Insulating materials and methods for battery box

Get all your technical information about electric bikes here.
Post Reply
bakaneko   100 W

100 W
Posts: 189
Joined: Oct 25 2018 6:25pm

Insulating materials and methods for battery box

Post by bakaneko » Aug 01 2020 7:41am

It is cooling down now but just a week ago it was like upper 80s to lower 90s and sunny. Things baked in the sun. I am finishing a fat tire 3.4kwH build atm and need to make a battery box. I want to make sure this thing is as cool as possible. So far, I have the following plan.

- White paint wooden/particle board box 1/4" with small orange accents
- 1/4" packing foam between batteries and box
- Vent holes in front of the battery box but how do I make this water proof? Do I need this?
- Do I do a double layer? So particle board -> foam -> particle board?

Any other suggestions?

99t4   10 mW

10 mW
Posts: 24
Joined: May 10 2020 10:31pm
Location: PNW

Re: Insulating materials and methods for battery box

Post by 99t4 » Aug 01 2020 1:21pm

Looks like you are more concerned with limiting the effect of solar radiation externally heating up your battery box. What about making a simple removable cover out of reflective material (mylar blanket or refletix?)

What kind of batteries?

If you insulate too much wouldn't you run the risk of trapping battery heat in the box?

bakaneko   100 W

100 W
Posts: 189
Joined: Oct 25 2018 6:25pm

Re: Insulating materials and methods for battery box

Post by bakaneko » Aug 01 2020 5:22pm

lipo. yeah solar radiation. i also dont want to make it too weird or eye catching.