Inside an LEV50 prismatic cell

jonescg

100 MW
Joined
Aug 7, 2009
Messages
4,224
Location
Perth, Western Australia
I'm sure you can google this stuff, but here it is for the curious.

20180221_100753.jpg
20180221_100721.jpg
20180221_100643.jpg

This cell was a failed cell from a Mitsubishi iMiEV battery. They are nominally 3.7 volts and 50 Ah.

Interesting that they wound up two separate accumulator piles and fused them in parallel, versus one big one. I guess the form factor might make it a little more energy dense. Alternatively, they may have 25 Ah and 75 Ah options down the line...
 
After Googling. !!...
It seems there are two versions of this cell ,.
After 2012, the improved GS-YUASA, LEV50N , having a different electrolite..
http://www.gs-yuasa.com/en/technic/vol9/pdf/009_01_026.pdf
https://pushevs.com/2015/11/04/gs-yuasas-improved-cells-lev50-vs-lev50n/
 
Aparently there are 75ah, 50ah, and 40 ah versions of the GS Yuasa LEV cells
The Mitsi Outlander PHEV uses a 40 ah version of this cell 80s, 1p config..12 kWh.
Nice video of the pack being dismantled...
https://youtu.be/Gf9fDbwF1K0
[youtube]Gf9fDbwF1K0[/youtube]
 