Hi,
Well where to start.
I bought two 48v 20amp batterys couple a weeks ago. All perfect. But then I seen a video on youtube where you can run a light off your charger input.
Well what did I do only go and try to check the volt output from it with my multimeter and BANG
Damn it anyways. I f'd it up. after paying over 850euro for the two batterys.
Well I tried to charge it but it won't charge. The part you plug the charger was all black. so I cut it off. I took off the shrink wrap but its got a plastic cover and very well wrapped so I went no further. It has a sticker it says LION KING on it.
The wires are all good back to the battery. I'm only getting a reading of 33.3v form the charger input, and 45.6v from the battery output.
What do you guys think I might have done burned out the bms or something else.
I am gutted.
I hope you's can help me guys, thanks
Well where to start.
I bought two 48v 20amp batterys couple a weeks ago. All perfect. But then I seen a video on youtube where you can run a light off your charger input.
Well what did I do only go and try to check the volt output from it with my multimeter and BANG
Damn it anyways. I f'd it up. after paying over 850euro for the two batterys.
Well I tried to charge it but it won't charge. The part you plug the charger was all black. so I cut it off. I took off the shrink wrap but its got a plastic cover and very well wrapped so I went no further. It has a sticker it says LION KING on it.
The wires are all good back to the battery. I'm only getting a reading of 33.3v form the charger input, and 45.6v from the battery output.
What do you guys think I might have done burned out the bms or something else.
I am gutted.
I hope you's can help me guys, thanks