A123 20AH LiFePO4 cells interconnexions

Batteries, Chargers, and Battery Management Systems.
bionicon   100 W

100 W
Posts: 260
Joined: Jun 28 2015 2:29pm
Location: Belgium

Re: A123 20AH LiFePO4 cells interconnexions

Post by bionicon » May 13 2018 12:12pm

Dui, ni shuo de dui wrote:
May 11 2018 1:08am
999zip999 wrote:
May 10 2018 11:30pm
#1 safety. Yes I found the high quality of these cells is the #1 they stay balance just bulk charging. What is the source for these cells and how much will you be paying ? I understand the need for a strong battery with that bike. What motor and controller do you run. Nice ride. Taking the let out and putting some high-powered cells in you would have a hard time keeping the front wheel down
Thanks :)

I'm using a 3000W QS motor and a software unlocked version of the sabvoton 72150, currently set up at 200 Amps continuous.
That's nice but not really amazing in terms of perfs so far. About an equivalent to a 125 or 200cc bike I guess.

I plan to make some mods to the sabvoton, using shunts to the current sensors to hopefully go around 300-400 Amps if it can actually go that far (still have to open it to check the mosfets first).
In which case, of course, I'll add watercooling so that it won't explode instantly :D

First step is to get the right battery and then I'll upgrade the other stuff, probably change the motor etc.
Ultimate goal is to make a bike with comparable specs as a basic 400-600cc engine.
Just want to know how much fase amps are you pulling? And whats the max faseamps that a unlocked 72150 can handle?

User avatar
Dui, ni shuo de dui   100 W

100 W
Posts: 122
Joined: Jan 29 2016 3:21am

Re: A123 20AH LiFePO4 cells interconnexions

Post by Dui, ni shuo de dui » May 13 2018 8:55pm

bionicon wrote:
May 13 2018 12:12pm


Just want to know how much fase amps are you pulling? And whats the max faseamps that a unlocked 72150 can handle?
I need to check again but it should be around 400-450 amps if I remember correctly

User avatar
Dui, ni shuo de dui   100 W

100 W
Posts: 122
Joined: Jan 29 2016 3:21am

Re: A123 20AH LiFePO4 cells interconnexions

Post by Dui, ni shuo de dui » May 13 2018 9:11pm

Ok so I finally moved on and ordered my battery and BMS.

For the Battery, it will be a 23S 2P (72V 40Ah). For now I just bought one, but I'll add another if it turns out to work as intended. Cost is 450 USD:

https://item.taobao.com/item.htm?spm=a2 ... t=6#detail

For the BMS, I'll go with this 300A one, including the screen and Bluetooth, for 80 bucks:
https://item.taobao.com/item.htm?spm=a2 ... t=6#detail

I should receive everything in a couple of weeks. Also need some little hardware, like anderson connectors, main switch, current sensor and stuff like that.

BTW, for those of you who need big, thick cables, here is my tip: Purchase some battery jumpers cables.
-They are super cheap
-They can handle a lot of current without heating
-They are already red and black
-They exist in various thicknesses and various insulator material

Stuff like that, you end up with 4 meters of super thick cable for 13 USD, enough to make several builds:
https://item.taobao.com/item.htm?id=134 ... 4.6#detail

User avatar
parabellum   10 MW

10 MW
Posts: 2057
Joined: Nov 19 2010 9:55am
Location: Dominican Republic, north.

Re: A123 20AH LiFePO4 cells interconnexions

Post by parabellum » May 13 2018 11:11pm

Dui, ni shuo de dui wrote:
May 13 2018 9:11pm
BTW, for those of you who need big, thick cables, here is my tip: Purchase some battery jumpers cables.
-They are super cheap
-They can handle a lot of current without heating
-They are already red and black
-They exist in various thicknesses and various insulator material
Unfortunately it is a worst choice in some location.
Here, it is 12AWG packaged in 1.5cmD insulator and mostly aluminium clad or iron clad crap. Welding wire is only way to go.

User avatar
Dui, ni shuo de dui   100 W

100 W
Posts: 122
Joined: Jan 29 2016 3:21am

Re: A123 20AH LiFePO4 cells interconnexions

Post by Dui, ni shuo de dui » May 14 2018 1:01am

parabellum wrote:
May 13 2018 11:11pm
Unfortunately it is a worst choice in some location.
Here, it is 12AWG packaged in 1.5cmD insulator and mostly aluminium clad or iron clad crap. Welding wire is only way to go.
I don't know where you live so that might be a possibility.
You might want to check with truck parts and accessories companies, they will use thicker gauge for sure.
Welding wire is OK but it's hard to find them color coded. Personnally I prefer to have an obvious color scheme to avoid any stupid mistake.

User avatar
Dui, ni shuo de dui   100 W

100 W
Posts: 122
Joined: Jan 29 2016 3:21am

Re: A123 20AH LiFePO4 cells interconnexions

Post by Dui, ni shuo de dui » May 23 2018 4:08am

Well I just received my new battery, YAY!

But unfortunately, those delivery morons kinda destroyed it...
It arrived pretty badly warped, I guess they just threw it on the floor.

Image


Image


Image


Image


Image

I managed to get it better using my giant vice:

Image

Image

Image


It's about 26 kilos, I quicly checked cells voltage and they all seem to be fine.

Image

Now I need to wire my smart BMS and power lines, hopefully I'll be able to finish the install of the first battery this week.

User avatar
amberwolf   100 GW

100 GW
Posts: 25486
Joined: Aug 17 2009 6:43am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: A123 20AH LiFePO4 cells interconnexions

Post by amberwolf » May 23 2018 3:44pm

FWIW, if it were packed correctly, that wouldn't have happened without pretty thorough destruction of the packaging. :/

Probalby could've been built stronger, too, but since it's designed to go into an enclosure on the vehicle that would do that job, it wouldn't have to be strong outside of that; it just has to depend on whatever packing or enclosure it is in to keep it intact.


FWIW, it's fortunate that it didn't warp more; it might've cut or torn tabs or balance wires and shorted cells out. :shock:

User avatar
Dui, ni shuo de dui   100 W

100 W
Posts: 122
Joined: Jan 29 2016 3:21am

Re: A123 20AH LiFePO4 cells interconnexions

Post by Dui, ni shuo de dui » May 23 2018 8:51pm

amberwolf wrote:
May 23 2018 3:44pm
FWIW, it's fortunate that it didn't warp more; it might've cut or torn tabs or balance wires and shorted cells out. :shock:
Yeah, that was very close!
Some of the tabs were less than 0.1mm apart from each other. A tiny bit more and they would have been shorted, I don't think that would have ended up pretty in the express company warehouse...

User avatar
agniusm   10 MW

10 MW
Posts: 2252
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: A123 20AH LiFePO4 cells interconnexions

Post by agniusm » May 28 2018 2:29pm


User avatar
Dui, ni shuo de dui   100 W

100 W
Posts: 122
Joined: Jan 29 2016 3:21am

Re: A123 20AH LiFePO4 cells interconnexions

Post by Dui, ni shuo de dui » Sep 12 2018 2:43am

A little update after using this battery for about 5 months: it is awesome.
Runs perfectly fine, doesn't heat, stays in balance, announced capacity seems to be there no matter how hard I ride it, it delivers any amount of current you might need with very little voltage sag... So far I have absolutely nothing to complain about, so if you have the opportunity to buy those kind of cells, don't hesitate for a second.