Hey guys,
I have brand new Samsung 25R cells (about 1 year old stock according to the codes) and also Sony VTC5 cells with the same MFG as the 25R.
Tested the internal resistance with a tester and both show 8.2ohm
Is there something I'm missing? because the 25R is rated for 8C and the VTC5 at 12C