methods
1 GW
I had a nice review thought up...
Then I remembered how F'ed the world is
This is how I fixed mine after our Accounted wasted HOURS on the phone with the totally inept "process" which insisted that the problem is with the battery and not the charger (or combo)
* Batteries discharge fine
* Battery BMS has kept the cells in perfect balance
* Batteries do not charge on the charger
I crow-barred the charge inhibit fet
I crow-barred the discharge inhibit fet (to avoid charging thru its body diode)
I gutted the charger and hard-wired it to a Dell 19.4V laptop charger
Yea yea.. dont care
Here are some pics
/...
There ya go
Now think about the EV industry...
Think about Autozone
Think about how many people are going to hack their cars like this
IT WILL BE THE ONLY CHOICE
THEREFORE ALL CHARGING INFRASTRUCTURE MUST BE ... compatible
DO NOT ASSUME - that EV's (or any Lithium Electronics) are "to spec"
Quite the oposite
-methods
Then I remembered how F'ed the world is
This is how I fixed mine after our Accounted wasted HOURS on the phone with the totally inept "process" which insisted that the problem is with the battery and not the charger (or combo)
* Batteries discharge fine
* Battery BMS has kept the cells in perfect balance
* Batteries do not charge on the charger
I crow-barred the charge inhibit fet
I crow-barred the discharge inhibit fet (to avoid charging thru its body diode)
I gutted the charger and hard-wired it to a Dell 19.4V laptop charger
Yea yea.. dont care
Here are some pics
/...
There ya go
Now think about the EV industry...
Think about Autozone
Think about how many people are going to hack their cars like this
IT WILL BE THE ONLY CHOICE
THEREFORE ALL CHARGING INFRASTRUCTURE MUST BE ... compatible
DO NOT ASSUME - that EV's (or any Lithium Electronics) are "to spec"
Quite the oposite
-methods
Attachments
-
FrontIntoRear_001.jpg16.1 KB · Views: 1,261
-
FrontIntoRear_004.jpg30.6 KB · Views: 1,261
-
FrontIntoRear_005.jpg21.5 KB · Views: 1,261
-
FrontIntoRear_006.jpg34.3 KB · Views: 1,261
-
FrontIntoRear_010.jpg19.9 KB · Views: 1,261
-
FrontIntoRear_011.jpg32.5 KB · Views: 1,261
-
FrontIntoRear_012.jpg50.1 KB · Views: 1,261
-
FrontIntoRear_014.jpg47.7 KB · Views: 1,261
-
FrontIntoRear_015.jpg50 KB · Views: 1,261
-
FrontIntoRear_020.jpg53.8 KB · Views: 1,261
-
FrontIntoRear_021.jpg52 KB · Views: 1,261
-
FrontIntoRear_022.jpg48.4 KB · Views: 1,261
-
FrontIntoRear_023.jpg39.6 KB · Views: 1,261
-
FrontIntoRear_024.jpg40.5 KB · Views: 1,261
-
FrontIntoRear_029.jpg51.4 KB · Views: 1,261
-
FrontIntoRear_030.jpg39.2 KB · Views: 1,261
-
FrontIntoRear_032.jpg47.7 KB · Views: 1,261
-
FrontIntoRear_033.jpg44.9 KB · Views: 1,261
-
FrontIntoRear_034.jpg47.4 KB · Views: 1,261
-
FrontIntoRear_036.jpg46 KB · Views: 1,261
-
FrontIntoRear_042.jpg33.1 KB · Views: 1,261
-
FrontIntoRear_043.jpg25.1 KB · Views: 1,261
-
FrontIntoRear_044.jpg37.6 KB · Views: 1,261
-
FrontIntoRear_047.jpg32.1 KB · Views: 1,261
-
FrontIntoRear_048.jpg36.4 KB · Views: 1,261
-
FrontIntoRear_049.jpg45.5 KB · Views: 1,261
-
FrontIntoRear_050.jpg44 KB · Views: 1,261