Manufacturing error Enduro swing arm

Get all your technical information about electric bikes here.
User avatar
Dirt biker
1 mW
1 mW
Posts: 18
Joined: Jun 08, 2017 4:39 pm

Re: Manufacturing error Enduro swing arm

Post by Dirt biker » Sep 14, 2017 11:29 am

bump, does anyone else have spacers/shims? or do you have the tabs directly against the bearing?

User avatar
Dirt biker
1 mW
1 mW
Posts: 18
Joined: Jun 08, 2017 4:39 pm

Re: Manufacturing error Enduro swing arm

Post by Dirt biker » Sep 20, 2017 6:12 pm

bent it a tiny bit more and had to use force to grind it past the edge, but it sits tight even both with and without the bolt.
So seems to be okay, but I wonder if this bending could damage the welds? Is that something I should worry about?