houston, we have puffing. this is a bad battery, correct?

Batteries, Chargers, and Battery Management Systems.
Post Reply
augidog   10 W

10 W
Posts: 84
Joined: Sep 29 2012 11:49am

houston, we have puffing. this is a bad battery, correct?

Post by augidog » Dec 30 2017 2:26pm

....
Last edited by augidog on Jan 08 2018 3:44am, edited 1 time in total.

User avatar
liveforphysics   100 GW

100 GW
Posts: 14137
Joined: Oct 29 2008 1:48am
Location: Santa Cruz, CA, USA

Re: houston, we have puffing. this is a bad battery, correct?

Post by liveforphysics » Dec 30 2017 2:57pm

Use gloves to put it in a bag and drop it off at a place that does battery recycling if it smells sickly sweet like cherries from a jar.
Each carcinogen vapor exposure includes a dice roll for cancer.

Each mutagen vapor exposure includes a dice roll for reproductive genetic defects in your children.

Each engine start sprays them into a shared atmosphere which includes beings not offered an opportunity to consent accepting these cancer experiences and defective genetics life experiences.

Every post is a free gift to the collective of minds composing the living bleeding edge of LEV development on our spaceship.

augidog   10 W

10 W
Posts: 84
Joined: Sep 29 2012 11:49am

Re: houston, we have puffing. this is a bad battery, correct?

Post by augidog » Dec 30 2017 3:20pm

....
Last edited by augidog on Jan 08 2018 3:45am, edited 1 time in total.

User avatar
wesnewell   100 GW

100 GW
Posts: 7170
Joined: Jan 31 2011 6:25pm
Location: Wylie, TX, USA

Re: houston, we have puffing. this is a bad battery, correct?

Post by wesnewell » Dec 30 2017 3:24pm

Personally, I'd open it up and and see if I could depuff the cells inside. I've depuffed many a lipo pack. Resealed and used for years longer. Over a year ago, I used some 5 year old depuffed lipo packs to replace the sla batteries in one of my ups's. Still working like a champ today.
APC : 001,045,1039
DATE : 2017-12-30 14:27:05 -0600
HOSTNAME : mythfe0
VERSION : 3.14.12 (29 March 2014) debian
UPSNAME : Conext
CABLE : USB Cable
DRIVER : USB UPS Driver
UPSMODE : Stand Alone
STARTTIME: 2017-12-30 00:55:55 -0600
MODEL : Conext CNB750
STATUS : ONLINE
LINEV : 121.0 Volts
LOADPCT : 9.0 Percent
BCHARGE : 100.0 Percent
TIMELEFT : 49.4 Minutes
MBATTCHG : -1 Percent
MINTIMEL : -1 Minutes
MAXTIME : 0 Seconds
OUTPUTV : 120.0 Volts
SENSE : Medium
DWAKE : 0 Seconds
DSHUTD : 0 Seconds
LOTRANS : 96.0 Volts
HITRANS : 136.0 Volts
RETPCT : 0.0 Percent
ITEMP : 29.2 C
ALARMDEL : 30 Seconds
BATTV : 27.9 Volts
LINEFREQ : 60.0 Hz
LASTXFER : Low line voltage
NUMXFERS : 0
TONBATT : 0 Seconds
CUMONBATT: 0 Seconds
XOFFBATT : N/A
SELFTEST : NO
STESTI : None
STATFLAG : 0x05000008
MANDATE : 2003-10-13
SERIALNO : QC0342230498
BATTDATE : 2016-07-20
NOMOUTV : 120 Volts
NOMINV : 120 Volts
NOMBATTV : 24.0 Volts
NOMPOWER : 440 Watts
FIRMWARE : 811.r1b.D USB FW:r1
END APC : 2017-12-30 14:27:07 -0600
Need Advice? https://endless-sphere.com/forums/viewt ... =3&t=66302
Mongoose 26" Ledge 2.1 mtb bike $99, yescomusa.com 48V 1000W rear hub kit $200, Hua Tong 72V 40A controller $35, 10ah 24s lipo $217=~43mph, range=45 miles @ 20mph. 25K miles and still going strong.
Huffy Fortress 3.0 with MXUS 3000 4T motor, 24s lipo, 96V 60A controller. Total cost with extras <$700. Top speed ~50mph
My videos https://www.youtube.com/channel/UC0KW4U ... _G2wQhptMg

augidog   10 W

10 W
Posts: 84
Joined: Sep 29 2012 11:49am

Re: houston, we have puffing. this is a bad battery, correct?

Post by augidog » Dec 30 2017 3:30pm

....
Last edited by augidog on Jan 08 2018 3:45am, edited 1 time in total.

User avatar
flippy   1 MW

1 MW
Posts: 1690
Joined: Aug 12 2015 3:07pm

Re: houston, we have puffing. this is a bad battery, correct?

Post by flippy » Dec 30 2017 5:58pm

Just get rid of it. No sense putting your nuts near basically a small bomb. I love some action while driving but not that kind of action...
Lithium beats liquid dinosaurs.

User avatar
spinningmagnets   100 GW

100 GW
Posts: 11728
Joined: Dec 21 2007 10:27pm
Location: Ft Riley, NE Kansas

Re: houston, we have puffing. this is a bad battery, correct?

Post by spinningmagnets » Dec 30 2017 8:53pm

Looks like 24V, since its Lithium, perhaps it's 7S?

If you decide you'd like to discharge it, certainly do it outside. Use two 12V car filament bulbs in series, or a 120V / 40W lightbulb. Put it on concrete in a place where it will not hurt anything if it does go up in flames (or in an old steel barbecue?). Discharge it until there is no more light coming from the bulbs, then perhaps put it in a 5-gallon bucket overnight, covered with saltwater.

Look up some youtubes of "lipo fire" to see what the worst case scenario looks like.

augidog   10 W

10 W
Posts: 84
Joined: Sep 29 2012 11:49am

Re: houston, we have puffing. this is a bad battery, correct?

Post by augidog » Dec 30 2017 9:19pm

....
Last edited by augidog on Jan 08 2018 3:45am, edited 2 times in total.

User avatar
Rassy   10 MW

10 MW
Posts: 2077
Joined: Apr 08 2007 10:58am
Location: Eugene, Oregon USA

Re: houston, we have puffing. this is a bad battery, correct?

Post by Rassy » Dec 30 2017 10:18pm

I didn't see in this thread where it was mentioned that this is a LiFePO4 chemistry battery. That may temper some of the worries about the danger of spontaneous combustion, I think...

I remember seeing somewhere that a fully discharged LiFePO4 battery was acceptable to dispose of in the trash, but that was some years ago, so...

I also think discharging through the charge wires bypasses the LVC and would allow a full discharge, but again not sure...
-Rassy-

Two Delta Trikes equipped with a Bafang BBS02
viewtopic.php?f=28&t=88536&p=1291260#p1291260

augidog   10 W

10 W
Posts: 84
Joined: Sep 29 2012 11:49am

Re: houston, we have puffing. this is a bad battery, correct?

Post by augidog » Dec 30 2017 11:42pm

....
Last edited by augidog on Jan 08 2018 3:45am, edited 1 time in total.

User avatar
fechter   100 GW

100 GW
Posts: 14953
Joined: Dec 31 2006 3:23pm
Location: California Bay Area, USA

Re: houston, we have puffing. this is a bad battery, correct?

Post by fechter » Dec 31 2017 12:28am

Bad voltmeter?

Sometimes you can get what amounts to a small battery formed when the probe tip touches a dissimilar metal and there is electrolyte present. If you press the probe tip hard, this couldn't happen.
"One test is worth a thousand opinions"

User avatar
dogman dan   100 GW

100 GW
Posts: 35699
Joined: May 17 2008 12:53pm
Location: Las Cruces New Mexico USA

Re: houston, we have puffing. this is a bad battery, correct?

Post by dogman dan » Jan 01 2018 8:41am

It will be safe enough to chuck when the LVC shuts it off. Best taken to a landfill, and put in the recycle part of it. Your local one, like a county place, surely has a place to put your old lead battery. Take it there.

Any DC motor can discharge it. I like to put my old batteries on my lawnmower to discharge them fully before disposal.

augidog   10 W

10 W
Posts: 84
Joined: Sep 29 2012 11:49am

Re: houston, we have puffing. this is a bad battery, correct?

Post by augidog » Jan 01 2018 12:31pm

....
Last edited by augidog on Jan 08 2018 3:46am, edited 2 times in total.

augidog   10 W

10 W
Posts: 84
Joined: Sep 29 2012 11:49am

Re: houston, we have puffing. this is a bad battery, correct?

Post by augidog » Jan 03 2018 10:35am

....
Last edited by augidog on Jan 08 2018 3:49am, edited 1 time in total.

User avatar
thunderheart   100 W

100 W
Posts: 212
Joined: Oct 08 2017 10:01am
Location: Armenia

Re: houston, we have puffing. this is a bad battery, correct?

Post by thunderheart » Jan 03 2018 6:58pm

wesnewell wrote:
Dec 30 2017 3:24pm
Personally, I'd open it up and and see if I could depuff the cells inside. I've depuffed many a lipo pack. Resealed and used for years longer. Over a year ago, I used some 5 year old depuffed lipo packs to replace the sla batteries in one of my ups's. Still working like a champ today.
A couple of days ago i depuffed two of these cells. A month ago they were used for testing a newly arrived power bank PCB, which had applied 5-6V to them and they had puffed immediately. The voltage was 0.01V on one and 1.07V on the second. After resting a month (or more) i recovered them using Miboxer C4-12 charger. Now they are looking just like new ones and the capacity is fully recovered. They show the same results under 1A discharge rate as when they were new.
Yinlong LTO Lithium Titanate safety tests: https://youtu.be/eAUYbSDEy6I
Toshiba SCiB LTO Lithium Titanate safety tests:https://youtu.be/XsrRDZxEFQE

LG M50 vs Samsung 48G:https://youtu.be/KGJDogOG4zw
LiFePO4: QB26650 2500mAh 50A vs A123 ANR26650M1B: https://youtu.be/GOSkte11lRc

augidog   10 W

10 W
Posts: 84
Joined: Sep 29 2012 11:49am

Re: houston, we have puffing. this is a bad battery, correct?

Post by augidog » Jan 04 2018 12:14am

....
Last edited by augidog on Jan 08 2018 3:46am, edited 1 time in total.

User avatar
flippy   1 MW

1 MW
Posts: 1690
Joined: Aug 12 2015 3:07pm

Re: houston, we have puffing. this is a bad battery, correct?

Post by flippy » Jan 04 2018 6:07am

augidog wrote:
Jan 03 2018 10:35am
this thing will just not die. after it started shutting off with the 5W light bulb, i started using my RC Watts meter by itself, a .2W draw. whenever i check on it, it's shut down, i've never caught at what voltage. i reconnect the meter, and it's bounced back to 24.4V.
that means there is a BMS inside triggering low voltage. rip apart the top.
Lithium beats liquid dinosaurs.

augidog   10 W

10 W
Posts: 84
Joined: Sep 29 2012 11:49am

Re: houston, we have puffing. this is a bad battery, correct?

Post by augidog » Jan 04 2018 11:45am

....
Last edited by augidog on Jan 08 2018 3:46am, edited 1 time in total.

augidog   10 W

10 W
Posts: 84
Joined: Sep 29 2012 11:49am

Re: houston, we have puffing. this is a bad battery, correct?

Post by augidog » Jan 05 2018 11:28am

....
Last edited by augidog on Jan 08 2018 3:46am, edited 1 time in total.

markz   100 GW

100 GW
Posts: 10175
Joined: Jan 09 2014 11:38pm
Location: Alberta Canada

Re: houston, we have puffing. this is a bad battery, correct?

Post by markz » Jan 05 2018 6:29pm

I would take it to a Firehall that takes in that sort of thing. I dumped my remaining LiPo's off there. The place by me had paints and oils you could also drop off. Which reminds me I have a Ziplock bag full of primary batteries that need to be dropped off. Off Topic - After I fix the problem with my current ebike battery. Just odd, my range last night was real bad, after I left the bike outside for an hour it must've been only -5C and I got halfway home, steady slope of 3-5% for a mile. Then today I am cruising ebike style, and battery stops at the bottom of the hill. Call my chaffeur for a ride home and open errrrr up, 15S8P and I got 5 and 9 spot on A pack dead, with B pack having 2.2V and 2.9V and the rest 3.8, 3.9V and 4.1V.