Got this new pneumatic spot welder that works awesome, only problem is that when welding 0.15 pure nickel the electrodes stick pretty hard.
If I turn down the power it doesn't stick that bad (or not at all) but the weld is not as strong.
I also tried going down from double pulse to single but it just weakens the weld alot.
Any tips?
If I turn down the power it doesn't stick that bad (or not at all) but the weld is not as strong.
I also tried going down from double pulse to single but it just weakens the weld alot.
Any tips?