lithium fire on Fiji. Airline plane

Post by AussieJester » Sep 03 2014 6:23pm

Thought this might be of interest, posted on Perth Now''
"Meanwhile, in another ATSB report released today, smoke billowing from the cargo hold of a Fiji Airways plane prior to takeoff prompted a Mayday call at Melbourne Airport on April 26.

Aerodrome rescue and firefighting service and Australian Federal Police were called, identifying the cause as an electrical short circuit in more than two dozen lithium-ion polymer batteries contained in a passenger’s luggage.

Fiji Airways has since issued a warning that any passenger found to be carrying undeclared lithium batteries will be offloaded and refused carriage."


KiM

User avatar
Samd   1.21 GW

1.21 GW
Posts: 3667
Joined: Jun 28 2011 11:08pm
Location: Ballarat, AU
Contact:

Re: lithium fire on Fiji. Airline plane

Post by Samd » Sep 03 2014 6:50pm

"Offloaded". Bloody hell.

Thats a lot of LiPO.
http://ballaratebikes.com/

ImageImageImage
"Knowledge is knowing that a tomato is a fruit. Wisdom is knowing that a 165mm rear shock can't deliver 220mm of rear swingarm travel." - Oprah Winfrey.

zombiess   1 GW

1 GW
Posts: 3005
Joined: Feb 01 2011 2:16am
Location: Ventura

Re: lithium fire on Fiji. Airline plane

Post by zombiess » Sep 03 2014 6:53pm

Samd wrote:Thats a lot of LiPO.
How much is it? They could be coin cells, they aren't giving any information other than 24, 24 batteries of what? Hearing aid, car battery sized?
Fundamentals United, Inc.

Drone Cops   1 µW

1 µW
Posts: 1
Joined: Sep 05 2014 4:27am

Re: lithium fire on Fiji. Airline plane

Post by Drone Cops » Sep 05 2014 4:34am

@zombiess. You nailed it exactly. The report was simply batteries and not specifically Li-Po batteries so a play on words on the investigators/reporters behalf. They could have been small 5V batteries for hearing aids, to AAA batteries to dry cells which are allowed to be carried and commonly used in transmitters.

Secondly, how the heck can this ever get through International security screening if this is what they allege. All sounds a bit wierd and ambiguos to me...

dnmun   100 GW

100 GW
Posts: 16190
Joined: Jun 09 2008 1:32pm
Location: portland, or and loveland, co

Re: lithium fire on Fiji. Airline plane

Post by dnmun » Sep 05 2014 8:53am

i doubt if coin cells would have caused smoke. it does show a lack of sense on the part of the smuggler since he could have packed more carefully and if he had just discharged the packs before boarding they could not have generated enuff heat to make smoke.

of course it woulda helped if the baggage was handled gently.

User avatar
Ykick   100 GW

100 GW
Posts: 5558
Joined: Nov 26 2009 6:10pm
Location: San Diego, California

Re: lithium fire on Fiji. Airline plane

Post by Ykick » Sep 05 2014 9:12am

I've been reading and studying air travel with RC Lipo batteries in the USA. Apparently, many RC enthusiasts often do this and if declared (placed on conveyor for X-ray) from carry-on luggage and any leads carefully insulated/protected TSA generally allows them.

Many airline pilots happen to be RC aero enthusiasts so it's not that uncommon of item to fly with in carry-on bag.

There used to be a limit around 300Wh of loose lithium cells but I no longer see that on TSA.gov and reading RC boards many folks haul much more than that amount to field events and competitions.

I need to get a folder going and try it for my frequent east-west commutes. I'd love to ride an ebike from SAN to my home - talk about mixed-mode commute!
Talent must not be wasted.... Those who have talent must hug it, embrace it, nurture it and share it lest it be taken away from you as fast as it was loaned to you.

- Frank Sinatra

Rodney64   1 MW

1 MW
Posts: 1851
Joined: Mar 30 2012 4:00am
Location: Perth Western Australia

Re: lithium fire on Fiji. Airline plane

Post by Rodney64 » Sep 05 2014 9:16am

Aussiejester I thought you were giving up bikes and going into guns

dnmun   100 GW

100 GW
Posts: 16190
Joined: Jun 09 2008 1:32pm
Location: portland, or and loveland, co

Re: lithium fire on Fiji. Airline plane

Post by dnmun » Sep 05 2014 12:00pm

i still think it is good practise to discharge the pack before shipping or including it in luggage. it is not hard to discharge a battery pack and in fact the lipo should be left discharged until it is needed and then charged up so to carry fully charged lipo on a plane is just plane wrong imo.

User avatar
wesnewell   100 GW

100 GW
Posts: 7170
Joined: Jan 31 2011 6:25pm
Location: Wylie, TX, USA

Re: lithium fire on Fiji. Airline plane

Post by wesnewell » Sep 05 2014 2:01pm

That depends on what you mean by discharged. Discharged to nominal voltage would be ok, but it's recommend to ship at store voltage, ~3.85V. That's how new packs are shipped.
Need Advice? https://endless-sphere.com/forums/viewt ... =3&t=66302
Mongoose 26" Ledge 2.1 mtb bike $99, yescomusa.com 48V 1000W rear hub kit $200, Hua Tong 72V 40A controller $35, 10ah 24s lipo $217=~43mph, range=45 miles @ 20mph. 25K miles and still going strong.
Huffy Fortress 3.0 with MXUS 3000 4T motor, 24s lipo, 96V 60A controller. Total cost with extras <$700. Top speed ~50mph
My videos https://www.youtube.com/channel/UC0KW4U ... _G2wQhptMg

User avatar
amberwolf   100 GW

100 GW
Posts: 31614
Joined: Aug 17 2009 6:43am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: lithium fire on Fiji. Airline plane

Post by amberwolf » Sep 05 2014 2:12pm

There's a lot of assumptions above: To be fair, it doesn't say whether the batteries *were* RC LiPo (or any other similar type), nor does it say what the charge state was. (unlikely that they will ever know).

User avatar
AussieJester   100 GW

100 GW
Posts: 8736
Joined: Mar 11 2008 3:33am
Location: Perth Western Australia

Re: lithium fire on Fiji. Airline plane

Post by AussieJester » Sep 05 2014 11:24pm

Am/have Rodney, got my second rifle yesterday as a matter of fact Howa.243.. I have also bought a 250cc quad bike I been out in the Bush on with two of my close motox riding buddies, that's more fun than any e-bike I have had however, I do intend in the future to resume with electrics in some capacity, thus I will remain active on ES as I have said all along...


KiM

MexicanBatman   1 W

1 W
Posts: 50
Joined: Jul 26 2013 3:36am

Re: lithium fire on Fiji. Airline plane

Post by MexicanBatman » Sep 06 2014 5:58am

amberwolf wrote:There's a lot of assumptions above: To be fair, it doesn't say whether the batteries *were* RC LiPo (or any other similar type), nor does it say what the charge state was. (unlikely that they will ever know).

The report is in the link below
http://www.atsb.gov.au/media/5092912/ao ... _final.pdf


It was all rc gear

I was off that night sadly but a friend was working, it was interesting there were 7 fire trucks etc... LOL


http://www.atsb.gov.au/media/5092912/ao ... _final.pdf

User avatar
wesnewell   100 GW

100 GW
Posts: 7170
Joined: Jan 31 2011 6:25pm
Location: Wylie, TX, USA

Re: lithium fire on Fiji. Airline plane

Post by wesnewell » Sep 06 2014 3:09pm

What an idiot. Looks like he just threw everything in the case and shut it. Note the cables still plugged into the chargers.
Need Advice? https://endless-sphere.com/forums/viewt ... =3&t=66302
Mongoose 26" Ledge 2.1 mtb bike $99, yescomusa.com 48V 1000W rear hub kit $200, Hua Tong 72V 40A controller $35, 10ah 24s lipo $217=~43mph, range=45 miles @ 20mph. 25K miles and still going strong.
Huffy Fortress 3.0 with MXUS 3000 4T motor, 24s lipo, 96V 60A controller. Total cost with extras <$700. Top speed ~50mph
My videos https://www.youtube.com/channel/UC0KW4U ... _G2wQhptMg

Post Reply