Hi All,
I was recently given a Cyclamatic Power Plus. The cycle parts on the bike seem good (apart from BB bearings, replaced now), so I decided to build a new battery pack for it.
I picked up 30 Panasonic NCR18650PFs and a Vruzend V2 kit. I also bought a cheap 10s BMS from ebay (https://www.ebay.co.uk/itm/262605636328) and a cheap 42V 2A charger.
Pack built, all looks good when not connected to anything. I got 35.2V when first built, all cells were individually tested at 3.52V, and each bank of 3 cells were looking good. As soon as I connect it to any load, voltage drops to near zero, but the actual value does seem to vary (up to 3V some times). The load can be the controller on its own, without the motor or throttle connected, but also got the same result when hooking it up to a fan heater.
I have double checked the wiring, but this is my first build so I am not excluding some newbie error here. I have checked the balance connectors using the points on the back of the PCB and between the battery -ve and ech wire I get the expected 3.52V, 7.04V etc. If I connect the same load directly to the battery terminals, everything seems fine. I also get working output if I connect the charger to the charge leads, and connect the load via the BMS.
I have charged the battery up to 4.0V and the same behavior exists. I am currently charging it up to full to see if that makes any difference.
I have raised a request with the eBay seller to suggest anything before I file a return, but am looking for any suggestions on what else could be wrong.
I was recently given a Cyclamatic Power Plus. The cycle parts on the bike seem good (apart from BB bearings, replaced now), so I decided to build a new battery pack for it.
I picked up 30 Panasonic NCR18650PFs and a Vruzend V2 kit. I also bought a cheap 10s BMS from ebay (https://www.ebay.co.uk/itm/262605636328) and a cheap 42V 2A charger.
Pack built, all looks good when not connected to anything. I got 35.2V when first built, all cells were individually tested at 3.52V, and each bank of 3 cells were looking good. As soon as I connect it to any load, voltage drops to near zero, but the actual value does seem to vary (up to 3V some times). The load can be the controller on its own, without the motor or throttle connected, but also got the same result when hooking it up to a fan heater.
I have double checked the wiring, but this is my first build so I am not excluding some newbie error here. I have checked the balance connectors using the points on the back of the PCB and between the battery -ve and ech wire I get the expected 3.52V, 7.04V etc. If I connect the same load directly to the battery terminals, everything seems fine. I also get working output if I connect the charger to the charge leads, and connect the load via the BMS.
I have charged the battery up to 4.0V and the same behavior exists. I am currently charging it up to full to see if that makes any difference.
I have raised a request with the eBay seller to suggest anything before I file a return, but am looking for any suggestions on what else could be wrong.