Battery won't charge

Post by marcoredit » Jan 02 2021 4:29am

Hi,
I connected the bms to the 14s battery and in output it shows 54 V. The cells charge is 3.89 on average. I connected the battery to the bike and the motor works, but when I try to charge the battery, it doesn't charge. The same battery charger works on other batteries.

What could it be?
Thanks and happy new year.
Attachments
01.jpg
01.jpg (189.9 KiB) Viewed 207 times
02.jpg
02.jpg (179.51 KiB) Viewed 207 times
03.jpg
03.jpg (161.25 KiB) Viewed 207 times

goatman   100 MW

100 MW
Posts: 2657
Joined: Jun 23 2019 6:50pm
Location: Surrey, B.C.

Re: Battery won't charge

Post by goatman » Jan 02 2021 10:43am

wheres the P-

marcoredit   1 W

1 W
Posts: 56
Joined: Jan 08 2014 7:05am
Location: Italy

Re: Battery won't charge

Post by marcoredit » Jan 02 2021 11:58am

My BMS has only B-, C-.

attach the schema I followed
Attachments
04.jpg
04.jpg (151.54 KiB) Viewed 194 times

Jonno   100 W

100 W
Posts: 207
Joined: Sep 30 2016 6:41am
Location: UK

Re: Battery won't charge

Post by Jonno » Jan 02 2021 1:20pm

Probably the wrong bms
Does your charger show fully charged when plugged in?
If it does then the bms is not for18650 cells that charge to 4.2v
Check which bms you purchased

Jonno
Modified EEB frame, 888 forks, 280mm DNM pit bike shock, QS273 40h V3 3.5t, Nucular Electronics 24F controller 300a, 92V @ 36ah 26650 cells, 300a BMS with bypass,
Hope V4 + Galfer 223mm discs + Variable regen braking.
Amongst other builds.

User avatar
E-HP   1 MW

1 MW
Posts: 1931
Joined: Nov 01 2018 9:20pm

Re: Battery won't charge

Post by E-HP » Jan 02 2021 1:30pm

marcoredit wrote:
Jan 02 2021 4:29am
Hi,
I connected the bms to the 14s battery and in output it shows 54 V. The cells charge is 3.89 on average. I connected the battery to the bike and the motor works, but when I try to charge the battery, it doesn't charge. The same battery charger works on other batteries.

What could it be?
Thanks and happy new year.
Are you sure it's not a 13S charger? 54V and change would be for a fully charged 13S battery.

marcoredit   1 W

1 W
Posts: 56
Joined: Jan 08 2014 7:05am
Location: Italy

Re: Battery won't charge

Post by marcoredit » Jan 02 2021 1:34pm


User avatar
E-HP   1 MW

1 MW
Posts: 1931
Joined: Nov 01 2018 9:20pm

Re: Battery won't charge

Post by E-HP » Jan 02 2021 1:43pm

Do you have a link to the charger, or a pic of the label?

Jonno   100 W

100 W
Posts: 207
Joined: Sep 30 2016 6:41am
Location: UK

Re: Battery won't charge

Post by Jonno » Jan 02 2021 2:17pm

.......or test the output voltage of the charger.

BMS looks correct


Jonno
Modified EEB frame, 888 forks, 280mm DNM pit bike shock, QS273 40h V3 3.5t, Nucular Electronics 24F controller 300a, 92V @ 36ah 26650 cells, 300a BMS with bypass,
Hope V4 + Galfer 223mm discs + Variable regen braking.
Amongst other builds.

marcoredit   1 W

1 W
Posts: 56
Joined: Jan 08 2014 7:05am
Location: Italy

Re: Battery won't charge

Post by marcoredit » Jan 02 2021 2:21pm

The charger I use
Attachments
05.jpg
05.jpg (214.56 KiB) Viewed 176 times

kcuf   100 W

100 W
Posts: 267
Joined: Sep 29 2018 3:21pm

Re: Battery won't charge

Post by kcuf » Jan 02 2021 2:35pm

what is the voltage of the charger

label isn't marked

use volt meter and measure

charger output not connected to battery

if 54v and change?

wrong charger

if 58v and change

something else wrong
In 2013 an ad appears on Russia social networks: Интернет-операторы хотели! Работа в шикарном офисе в Ольгино !!!, зарплата 25960 рублей в месяц

marcoredit   1 W

1 W
Posts: 56
Joined: Jan 08 2014 7:05am
Location: Italy

Re: Battery won't charge

Post by marcoredit » Jan 02 2021 3:14pm

The charger output is 58.8V.
So something else is wrong. Maybe the 15 wires are wrong connected?
Attachments
06.jpg
06.jpg (220.48 KiB) Viewed 166 times

User avatar
fechter   100 GW

100 GW
Posts: 15171
Joined: Dec 31 2006 3:23pm
Location: California Bay Area, USA

Re: Battery won't charge

Post by fechter » Jan 02 2021 8:22pm

I have the same single port model BMS on one of my packs and have had no issues with it.

You could try completely disconnecting it and reconnecting it. It looks like you have it wired correctly. If any of the balance wires were misconnected, you should not have output to run the motor.

It may be a defective BMS board.
"One test is worth a thousand opinions"

marcoredit   1 W

1 W
Posts: 56
Joined: Jan 08 2014 7:05am
Location: Italy

Re: Battery won't charge

Post by marcoredit » Jan 03 2021 11:18am

So I'll try to check alla the wires again and then change the BMS.

Thank you

kcuf   100 W

100 W
Posts: 267
Joined: Sep 29 2018 3:21pm

Re: Battery won't charge

Post by kcuf » Jan 04 2021 10:08pm

many bms die easily

high power gets expensive

consider low power charge bms only

discharge directly off tabs



outdoor battery discharge

no bms usually safe enuf

controller lvc should match 14s



cheap ebay solution

10-20A 14s bms wired charge only
In 2013 an ad appears on Russia social networks: Интернет-операторы хотели! Работа в шикарном офисе в Ольгино !!!, зарплата 25960 рублей в месяц

Voltron   1 GW

1 GW
Posts: 3072
Joined: May 02 2013 4:53pm
Location: Santa Barbara CA

Re: Battery won't charge

Post by Voltron » Jan 04 2021 11:33pm

Have you actually pulled the balance wire plug out, and checked the voltages at the terminals there, starting from one end of the plug? If you do, you really really want to have steady hands as they are pretty close together and easy to touch the meter probes together, which I find doesn't make a big spark at that voltage, but is just enough to deform the plastic plug body around the terminals from the heat.