Here is the best magnet bonding epoxy out there that I know of: Hysol EA9394 177 deg C rated capability based on maintaining 1Ksi Shear Strength.

NASA reference for Hysol EA9394 use bonding magnets in space flight generators (Page 264, marked 252-3 in report) http://www.scribd.com/doc/40109738/NASA ... ual-Report

Data sheet (with loads of good info): http://www.mtpinc-exporter.com/chemical ... 209394.pdf

Independent Sandia test report: http://prod.sandia.gov/techlib/access-c ... 950229.pdf

Where to buy it for $16 bucks through KR Anderson: http://www.kranderson.com/shop/Henkel-L ... 0ML-SEMPAK

This stuff is amazing. It has been tested in JP4 and hydraulic oil and held up fine per the data sheet. The data sheet also shows 600psi shear strength up to 400 degF!!!

A hint that makes the bond even stronger (applicable to all epoxies): Be very careful mixing to have as little air entrained as possible. Entrained air makes it weaker, but not to a failure level. I am talking about getting the last 15% out of this material with respect to bond strength. Also note the cure kinetics in the first NASA article and the data sheet. This material likes a higher than room temperature cure after one day at room temperature. Like 150 deg F for an hour or so after a day at room temperature.

PS:If anyone is using epoxy in a production environment, just buy the THINKY mixer that meets your specifications and that you can afford. These centrifugal, planetary mixers (some with vacuum capability) are just the finest for preparing epoxies and epoxy compounds. It doesn't get any better!
http://www.thinkyusa.com/products/

A few hints from Fechter from the thread where I discussed this epoxy:
"Also make sure the surfaces are clean and have no traces of oil. I think when they manufacture the steel parts they are coated with oil and they don't always do a good job of getting all the oil off.

After mixing epoxy, a good way to get the air out is to pull a vacuum on the mixuture. I like to load the mixed epoxy into a large syringe, then push as much air out as possible, block off the tip and pull the plunger back. This expands all the air bubbles and allows them to float to the surface. The syringe makes it handy for applying the epoxy afterwards.

You can get some flavors of the Hysol stuff from McMaster-Carr."
Last edited by bigmoose on Aug 07 2011 6:47pm, edited 3 times in total.
"Live simply. Love generously. Care deeply. Speak kindly. Leave the rest to God..." all the best, Dave

User avatar
liveforphysics   100 GW

100 GW
Posts: 14143
Joined: Oct 29 2008 1:48am
Location: Long Beach, CA, USA

Re: Very Good Magnet Bonding Epoxy

Post by liveforphysics » Apr 23 2011 8:38pm

Excellent to know for all of us tinkers.

Thank you Moose!
Each carcinogen vapor exposure includes a dice roll for cancer.

Each mutagen vapor exposure includes a dice roll for reproductive genetic defects in your children.

Each engine start sprays them into a shared atmosphere which includes beings not offered an opportunity to consent accepting these cancer experiences and defective genetics life experiences.

Every post is a free gift to the collective of minds composing the living bleeding edge of LEV development on our spaceship.

Kingfish   10 GW

10 GW
Posts: 4064
Joined: Feb 03 2010 11:23am
Location: Redmond, WA-USA, Earth, Sol, Orion–Cygnus Arm, Milky Way. Age: > yesterday < tomorrow
Contact:

Re: Very Good Magnet Bonding Epoxy

Post by Kingfish » Apr 24 2011 4:13pm

Bookmarked, KF :)
* My 2WD Garden Wall
* Kinaye MotorSports
* Primary ride: 2WD Disc 9C 2806-equiv / Dual Lyen 12FET / 20S7P LiPo.
* Epics: Going to California: 2011 8)
* 50-mph, 101, 10k-Club. 12,527 miles-to-date, 7037 as 2WD.

It is by caffeine alone I set my mind in motion.
It is by the beans of Java that thoughts acquire speed.
The hands acquire shakes, the shakes become a warning.
It is by caffeine alone I set my mind in motion.

User avatar
spinningmagnets   100 GW

100 GW
Posts: 11999
Joined: Dec 21 2007 10:27pm
Location: Ft Riley, NE Kansas

Re: Very Good Magnet Bonding Epoxy

Post by spinningmagnets » May 30 2011 6:12pm

A thread about adding hall sensors, turns into discussion on popular epoxies used:
http://endless-sphere.com/forums/viewto ... 1&p=411378
by electricwheels.de
We are using 3M DP 490 epoxy, workable potting time about 1 - 1.5 hrs, sets in about 8 hrs to a workable / usable condition, then cures during the next few days. Incredible stuff, high temp & age resistant, also ideal to stick neodym magnets to surfaces or fix small holes. Is hard, tough, expensive but really good. Look at the spec sheet and you'll know what I mean.
Doctorbass
The DP420 is the same stuff, but the work life is only 20 minutes.. just enough to place the hall sensor. Then, put that in an oven at 170F for 30 minutes and than leave them to cool down during 2-3 hours.. the epoxy will become as hard as metal! Ebay often offer the DP460 and DP420.

I know alot these DP epoxy from 3M I used them nearly once a week at my job. My torque arms ( the two on my giant DH) are glued with the DP420, and with 20kW burst on that motor they never failed ! DP scotchweld from 3M are some of the best!... also to fix magnets to the metal parts.

User avatar
Doctorbass   100 GW

100 GW
Posts: 7442
Joined: Apr 08 2007 2:24am
Location: Quebec, Canada East
Contact:

Re: Very Good Magnet Bonding Epoxy

Post by Doctorbass » Aug 31 2011 8:52am

3M DP-460 or DP-460 scotchweld products are also excellent products!

They are also recommanded by the manufacture for bounding magnet material.

4600psi shear strengh at ambiant with great derating

I "weld" my torque arms to the frame with it and it is MORE than enough.

4 of my ebikes are now equiped with that technic, two use regen at up to 6kW and run 20kW burst and one towed two time a schoolbus and the T-A is bonding is still intact and no sing of failure.

they also endured -30 during winter as well as 30 celsius during summer + the heat o fthe motor thru the axel.. and never had any problem.

I have a friend who had his X5 magnets that unstick during cold winter and hard power demand. ( magnet was rotating inside the hub!!! but no wheel spining... just like a friction clutch!!! he repaired them with the DP460 and that is still perfect

At work we use it in many aerospace project since many years

100% satisfied

cost around 40$ for a 43ml tube with the plunger

Doc
CURRENT PROJECT: 2WD duo MXUS/Max-E ebike 32kW
http://endless-sphere.com/forums/viewto ... =3&t=65764
-Fastest speed record 117 km/h on flat
-Fastest 1/4 mile@ 114km/h on flat and 16.316 sec
-Succeded to haul a 19200 pounds schoolbus!
113kmh Gianthttp://www.evalbum.com/3406
Mongoosehttp://www.evalbum.com/1947
YOUTUBE---https://m.youtube.com/user/Doctorbasss
http://twitter.com/DocbassMelancon
I speak FRENCH and english

Post Reply