Snapped axle on Crystalyte TC100 hub motor, almost died

Get all your technical information about electric bikes here.
NeedForSpeed   1 W

1 W
Posts: 64
Joined: Dec 31 2017 12:25pm

Snapped axle on Crystalyte TC100 hub motor, almost died

Post by NeedForSpeed » Aug 30 2018 6:32pm

:shock: almost killed myself, luckily I was just taking off from a stop light when the left axle of my hub motor snapped off.

My initial shock has led me to think of scrapping the whole thing cause I could have easily been dead if it happened at 45pmh.

I am pretty sure there was just way too much reverse torque going on, cause I had my regen setup to kick in when the throttle is released, so there was pretty frequent torquing going on for the last few months, plus the bike is pretty heavy ~120lbs plus me at 220lbs which I imagine wasn’t helping. The frame is all steel (EEB Full Suspension frame), so i didn't think about also strapping on some torque arms, which may have helped.

Anyways, curious if this happened to anyone else.

I _may_ consider replacing the axle (any advice on that would be appreciated) and then just turn regen down a ton, or turn it off all together. I’m also considering just selling everything cause I don’t want to be driving a death trap, and maybe I can convince my wife to let me buy a motorcycle since that’s really why I built this big ass bike in the first place.

So if anyone is interested in buying parts, I might list them out and give a good discount. Not sure yet.
Image from iOS.jpg
Image from iOS (4).jpg
Image from iOS (4).jpg (474.95 KiB) Viewed 2002 times
Image from iOS (3).jpg
Image from iOS (2).jpg
Image from iOS (2).jpg (396.09 KiB) Viewed 2002 times
Image from iOS (1).jpg
Image from iOS (1).jpg (313.7 KiB) Viewed 2002 times
https://www.instagram.com/bostonebiker/

I like to go fast 😎. Currently maintaining and improving a custom EEB frame build with a QS 273 motor and sabvoton controller. Custom built 20s10p battery with LG HG2 cells.

User avatar
Chalo   100 GW

100 GW
Posts: 9014
Joined: Apr 29 2009 11:29pm
Location: Austin, Texas

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by Chalo » Aug 30 2018 7:13pm

That's the wrong way to anchor the hub's reaction torque, and now you understand why. How does it feel that this obvious bad design was for the purpose of the manufacturer saving maybe one dollar?

Edit:

I can see how the above would be interpreted as chastising the OP for not using torque arms. That's not what I was trying to say, though. I was calling out the manufacturer along with all the other Chinese hub motor manufacturers for using a flatted axle to transmit torque. Its dumb.
Last edited by Chalo on Aug 31 2018 1:27pm, edited 1 time in total.
This is to express my gratitude to Justin of Grin Technologies for his extraordinary measures to save this forum for the benefit of all.

User avatar
liveforphysics   100 GW

100 GW
Posts: 14167
Joined: Oct 29 2008 1:48am
Location: Long Beach, CA, USA

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by liveforphysics » Aug 30 2018 7:15pm

Double sided strong torque arms can help keep the torque forces balanced between both ends of the axle. That snap looks like it may be corrosion initiated fracture propagation.
Each carcinogen vapor exposure includes a dice roll for cancer.

Each mutagen vapor exposure includes a dice roll for reproductive genetic defects in your children.

Each engine start sprays them into a shared atmosphere which includes beings not offered an opportunity to consent accepting these cancer experiences and defective genetics life experiences.

Every post is a free gift to the collective of minds composing the living bleeding edge of LEV development on our spaceship.

User avatar
wturber   10 MW

10 MW
Posts: 2131
Joined: Aug 23 2017 8:52pm
Location: Fountain Hills,AZ
Contact:

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by wturber » Aug 30 2018 7:27pm

liveforphysics wrote:
Aug 30 2018 7:15pm
Double sided strong torque arms can help keep the torque forces balanced between both ends of the axle. That snap looks like it may be corrosion initiated fracture propagation.
That's what I was thinking as well. The perimeter of the break is rust colored which makes me think this failure has been in progress for some time now.
"Commuter - DC Booster"
Iron Horse 3.0 hardtail - 48V / 1000W / 470rpm generic Chinese DD Hub motor (ebay)
8 x 36v 4.3ah 10s 2P battery packs - 1500W 30A DC Boost Converter delivers 54v and about 1000 watts peak
53T/42T Sakae Road cranks - 30mph+ on flats
viewtopic.php?f=2&t=90369

User avatar
wturber   10 MW

10 MW
Posts: 2131
Joined: Aug 23 2017 8:52pm
Location: Fountain Hills,AZ
Contact:

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by wturber » Aug 30 2018 7:35pm

400% digital magnification here. It would be better to get a close-up photo and not use the digital processing. Nonetheless, rust preceding the break seems pretty obvious. So did it crack first, rust a bit, and then break or did corrosion on the outside spread inward? That's well beyond my expertise level.

CorrosionFailure.jpg
"Commuter - DC Booster"
Iron Horse 3.0 hardtail - 48V / 1000W / 470rpm generic Chinese DD Hub motor (ebay)
8 x 36v 4.3ah 10s 2P battery packs - 1500W 30A DC Boost Converter delivers 54v and about 1000 watts peak
53T/42T Sakae Road cranks - 30mph+ on flats
viewtopic.php?f=2&t=90369

User avatar
Chalo   100 GW

100 GW
Posts: 9014
Joined: Apr 29 2009 11:29pm
Location: Austin, Texas

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by Chalo » Aug 30 2018 7:46pm

wturber wrote:
Aug 30 2018 7:27pm
liveforphysics wrote:
Aug 30 2018 7:15pm
That snap looks like it may be corrosion initiated fracture propagation.
That's what I was thinking as well. The perimeter of the break is rust colored which makes me think this failure has been in progress for some time now.
That's how metal fatigue works. You get a microscopic crack, and it progresses at a slow but exponentially accelerating pace as the part is stressed. When there isn't enough material left to carry the load, it breaks.

Corrosion could have been the cause of the initial crack, but then so could have poor workmanship (e.g. sharp inside corner, flawed surface finish). But the real cause is the needlessly high material stress level due to the torque carrying interface being too small for the job it's being asked to do.

There is no valid excuse for this now pervasive bad design. Heinzmann was in the business first, and the way they solved the problem is both effective and cheap:
Image
This is to express my gratitude to Justin of Grin Technologies for his extraordinary measures to save this forum for the benefit of all.

User avatar
zro-1   1 kW

1 kW
Posts: 360
Joined: Jul 31 2012 9:09am
Location: Atlanta, GA
Contact:

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by zro-1 » Aug 30 2018 8:01pm

I am no chemist, but in my research into electroplating and oxidation, I've come to understand that oxidation only happens at the surface, where oxygen can come into contact with the metal.

Since there's rust penetrating in to where the faces of the axle were machined from the main part of the axle, I'd say the crack had started before the failure. That being said, oxidation expands surface area, so corrosion getting in to that part of the axle would have created outward forces that could have accelerated the failure (like Ice expanding in cracked pavement).

NeedForSpeed: I'm really glad you're OK. In this case, since the cracking started at the base of the point where the flats were machined, I don't agree with Chalo's comment (I'm not trying to start a flame-war here) that torque arms would have prevented this. A torque arm placed right against that face where the cable exits still wouldn't have prevented that particular fracture (IMHO). In any case, I'm glad you're OK, and please don't let this turn you off to eBikes.

EDIT: I was writing this as Chalo was posting his follow-up comment. My comments are only pertaining to his original post in this thread.
~01~

User avatar
zro-1   1 kW

1 kW
Posts: 360
Joined: Jul 31 2012 9:09am
Location: Atlanta, GA
Contact:

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by zro-1 » Aug 30 2018 8:06pm

Chalo wrote:
Aug 30 2018 7:46pm
Corrosion could have been the cause of the initial crack, but then so could have poor workmanship (e.g. sharp inside corner, flawed surface finish).
I agree with this part of Chalo's follow-up. I think that point where the flats and the rest of the axle met up was the weak point. Again, just my humble opinion.

EDIT AGAIN:
I guess what I'm trying to say is that based on where the break happened, even with 2 or 4 torque arms, the break would have happened eventually. The TAs may have slowed it down a little, but I think it was inevitable based on where the break happened.
Last edited by zro-1 on Aug 30 2018 8:15pm, edited 1 time in total.
~01~

User avatar
wturber   10 MW

10 MW
Posts: 2131
Joined: Aug 23 2017 8:52pm
Location: Fountain Hills,AZ
Contact:

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by wturber » Aug 30 2018 8:12pm

I think you are missing Chalo's point. His point was that the torque should not be carried by the small dimensions of a flattened axle. He'd agree that an added torque arm would not help. His point is that the Heinzmann design distributes the torque through material of a larger dimension resulting in smaller localized stresses and a more robust and reliable design.

Or more directly, he's saying the flattened axle design is garbage.
"Commuter - DC Booster"
Iron Horse 3.0 hardtail - 48V / 1000W / 470rpm generic Chinese DD Hub motor (ebay)
8 x 36v 4.3ah 10s 2P battery packs - 1500W 30A DC Boost Converter delivers 54v and about 1000 watts peak
53T/42T Sakae Road cranks - 30mph+ on flats
viewtopic.php?f=2&t=90369

User avatar
zro-1   1 kW

1 kW
Posts: 360
Joined: Jul 31 2012 9:09am
Location: Atlanta, GA
Contact:

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by zro-1 » Aug 30 2018 8:16pm

Ohhhh OK. I get it now. Sorry for being slow on that and adding noise to the thread.
~01~

User avatar
e-beach   1.21 GW

1.21 GW
Posts: 3867
Joined: Jan 10 2012 9:48pm
Location: Any Los Angeles area beach I am at. Or Santa Monica or possibly the south bay beaches.

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by e-beach » Aug 30 2018 9:57pm

Is it the pictures, or did that axle have rust almost to the middle? It looks like is was cracking for a while from the pictures.
Favorite Quotes:
"This is L.A., sugar. There is no 'over the top." Chris Erskine
"At a certain point the entropy wins." Maria Helena Braga

Current Build: ProFlex 757 Expert full suspension. Yescomusa 36v 800w Rear DD, upgraded 10AWG solid core through axle phase wires. 15ah Headway, 1000+ cycles, 80% DOD 30A Tronsung controller.

Past: Trek 4500 Yescomusa 36v 800w front DD.
Liahona, Yescomusa 36v 800w generic front DD.
1992 Trek 800, Yescomusa 800w 36v front DD.

User avatar
madin88   1 GW

1 GW
Posts: 3120
Joined: May 27 2013 2:02am
Location: Austria

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by madin88 » Aug 31 2018 2:30am

What a luck that this happened at low speed.

When a axle brakes, it often is because the nut has been tightened to much and then the capability to transfer torque suffers.
Or with other words: for lowering the stress on the axle you should tight the nut just A LITTLE BIT and the clamping dropouts will do the rest (of course given that the alignment is ok and there is no play in the dropouts).
If there is some play (you often can hear a "click" when switching between regen / accelerating), people often think the big nut needs to be tightened more, but this is not good. Better reduce the play by adding small metal sheets (available in 0,05mm or less) so the clamping mechanism function properly.

I am not saying you did something wrong, i just wanted to bring this up as it is really important.
- 10kW belt drive with Neumotor 8057: [url]viewtopic.php?
- KTM Hardtail Pedelec / eZee V2 6T / 27,5" / Kelly KBSX @ 1,5kW / Torque PAS / CA-V3 / 13s4p Sanyo GA in Shark case

Warren   100 kW

100 kW
Posts: 1417
Joined: Oct 05 2010 11:35am

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by Warren » Aug 31 2018 11:39am

Well f__k! I have a TC4080 on a 130 pound, non-suspension bike with vertical steel dropouts, running two Grin torque arms. I do all my braking, down to 12 mph where the regen drops out, regen only, up to -2000 watts, for 17K miles now. I figured I was golden with the two torque arms. This has put a little brown in my shorts, for sure. :-(

billvon   1 GW

1 GW
Posts: 3051
Joined: Sep 16 2007 9:53pm
Location: san diego

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by billvon » Aug 31 2018 12:57pm

madin88 wrote:
Aug 31 2018 2:30am
When a axle brakes, it often is because the nut has been tightened to much and then the capability to transfer torque suffers.
Or with other words: for lowering the stress on the axle you should tight the nut just A LITTLE BIT and the clamping dropouts will do the rest (of course given that the alignment is ok and there is no play in the dropouts).
If there is some play (you often can hear a "click" when switching between regen / accelerating), people often think the big nut needs to be tightened more, but this is not good. Better reduce the play by adding small metal sheets (available in 0,05mm or less) so the clamping mechanism function properly.
Agree you should not overtighten.

However, undertightening (so you get the axle moving back and forth slightly every regen/accel cycle) can be worse.

1) You are loosening the nut a little every time, so you have to keep tightening it daily.
2) Every time it hits its limits it wears the contact point a little more. Wear it enough and it will cam out.

The right solution is a non-axle-based torque arm, like the old EMS system used to use (and like Justin's hub uses.) But absent that, you have to find the tightening torque that prevents motion but also doesn't overstress the axle.
--bill von

User avatar
fechter   100 GW

100 GW
Posts: 15405
Joined: Dec 31 2006 3:23pm
Location: California Bay Area, USA

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by fechter » Aug 31 2018 1:17pm

There are several factors involved here. One is corrosion. It looks pretty obvious there was significant corrosion going on. If the axle was never exposed to water, it may have survived longer, maybe much longer. Another factor is high stress. Balancing the forces on both sides of the motor would help as Luke pointed out. High regen levels also increase the stresses. If the stress is high enough for the metal to exceed the elastic range, it will fail quite quickly. Intrinsically shitty design is another factor, as Chalo points out. Using flats on an axle might be OK for a 250w motor, but even at 750w they tend to spin out.

So how to avoid this? Avoid all of the above or mitigate them.

I avoid riding in the rain, but somebody who commutes may not have this option. Paint, oil or something to inhibit corrosion around the area would help.

Balance the torque on both sides of the axle as much as possible (two torque arms).

Use the proper torque to tighten the nuts. Too much or not enough are both bad.

Limit how much regen or thrust is used. Ideally we'd want to not have a limit other than where the tire skids, but hammering back and forth between throttle and regen seems to be particularly destructive. Take any piece of metal and bend it back and forth a bunch of times and see what happens.

The best thing is to avoid this kind of design all together. If the axle was sufficiently large in cross section it would work OK. The more power you run, the bigger it needs to be.
"One test is worth a thousand opinions"

999zip999   100 GW

100 GW
Posts: 10089
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by 999zip999 » Aug 31 2018 1:38pm

I don't see any torque arm pics. I missing something.?

User avatar
wturber   10 MW

10 MW
Posts: 2131
Joined: Aug 23 2017 8:52pm
Location: Fountain Hills,AZ
Contact:

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by wturber » Aug 31 2018 1:54pm

999zip999 wrote:
Aug 31 2018 1:38pm
I don't see any torque arm pics. I missing something.?
He wasn't using torque arms per se. But the axle never spun out either.

So I zoomed into the dropouts in his picture, and it seems to me that the steel there is 5/16" thick or even thicker. These aren't your typical dropouts from what I can see. You might think of them as having integral torque arms. It's anybody's guess how hard he torques down the axle nuts.


dropouts.jpg
dropouts.jpg (71.7 KiB) Viewed 1879 times
"Commuter - DC Booster"
Iron Horse 3.0 hardtail - 48V / 1000W / 470rpm generic Chinese DD Hub motor (ebay)
8 x 36v 4.3ah 10s 2P battery packs - 1500W 30A DC Boost Converter delivers 54v and about 1000 watts peak
53T/42T Sakae Road cranks - 30mph+ on flats
viewtopic.php?f=2&t=90369

User avatar
wturber   10 MW

10 MW
Posts: 2131
Joined: Aug 23 2017 8:52pm
Location: Fountain Hills,AZ
Contact:

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by wturber » Aug 31 2018 1:59pm

BTW, the "almost died" in the title reminds me of this bit by Ron White.


"Commuter - DC Booster"
Iron Horse 3.0 hardtail - 48V / 1000W / 470rpm generic Chinese DD Hub motor (ebay)
8 x 36v 4.3ah 10s 2P battery packs - 1500W 30A DC Boost Converter delivers 54v and about 1000 watts peak
53T/42T Sakae Road cranks - 30mph+ on flats
viewtopic.php?f=2&t=90369

markz   100 GW

100 GW
Posts: 12227
Joined: Jan 09 2014 11:38pm

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by markz » Aug 31 2018 3:46pm

NeedForSpeed wrote:
Aug 30 2018 6:32pm
45pmh.
I had to convert to get an idea of speed
45mph = 72kph
On a bicycle, with bicycle parts.

Glad nothing happened to you.

User avatar
wturber   10 MW

10 MW
Posts: 2131
Joined: Aug 23 2017 8:52pm
Location: Fountain Hills,AZ
Contact:

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by wturber » Aug 31 2018 4:32pm

markz wrote:
Aug 31 2018 3:46pm
NeedForSpeed wrote:
Aug 30 2018 6:32pm
45pmh.
I had to convert to get an idea of speed
45mph = 72kph
On a bicycle, with bicycle parts.
Like he said, he got this instead of getting a motorcycle. The way I see it, he basically built a low powered motorcycle.
"Commuter - DC Booster"
Iron Horse 3.0 hardtail - 48V / 1000W / 470rpm generic Chinese DD Hub motor (ebay)
8 x 36v 4.3ah 10s 2P battery packs - 1500W 30A DC Boost Converter delivers 54v and about 1000 watts peak
53T/42T Sakae Road cranks - 30mph+ on flats
viewtopic.php?f=2&t=90369

NeedForSpeed   1 W

1 W
Posts: 64
Joined: Dec 31 2017 12:25pm

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by NeedForSpeed » Sep 02 2018 12:05pm

Thanks for all the replies, interesting stuff, I hadn’t considered rust as potential the culprit, or a contributor.

Yea that’s an all steel frame and pretty thick, so didn’t think torque arms were even necessary.

And yes all bicycle components, aside from the all steel frame, but they’re all pretty heavy duty downhill MTB parts, which I figured could handle the stress okay for the most part (eg rock shox double dual crown fork, Magura brakes)

Thinking about things some more, I’m realizing the only thing that really freaks me out about building a DIY high speed bike is the axle torque on a hub motor. I’m now considering a mid drive motor instead, Potentially a MARS 0913. My hub motor days are behind me.
https://www.instagram.com/bostonebiker/

I like to go fast 😎. Currently maintaining and improving a custom EEB frame build with a QS 273 motor and sabvoton controller. Custom built 20s10p battery with LG HG2 cells.

User avatar
wturber   10 MW

10 MW
Posts: 2131
Joined: Aug 23 2017 8:52pm
Location: Fountain Hills,AZ
Contact:

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by wturber » Sep 02 2018 12:19pm

You might want to look at TangentDave's motor.

viewtopic.php?f=28&t=70099
"Commuter - DC Booster"
Iron Horse 3.0 hardtail - 48V / 1000W / 470rpm generic Chinese DD Hub motor (ebay)
8 x 36v 4.3ah 10s 2P battery packs - 1500W 30A DC Boost Converter delivers 54v and about 1000 watts peak
53T/42T Sakae Road cranks - 30mph+ on flats
viewtopic.php?f=2&t=90369

SirLongAss   100 mW

100 mW
Posts: 47
Joined: Aug 26 2018 10:55am

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by SirLongAss » Sep 02 2018 10:30pm

I don't wanna sound like a dick but this is what happens when you aren't doing checks/maintenance. The rust was clearly visble outside the axle and if I saw it on my bike's axle, I'd be very suspicious.

NeedForSpeed   1 W

1 W
Posts: 64
Joined: Dec 31 2017 12:25pm

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by NeedForSpeed » Sep 03 2018 12:42am

Fair enough. My defense is ignorance. Hadn’t considered that would ever be an issue.
https://www.instagram.com/bostonebiker/

I like to go fast 😎. Currently maintaining and improving a custom EEB frame build with a QS 273 motor and sabvoton controller. Custom built 20s10p battery with LG HG2 cells.

User avatar
Chalo   100 GW

100 GW
Posts: 9014
Joined: Apr 29 2009 11:29pm
Location: Austin, Texas

Re: Snapped axle on Crystalyte TC100 hub motor, almost died

Post by Chalo » Sep 03 2018 1:08am

SirLongAss wrote:
Sep 02 2018 10:30pm
I don't wanna sound like a dick but this is what happens when you aren't doing checks/maintenance. The rust was clearly visble outside the axle and if I saw it on my bike's axle, I'd be very suspicious.
I don't think that's true at all. I work on all kinds of rusty bikes with all kinds of high mileage, and rust has not caused them to break. This is the consequence of bad, lazy, cheapskate design and poor manufacturing, and nothing else.

Rust makes fasteners stick, sometime permanently. It's ugly, and it can abrade moving parts. But rust doesn't get inside a metal part unless that part is cracked. This part cracked because it sucked, not because it had rust on it.
This is to express my gratitude to Justin of Grin Technologies for his extraordinary measures to save this forum for the benefit of all.