Bosch lights flashing

Joined
Feb 2, 2016
Messages
8
Hi, recently after a bad weather ride my battery will not charge anymore. I connect it to the charger, it seems to start, but after two seconds three light are flashing.

Screen%20Shot%202015-02-24%20at%209.43.48%20PM.png


Reading about the problem seems to indicate wrong pack temperature, but after 12 hours rest and try again no change.
https://newwheel.net/questions/pages/viewpage.action?pageId=7274687

Put it on the bike and it works then but can't charge it. Have tried this reset-trick, holding button for 10 sec, doesn't help.

Anyone know something about this?
 
Well... I read on a german forum that some person had the same problem and that it was mouisture related.

https://www.pedelecforum.de/forum/index.php?threads/performance-akku-feuchtigkeitsproblem-wasserschaden-3-led%C2%B4s-blinken-fehler-200.36253/

I have never had problems with the battery before in about 4000 km of riding so I guess maybe some seal is about to give up.

Put in on the living room radiator (medium temp) for a few hours and tried again and now I can charge it! Have only tried charge to storage and put it away for now. But it feels ok now.
 
Back