3.9C cell with 28mΩ resistance?

General Discussion about electric bicycles.
Post Reply
User avatar
rg12   10 kW

10 kW
Posts: 915
Joined: Jul 26 2014 4:22pm

3.9C cell with 28mΩ resistance?

Post by rg12 » Apr 16 2018 4:58am

Hey Guys,

I measured the awesome Samsung 25R (8C) and it has 8mΩ resistance.
Then tested the LG M26 (3.9C) and it has 28mΩ resistance.

Is that normal for a 3.9C cell to have such high resistance?
All cells are new and tested on a few different batches and they all show the exact same numbers.
Mongoose EC-D 2007 (18" motocross wheels), 21s 10Ah LiPo, Greentime 72V 110A Controller (soldered shunt), 9kg Hub Motor

User avatar
MadRhino   100 GW

100 GW
Posts: 5587
Joined: Sep 03 2010 5:28pm
Location: Montreal QC Canada

Re: 3.9C cell with 28mΩ resistance?

Post by MadRhino » Apr 16 2018 6:09am

The state of charge and temperature does affect impedance of a cell. Those parameters should be measured equal, to compare 2 cells.

Then, both impedance readings that you have measured are within the manufacturers spec
Your Samsung cell impedance should be 7 to 16 m/ohm, 28 m/ohm after trip
If my memory is good, I recall your LG cell should be 60 m/ohm after trip. So, probably twice the impedance of the Samsung cell when in exact same state of charge and temperature.
Make it fool-proof, and I will make a better fool.
Current bikes
Street: https://s20.postimg.org/ewrvugywt/Session_04_2015.jpg
Dirt: https://s20.postimg.org/lbqwr55ml/IMG_0157.jpg

User avatar
fechter   100 GW

100 GW
Posts: 13065
Joined: Dec 31 2006 3:23pm
Location: California Bay Area, USA

Re: 3.9C cell with 28mΩ resistance?

Post by fechter » Apr 16 2018 8:51am

It might depend on how you are making the measurement too. AC measurements are pretty useless.
"One test is worth a thousand opinions"

User avatar
rg12   10 kW

10 kW
Posts: 915
Joined: Jul 26 2014 4:22pm

Re: 3.9C cell with 28mΩ resistance?

Post by rg12 » Apr 17 2018 3:55am

It's a DC cell IR tester.
Both tested brand new, same temp, same state of charge.
Charged many from different batches (all new) and all have the same specs.
Can it be that a 4C cell has almost 4 times higher IR than 8C?
Mongoose EC-D 2007 (18" motocross wheels), 21s 10Ah LiPo, Greentime 72V 110A Controller (soldered shunt), 9kg Hub Motor

User avatar
rg12   10 kW

10 kW
Posts: 915
Joined: Jul 26 2014 4:22pm

Re: 3.9C cell with 28mΩ resistance?

Post by rg12 » Apr 21 2018 8:39am

rg12 wrote:
Apr 17 2018 3:55am
It's a DC cell IR tester.
Both tested brand new, same temp, same state of charge.
Charged many from different batches (all new) and all have the same specs.
Can it be that a 4C cell has almost 4 times higher IR than 8C?
Bump...
Mongoose EC-D 2007 (18" motocross wheels), 21s 10Ah LiPo, Greentime 72V 110A Controller (soldered shunt), 9kg Hub Motor

User avatar
MadRhino   100 GW

100 GW
Posts: 5587
Joined: Sep 03 2010 5:28pm
Location: Montreal QC Canada

Re: 3.9C cell with 28mΩ resistance?

Post by MadRhino » Apr 22 2018 1:59am

rg12 wrote:
Apr 21 2018 8:39am
rg12 wrote:
Apr 17 2018 3:55am
It's a DC cell IR tester.
Both tested brand new, same temp, same state of charge.
Charged many from different batches (all new) and all have the same specs.
Can it be that a 4C cell has almost 4 times higher IR than 8C?
Bump...
You will know when you pull 4C continuous off them. My guess is they will get hot.
Make it fool-proof, and I will make a better fool.
Current bikes
Street: https://s20.postimg.org/ewrvugywt/Session_04_2015.jpg
Dirt: https://s20.postimg.org/lbqwr55ml/IMG_0157.jpg

User avatar
parabellum   10 MW

10 MW
Posts: 2056
Joined: Nov 19 2010 9:55am
Location: Dominican Republic, north.

Re: 3.9C cell with 28mΩ resistance?

Post by parabellum » Apr 22 2018 10:22pm

rg12 wrote:
Apr 21 2018 8:39am
rg12 wrote:
Apr 17 2018 3:55am
It's a DC cell IR tester.
Both tested brand new, same temp, same state of charge.
Charged many from different batches (all new) and all have the same specs.
Can it be that a 4C cell has almost 4 times higher IR than 8C?
Bump...
Looks fine 3.2W waste heat on 25R and 2.9W waste heat on M26. M26 will have to tolerate it for double time span but area of the the cell is enough to dissipate it.