Dave's 80:1 RC mid drive kit build log

Discussions related to motors other than hub motors.
This includes R/C motors, botttom bracket, roller and geared drives.
knurf   10 W

10 W
Posts: 78
Joined: Aug 29 2016 12:15am

Re: Dave's 80:1 RC mid drive kit build log

Post by knurf » Aug 04 2018 6:17pm

I'd say try it out first, especially if its a 3220 kit or similar. There's a lot of torque to go around..

User avatar
tangentdave   1 kW

1 kW
Posts: 436
Joined: Jun 06 2015 11:40am
Location: Seattle, WA
Contact:

Re: Dave's 80:1 RC mid drive kit build log

Post by tangentdave » Aug 04 2018 6:24pm

36t rear with a 32t front is enough to climb any trail. You could go larger rear if your wanted to make climbing the sides of quarry pits easy on the motor, but the 36t/32t combo could do that too.
GGMT/Tangent 8kW
tangentmotors.com

User avatar
cr0m08   100 mW

100 mW
Posts: 41
Joined: Feb 09 2015 9:21am
Location: Perth, Australia

Re: Dave's 80:1 RC mid drive kit build log

Post by cr0m08 » Aug 05 2018 3:17am

I can confirm the 3220 kit has loads of grunt. I'm running 20-38 motor-crank 32-17/34 rear. Damn thing lifts front wheel in lowest 3 gears, I mean seriously gotta be carful on throttle.
But if you really want to run a saint to a 42T..... just fit the Oneup RadR cage on the saint. But I don't think you need it!
https://www.oneupcomponents.com/products/radr-cage
I put Rad cage (not RadR) on my shadow XT 10 speed and it reaches 42T no problem.
2015 Nukeproof Pulse, 3220/HV160 @12S V1.5, 26x2.8" Nextie 50mm wheel set
2006 KeeWee Cromo Eight, 3210/HV80 @12S V1.5, 24x3" wheel set.
1998 Marin B17, Mac 10T @18S in 19" Kris Holme Trials rims, 19x2.5" wheel set (still to finish)
part build Basman 346, QS205 hub motor @12S in 24x3" wheel set. (still to finish)

Ham   100 W

100 W
Posts: 291
Joined: Feb 18 2016 3:08am

Re: Dave's 80:1 RC mid drive kit build log

Post by Ham » Aug 05 2018 3:45am

tangentdave wrote:
Aug 04 2018 12:52pm
John's Airborne Plauge uses a 168mm long mount. There's not much room between the crankset and the motor freewheel for a tension device if the two centers are closer (168 from center of BB to center of motor). Perhaps a gear solution like the Paradox kit could get it closer...but chains are pretty damn robust.
Thanks Dave, much appreciated. Still exploring options for the mounting on a new frame
http://www.HamsFitness.com Strength, Conditioning & Diet

User avatar
tangentdave   1 kW

1 kW
Posts: 436
Joined: Jun 06 2015 11:40am
Location: Seattle, WA
Contact:

Re: Dave's 80:1 RC mid drive kit build log

Post by tangentdave » Aug 09 2018 12:00pm

Ok, have posted a couple 'service bulletins' on the website. Nothing ground breaking- how to shift the BB spindle left/right for chainline and a walk through of the greasing interval. It's looking like an initial grease change around the 100-200 mile point isn't a bad idea, and probably every 500-750 miles thereafter (depending on abuse of course). If you're like me and ride with enough throttle to keep the unit at 100C, a more frequent grease interval isn't a bad idea either. Vigogrease has a pretty high operating temp (over 300F), but changing the grease literally only takes a few minutes and it's cheap stuff.

The only tools needed for the maintentance are a 4mm hex wrench, a long M6 bolt that's fully threaded, and Vigogrease. All this is available online and I've made up little packets for people if they prefer to not to think about it. I also add a touch of hexagonal Boron Nitride to the Tangent grease. Each dispenser holds 20mL and is the proper amount to use during the maintenance.

20180808_135350.jpg
GGMT/Tangent 8kW
tangentmotors.com

totolito   100 mW

100 mW
Posts: 35
Joined: Jul 20 2012 12:17pm

Re: Dave's 80:1 RC mid drive kit build log

Post by totolito » Aug 10 2018 3:24am

Thanks Dave, I have to get one!

E1Allen   1 mW

1 mW
Posts: 19
Joined: Mar 26 2018 4:20am

Re: Dave's 80:1 RC mid drive kit build log

Post by E1Allen » Aug 13 2018 8:58pm

Do you include a grease kit with the initial purchase for the 100m grease swap?

Ham   100 W

100 W
Posts: 291
Joined: Feb 18 2016 3:08am

Re: Dave's 80:1 RC mid drive kit build log

Post by Ham » Aug 14 2018 8:51am

Hi Guys,

I have a a few questions if anyone can help.

I am looking to relocate my controller and am wondering if the standard 8 awg wiring for the kit is suitable for extending the three cables from the motor to the controller or if something more heavy duty is required to handle phase currents as the motor cables are much stiffer due to a heavy copper (?) fill?

Also I am exploring the possibility of power isolation switches for the battery like the big reg key ones we see on track cars, now I assume they are rated for very high cranking amps so could handle the 100-150 ish battery amps we pull for the 3220 motor but I am trying to find what the continuous rating is for them as I'd hate to install one and then melt it immediately!

This power isolation switch also led me to wondering about if we can install a secondary key switch for the cycle analyst...just an added layer of security?

Thanks for any help
http://www.HamsFitness.com Strength, Conditioning & Diet

E1Allen   1 mW

1 mW
Posts: 19
Joined: Mar 26 2018 4:20am

Re: Dave's 80:1 RC mid drive kit build log

Post by E1Allen » Aug 14 2018 2:20pm

I am looking to relocate my controller and am wondering if the standard 8 awg wiring for the kit is suitable for extending the three cables from the motor to the controller or if something more heavy duty is required to handle phase currents as the motor cables are much stiffer due to a heavy copper (?) fill?

Where were you thinking about relocating to? Shorter phase wires the better. I think I have about 12" phase wires on my eskate. 8ga phase wires I think is plenty on short distances.

User avatar
tangentdave   1 kW

1 kW
Posts: 436
Joined: Jun 06 2015 11:40am
Location: Seattle, WA
Contact:

Re: Dave's 80:1 RC mid drive kit build log

Post by tangentdave » Aug 14 2018 3:05pm

Personally, I'd use 8ga to extend the phase wires. The Astro phase cables seem stiff because they're made of fewer but thicker individual copper strands than 'flexible' cables with many tiny strands. The length of wire between the ESC and engine is much less important than the length between ESC and battery pack (although never disconnect the ESC while engine is turning, catastrophic ESC damage can result).

E1, your kit will have a maintenance packet, they all will.
GGMT/Tangent 8kW
tangentmotors.com

Clyon2   1 mW

1 mW
Posts: 13
Joined: Dec 10 2017 9:21am

Re: Dave's 80:1 RC mid drive kit build log

Post by Clyon2 » Aug 14 2018 4:41pm

Re battery isolation: After an event that let all the magic smoke out of my Luna switch, I installed a switchable breaker rated at 48 V, 150 amps. Different values are available to be chosen depending on where you want the circuit to blow. This is under rated for a 52 v battery, however as we are not switching under load and will infrequently flip the breaker - I am betting it will last with little risk of arcing welding contacts or other dire failures.
Bussmann CB285-150 Surface-Mount Circuit Breakers, 150 Amps

Working well so far.

knurf   10 W

10 W
Posts: 78
Joined: Aug 29 2016 12:15am

Re: Dave's 80:1 RC mid drive kit build log

Post by knurf » Aug 14 2018 11:25pm

Just being able to quickly reach the main battery XT90 provides with a lot of safety already. I’ve had to pull it on a runaway throttle once (on another bike, not a tangent kit) and it was pretty controlled.

But I would like a motorcycle style killswich too, reachable by just moving my thumb. Letting go of the handlebar in that situation can be a bit scary :)

Ham   100 W

100 W
Posts: 291
Joined: Feb 18 2016 3:08am

Re: Dave's 80:1 RC mid drive kit build log

Post by Ham » Aug 14 2018 11:26pm

tangentdave wrote:
Aug 14 2018 3:05pm
Personally, I'd use 8ga to extend the phase wires. The Astro phase cables seem stiff because they're made of fewer but thicker individual copper strands than 'flexible' cables with many tiny strands. The length of wire between the ESC and engine is much less important than the length between ESC and battery pack (although never disconnect the ESC while engine is turning, catastrophic ESC damage can result).

E1, your kit will have a maintenance packet, they all will.
Thanks Dave,

I'll pick some more up tomorrow. I was only asking as I assumed the motor wire needed to be thicker due to higher peak phase amps and having melted my battery wires already :)
http://www.HamsFitness.com Strength, Conditioning & Diet

User avatar
cr0m08   100 mW

100 mW
Posts: 41
Joined: Feb 09 2015 9:21am
Location: Perth, Australia

Re: Dave's 80:1 RC mid drive kit build log

Post by cr0m08 » Aug 15 2018 12:15am

From the CastleCreations site on wiring for ESC,
"With a sensorless brushless system, extremely low resistance wire is required to enable the ESC to read the extremely low voltage back EMF; this is crucial in ensuring smooth easy motor starts."
I thought I also remember reading the phase wires should be kept short for the same reason, but I can't find it at moment (um maybe I got that bit wrong :shock: )
2015 Nukeproof Pulse, 3220/HV160 @12S V1.5, 26x2.8" Nextie 50mm wheel set
2006 KeeWee Cromo Eight, 3210/HV80 @12S V1.5, 24x3" wheel set.
1998 Marin B17, Mac 10T @18S in 19" Kris Holme Trials rims, 19x2.5" wheel set (still to finish)
part build Basman 346, QS205 hub motor @12S in 24x3" wheel set. (still to finish)

knurf   10 W

10 W
Posts: 78
Joined: Aug 29 2016 12:15am

Re: Dave's 80:1 RC mid drive kit build log

Post by knurf » Aug 15 2018 2:07am

Also a heads up; if you're messing with the bullet and phase wires from the astro, be careful to make sure ALL of these strands are soldered to individually. I had an ongoing problem with overheating with my kit because of this.

So the bunch of thicker strands going into the bullet connector from the motor - these are made of the actual motor winding wire, so each will be isolated from each other. Make sure they are stripped of isolation and soldered properly. The motor should really have flexible wires going out instead, as these are probably much more sensitive to wiggling.

User avatar
cr0m08   100 mW

100 mW
Posts: 41
Joined: Feb 09 2015 9:21am
Location: Perth, Australia

Re: Dave's 80:1 RC mid drive kit build log

Post by cr0m08 » Aug 16 2018 9:58pm

I decided to follow Dave's upgrade of ESC and add more cooling to my HV160. A little time after I bought it, Dave advised me there had been some reliability issues with HV160. I'm running 12s not 14s with slightly lower gearing, and I'm hoping this will help its reliability. But I thought, a little extra cooling couldn't hurt. So for those that have HV160, this is what I did. I found heatsinks 13x60mm (4) in local electronics shop. Two can be put on the back of unit if cut away the excess plastic strip up the rear (cut heat sink to 55mm length). And one on each side of the existing heat sinks. I used half millimetre thick adhesive heat transfer tape as I couldn't easily source locally any adhesive heat sink past. I also used 32mm long PCB spacers to lift the HV160 from its mount point and allow room for the rear heatsink. Anyone with HV160 experience, think this will help? I'm planning to attack my HV80 next with similar, smaller heat sinks.
Attachments
3866.JPG
3866.JPG (270.13 KiB) Viewed 912 times
3908.JPG
3908.JPG (277.46 KiB) Viewed 912 times
3912.JPG
3912.JPG (360.66 KiB) Viewed 912 times
3918.JPG
3918.JPG (291.67 KiB) Viewed 912 times
4047.JPG
4047.JPG (337.92 KiB) Viewed 912 times
2015 Nukeproof Pulse, 3220/HV160 @12S V1.5, 26x2.8" Nextie 50mm wheel set
2006 KeeWee Cromo Eight, 3210/HV80 @12S V1.5, 24x3" wheel set.
1998 Marin B17, Mac 10T @18S in 19" Kris Holme Trials rims, 19x2.5" wheel set (still to finish)
part build Basman 346, QS205 hub motor @12S in 24x3" wheel set. (still to finish)

Ham   100 W

100 W
Posts: 291
Joined: Feb 18 2016 3:08am

Re: Dave's 80:1 RC mid drive kit build log

Post by Ham » Aug 16 2018 11:24pm

Nice timing, I'm cutting my alu heat sink for my talon today and we have similar ideas.

I originally ran a 160 and overheated it/water damaged it a year or so ago so will be interested to see how you get on.
http://www.HamsFitness.com Strength, Conditioning & Diet

User avatar
cr0m08   100 mW

100 mW
Posts: 41
Joined: Feb 09 2015 9:21am
Location: Perth, Australia

Re: Dave's 80:1 RC mid drive kit build log

Post by cr0m08 » Aug 17 2018 1:29am

hahaha, yeah my mount location is shitty for potential water damage, great for air flow cooling (bottom side of downtube), BUT ! My Location being Western Australia, from Perth going north and east, is in my opinion, god damn desert! Summer temp's are 38-45C most of the summer with little chance of rain. Still is chances of water damage after a lingering puddle perhaps. Having also smashed my hip years ago and still retain metal in there, I'm a bit scared riding when its wet and greasy :roll: , so usually don't. I probably ride a bit tame compared to most of the Tangent owners, but I just can't resist the awesome power wheelies and the occasional rush of blood that turns the brain off and the wrist on! Thanks Dave! :D
But I'll post if any further issues happen.
2015 Nukeproof Pulse, 3220/HV160 @12S V1.5, 26x2.8" Nextie 50mm wheel set
2006 KeeWee Cromo Eight, 3210/HV80 @12S V1.5, 24x3" wheel set.
1998 Marin B17, Mac 10T @18S in 19" Kris Holme Trials rims, 19x2.5" wheel set (still to finish)
part build Basman 346, QS205 hub motor @12S in 24x3" wheel set. (still to finish)

User avatar
tangentdave   1 kW

1 kW
Posts: 436
Joined: Jun 06 2015 11:40am
Location: Seattle, WA
Contact:

Re: Dave's 80:1 RC mid drive kit build log

Post by tangentdave » Aug 17 2018 12:44pm

Yes to those cooling fins. I notice a difference on the Talons with the extra fins. I'm not sure the reason for the Talon showing higher reliability than the HV160, but the RC forums generally agree the Talon is tougher and runs cooler.

Full disclosure: I'm seeing a decrease in reliability of the Talons over the last 6 months. There have been about 5 out of 30 or so that I've shipped with gen2 kits that have either fireballed or simply quit on customers during the initial break-in period (first 10-20 miles). Previously with gen1, 2 Talons out of 60 died not due to water damage. I'm speculating here, but I think Castle may have altered something- all the ESCs now arrive with the latest firmware (released 4 months ago), which means they've been manufactured recently. The previous ESCs that didn't die as often arrived with old firmware (sometimes years old). The other differences with the gen2 kit are integrated engine (each is tested with a megger to >1Mohm phase isolation) and a switch to oxygen-free copper battery cables (from copper-clad aluminum). According to a couple enginerd websites, the calculated inductance of a given cable is near identical whether it's Al or Cu.

I think it's time to start with FOC anyway, reports are it reduces our motor heat by half (oh man the Talon makes a lot of torque tho).

-dave
GGMT/Tangent 8kW
tangentmotors.com

User avatar
cr0m08   100 mW

100 mW
Posts: 41
Joined: Feb 09 2015 9:21am
Location: Perth, Australia

Re: Dave's 80:1 RC mid drive kit build log

Post by cr0m08 » Aug 17 2018 10:31pm

I'm not up with the tech at mo, can someone briefly lay out the difference between our CC HV units and the FOC and VESC units? Or point me to a thread that does? Don't really want to take Daves thread too far off topic.
2015 Nukeproof Pulse, 3220/HV160 @12S V1.5, 26x2.8" Nextie 50mm wheel set
2006 KeeWee Cromo Eight, 3210/HV80 @12S V1.5, 24x3" wheel set.
1998 Marin B17, Mac 10T @18S in 19" Kris Holme Trials rims, 19x2.5" wheel set (still to finish)
part build Basman 346, QS205 hub motor @12S in 24x3" wheel set. (still to finish)

User avatar
cr0m08   100 mW

100 mW
Posts: 41
Joined: Feb 09 2015 9:21am
Location: Perth, Australia

Re: Dave's 80:1 RC mid drive kit build log

Post by cr0m08 » Aug 17 2018 10:36pm

Also I would have thought the Talon's physical build would be reason for its reliability? With the 20A bec inbuilt it has more physical mass/die-cast metal body to create heatsink to start with for both ESC and BEC. So following the historical findings of hub motors, those with more mass can absorb more energy and have more chance to dissipate the heat before saturation once power levels drop?
2015 Nukeproof Pulse, 3220/HV160 @12S V1.5, 26x2.8" Nextie 50mm wheel set
2006 KeeWee Cromo Eight, 3210/HV80 @12S V1.5, 24x3" wheel set.
1998 Marin B17, Mac 10T @18S in 19" Kris Holme Trials rims, 19x2.5" wheel set (still to finish)
part build Basman 346, QS205 hub motor @12S in 24x3" wheel set. (still to finish)

E1Allen   1 mW

1 mW
Posts: 19
Joined: Mar 26 2018 4:20am

Re: Dave's 80:1 RC mid drive kit build log

Post by E1Allen » Aug 18 2018 12:44am

I'll be doing some testing hopefully by the end of September with VESCs

User avatar
tangentdave   1 kW

1 kW
Posts: 436
Joined: Jun 06 2015 11:40am
Location: Seattle, WA
Contact:

Re: Dave's 80:1 RC mid drive kit build log

Post by tangentdave » Aug 18 2018 2:56pm

Castle uses passive freewheeling in their ESCs. Ideally we want active freewheeling so partial throttle/load situations don't generate so much heat in the ESC.





FOC is entirely different and more advanced than active freewheeling.
GGMT/Tangent 8kW
tangentmotors.com

Ham   100 W

100 W
Posts: 291
Joined: Feb 18 2016 3:08am

Re: Dave's 80:1 RC mid drive kit build log

Post by Ham » Aug 19 2018 4:54am

That was a great explanation in the video. I kind of even understood the concept!
http://www.HamsFitness.com Strength, Conditioning & Diet

User avatar
cr0m08   100 mW

100 mW
Posts: 41
Joined: Feb 09 2015 9:21am
Location: Perth, Australia

Re: Dave's 80:1 RC mid drive kit build log

Post by cr0m08 » Aug 23 2018 1:27am

Just wondering if anyone made progress with the rather expensive 200A VESC? Looked like a couple people were going to try it?
http://www.fightingrobots.co.uk/threads ... ted/page19
https://vesc-project.com/node/339

Do I understand correctly that these units run in sine wave, so better efficiency, but still sensorless so can suit the astro 3220?
2015 Nukeproof Pulse, 3220/HV160 @12S V1.5, 26x2.8" Nextie 50mm wheel set
2006 KeeWee Cromo Eight, 3210/HV80 @12S V1.5, 24x3" wheel set.
1998 Marin B17, Mac 10T @18S in 19" Kris Holme Trials rims, 19x2.5" wheel set (still to finish)
part build Basman 346, QS205 hub motor @12S in 24x3" wheel set. (still to finish)

Post Reply