Hot-setting 6061 Frame

Get all your technical information about electric bikes here.
Post Reply
coolbobjoe   1 W

1 W
Posts: 60
Joined: Jul 06 2017 4:03am

Hot-setting 6061 Frame

Post by coolbobjoe » Feb 11 2018 4:04am

Looking into the newer QS Motors line with 200mm dropout widths for a custom Ebike project based on the A2B Octave/Metro Frames.
Have developed newer 1/4" 4130 dropouts for both sides of the swingarm but am now looking to stretch the dropouts width from 155mm to 200mm to accept their higher torque motors. I can get 200Nm of torque roughly out of their 155 versions but 350!!! from their 200mm versions. Cold-setting is most likely not going to work as its 45mm of stretch on a hefty aluminum swingarm when only 15mm works on small road bike frames. Heat-treatment after and/or before seems necessary. Near the silicone valley area so manufacturing/prodtuction will be easy enough once I get a game plan going. what does ES think?

Buk___   10 kW

10 kW
Posts: 750
Joined: Jul 28 2017 5:59pm

Re: Hot-setting 6061 Frame

Post by Buk___ » Feb 11 2018 9:23am

coolbobjoe wrote:
Feb 11 2018 4:04am
Looking into the newer QS Motors line with 200mm dropout widths for a custom Ebike project based on the A2B Octave/Metro Frames.
Have developed newer 1/4" 4130 dropouts for both sides of the swingarm but am now looking to stretch the dropouts width from 155mm to 200mm to accept their higher torque motors. I can get 200Nm of torque roughly out of their 155 versions but 350!!! from their 200mm versions. Cold-setting is most likely not going to work as its 45mm of stretch on a hefty aluminum swingarm when only 15mm works on small road bike frames. Heat-treatment after and/or before seems necessary. Near the silicone valley area so manufacturing/prodtuction will be easy enough once I get a game plan going. what does ES think?
Besides all the risks of getting the set even and the post bend heat treatment right; isn't moving the rear cogs over 22.5mm going to make getting a good chainline impossible?

coolbobjoe   1 W

1 W
Posts: 60
Joined: Jul 06 2017 4:03am

Re: Hot-setting 6061 Frame

Post by coolbobjoe » Feb 11 2018 11:32am

a straight chainline is the least of my concerns at this point. My 100-200W of human pedal power is nothing compared to the 9kw coming from my hub motor. The pedals would be taken off at this point if it were not for the ALMIGHTY POWERS THAT BE WATCHING US ROADWAYS if you know what I mean. It currently runs a 7 speed freewheel to a decently complicated tensioning system for the full suspension. I never take it out of 7th gear at this point so a single speed freewheel conversion will probably come along with the ride on this one. I can adjust where my chain lies through two pulleys before and after the chainring to account for quite a bit of play. have enough room for adjustment to fit a 10 sp. freewheel in there but not really worth the effort at this point in time as roughly only 1% of my power is actually coming through my pedal system.

coolbobjoe   1 W

1 W
Posts: 60
Joined: Jul 06 2017 4:03am

Re: Hot-setting 6061 Frame

Post by coolbobjoe » Feb 11 2018 11:32am

Buk___ wrote:
Feb 11 2018 9:23am
coolbobjoe wrote:
Feb 11 2018 4:04am
Looking into the newer QS Motors line with 200mm dropout widths for a custom Ebike project based on the A2B Octave/Metro Frames.
Have developed newer 1/4" 4130 dropouts for both sides of the swingarm but am now looking to stretch the dropouts width from 155mm to 200mm to accept their higher torque motors. I can get 200Nm of torque roughly out of their 155 versions but 350!!! from their 200mm versions. Cold-setting is most likely not going to work as its 45mm of stretch on a hefty aluminum swingarm when only 15mm works on small road bike frames. Heat-treatment after and/or before seems necessary. Near the silicone valley area so manufacturing/prodtuction will be easy enough once I get a game plan going. what does ES think?
Besides all the risks of getting the set even and the post bend heat treatment right; isn't moving the rear cogs over 22.5mm going to make getting a good chainline impossible?
a straight chainline is the least of my concerns at this point. My 100-200W of human pedal power is nothing compared to the 9kw coming from my hub motor. The pedals would be taken off at this point if it were not for the ALMIGHTY POWERS THAT BE WATCHING US ROADWAYS if you know what I mean. It currently runs a 7 speed freewheel to a decently complicated tensioning system for the full suspension. I never take it out of 7th gear at this point so a single speed freewheel conversion will probably come along with the ride on this one. I can adjust where my chain lies through two pulleys before and after the chainring to account for quite a bit of play. have enough room for adjustment to fit a 10 sp. freewheel in there but not really worth the effort at this point in time as roughly only 1% of my power is actually coming through my pedal system.

12-C   100 W

100 W
Posts: 176
Joined: Oct 14 2016 9:22pm

Re: Hot-setting 6061 Frame

Post by 12-C » Feb 11 2018 10:06pm

I might think that hacking one side off at a time and rewelding/sistering the opposite side might allow you to get it more even and true; then repeat for the other side. Do the heat treatment after welding and you are set....

coolbobjoe   1 W

1 W
Posts: 60
Joined: Jul 06 2017 4:03am

Re: Hot-setting 6061 Frame

Post by coolbobjoe » Feb 12 2018 6:29pm

12-C wrote:
Feb 11 2018 10:06pm
I might think that hacking one side off at a time and rewelding/sistering the opposite side might allow you to get it more even and true; then repeat for the other side. Do the heat treatment after welding and you are set....
Very solid idea actually. Any thoughts on filling the swingarm with more material while im in there already?

SlowCo   100 kW

100 kW
Posts: 1468
Joined: Jan 05 2015 5:43pm
Location: The Netherlands

Re: Hot-setting 6061 Frame

Post by SlowCo » Feb 12 2018 7:02pm

If you will go to a single speed then just mill the axle flats further so you make the drop out width of the axle smaller.

User avatar
Chalo   100 GW

100 GW
Posts: 7961
Joined: Apr 29 2009 11:29pm
Location: Austin, Texas

Re: Hot-setting 6061 Frame

Post by Chalo » Feb 12 2018 7:06pm

Please register and insure your motorcycle, and stay out of bicycle facilities. Thanks.
This is to express my gratitude to Justin of Grin Technologies for his extraordinary measures to save this forum for the benefit of all.

User avatar
liveforphysics   100 GW

100 GW
Posts: 14134
Joined: Oct 29 2008 1:48am
Location: Santa Cruz, CA, USA

Re: Hot-setting 6061 Frame

Post by liveforphysics » Feb 12 2018 7:54pm

I would try to do it cold, because once it's been hot from welding or a torch, it will be T-0, T-1 temper and has something like 1/5th to 1/7th the initial strength of T-6 6061.
Each carcinogen vapor exposure includes a dice roll for cancer.

Each mutagen vapor exposure includes a dice roll for reproductive genetic defects in your children.

Each engine start sprays them into a shared atmosphere which includes beings not offered an opportunity to consent accepting these cancer experiences and defective genetics life experiences.

Every post is a free gift to the collective of minds composing the living bleeding edge of LEV development on our spaceship.

coolbobjoe   1 W

1 W
Posts: 60
Joined: Jul 06 2017 4:03am

Re: Hot-setting 6061 Frame

Post by coolbobjoe » Feb 12 2018 8:24pm

SlowCo wrote:
Feb 12 2018 7:02pm
If you will go to a single speed then just mill the axle flats further so you make the drop out width of the axle smaller.
Are you saying to bore into the swingarm as to make the axle inside of it basically? Not really down on removing material from the already weak link in a chain

coolbobjoe   1 W

1 W
Posts: 60
Joined: Jul 06 2017 4:03am

Re: Hot-setting 6061 Frame

Post by coolbobjoe » Feb 12 2018 9:54pm

Chalo wrote:
Feb 12 2018 7:06pm
Please register and insure your motorcycle, and stay out of bicycle facilities. Thanks.
Work in a bicycle shop so can't really get out of here! lololol but seriously please take the hate somewhere else though! We have videos of people doing near 100mph through the streets on their bikes on here.... :lol:

SlowCo   100 kW

100 kW
Posts: 1468
Joined: Jan 05 2015 5:43pm
Location: The Netherlands

Re: Hot-setting 6061 Frame

Post by SlowCo » Feb 13 2018 1:32pm

coolbobjoe wrote:
Feb 12 2018 8:24pm
SlowCo wrote:
Feb 12 2018 7:02pm
If you will go to a single speed then just mill the axle flats further so you make the drop out width of the axle smaller.
Are you saying to bore into the swingarm as to make the axle inside of it basically? Not really down on removing material from the already weak link in a chain
No.
Remove the axle from the motor and (have someone) mill the axle flats further to the center both sides as much as possible. On the disk brake side as much so the disk has minimum clearance with the swing arm. You could even turn down the aluminium motor cover so the disk sits closer to the cover if you will use a bicycle brake caliper (slimmer than a scooter caliper). On the freewheel side mill the flats as much so the single speed freewheel can just rotate freely. Maybe you can gain enough to get the drop out width of the axle closer to the inside width of the swing arm so just a little stretching is necessary.

WoodlandHills   10 kW

10 kW
Posts: 749
Joined: Nov 11 2015 12:27pm
Location: Ortega River, JAX, FL

Re: Hot-setting 6061 Frame

Post by WoodlandHills » Feb 13 2018 1:50pm

I would be very surprised if you could find a heat treater willing to take on your project due to the liability issues. If you do find a shop to do the work for you may find that the process distorts your part requiring cold straightening afterwards. If I was building a cycle capable of 100mph+ speeds I would want to be sure the work was done correctly and would want any welder to be certified and any heat treater to be certified for aviation/aerospace work.

coolbobjoe   1 W

1 W
Posts: 60
Joined: Jul 06 2017 4:03am

Re: Hot-setting 6061 Frame

Post by coolbobjoe » Feb 13 2018 1:54pm

SlowCo wrote:
Feb 13 2018 1:32pm
coolbobjoe wrote:
Feb 12 2018 8:24pm
SlowCo wrote:
Feb 12 2018 7:02pm
If you will go to a single speed then just mill the axle flats further so you make the drop out width of the axle smaller.
Are you saying to bore into the swingarm as to make the axle inside of it basically? Not really down on removing material from the already weak link in a chain
No.
Remove the axle from the motor and (have someone) mill the axle flats further to the center both sides as much as possible. On the disk brake side as much so the disk has minimum clearance with the swing arm. You could even turn down the aluminium motor cover so the disk sits closer to the cover if you will use a bicycle brake caliper (slimmer than a scooter caliper). On the freewheel side mill the flats as much so the single speed freewheel can just rotate freely. Maybe you can gain enough to get the drop out width of the axle closer to the inside width of the swing arm so just a little stretching is necessary.
Ah, very interesting idea!

SlowCo   100 kW

100 kW
Posts: 1468
Joined: Jan 05 2015 5:43pm
Location: The Netherlands

Re: Hot-setting 6061 Frame

Post by SlowCo » Feb 13 2018 3:05pm

I did this to a 9C hub motor. It only needed one side and 7mm milling to fit but I liked that better than expanding the aluminium swing arm of my bike.

User avatar
amberwolf   100 GW

100 GW
Posts: 30778
Joined: Aug 17 2009 6:43am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: Hot-setting 6061 Frame

Post by amberwolf » Feb 13 2018 4:28pm


User avatar
Chalo   100 GW

100 GW
Posts: 7961
Joined: Apr 29 2009 11:29pm
Location: Austin, Texas

Re: Hot-setting 6061 Frame

Post by Chalo » Feb 13 2018 5:17pm

coolbobjoe wrote:
Feb 12 2018 9:54pm
Chalo wrote:
Feb 12 2018 7:06pm
Please register and insure your motorcycle, and stay out of bicycle facilities. Thanks.
Work in a bicycle shop so can't really get out of here! lololol but seriously please take the hate somewhere else though! We have videos of people doing near 100mph through the streets on their bikes on here.... :lol:
I also work in a bicycle shop, and in a pedicab fab shop. I ride and build e-bikes and I design and build e-pedicabs. I don't hate them. But your bike isn't a bicycle; it's a motorcycle. I don't hate those either, but they have their own set of rules that exists whether you like it or not. Follow them.
This is to express my gratitude to Justin of Grin Technologies for his extraordinary measures to save this forum for the benefit of all.

User avatar
liveforphysics   100 GW

100 GW
Posts: 14134
Joined: Oct 29 2008 1:48am
Location: Santa Cruz, CA, USA

Re: Hot-setting 6061 Frame

Post by liveforphysics » Feb 13 2018 5:28pm

WoodlandHills wrote:
Feb 13 2018 1:50pm
I would be very surprised if you could find a heat treater willing to take on your project due to the liability issues. If you do find a shop to do the work for you may find that the process distorts your part requiring cold straightening afterwards. If I was building a cycle capable of 100mph+ speeds I would want to be sure the work was done correctly and would want any welder to be certified and any heat treater to be certified for aviation/aerospace work.

You actually only get one shot at welding and heat-treating an area afterwards. Because the HAZ area precipitates out various alloying components in the 6061, it can not longer achieve T-6 temper on a re-treatment, and is lucky to achieve T-4 on a second treatment even if you had the best aerospace guys in the world doing it.

A bunch of distributed cold bend locations, each with only a small amount of metal displacement to not begin a crack formation, and no heating involved would be the path forward for high strength.

If it's aluminum that's already been welded and heat treated, and you heat it or weld it again after, it's become scrap metal.
Each carcinogen vapor exposure includes a dice roll for cancer.

Each mutagen vapor exposure includes a dice roll for reproductive genetic defects in your children.

Each engine start sprays them into a shared atmosphere which includes beings not offered an opportunity to consent accepting these cancer experiences and defective genetics life experiences.

Every post is a free gift to the collective of minds composing the living bleeding edge of LEV development on our spaceship.

Post Reply