsink or cover on both top and bottom
IMG_1377a.jpg
Photo 2: bms with top cover removed
IMG_1379a.jpg
Photo 3: bms with bottom cover removed
This bms will be put inside a battery case which has very limited space for bms. Even thought I plan to give up the space of 9 x 18650 cells for it, I still need to cut away a small piece (about 2 x 4mm) of the PCB on two sides as marked in red on the below photo 4. I guess it is okay to do because there is no components and/or circuits nearby. But I am not an expert, therefore, I contacted the seller and ask them if it is okay to do so. The seller only said no and refused to tell me the reason why. Now, I would like somebody from this forum to comment on whether it is okay to do so. If no, please explain the reason so that I can learn something.
IMG_1407a.jpg
Photo 4: the red circles indicate the area that I need to cut
Also, I only got the Chinese instructions and Bluetooth app from the seller. I can understand Chinese but the English ones will be much better for me. If any body has the English version of installation instructions and Bluetooth app, please send me a copy.

Originally, I plan to ask the factory directly on the above questions. But I could not find the website and contact information of the factory from the internet. This bms should be from the same factory as the one with photos posted by ElectricGod on Sep 11, 2018 (https://endless-sphere.com/forums/viewt ... &start=700). If anybody knows about the factory contact and website, please advise.

User avatar
izeman   10 GW

10 GW
Posts: 4929
Joined: Jun 21 2011 8:25am
Location: vienna, austria
Contact:

Re: bluetooth BMS?

Post by izeman » Dec 03 2018 2:05pm

The top and bottom side of the PCB copper are connected to each other. You can see this, because there are small holes with copper inside. You can check that with a DMM. And if this is the case there should be NO PROBLEM to cut out these small rectangles. You will remove a bit of the copper but this should be no problem at all. Especially as you connected two wires on each side balancing the load.

User avatar
tmho   100 W

100 W
Posts: 287
Joined: Jan 09 2011 3:25pm
Location: Richmond, BC, Canada

Re: bluetooth BMS?

Post by tmho » Dec 04 2018 3:54am

izeman wrote:
Dec 03 2018 2:05pm
The top and bottom side of the PCB copper are connected to each other. You can see this, because there are small holes with copper inside. You can check that with a DMM. And if this is the case there should be NO PROBLEM to cut out these small rectangles. You will remove a bit of the copper but this should be no problem at all. Especially as you connected two wires on each side balancing the load.
Hi izeman, thanks for your comment. I have checked that accordingly, and you are correct that the top and bottom side of the PCB copper are connected to each other.

User avatar
izeman   10 GW

10 GW
Posts: 4929
Joined: Jun 21 2011 8:25am
Location: vienna, austria
Contact:

Re: bluetooth BMS?

Post by izeman » Dec 04 2018 4:36am

I personally just would cut it. But that's my personal opinion only. ;)

User avatar
tmho   100 W

100 W
Posts: 287
Joined: Jan 09 2011 3:25pm
Location: Richmond, BC, Canada

Re: bluetooth BMS?

Post by tmho » Dec 04 2018 4:51am

izeman wrote:
Dec 04 2018 4:36am
I personally just would cut it. But that's my personal opinion only. ;)
I will cut it accordingly.

User avatar
izeman   10 GW

10 GW
Posts: 4929
Joined: Jun 21 2011 8:25am
Location: vienna, austria
Contact:

Re: bluetooth BMS?

Post by izeman » Dec 04 2018 5:35am

izeman wrote:
Dec 04 2018 4:36am
I personally just would cut it. But that's my personal opinion only. ;)
You should add some isolation layer, because you expose the pcb layer to the outside, and you don't want any of the two sides touch the frame or each other!

User avatar
ElectricGod   100 MW

100 MW
Posts: 2851
Joined: Nov 01 2015 5:24pm
Location: 3 OH 3

Re: bluetooth BMS?

Post by ElectricGod » Dec 04 2018 1:44pm

I don't see any issues with cutting into that area with all the through holes in it that connect the traces on both sides of the board together. There is a slim chance that some tiny trace is inside a third layer of the board, but I seriously doubt it. There's far better ways to run something like that without having to pass between all those interconnect holes. I'd be willing to cut into those areas without worrying about causing issues.

I do have 2 things that I'd do in the process.
1. The power traces on a 100 amp board ought to have lots of copper on them. All I see here is the traces and solder on them. They really need copper added to them. That means copper at C-, P-, B- and right before the shunts. 14 awg copper wire commonly found in household wiring will do the trick. If you don't want to buy some Romex, I bet there is a construction site near by you that has scraps laying about that you could scavenge from.

2. Since you are undermining that interconnect section a fair bit by removing large portions of it, Use some more 14 awg wire to wrap around one side of the board to the other.

Note: Copper wire is round. However, copper is very ductile. That means it can be smashed and bent easily without compromising its integrity. Strip off the insulation from a length of wire and use a hammer to flatten the wire out. No harm done and this will lower it's profile on the board.
XB-502: viewtopic.php?f=10&t=83302&p=1222730#p1222730

Currie scooter: viewtopic.php?f=35&t=83830&p=1227407#p1227407

Benjamin Franklin - "Any fool can criticize, condemn and complain and most fools do."

User avatar
ElectricGod   100 MW

100 MW
Posts: 2851
Joined: Nov 01 2015 5:24pm
Location: 3 OH 3

Re: bluetooth BMS?

Post by ElectricGod » Dec 04 2018 1:56pm

I snagged your pics and blew them up a good bit to get a closer look. Sorry for the grainy pics.

Board top:


Image

Board bottom:

Image

Notice the red boxes. They are P- and this board has no direct way to let you solder a connection here. For power output to your EV, you want to use P- and NOT C-. P- is Power output and C- is Charge input....dumb to NOT have this! However, you can add P- to this BMS. 14 awg wire is handy stuff. Solder 2 strands of it on top of the mosfet tabs once you replace all the B- chinesium mosfets. If those 14 awg copper stands extend to the edge of the board, now you can solder onto them for P- access.

Notice the orange boxes on the board top. There are identical places on the bottom of the board too that I did not mark since the bottom is unpopulated. These areas are inadequate as is. They really need copper reinforcing...even for 100 amps.

Notice the blue box. It says "ANTBMS-16S". That gives you a clue to the manufacturer. The 24S and 32S smart BMS mentioned in this thread are also commonly referred to as "ANT BMS", but they use different components. I'm not sure, but it's possible the same app that works for the 24 and 32S versions will also work for this BMS. Worse case, google for ANTBMS-16S and see what you find.

This BMS is not like the other smart BMS's talked about here. It may come from the same factory, but I don't think so. See that single large IC on the board top? That's the charge controller. The smaller IC is possibly an atmel 328. It is unlikely that the same software we use for the smaller smart BMS discussed here will also work with this BMS. It's probable that the app for the larger ANT BMS's talked about here also won't work for your BMS.

This BMS has loads of potential for insane current handling. One whole side of the BMS is unpopulated. I bet that set of mosfets on there are garbage. Or if they are some well known mosfet, they are Chinesium versions. AKA, pull off all the mosfets on B- and replace with at least legit IRF4110's and then add a load more to the other side of the board on B-. You will be adding a bunch more .005 ohms shunts too. I bet with all of them being legit 4110's that this BMS could do 300 amps all day long. If you use larger shunts and better than IRF4110's...maybe 400 amps.

Of course if that 100A spec is already overkill for you, then don't bother. If it was my BMS, I'd be modding it. =)

Can you post the URL where you found this BMS please?
XB-502: viewtopic.php?f=10&t=83302&p=1222730#p1222730

Currie scooter: viewtopic.php?f=35&t=83830&p=1227407#p1227407

Benjamin Franklin - "Any fool can criticize, condemn and complain and most fools do."

User avatar
ElectricGod   100 MW

100 MW
Posts: 2851
Joined: Nov 01 2015 5:24pm
Location: 3 OH 3

Re: bluetooth BMS?

Post by ElectricGod » Dec 04 2018 2:58pm

One more post on this BMS...

Small components, board top:
The large IC in the orange box is the charge controller. I don't know what part it is. The red box looks like 2 DC-DC converters. Probably one supplies 5 volts and the other 12 volts. Under the grey thermal gap filler in the green box is a bunch of SMT resistors. I can't see them so I have no idea of their size or wattage. I bet they are .25 watt resistors or less. That would imply this BMS can do a max of about 1 amp balance current. What are those 2 connectors in the blue boxes. I have some 7S smart BMS's that have input and output connectors on them so that multiple BMS's can be daisy chained together. This allows you to have up to 22 of them in series or 154S. These connectors may serve the same purpose or they may support external balance boards so that this one BMS can control far more than 16 cells. The left connector has 3 pins and the right one 5. I see a single opto-isolator on the board and space for 3 more. Maybe the 5 pin connector is for an LCD in which case a single opto-isolator is all that's needed. If the 5 pin connector was used for connecting to another BMS, then TX and RX would be needed and that means at least 2 opto-isolators.

Image

Small components, board bottom:
The green box is a BT06 bluetooth module. This exact module is used on the 24S and 32S ANT BMS's, but is NOT used on the smaller smart BMS presented in this thread. The red box is an STM32 CPU. In my last post I thought it might be an atmel 328...that's incorrect. The STM32 is also used on the 24S and 32S ANT BMS's. The orange box is the active balance components. Those transistors are pretty small. No bigger than the ones used on the smaller smart BMS's. I suspect this BMS really balances at no more than 50mA...like they do.

Image
XB-502: viewtopic.php?f=10&t=83302&p=1222730#p1222730

Currie scooter: viewtopic.php?f=35&t=83830&p=1227407#p1227407

Benjamin Franklin - "Any fool can criticize, condemn and complain and most fools do."

User avatar
tmho   100 W

100 W
Posts: 287
Joined: Jan 09 2011 3:25pm
Location: Richmond, BC, Canada

Re: bluetooth BMS?

Post by tmho » Dec 04 2018 3:27pm

Hi ElectriGod, thanks for your comments.
Sorry, I am now in Asia. I will head for the airport for a 6-day trip in Malaysia in about an hour. Therefore, I only have time to post a short reply. But definitely will post more after the trip.

"Can you post the URL where you found this BMS"

I found it at https://item.taobao.com/item.htm?spm=a1 ... nfs4840103. But I don't suggest people buying from them because of the poor customer service and not professional enough as I mentioned in my first post.

There is another taobao seller selling the same bms but the price is higher, and the link is https://item.taobao.com/item.htm?spm=a1 ... 0867089295. And I think sooner or later, there should be sellers selling them in Ebay or Aliexpress.

User avatar
ElectricGod   100 MW

100 MW
Posts: 2851
Joined: Nov 01 2015 5:24pm
Location: 3 OH 3

Re: bluetooth BMS?

Post by ElectricGod » Dec 04 2018 6:41pm

tmho wrote:
Dec 03 2018 11:38am
If anybody knows about the factory contact and website, please advise.
I found your BMS on ebay.
https://www.ebay.com/itm/320A-7S-16S-8S ... 0169.m2942
XB-502: viewtopic.php?f=10&t=83302&p=1222730#p1222730

Currie scooter: viewtopic.php?f=35&t=83830&p=1227407#p1227407

Benjamin Franklin - "Any fool can criticize, condemn and complain and most fools do."

User avatar
ElectricGod   100 MW

100 MW
Posts: 2851
Joined: Nov 01 2015 5:24pm
Location: 3 OH 3

Re: bluetooth BMS?

Post by ElectricGod » Dec 04 2018 6:43pm

tmho wrote:
Dec 04 2018 3:27pm
Hi ElectriGod, thanks for your comments.
Sorry, I am now in Asia. I will head for the airport for a 6-day trip in Malaysia in about an hour. Therefore, I only have time to post a short reply. But definitely will post more after the trip.

"Can you post the URL where you found this BMS"

I found it at https://item.taobao.com/item.htm?spm=a1 ... nfs4840103. But I don't suggest people buying from them because of the poor customer service and not professional enough as I mentioned in my first post.

There is another taobao seller selling the same bms but the price is higher, and the link is https://item.taobao.com/item.htm?spm=a1 ... 0867089295. And I think sooner or later, there should be sellers selling them in Ebay or Aliexpress.
I'm familiar with taobao. If you are in Asia, they will sell to you, but the rest of the world...not so much.
Last edited by ElectricGod on Dec 05 2018 3:30pm, edited 1 time in total.
XB-502: viewtopic.php?f=10&t=83302&p=1222730#p1222730

Currie scooter: viewtopic.php?f=35&t=83830&p=1227407#p1227407

Benjamin Franklin - "Any fool can criticize, condemn and complain and most fools do."

Post Reply