Carbon FATbike BBSHD

Get all your technical information about electric bikes here.
Post Reply
bbq870   1 W

1 W
Posts: 64
Joined: Sep 20 2014 10:51pm

Carbon FATbike BBSHD

Post by bbq870 » Dec 06 2015 1:08am

hello everybody.
I am reading this forum a while now and I think I´m ready to start my Fatbike build.
It will be a carbon fatbike with carbon wheels.
the motor will be the new Bafang 1000W middrive BBSHD.

I have some questions now, where I didn´t find an answer in other threads...
is it possible to use carbon rims on a 1000W ebike?
do I need stronger spokes as normal?


plan A.
the manufacturer can STRENGTHEN the rims with extra layers of carbon.
(not sure why he´s doing that, maybe he plans to build ebikes-rims in the future)
Bildschirmfoto 2015-12-06 um 14.20.58.png
Bildschirmfoto 2015-12-06 um 14.20.58.png (237.91 KiB) Viewed 1205 times
plan B.
I could get trispoke carbon wheels also, they seem stronger but.....
1.price is double than normal wheel.
2. no IHG (internal gear hub) possible for those rims.
3. I´m not convinced by their look so far...


cheers!
Bildschirmfoto 2015-12-06 um 14.16.31.png
Bildschirmfoto 2015-12-06 um 14.16.31.png (247.99 KiB) Viewed 1205 times

Phife   1 W

1 W
Posts: 63
Joined: Sep 25 2015 9:58pm
Location: Kelowna, BC. Canada

Re: Carbon FATbike BBSHD

Post by Phife » Dec 06 2015 10:49am

Are you sure the BBSHD will even fit in a Carbon BB shell? I know that the BB shells on normal carbon bikes are too thick for the BBS02 to fit. I suspect there will be a similar issue here.
2008 Full Suspension Giant Reign 2 with 48v 750W BBS02. Click Here
2014 Specialized Stumpjumper Comp Evo FSR with Luna Cycle 3000w Mid Drive, 52V 20ah Backpack Battery. Click Here

bbq870   1 W

1 W
Posts: 64
Joined: Sep 20 2014 10:51pm

Re: Carbon FATbike BBSHD

Post by bbq870 » Dec 06 2015 11:50am

do you mean the width of the BB?
it will be 120mm wide.

edit:
width=inner diameter?
I don't know that measurement. I thought all crancsets will fit.

bbq870   1 W

1 W
Posts: 64
Joined: Sep 20 2014 10:51pm

Re: Carbon FATbike BBSHD

Post by bbq870 » Dec 06 2015 12:06pm

here is a picture of the frame
image.jpg
image.jpg (31.75 KiB) Viewed 1133 times

WoodlandHills   10 kW

10 kW
Posts: 748
Joined: Nov 11 2015 12:27pm
Location: Ortega River, JAX, FL

Re: Carbon FATbike BBSHD

Post by WoodlandHills » Dec 06 2015 12:34pm

It looks like the material around the BB is too thick for the drive: the wall thickness is too great for the space allowed by the drive. Also it looks like the position of the down tube will force the drive to hang below the BB and not in front.

Phife   1 W

1 W
Posts: 63
Joined: Sep 25 2015 9:58pm
Location: Kelowna, BC. Canada

Re: Carbon FATbike BBSHD

Post by Phife » Dec 06 2015 12:42pm

I mean the thickness of the carbon around the BB Shell. In your picture it is the black carbon around the metal ring. I dont remember the details, I just remember reading that some people on here couldnt get a BBS02 on any carbon frame bike. Not sure if the HD is any different.
2008 Full Suspension Giant Reign 2 with 48v 750W BBS02. Click Here
2014 Specialized Stumpjumper Comp Evo FSR with Luna Cycle 3000w Mid Drive, 52V 20ah Backpack Battery. Click Here

bbq870   1 W

1 W
Posts: 64
Joined: Sep 20 2014 10:51pm

Re: Carbon FATbike BBSHD

Post by bbq870 » Dec 06 2015 10:37pm

:cry: :cry: :cry:
that is NOT good.... thanks for the advise!
hmm. its too expensive to "just try". maybe I need plan B for the motor also...
maybe build a "DUAL drive Tesla bike" with 2x hubmotor :evil:

but for the RIMS...
has anyone concerns about the strength of carbon rims?

cheers

User avatar
Green Machine   100 kW

100 kW
Posts: 1464
Joined: Jan 18 2010 3:31am
Location: it doesnt matter .... spark a revolution
Contact:

Re: Carbon FATbike BBSHD

Post by Green Machine » Jun 13 2016 12:24am

hey i fell into this same thing....

i got a beautiful carbon mountain bike frame only to find the bbshd would not fit....