Sur-Ron - New Mid drive Bike

Discussions related to motors other than hub motors.
This includes R/C motors, botttom bracket, roller and geared drives.
User avatar
liveforphysics   100 GW

100 GW
Posts: 14134
Joined: Oct 29 2008 1:48am
Location: Santa Cruz, CA, USA

Re: Sur-Ron - New Mid drive Bike

Post by liveforphysics » May 31 2019 1:14pm

That's such a bad ass bike! Nice build, and great riding skills!
wuhaichao443 wrote:
May 31 2019 4:10am
some day
Each carcinogen vapor exposure includes a dice roll for cancer.

Each mutagen vapor exposure includes a dice roll for reproductive genetic defects in your children.

Each engine start sprays them into a shared atmosphere which includes beings not offered an opportunity to consent accepting these cancer experiences and defective genetics life experiences.

Every post is a free gift to the collective of minds composing the living bleeding edge of LEV development on our spaceship.

wuhaichao443   10 mW

10 mW
Posts: 27
Joined: Apr 22 2019 5:05am

Re: Sur-Ron - New Mid drive Bike

Post by wuhaichao443 » Jun 01 2019 5:39am

fechter wrote:
May 31 2019 9:44am
What rear tire is that? Looks awesome.
“yuanxing”3.5*17 from china

wuhaichao443   10 mW

10 mW
Posts: 27
Joined: Apr 22 2019 5:05am

Re: Sur-Ron - New Mid drive Bike

Post by wuhaichao443 » Jun 01 2019 5:50am

Offroader wrote:
May 31 2019 12:54pm
fechter wrote:
May 31 2019 9:44am
What rear tire is that? Looks awesome.
It does look nice. How does it handle and how does the rear suspension handle with the increased weight?

Was it worth to go with something so big and heavy over the stock tire?
My advice: enjoy the performance of big teeth and ignore the weight lag

Joachim   1 kW

1 kW
Posts: 435
Joined: Jul 30 2015 1:02pm
Contact:

Re: Sur-Ron - New Mid drive Bike

Post by Joachim » Jun 01 2019 2:09pm

Cant wait for a bigger battery and the belt drive kit :P
Building a 55Ah/3.1Kwh battery to have a good range in sport mode.
Next week i hope to instal the belt drive to make my surron silent.

55Ah wil give me60 to 70% extra range....60/70km in sport and 100/120km in ep mode ?

19P 10mmx0,2mm pure nickel so i can upgrade the controller later for extra power :evil:
Image

User avatar
3DTOPO   1 kW

1 kW
Posts: 415
Joined: Apr 11 2018 2:21am

Re: Sur-Ron - New Mid drive Bike

Post by 3DTOPO » Jun 01 2019 6:27pm

wuhaichao443 wrote:
Jun 01 2019 5:39am
fechter wrote:
May 31 2019 9:44am
What rear tire is that? Looks awesome.
“yuanxing”3.5*17 from china
Anyone know where we can we get a 17" wheel for the Sur Ron?

User avatar
efMX Trials Electric Freeride   1 MW

1 MW
Posts: 1688
Joined: Feb 15 2013 4:43pm

Re: Sur-Ron - New Mid drive Bike

Post by efMX Trials Electric Freeride » Jun 01 2019 7:31pm

3DTOPO wrote:
Jun 01 2019 6:27pm
wuhaichao443 wrote:
Jun 01 2019 5:39am
fechter wrote:
May 31 2019 9:44am
What rear tire is that? Looks awesome.
“yuanxing”3.5*17 from china
Anyone know where we can we get a 17" wheel for the Sur Ron?
Josh from motoped and surron forums has been building motobike and ebike wheels for a few years now, located in Maine.. : https://facebook.com/groups/11429094823 ... 7513648886

also on ebay : https://www.google.com/search?q=wickedwheelwerks%20ebay
Last edited by efMX Trials Electric Freeride on Jun 22 2019 7:37pm, edited 1 time in total.
some ride & sk8 videos:
metacafe.com/channels/NATAS666DAMIEN
http://www.youtube.com/natas666damien
i have nothing for sale.. :)

User avatar
3DTOPO   1 kW

1 kW
Posts: 415
Joined: Apr 11 2018 2:21am

Re: Sur-Ron - New Mid drive Bike

Post by 3DTOPO » Jun 01 2019 7:38pm

efMX Trials Electric Freeride wrote:
Jun 01 2019 7:31pm
3DTOPO wrote:
Jun 01 2019 6:27pm
wuhaichao443 wrote:
Jun 01 2019 5:39am
fechter wrote:
May 31 2019 9:44am
What rear tire is that? Looks awesome.
“yuanxing”3.5*17 from china
Anyone know where we can we get a 17" wheel for the Sur Ron?
Josh from motoped and surron forums has been building motobike and ebike wheels for a few years and now, located in Maine.. : https://facebook.com/groups/11429094823 ... 7513648886
Awesome, thanks! I just requested to join the group.

User avatar
Offroader   100 MW

100 MW
Posts: 2568
Joined: Sep 08 2013 9:03pm
Location: USA

Re: Sur-Ron - New Mid drive Bike

Post by Offroader » Jun 02 2019 4:17pm

Took my bike into Manhattan for the first time. I was worried about bringing this beast of a bike on my local ferry boat that I need to take in order to get into Manhattan. They do allow bikes and electric bikes, but the Sur-Ron is more like a motorcycle than an electric bicycle. Luckily they didn't give me any issues. This is good because I plan on commuting with the bike every so often to Times Square where my job is.

This bike is great for city riding. It turns very good with the smaller 19" wheels. It can also climb any stairs with ease and there are lots of stairs. You can ride up the longest stairs very easily with this bike. I climbed the stairs in the picture below a couple of times without any issues. You should see how the people react when you climb stairs with the bike, its like they have never seen a bike before climb stairs :mrgreen: .

You can pretty much do what ever you want with the bike in Manhattan because the police will never bother you, its just too crowded a city for them to care.
Hands down this is a very good bike for having fun in an large urban city for doing urban assault riding, with lots of jumps to flat ground and stairs.

Image

Some long stairs I climbed with the bike.
Image

Image

User avatar
that1guy   10 mW

10 mW
Posts: 34
Joined: Jun 19 2014 5:07pm
Location: Mountain View, California, USA

Re: Sur-Ron - New Mid drive Bike

Post by that1guy » Jun 02 2019 10:15pm

I've been using my own power supply to charge the surron at work for the past week - it's been working fine. But today I arrived with 14% charge and my power supply won't charge the surron battery. I measured 53V on the surron charge connector and main terminals. Anybody else experience this?

I wonder if the battery is perhaps too hot to charge. The outside case is warm to the touch.

UPDATE: battery is charging now after I gave it 15 minutes to cool down. The state of charge indicator was initially blinking "14%", but then it went solid, after which i was able to charge.

User avatar
that1guy   10 mW

10 mW
Posts: 34
Joined: Jun 19 2014 5:07pm
Location: Mountain View, California, USA

Re: Sur-Ron - New Mid drive Bike

Post by that1guy » Jun 03 2019 12:27am

I did an experiment to find maximum charging current that the surron BMS will allow:
20A is ok, but it will shut off at 25A. Thought this would be useful for those experimenting with a non-surron chargers.

Uran93   10 mW

10 mW
Posts: 30
Joined: Apr 10 2018 5:26pm

Re: Sur-Ron - New Mid drive Bike

Post by Uran93 » Jun 03 2019 3:25pm

Offroader wrote:
May 24 2019 6:18pm
You really would need nothing else to install the fox fork other than head tube spacers if you reuse the sur-ron headset. You would have to remove the crown race from your old fork, you would have to be careful, using a razor blade to start it and then slowly wedge larger stuff in there to lift it. Don't knock it out with a screw driver and hammer or you will bend it.

You could use a screw driver to wedge in the space under the crown race to help lift it after using a knocked in razor blade to start it.

Honestly, I haven't understood anything you wrote in this paragraph. Could you or anybody explain or put in some pictures please?
You just scared me))

Uran93   10 mW

10 mW
Posts: 30
Joined: Apr 10 2018 5:26pm

Re: Sur-Ron - New Mid drive Bike

Post by Uran93 » Jun 03 2019 3:32pm

Joachim wrote:
May 22 2019 2:39pm
I am now Building a new battery for my surron to have more range. just a pack,cells in spacers/fiberglas plate/heatshrink and foam for demping.

What is wisdom...use 2900mah cells are go max for 3300mah/3400mah cells ?

The battery become 16S-18P ( maby 19P)

Cells i can use for the battery:
Panasonic NCR PF 2900mah 10A discharge. 52Ah-2995Wh
Panasonic NCR BD 3200mah 10A discharge. 57Ah-3280Wh
Sony US18650NC1 2900mah 10A discharge. 52Ah-2995Wh
Samsung INR18650-35E 3400mah 10A discharge. 61Ah-3510Wh
Samsung INR18650-30Q 3000mah 15A discharge. 54Ah-3110Wh

I am not a fan of the 3000+mah 18650 cells and the GA,s are way to expensive for a 10A max discharge cel.

I go with the good old Panasonic PF cells.
The battery i make is a 16S-19p/55Ah-3100Wh just for good range in the sport mode.
Image
Image
Great efforts! My respect. Looking for bigger (longer handle battery also).

Could you please explain how did you calculate these numbers?
Multiple what on what? I'm a total zero in this subject and need to understand the basics.

Cells i can use for the battery:
Panasonic NCR PF 2900mah 10A discharge. 52Ah-2995Wh
Panasonic NCR BD 3200mah 10A discharge. 57Ah-3280Wh
Sony US18650NC1 2900mah 10A discharge. 52Ah-2995Wh
Samsung INR18650-35E 3400mah 10A discharge. 61Ah-3510Wh
Samsung INR18650-30Q 3000mah 15A discharge. 54Ah-3110Wh

Joachim   1 kW

1 kW
Posts: 435
Joined: Jul 30 2015 1:02pm
Contact:

Re: Sur-Ron - New Mid drive Bike

Post by Joachim » Jun 04 2019 2:43am

Uran93 wrote:
Jun 03 2019 3:32pm
Joachim wrote:
May 22 2019 2:39pm
I am now Building a new battery for my surron to have more range. just a pack,cells in spacers/fiberglas plate/heatshrink and foam for demping.

What is wisdom...use 2900mah cells are go max for 3300mah/3400mah cells ?

The battery become 16S-18P ( maby 19P)

Cells i can use for the battery:
Panasonic NCR PF 2900mah 10A discharge. 52Ah-2995Wh
Panasonic NCR BD 3200mah 10A discharge. 57Ah-3280Wh
Sony US18650NC1 2900mah 10A discharge. 52Ah-2995Wh
Samsung INR18650-35E 3400mah 10A discharge. 61Ah-3510Wh
Samsung INR18650-30Q 3000mah 15A discharge. 54Ah-3110Wh

I am not a fan of the 3000+mah 18650 cells and the GA,s are way to expensive for a 10A max discharge cel.

I go with the good old Panasonic PF cells.
The battery i make is a 16S-19p/55Ah-3100Wh just for good range in the sport mode.
Image
Image
Great efforts! My respect. Looking for bigger (longer handle battery also).

Could you please explain how did you calculate these numbers?
Multiple what on what? I'm a total zero in this subject and need to understand the basics.

Cells i can use for the battery:
Panasonic NCR PF 2900mah 10A discharge. 52Ah-2995Wh
Panasonic NCR BD 3200mah 10A discharge. 57Ah-3280Wh
Sony US18650NC1 2900mah 10A discharge. 52Ah-2995Wh
Samsung INR18650-35E 3400mah 10A discharge. 61Ah-3510Wh
Samsung INR18650-30Q 3000mah 15A discharge. 54Ah-3110Wh
I need more range not topspeed so i keep the same voltage 60V nominal(16 cells in serie).
a cel mah x the number you can put maximum in parallel wil give you the total Ah/Wh.
Panasonic pf cel: 2900mahx 19 cells in parallel = 55.1Ah this x the nominal voltage from 16s/57,6= 3173Wh/3.17Kwh .
The more you can put in parallel the bigger the Ah/Wh, total pack 304 cells is the max for me to fit and not to heavy

User avatar
Offroader   100 MW

100 MW
Posts: 2568
Joined: Sep 08 2013 9:03pm
Location: USA

Re: Sur-Ron - New Mid drive Bike

Post by Offroader » Jun 04 2019 9:27am

Uran93 wrote:
Jun 03 2019 3:25pm
Offroader wrote:
May 24 2019 6:18pm
You really would need nothing else to install the fox fork other than head tube spacers if you reuse the sur-ron headset. You would have to remove the crown race from your old fork, you would have to be careful, using a razor blade to start it and then slowly wedge larger stuff in there to lift it. Don't knock it out with a screw driver and hammer or you will bend it.

You could use a screw driver to wedge in the space under the crown race to help lift it after using a knocked in razor blade to start it.

Honestly, I haven't understood anything you wrote in this paragraph. Could you or anybody explain or put in some pictures please?
You just scared me))
When changing your front fork you will have to deal with the headset. The Sur-Ron headset is a cheap one and has many parts. It also seems to get damaged easily and parts of it bent. Take a look at some of the pictures of the Sur-Ron headset.

Then you will have to remove the crown race carefully from your RST Killah fork and install it on your Fox fork. Care needs to be taken to remove this and probably best to start with a razor blade and knock it in with a hammer to give you enough space to carefully knock in a flat head screw driver to slowly pry it off the fork. Then you need to knock it back down flat on your FOX fork. If you damage it, like if you knock it up with a screw driver at the end of the crown race and bend it like they show on some you tube videos you will have to buy another one. Good luck finding a Sur-Ron crown race, then you will need to install a hope or Cane creek new headset.

Here is the stock Sur Ron headset. Complete garbage but it works, look how many pieces it is. Take careful attention how it comes apart because you will have to remember how it goes back together.

Image

Image

Image

You can see the Sur-Ron Crown Race installed at the very bottom and the bearing is sitting above it.
Image





The Sur-Ron Crown Race removed from the fork, you will have to carefully remove this from your RST Killah Fork using a razor to start it and then knock something a little thicker in to carefully lift it up. You can see mine is dented on the edge from trying to knock it up with a hammer and screw driver from its edges. I didn't care about mine since I bought a new Cane Creek 40 headset. You can use a hammer and screw driver but only to wedge it in under the crown race after you slightly lifted it with knocking in a razor blade to start it.

Image

Image

Just for an example, here is a cane creek 40 crown race installed. You can see its pushed all the way down on the fork and its difficult to lift it up. The only way to get it started to remove it is to use a hammer and knock in a razor blade. Then after lifting it up slightly with a razor blade, knock in something slightly larger like a flat head screw driver to slowly lift it. Make sure to alternate sides while lifting it.

Image

Image


If you want to use another headset, like the cane creek 40. You will have to install headset cups. It is difficult to do without proper tools. If you use threaded rod and wood, which works, it takes a lot of force to get those headset cups pressed into the frame. The cups will go in uneven and you have to keep unloosening everything to try to get them to go in straight. A real difficult not fun job. If you had proper tools it probably would go a lot smoother but I didn't want to buy a head set press. You may just want to go to your local bike store for them to do it for you to be honest as they have the tools.

The cane creek 40 is nice and has a lot less pieces than the stock sur-ron headset. It has just a single sealed bearing.

Below I'm stalling my new cane creek 40 head set cups.
Image

User avatar
3DTOPO   1 kW

1 kW
Posts: 415
Joined: Apr 11 2018 2:21am

Re: Sur-Ron - New Mid drive Bike

Post by 3DTOPO » Jun 05 2019 2:14am

New special edition LB X-series announced:

https://electrek.co/2019/06/04/special- ... tric-bike/

Seems like the main difference is it comes with a 200mm BoXXer Debonair Rock Shox fork.

Tommm   10 kW

10 kW
Posts: 788
Joined: Apr 03 2018 2:32am

Re: Sur-Ron - New Mid drive Bike

Post by Tommm » Jun 05 2019 5:24am

3DTOPO wrote:
Jun 05 2019 2:14am
New special edition LB X-series announced:

https://electrek.co/2019/06/04/special- ... tric-bike/

Seems like the main difference is it comes with a 200mm BoXXer Debonair Rock Shox fork.
If they are serious about offroading they should upgrade the linkages because they broke in this thread.

User avatar
Liu   1 mW

1 mW
Posts: 19
Joined: Apr 19 2019 10:52am
Location: Germany

Re: Sur-Ron - New Mid drive Bike

Post by Liu » Jun 05 2019 5:57am

Offroader wrote:
Jun 02 2019 4:17pm
Took my bike into Manhattan for the first time. I was worried about bringing this beast of a bike on my local ferry boat that I need to take in order to get into Manhattan. They do allow bikes and electric bikes, but the Sur-Ron is more like a motorcycle than an electric bicycle. Luckily they didn't give me any issues. This is good because I plan on commuting with the bike every so often to Times Square where my job is.

This bike is great for city riding. It turns very good with the smaller 19" wheels. It can also climb any stairs with ease and there are lots of stairs. You can ride up the longest stairs very easily with this bike. I climbed the stairs in the picture below a couple of times without any issues. You should see how the people react when you climb stairs with the bike, its like they have never seen a bike before climb stairs :mrgreen: .

You can pretty much do what ever you want with the bike in Manhattan because the police will never bother you, its just too crowded a city for them to care.
Hands down this is a very good bike for having fun in an large urban city for doing urban assault riding, with lots of jumps to flat ground and stairs.

Image

Some long stairs I climbed with the bike.
Image

Image
You can pretty much do what ever you want with the bike in Manhattan because the police will never bother you, its just too crowded a city for them to care. :bigthumb:
I have to say that it’s great in Manhattan. You are so lucky, the police are too busy to look at you.
If in Germany the policeman always leisurely driving around the street with BMW 3 KOMBI. If it is a non-road legal version on public road, will be noticed and arrested soon :oops:

User avatar
Compoundbike   10 W

10 W
Posts: 77
Joined: Aug 25 2016 3:22pm
Location: Switzerland

Re: Sur-Ron - New Mid drive Bike

Post by Compoundbike » Jun 05 2019 12:33pm

are here users from Switzerland or Germany ?

User avatar
Offroader   100 MW

100 MW
Posts: 2568
Joined: Sep 08 2013 9:03pm
Location: USA

Re: Sur-Ron - New Mid drive Bike

Post by Offroader » Jun 05 2019 12:53pm

Liu wrote:
Jun 05 2019 5:57am


You can pretty much do what ever you want with the bike in Manhattan because the police will never bother you, its just too crowded a city for them to care. :bigthumb:
I have to say that it’s great in Manhattan. You are so lucky, the police are too busy to look at you.
If in Germany the policeman always leisurely driving around the street with BMW 3 KOMBI. If it is a non-road legal version on public road, will be noticed and arrested soon :oops:
What is a BMW 3 KOMBI? Can't seem to find anything about it.

USA is not all like Manhattan, many cities I wouldn't mess around in. Manhattan the police are are not even aloud to raise their voice at you, their powers were taken away a long time ago. They are also certainly not allowed to chase bikes and they are extremely worried about being sued for doing anything wrong. We sue police over here for just giving us a bad look.

The city is also so crowded that if they did try and pull you over you would just act like you didn't hear them and get lost in the traffic. We don't have any motorcycle police over here.

If they did try and chase me I'd like to see them ride up these stairs after me :wink: .

Image

User avatar
fechter   100 GW

100 GW
Posts: 14731
Joined: Dec 31 2006 3:23pm
Location: California Bay Area, USA

Re: Sur-Ron - New Mid drive Bike

Post by fechter » Jun 05 2019 3:28pm

Offroader wrote:
Jun 05 2019 12:53pm
What is a BMW 3 KOMBI? Can't seem to find anything about it.
I think it's the wagon version:
BMW.jpg
BMW.jpg (42.77 KiB) Viewed 1876 times
San Francisco is pretty much like Manhattan. The police are busy with more serious crimes. Unfortunately I live 20 miles away and the cops in my neighborhood are bored. I was pulled over but had plates, turn signals, mirrors, and insurance so they couldn't find anything to write me up for other than saying I was speeding (which I wasn't at the time). Now I call my bike the "Cop Magnet".
"One test is worth a thousand opinions"

Duncan75   10 mW

10 mW
Posts: 29
Joined: Oct 21 2018 12:59pm

Re: Sur-Ron - New Mid drive Bike

Post by Duncan75 » Jun 05 2019 5:41pm

I think that Sur-Rons are still something relatively new and cops also pull us over out of curiosity. But I agree that it's a bummer to be around cops that are bored.

User avatar
Offroader   100 MW

100 MW
Posts: 2568
Joined: Sep 08 2013 9:03pm
Location: USA

Re: Sur-Ron - New Mid drive Bike

Post by Offroader » Jun 06 2019 6:53am

I believe it is important not to wear a full face helmet and purposely wear a bicycle helmet. I see many of you guys over in Europe wearing full face helmets. Unless you can legally ride the bike, you are drawing lots of attention wearing a full face helmet.

User avatar
Rix   100 GW

100 GW
Posts: 6898
Joined: Mar 29 2012 11:26am
Location: Fallon NV USA

Re: Sur-Ron - New Mid drive Bike from China

Post by Rix » Jun 06 2019 1:17pm

Hyena wrote:
Jan 02 2018 8:29pm
Further more, I shot this video a few days ago :mrgreen:

If you guys ride your SurRon like Hyena does in this video, you won't get pulled over by the fuzz. :bigthumb: :lol:

User avatar
3DTOPO   1 kW

1 kW
Posts: 415
Joined: Apr 11 2018 2:21am

Re: Sur-Ron - New Mid drive Bike

Post by 3DTOPO » Jun 07 2019 7:20pm

efMX Trials Electric Freeride wrote:
Jun 01 2019 7:31pm
3DTOPO wrote:
Jun 01 2019 6:27pm
wuhaichao443 wrote:
Jun 01 2019 5:39am
fechter wrote:
May 31 2019 9:44am
What rear tire is that? Looks awesome.
“yuanxing”3.5*17 from china
Anyone know where we can we get a 17" wheel for the Sur Ron?
Josh from motoped and surron forums has been building motobike and ebike wheels for a few years and now, located in Maine.. : https://facebook.com/groups/11429094823 ... 7513648886
Josh is recommending an 18" rear wheel with a 21" front. What do you guys think?

Anyone running that on the Sur Ron?

User avatar
efMX Trials Electric Freeride   1 MW

1 MW
Posts: 1688
Joined: Feb 15 2013 4:43pm

Re: Sur-Ron - New Mid drive Bike

Post by efMX Trials Electric Freeride » Jun 07 2019 8:27pm

3DTOPO wrote:
Jun 07 2019 7:20pm
efMX Trials Electric Freeride wrote:
Jun 01 2019 7:31pm
3DTOPO wrote:
Jun 01 2019 6:27pm
wuhaichao443 wrote:
Jun 01 2019 5:39am


“yuanxing”3.5*17 from china
Anyone know where we can we get a 17" wheel for the Sur Ron?
Josh from motoped and surron forums has been building motobike and ebike wheels for a few years and now, located in Maine.. : https://facebook.com/groups/11429094823 ... 7513648886
Josh is recommending an 18" rear wheel with a 21" front. What do you guys think?

Anyone running that on the Sur Ron?
do you have a link, specs, etc for the rims he recommended?? i would be concerned with weight and range for surron (josh is riding on ice;).. 18" rims are normally for full size motocross bikes and will weigh accordingly, same with tires.. also consider the head angle and handling change with different wheel sizes..
some ride & sk8 videos:
metacafe.com/channels/NATAS666DAMIEN
http://www.youtube.com/natas666damien
i have nothing for sale.. :)

Post Reply