AERDU 36v battery pack from Ali Express

Post by nukezero » Mar 25 2019 2:45pm

What does everyone think about buying this AERDU battery pack on Aliexpress?

https://www.aliexpress.com/store/produc ... 1b23ZpG1RX

It uses Sanyo GA cells. I think I read a review on another forum that the seller "Sunway store" is reputable and does sell legitimate bare cells. But I just want to be sure.

I am looking for a 36v 10s4p in that tight configuration to fit in my wife's townie.

User avatar
flippy   10 MW

10 MW
Posts: 2171
Joined: Aug 12 2015 3:07pm

Re: AERDU 36v battery pack from Ali Express

Post by flippy » Mar 25 2019 4:44pm

not possible for that price.

if i buy those cells in bulk directly from the importer in europe then i have to pay 3 euro and change, that amounts to 140 euro just in cells.
if they are genuine then i expect discards or otherwise a QC fail product. certainly not genuine stuff that came out the front of the factory...
if they can supply GA cells for 2~2.5 euro per cell then i want to know who their supplier is and how they make any money.
Lithium beats liquid dinosaurs.

nukezero   10 kW

10 kW
Posts: 556
Joined: Jul 02 2013 5:00pm
Location: Los Angeles, CA

Re: AERDU 36v battery pack from Ali Express

Post by nukezero » Mar 25 2019 5:02pm

Thanks for the heads up

Hillhater   100 GW

100 GW
Posts: 11411
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: AERDU 36v battery pack from Ali Express

Post by Hillhater » Mar 25 2019 5:18pm

I assume you guys are aware of ES member. "Tumich" in Europe, who sells new 18650's ,including GA's,..at good prices and with a solid reputation .
He also has quality pre-made packs ..10s,4p...but without BMS, at good prices ($123.0 )
viewtopic.php?f=31&t=61608
Or this one ..
viewtopic.php?f=9&p=1454470#p1454470
But i have no personal experience with that vendor
This forum owes its existence to Justin of ebikes.ca

User avatar
flippy   10 MW

10 MW
Posts: 2171
Joined: Aug 12 2015 3:07pm

Re: AERDU 36v battery pack from Ali Express

Post by flippy » Mar 26 2019 4:38am

considering he has cells with spot weld marks they are lifted out of (used) battery packs.
i have no doubt they are genuine but i do wonder how long have they been on the shelf and why the batteries that originally held the cells are discarded.

buying brand new from a place like nkon ensures you have the real deal without any earmarks.
Lithium beats liquid dinosaurs.

Hillhater   100 GW

100 GW
Posts: 11411
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: AERDU 36v battery pack from Ali Express

Post by Hillhater » Mar 26 2019 5:59pm

"Tumich" also lists new, fresh, boxed, cells
Many ES members have bought used and new from him with no issues that i am aware of.
But , really its just a matter of being confident with which ever supplier you use.
You cannot do that with random Alibaba vendors !
This forum owes its existence to Justin of ebikes.ca

Ray1234   1 µW

1 µW
Posts: 1
Joined: Sep 06 2020 5:41pm

Re: STAY AWAY AERDU 36v battery pack from Ali Express

Post by Ray1234 » Sep 06 2020 6:06pm

I ordered AERDU 36v, 12A battery pack, and the charger from Ali Express. It took a few months to arrive in Canada and boy..big surprise.. The battery lasts only around 15 to 20 minutes full charge on a ebike with 500W motor.. Definitely contains dead cells since the output is also nowhere close to 12A. The charger came out of the box defective. No light and the output is around 12v..In conclusion, STAY AWAY from this seller. It is a huge hassle to ask for a refund since the money protection is only for 90 days and if you are lucky to receive it before the 90 days and you want to send it back, they never issue a return ticket. I have been waiting on it for a week now. Of course in my case, it took 4 months for it to arrive.

Anikea   100 µW

100 µW
Posts: 7
Joined: Jun 11 2020 10:02pm

BEWARE AERDU 36v battery pack from Ali Express

Post by Anikea » Oct 31 2020 3:27am

Unfortunately it's the same for me.
The battery was sold as an LG-MH1 cell, meanwhile the description has been changed so that the trader can talk himself out of it, it would only be cells with the capacity of LG-MH1. But the capacity is much lower.

Instead of the promised 12.8 AH, the battery has just 9.5 AH and that with only 2A load. The seller is preparing a new test with a final battery voltage of 25V! Although the description says that the BMS turns off at 28V. But the BMS does not lock at all but would allow a discharge to the point of cell death.

Even if you can prove that the cells are not branded cells and have a much too low capacity, the seller will not refund a cent.

These are cheap china cells with a very poor internal resistance, the voltage break down for 2V with a very low load.
The BMS also has no short-circuit protection, full voltage and full current are also applied to the charging cable.


Conclusion: bad cells and a high price and a seller who waste your time and laughs at you. I can only strongly advise you not to buy anything there!

User avatar
flippy   10 MW

10 MW
Posts: 2171
Joined: Aug 12 2015 3:07pm

Re: AERDU 36v battery pack from Ali Express

Post by flippy » Oct 31 2020 5:22pm

called it. :roll: