Hello
This happened after about a week of running the Kol motor at 60V, this is quite common if you really turn the wick up on these motors, I have found a place that will make the rotor from a magnet! this would be great and would mean you can run higher rpms without the magnets flying off.
Sensible power limits still need to be adhered to of course but it would make this nice cheap little motor virtually indestructible for PA use.
See Pictures.
Knoxie
This happened after about a week of running the Kol motor at 60V, this is quite common if you really turn the wick up on these motors, I have found a place that will make the rotor from a magnet! this would be great and would mean you can run higher rpms without the magnets flying off.
Sensible power limits still need to be adhered to of course but it would make this nice cheap little motor virtually indestructible for PA use.
See Pictures.
Knoxie