I have a 7P20S battery with 140 cells and 3 of 20 of the series are not charging fully- it is about 9 months old and only done say 30 cycles. I am using a Adaptto Max-E Controller and BMS.

17 the cells are very close to 4.16V. I have 3 that are low, 3.53, 3.7 and 3.8. these are on 3 different bms boards- all in position 2.

This severely limits the range of the bike since the BMS starts shutting down when the the lowest cell hits minimum- usually when the pack is showing over 80%:-((

I can't really believe I have bad cells in this pack already. Anyone have any ideas what i can try to re-balance this pack?

thanks in advance.

g

User avatar
dogman dan
100 GW
100 GW
Posts: 34565
Joined: May 17, 2008 12:53 pm
Location: Las Cruces New Mexico USA

Re: 7P20S- 3 cells not charging to max

Post by dogman dan » Feb 13, 2018 8:17 am

At 4.16v, you don't have any bad cells in the battery. 3 of your groups are only showing the normal wear early, at worst.

They might just be out of balance too, so try balancing more, manually, or just the ride around the block and charge again method. Charge full, wait 30 min, then try to recharge again. If the charger wont start, ride around the block, not even close to a mile, then recharge. This will repeat the charger/bms balancing cycle.

Eventually, normal for all your cells will be 4.15v or so. But right now I think it's just out of balance.

User avatar
amberwolf
100 GW
100 GW
Posts: 24543
Joined: Aug 17, 2009 6:43 am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: 7P20S- 3 cells not charging to max

Post by amberwolf » Feb 13, 2018 1:50 pm

If the BMSes have a balance function, then each group 2's balancer may be stuck partly on, continously draining those cells at a low rate.

Or, the BMSes are powered by only the group 2 cells (which would be odd), and have a high power usage (also odd), causing those groups to drain constantly.


I'ts also possible that you happen to have 3 groups of bad cells, all in the same position in the pack, but it's much more likely there is a design or manufacture problem with the BMSes.

User avatar
flippy
100 W
100 W
Posts: 246
Joined: Aug 12, 2015 3:07 pm

Re: 7P20S- 3 cells not charging to max

Post by flippy » Feb 14, 2018 3:30 am

manually charge the low cells up to 4.2 and match them with the rest. charge slowly (under 1A) directly tru the balance wires.