Post by agniusm » Jun 29 2013 12:13pm

Yet another frame. This time going amberwolf style. Went to a scrap yard, picked up 7 chinese, russian bike frames, few old steel bed ends, 65kg of steel. This is my catch:

Image
Today i felt inspiration and went to my workshop to do some chopping chop-shop style. Here is what i came up with:
Image
Image
Image
Image
Image 

The system i am thinking about:

500/1000W 6t MAC motor on 20" 80mm wide rim with 3" tyre
Front - 24" 56mm rim with 2.5" tyre
12FET infineon - 40A
20AH <10C 16S lifepo4 with built in BMS
3A DC converter
6A onboard charger
Single speed chain drive

Still need to finish bottom cage for stiffen the bike and electronics components for stealth;
Make 10mm dropouts and weld them on;
Order woven wooden basket;
Look for short cranks(dont know if thats what they called) for pedals as there is little space from the pedals to the cargo cage;
Figure brakes

I think this bike would be able to carry family of three, two adults and a child or some cargo. I have another cargo bike coming slowly but remote steering is a job and half to get it right, in the mean time this is simple, nice side project. Anyway, when i am done with these, i will have 4 fully custom bikes on my account:)
If you have any suggestions, get them down
Cheerios

P.S. This the second time i am posting in wrong thread for some reason, probably need to have less windows opened.
MODS, please move it to technical section for me. Sorry for inconvenience.

User avatar
dogman dan   100 GW

100 GW
Posts: 34420
Joined: May 17 2008 12:53pm
Location: Las Cruces New Mexico USA

Re: Longtail cargo bike project

Post by dogman dan » Jun 29 2013 5:50pm

Done. Looks cool, love seeing what you are up to.

No doubt you aren't finished, but it looks to me like it's weak vertically, right behind the front seatpost. Needs some gussets or diagonals to haul lots of weight on that platform.

User avatar
agniusm   10 MW

10 MW
Posts: 2252
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: Longtail cargo bike project

Post by agniusm » Jun 29 2013 6:05pm

dogman wrote:Done. Looks cool, love seeing what you are up to.

No doubt you aren't finished, but it looks to me like it's weak vertically, right behind the front seatpost. Needs some gussets or diagonals to haul lots of weight on that platform.
Sure it does. Ran out of bed ends and time, good enough for 5 hour work I think :) Waiting for monday when scrap yard will open

User avatar
agniusm   10 MW

10 MW
Posts: 2252
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: Longtail cargo bike project

Post by agniusm » Jun 30 2013 7:52am

Had overnight thought and will rebuild rear fork from larger tube.
I was wandering if anyone knows what largest tire will allow MAC motor clearance for belt drive system?
At the moment the thinking is to use 80mm rim with 4 1/4" tyre
Also what shortest cranks available for reasonable money?

User avatar
agniusm   10 MW

10 MW
Posts: 2252
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: Longtail cargo bike project

Post by agniusm » Jul 02 2013 9:44am

Got my 4th torque arms made:
Image
Image
Image

They are massive, 12mm thick

Revised rear end as it was looking weak:

Image
Image
Image
Image
Image
Image

User avatar
docnjoj   100 GW

100 GW
Posts: 5775
Joined: Sep 29 2007 5:26pm
Location: Fairhope AL

Re: Longtail cargo bike project

Post by docnjoj » Jul 02 2013 1:50pm

You should consider selling those torque arms. They are the first I have seen that you could get with the pinch bolts.
otherDoc
E-bike stable at our house

Steintrike Mad Max full suspension trike rear Cute 100H going on: Whoops, Cute wheel broke but I fixed it.
Sun USX delta trike EbikeKit small geared front wheel sort of front suspension for wife

Agniusm/A123 AMP 20 36 volts on the Steini has been taken off.
2x16000 Multisport from HK now gone as they died after 2 years
New Luna 10S bottle battery 13.6AH now on mine
Relatively New 10S4Px2 for wife's bike giving 20ah @ 40 volts home made Panasonic from Tumich. BMS's rule.

User avatar
dogman dan   100 GW

100 GW
Posts: 34420
Joined: May 17 2008 12:53pm
Location: Las Cruces New Mexico USA

Re: Longtail cargo bike project

Post by dogman dan » Jul 03 2013 7:14am

OOO! I'm liking that a lot now!

User avatar
agniusm   10 MW

10 MW
Posts: 2252
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: Longtail cargo bike project

Post by agniusm » Jul 11 2013 3:30pm

Revision to the front end:
Image
Image

User avatar
agniusm   10 MW

10 MW
Posts: 2252
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: Longtail cargo bike project

Post by agniusm » Sep 21 2013 3:26am

Hi. Question: i will need to guide the chain under the back frame as there will be a battery and all electronics box in there. Can i use jockey wheels for that purpose:
Image
It says it has sealed bearings, 7075Al?

User avatar
agniusm   10 MW

10 MW
Posts: 2252
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: Longtail cargo bike project

Post by agniusm » Sep 30 2013 7:46am

Parts are coming in slow but stady:

Image

User avatar
agniusm   10 MW

10 MW
Posts: 2252
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: Longtail cargo bike project

Post by agniusm » Nov 20 2013 2:55pm

Few more parts arrievd:Image
Image

User avatar
agniusm   10 MW

10 MW
Posts: 2252
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: Longtail cargo bike project

Post by agniusm » Nov 29 2013 5:09pm

Could someone suggest a stem riser/extender? It would be good to get 180-200mm rise. Semi integrated headset bearings, 1-1/8 inch.
Thanks

User avatar
dogman dan   100 GW

100 GW
Posts: 34420
Joined: May 17 2008 12:53pm
Location: Las Cruces New Mexico USA

Re: Longtail cargo bike project

Post by dogman dan » Nov 30 2013 8:01am

You need the bars higher? I just found it easiest to use a bmx handlebar, that has the rise built into it. Like in the earlier pix.

A long fork steer tube will allow lots of spacers though, if you don't cut the tube shorter. Looks like you have some length there now.

I don't know of any threadless handlebar stems that have much rise in them. If that fork is threaded, then the stems for comfort bikes are the tallest I have seen. Hunt one on ebay I suppose.

User avatar
agniusm   10 MW

10 MW
Posts: 2252
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: Longtail cargo bike project

Post by agniusm » Nov 30 2013 8:29am

The only one i found that will do is SATORI EASY UP STEM RISER. I wander if they are reliable and worth a try.
EDIT:
OK, bit the bullet and ordered it along with 70mm 10degree Token stem. Will see how all mates together.
Now thinking on the other hand easy up stem sounds good if there is more people using one bike. QR type adjustment of stem height is a good thing.

User avatar
agniusm   10 MW

10 MW
Posts: 2252
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: Longtail cargo bike project

Post by agniusm » May 10 2018 6:51am

Reviving this one. 20S battery, BT bms, and kls7030s. Made a box for all the stuff. Will have marine plywood deck and aluminium box:

Image

Image

Image

Image

Image

Image

User avatar
docnjoj   100 GW

100 GW
Posts: 5775
Joined: Sep 29 2007 5:26pm
Location: Fairhope AL

Re: Longtail cargo bike project

Post by docnjoj » May 12 2018 6:52am

I see that you still have the skillz! What kind of batteries are those?
otherDoc
E-bike stable at our house

Steintrike Mad Max full suspension trike rear Cute 100H going on: Whoops, Cute wheel broke but I fixed it.
Sun USX delta trike EbikeKit small geared front wheel sort of front suspension for wife

Agniusm/A123 AMP 20 36 volts on the Steini has been taken off.
2x16000 Multisport from HK now gone as they died after 2 years
New Luna 10S bottle battery 13.6AH now on mine
Relatively New 10S4Px2 for wife's bike giving 20ah @ 40 volts home made Panasonic from Tumich. BMS's rule.

User avatar
agniusm   10 MW

10 MW
Posts: 2252
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: Longtail cargo bike project

Post by agniusm » May 17 2018 1:57am

Hi mate. Was away for long time but i am back :). Those are the batteries which is the reason i was away and two kids i made :) They are no solder/weld modules i developed for 18650 cells and inside LG 2500mah 6P (www.18650.lt)
Its hard to forget hard learned skilzzz :D

Got the deck made. Was sketching up aluminium body of the cargo box. Not as easy to make it fold with minimal weld lines but i am there. Just need to print template and get weldin bendin.

Image

User avatar
docnjoj   100 GW

100 GW
Posts: 5775
Joined: Sep 29 2007 5:26pm
Location: Fairhope AL

Re: Longtail cargo bike project

Post by docnjoj » May 18 2018 5:31am

That is a quality template! Are you saying that your weld free battery holder is not available?
otherDoc
E-bike stable at our house

Steintrike Mad Max full suspension trike rear Cute 100H going on: Whoops, Cute wheel broke but I fixed it.
Sun USX delta trike EbikeKit small geared front wheel sort of front suspension for wife

Agniusm/A123 AMP 20 36 volts on the Steini has been taken off.
2x16000 Multisport from HK now gone as they died after 2 years
New Luna 10S bottle battery 13.6AH now on mine
Relatively New 10S4Px2 for wife's bike giving 20ah @ 40 volts home made Panasonic from Tumich. BMS's rule.

User avatar
agniusm   10 MW

10 MW
Posts: 2252
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: Longtail cargo bike project

Post by agniusm » May 19 2018 9:49am

OH, it is available for basically a year now :) 2P through to 8P

User avatar
docnjoj   100 GW

100 GW
Posts: 5775
Joined: Sep 29 2007 5:26pm
Location: Fairhope AL

Re: Longtail cargo bike project

Post by docnjoj » May 21 2018 7:26am

Are these modules and kits actually ready for sale. They look brilliant!
otherDoc
E-bike stable at our house

Steintrike Mad Max full suspension trike rear Cute 100H going on: Whoops, Cute wheel broke but I fixed it.
Sun USX delta trike EbikeKit small geared front wheel sort of front suspension for wife

Agniusm/A123 AMP 20 36 volts on the Steini has been taken off.
2x16000 Multisport from HK now gone as they died after 2 years
New Luna 10S bottle battery 13.6AH now on mine
Relatively New 10S4Px2 for wife's bike giving 20ah @ 40 volts home made Panasonic from Tumich. BMS's rule.

User avatar
agniusm   10 MW

10 MW
Posts: 2252
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: Longtail cargo bike project

Post by agniusm » May 21 2018 8:49am

Yes, you can buy them right now since last July. Go to www.18650.lt

User avatar
agniusm   10 MW

10 MW
Posts: 2252
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: Longtail cargo bike project

Post by agniusm » May 22 2018 1:27am

So i went the hard way with aluminium. Just forced myself and threw a foldable chassis in sketchup. Designed with minimal welds but still there is some. Had to force myself in advancing of welding aluminium. Turned out alright.

Image

Image

Image

Image

Image

Image

Image

Have set up my BT BMS and all worked from the first time, nothing blew :)