QS motor magnet max temp before demag ?

Electric Motors and Controllers

QS motor magnet max temp before demag ?

Postby Doctorbass » Wed Mar 15, 2017 3:50 pm

I am not sure if i made a mistake about max magnet temp

Yesterday i have painted the magnets of my 4T QS205 50H and baked the paint at 78 celsius for 24h witch is the temp i usually use as it worked nice and i never noticed demag on all my previous motor

I was sure that the operating temp of that QS motor was like 90-100 celsius, however i saw in the spec that QS have that these have workingtemp to 70 celsius and max 120celsius

so i wonder if 78 celsius from a 70 working temp for long period of 24h could have some effect .. well i guess it is not close to the curi point witch i suppose is 120 celsius or maybe 150...

The spec i have found for the QS are these one:


( the temp above are for the stator but the relationship with magnet is uncertain...)


"Note: QS Motor could work 120 ℃ in half an hour without damage.
Conservative Suggestion (Setting of Controller)
When it's 130 ℃ inside of motor (in 30s), the current should be limited 50%.
When it's 150 ℃, the controller shut down.
When it drop down to 110℃, the controller work again."

What do you think?

Doc
CURRENT PROJECT: 2WD duo MXUS/Max-E ebike 32kW
http://endless-sphere.com/forums/viewtopic.php?f=3&t=65764
-Fastest speed record 117 km/h on flat
-Fastest 1/4 mile@ 114km/h on flat and 16.316 sec
-Succeded to haul a 19200 pounds schoolbus!
113kmh Gianthttp://www.evalbum.com/3406
Mongoosehttp://www.evalbum.com/1947
YOUTUBE---https://m.youtube.com/user/Doctorbasss
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 8139
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: QS motor magnet max temp before demag ?

Postby Punx0r » Thu Mar 16, 2017 3:57 am

I'd be surprised if you'd done any damage at 70°C...

Can you check the KV of the motor? It should have risen if the magnets have lost any strength.
Punx0r
10 GW
10 GW
 
Posts: 4099
Joined: Thu May 03, 2012 8:16 am
Location: England

Re: QS motor magnet max temp before demag ?

Postby Doctorbass » Thu Mar 16, 2017 4:12 pm

Punx0r wrote:I'd be surprised if you'd done any damage at 70°C...

Can you check the KV of the motor? It should have risen if the magnets have lost any strength.


Yes that's a good point i will check the kv :)

Doc
CURRENT PROJECT: 2WD duo MXUS/Max-E ebike 32kW
http://endless-sphere.com/forums/viewtopic.php?f=3&t=65764
-Fastest speed record 117 km/h on flat
-Fastest 1/4 mile@ 114km/h on flat and 16.316 sec
-Succeded to haul a 19200 pounds schoolbus!
113kmh Gianthttp://www.evalbum.com/3406
Mongoosehttp://www.evalbum.com/1947
YOUTUBE---https://m.youtube.com/user/Doctorbasss
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 8139
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: QS motor magnet max temp before demag ?

Postby madin88 » Thu Mar 16, 2017 4:38 pm

from what i know, the max temperature the magnets can withstand depends also on the return of the magnetic field.
In free air (without any return) it is worst, and in an assembled motor the temperature can be higher.

normally, 70°C should be no problem
measuring kV -> good luck with modern sine wave controllers :P
here it is more the opposite (at least with Adaptto) -> you adjust the controller with manual tuning as close as possible to the motors kV you know from the datasheet (momentan battery voltage minus about 7% for sine wave)

probabaly an old lyen controller is what you need to find it out.
Last edited by madin88 on Thu Mar 16, 2017 4:39 pm, edited 1 time in total. View post history.
- Votec V-FR frame / MXUS 3T / 17" Mitas MC11 / Adaptto Max-E / 20s12p 25R -> approved as L1e moped and fully road legal in EU :)
- Vector white / MXUS 4T / 24" Hookworms / Adaptto Max-E / 22s11p 25R
- KTM Hardtail Pedelec / eZee V2 6T / 27,5" / Kelly KBSX @ 1,5kW / Torque PAS / CA-V3 / 13s4p Sanyo GA in Shark case
User avatar
madin88
10 MW
10 MW
 
Posts: 2110
Joined: Mon May 27, 2013 2:02 am
Location: Austria

Re: QS motor magnet max temp before demag ?

Postby Biff » Thu Mar 16, 2017 6:52 pm

I have found that magnets demag at much lower temperatures when they are not in motors.
Biff
100 W
100 W
 
Posts: 244
Joined: Mon May 26, 2008 10:58 am
Location: Kelowna, BC

Re: QS motor magnet max temp before demag ?

Postby Pajda » Fri Mar 17, 2017 2:43 am

I think that neodymium magnets are produced in temperature grades, see this table: http://e-magnetsuk.com/neodymium_magnet ... tings.aspx and I believe that every "better" PMSM producer is using 150°C grade magnets.
Pajda
10 W
10 W
 
Posts: 74
Joined: Sun Jan 24, 2016 3:45 am
Location: Czech Republic

Re: QS motor magnet max temp before demag ?

Postby Doctorbass » Fri Mar 17, 2017 10:33 am

I have contacted Vito and he said the magnets of the QS205 50H motor are 35SH type.

I still wonder if the rotor only for 24h period at 78 celsius is still borderline...

I have found this great recommendation too witch correspond with what you also said guys:

" a magnet rated for a recommended maximum working temperature of 150 degrees C may start to demagnetise significantly at 100 degrees C if the design is poor or a magnet rated for a recommended maximum working temperature of 80 degrees C may start to demagnetise significantly at 100 degrees C is the design is really good."
(from http://e-magnetsuk.com)


This is geting confusing as i also found on another website the spec of the 35SH: withc mention max operating temp of 150 celsius.. ( reference: http://www.magnetsales.com/neo/neoprops.htm)
Attachments
35SH magnet temp.jpg
(207.06 KiB) Downloaded 4 times
Last edited by Doctorbass on Fri Mar 17, 2017 10:34 am, edited 1 time in total. View post history.
CURRENT PROJECT: 2WD duo MXUS/Max-E ebike 32kW
http://endless-sphere.com/forums/viewtopic.php?f=3&t=65764
-Fastest speed record 117 km/h on flat
-Fastest 1/4 mile@ 114km/h on flat and 16.316 sec
-Succeded to haul a 19200 pounds schoolbus!
113kmh Gianthttp://www.evalbum.com/3406
Mongoosehttp://www.evalbum.com/1947
YOUTUBE---https://m.youtube.com/user/Doctorbasss
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 8139
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: QS motor magnet max temp before demag ?

Postby Doctorbass » Fri Mar 17, 2017 10:41 am

I have two brand new QS motor so if i can get a gaussmeter i will measure teh magnetic field and compare...

Doc
CURRENT PROJECT: 2WD duo MXUS/Max-E ebike 32kW
http://endless-sphere.com/forums/viewtopic.php?f=3&t=65764
-Fastest speed record 117 km/h on flat
-Fastest 1/4 mile@ 114km/h on flat and 16.316 sec
-Succeded to haul a 19200 pounds schoolbus!
113kmh Gianthttp://www.evalbum.com/3406
Mongoosehttp://www.evalbum.com/1947
YOUTUBE---https://m.youtube.com/user/Doctorbasss
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 8139
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: QS motor magnet max temp before demag ?

Postby Doctorbass » Fri Mar 17, 2017 11:04 am

I also found that info about ferrofluid temperature:

(reference: Wikipedia)

However, ferrofluids lose their magnetic properties at sufficiently high temperatures, known as the Curie temperature.


I also expect to use ferrofluid in the Qs205..

Doc
CURRENT PROJECT: 2WD duo MXUS/Max-E ebike 32kW
http://endless-sphere.com/forums/viewtopic.php?f=3&t=65764
-Fastest speed record 117 km/h on flat
-Fastest 1/4 mile@ 114km/h on flat and 16.316 sec
-Succeded to haul a 19200 pounds schoolbus!
113kmh Gianthttp://www.evalbum.com/3406
Mongoosehttp://www.evalbum.com/1947
YOUTUBE---https://m.youtube.com/user/Doctorbasss
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 8139
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: QS motor magnet max temp before demag ?

Postby brumbrum » Fri Mar 17, 2017 11:14 am

Doctorbass wrote:I have two brand new QS motor so if i can get a gaussmeter i will measure teh magnetic field and compare...

Doc


A comparison would be excellent.
User avatar
brumbrum
10 kW
10 kW
 
Posts: 875
Joined: Sat Oct 30, 2010 3:29 pm
Location: Wales U.K

Re: QS motor magnet max temp before demag ?

Postby steveo » Fri Mar 17, 2017 2:40 pm

How do you think this will compare vs the x5403?

50mm stator.. nice copper fill from what i've seen.. and it come up the 17.71kv version... and around 29lbs!

i wonder what the efficiency rating of a x5403 was?.. this seems to be around 90%.. .. i know my hub-monster according to johnincr is up to 94% efficient but around 60lbs with tire.

-steveo
Last edited by steveo on Fri Mar 17, 2017 2:44 pm, edited 1 time in total. View post history.
Repair Thread
http://endless-sphere.com/forums/viewto ... =3&t=27170
Hub Monster bike ~ 24s7p A123 15.4ah/18kv Six Phase Motor/Dual Max-E Adapttos/32kw~42.91Hp/Est 140LBS
X6 Kmx Trike ~ 24s4p 20ah/X6 MHM 602/Infinion EB324 IRFB 4110/20Kw~26.82Hp/Est 120LBS ~SOLD~
Lightening rods bike ~ 18s2p 10ah/1500w Inrunner/Infinion EB312 IRFB4110/2KW~2.68hp/Est 60LBS
EV Outboard ~ 12s8p 40ah/5KW GM Inrunner/Infinion EB324 IRFB 4110/18Hp Evinrude Drive/Est 100lbs
http://www.youtube.com/user/trdfreak03
User avatar
steveo
10 MW
10 MW
 
Posts: 2190
Joined: Sat Oct 06, 2007 3:07 pm
Location: Woodbridge, Ontario

Re: QS motor magnet max temp before demag ?

Postby Doctorbass » Fri Mar 17, 2017 3:05 pm

steveo wrote:How do you think this will compare vs the x5403?

50mm stator.. nice copper fill from what i've seen.. and it come up the 17.71kv version... and around 29lbs!

i wonder what the efficiency rating of a x5403 was?.. this seems to be around 90%.. .. i know my hub-monster according to johnincr is up to 94% efficient but around 60lbs with tire.

-steveo



The QS205 is an excellent choice in term of power and continuous power. The 5403 i had was surprizingly a cold motor however i had modified it alot with liquid cooling.

The 205 is like the famous cormotor. it is heavy yes but it is a perfect match for 5+kW controller.

I bought a 3T and a 4T ( 11.5kv) and (9kv)... and the 9kv is my favorite when used with field weakening to boost speed because it have excellent torque and powerband can be extended with the Field weakening.

the famous 5403 and the 5304 have also the same kv of 9 if i remember correctly.

now let's go back to original subject :(demag and temp) wink:

Doc
CURRENT PROJECT: 2WD duo MXUS/Max-E ebike 32kW
http://endless-sphere.com/forums/viewtopic.php?f=3&t=65764
-Fastest speed record 117 km/h on flat
-Fastest 1/4 mile@ 114km/h on flat and 16.316 sec
-Succeded to haul a 19200 pounds schoolbus!
113kmh Gianthttp://www.evalbum.com/3406
Mongoosehttp://www.evalbum.com/1947
YOUTUBE---https://m.youtube.com/user/Doctorbasss
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 8139
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: QS motor magnet max temp before demag ?

Postby macribs » Mon Mar 20, 2017 5:39 pm

For future references when painting and curing a motor I would recommend a pid and and old fashion heater, the kind that got analog switch and heat up the elements to glowing red while a fan blast the heated air out to the room. I tried to use my old brewery heater from a water heater but that just tripped the fuses and tempsensors. I did a heating chamber of some old brownstone bricks and some leftover prefab heat resistance sheets to make a "small oven". I used the same pid and temp probe I use for beer brewing. I got a tip from the shop how temperatures came to play for curing, so I sat the temp to max 45 min 44 celsius and closed the heat chamber and left motor for the weekend. Those pids are fairly quick to response to temp changes and turn the heat source on/off to match the set min/max temp. Of course you can choose higher temps to shorten the curing period.

No sticky paint left on my fingers when I closed down the "curing oven" on sunday night. And temps so low it should not affect the magnets. Side covers I forgot in the garage door opening when my cell rang, and one hour later the sun had baked those covers so hot I jerked my arms back when I tried to move them. That mat flat black really can suck up heat from the sun :oops:
Last edited by macribs on Mon Mar 20, 2017 5:49 pm, edited 1 time in total. View post history.
User avatar
macribs
100 MW
100 MW
 
Posts: 2884
Joined: Tue Jul 22, 2014 5:59 pm

Re: QS motor magnet max temp before demag ?

Postby madin88 » Wed Mar 22, 2017 11:41 am

I wonder what paint you have used. Was ist the krylon deep black? :)

Doc, maybe you remember that i also have painted the entire inner surface of one MXUS 3000 V2 motor and the parts i have also put in the oven for drying. Back on the bike, the motor did overheat quicker than usually (especially when loaded high), because the magnets got weakened.
The temperature was set to 70-80°C, but as mentioned such regualtion is very inaccurate.

Did you have already compared the strength with the gaussmeter?

At that time i used a piece of metal and measured the force it takes to remove it from the magnets with a scale.
It wasn't that accurate, but the results did show reproducible lower strength.

In the end, the dry process in the oven of the rotor did not help anything i believe, because i could chafe off the paint from the magnets easy with my fingers :|
On the other surfaces the paint holds extremely well. I was surprised how well it hold on the strands of the windings.

Did you do any surface preparation on the magnets?
- Votec V-FR frame / MXUS 3T / 17" Mitas MC11 / Adaptto Max-E / 20s12p 25R -> approved as L1e moped and fully road legal in EU :)
- Vector white / MXUS 4T / 24" Hookworms / Adaptto Max-E / 22s11p 25R
- KTM Hardtail Pedelec / eZee V2 6T / 27,5" / Kelly KBSX @ 1,5kW / Torque PAS / CA-V3 / 13s4p Sanyo GA in Shark case
User avatar
madin88
10 MW
10 MW
 
Posts: 2110
Joined: Mon May 27, 2013 2:02 am
Location: Austria

Re: QS motor magnet max temp before demag ?

Postby Doctorbass » Wed Mar 22, 2017 5:11 pm

madin88 wrote:I wonder what paint you have used. Was ist the krylon deep black? :) Simply Krylon ultra mat flat black 1602, 97% absorption on large spectrum

Doc, maybe you remember that i also have painted the entire inner surface of one MXUS 3000 V2 motor and the parts i have also put in the oven for drying. Back on the bike, the motor did overheat quicker than usually (especially when loaded high), because the magnets got weakened.
The temperature was set to 70-80°C, but as mentioned such regualtion is very inaccurate. Well that is sad that yours overheated and that you noticed permanent damage!... On my side, the Oven i have used is a special equippent with very accurate Honewell PID temp controller. The temp remained below 78 degree c ( i had set the shutdown alarm to 80 to be sure )

Did you have already compared the strength with the gaussmeter? not yet , i'm actually looking for a gaussmeter. at work we have one very professional, but i can't locate it

At that time i used a piece of metal and measured the force it takes to remove it from the magnets with a scale.
It wasn't that accurate, but the results did show reproducible lower strength. Yeah that good idea. But i think if i have mathetic field loss it should not be so high as it is right in the knee of the curve according to the 35HS spec sheet at 78 degree C.

In the end, the dry process in the oven of the rotor did not help anything i believe, because i could chafe off the paint from the magnets easy with my fingers :|
On the other surfaces the paint holds extremely well. I was surprised how well it hold on the strands of the windings. Yes you are right, and i remember that last time i painted the magnet on my previous motor, i applied a very thin layer of residual epoxy coming from the excess of sides of the magnet brick, amd applied it on all teh inner surface of the magnet witch helped the paint to stick on these. Then i applied the paint. Yes that paint stick very well on most surface including the winding

Did you do any surface preparation on the magnets?
Yes, i cleaned the magnet with aceton and then isopropylic alcool.

Doc
CURRENT PROJECT: 2WD duo MXUS/Max-E ebike 32kW
http://endless-sphere.com/forums/viewtopic.php?f=3&t=65764
-Fastest speed record 117 km/h on flat
-Fastest 1/4 mile@ 114km/h on flat and 16.316 sec
-Succeded to haul a 19200 pounds schoolbus!
113kmh Gianthttp://www.evalbum.com/3406
Mongoosehttp://www.evalbum.com/1947
YOUTUBE---https://m.youtube.com/user/Doctorbasss
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 8139
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: QS motor magnet max temp before demag ?

Postby Doctorbass » Wed Apr 19, 2017 8:08 pm

GOT MY GAUSSMETER!! :mrgreen:

made in china but very impressive and give repeatable measurement value.

It have 4 effectives digits so it is accurate.

I have measured the only rotor i have at the moment as my two personnla rotor from the 205 are at IREQ lab for 2 days at the moment.

That rotor was damaged by rust and might be also damaged by heat but this is impossible to tell as that motor was on a adaptto at 12kw but WITHOUt temp sensor connected by the user :lol:

once i get the rotor of my 4T motor that got 78 celsius fgor 12 hours i wil test and post results, but from now let see what a 4T motor stator and damaged 5T motor can get as magnetic field!

go to this link! : https://endless-sphere.com/forums/viewtopic.php?f=30&t=87751&p=1281093#p1281093

or see the video directly: :wink:




Doc
Doc
Last edited by Doctorbass on Wed Apr 19, 2017 8:09 pm, edited 1 time in total. View post history.
CURRENT PROJECT: 2WD duo MXUS/Max-E ebike 32kW
http://endless-sphere.com/forums/viewtopic.php?f=3&t=65764
-Fastest speed record 117 km/h on flat
-Fastest 1/4 mile@ 114km/h on flat and 16.316 sec
-Succeded to haul a 19200 pounds schoolbus!
113kmh Gianthttp://www.evalbum.com/3406
Mongoosehttp://www.evalbum.com/1947
YOUTUBE---https://m.youtube.com/user/Doctorbasss
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 8139
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: QS motor magnet max temp before demag ?

Postby DasDouble » Thu Apr 20, 2017 3:30 pm

@Doc, could you please explain me why you have put that brown paper between your stator and the side plate of your motor? It looks like some classic baking paper which is used for making pizza.. :roll: :D
Highpower Ebike enthusiast.
-Built own ebike: ✔
-Built own high quality 3.2kWh LiIon battery: ✔
-Overtake Porsche with own Ebike: ✔
-Take off with ebike: ✖

~14kW, 3.2kWh LiIon, QS 205 8ml ff
User avatar
DasDouble
10 kW
10 kW
 
Posts: 954
Joined: Sun Jul 12, 2015 1:35 pm
Location: GERMANIA :D

Re: QS motor magnet max temp before demag ?

Postby macribs » Thu Apr 20, 2017 3:37 pm

My guess is that he has been masking up the motor before he sprayed the motor. I am sure the paper was removed before he assembled the motor.
User avatar
macribs
100 MW
100 MW
 
Posts: 2884
Joined: Tue Jul 22, 2014 5:59 pm

Re: QS motor magnet max temp before demag ?

Postby Doctorbass » Thu Apr 20, 2017 4:11 pm

DasDouble wrote:@Doc, could you please explain me why you have put that brown paper between your stator and the side plate of your motor? It looks like some classic baking paper which is used for making pizza.. :roll: :D


Ah excellent question!

in fact that,s the residual brown paper that i used for painting.. however that part is the negative part of the paper i used to protect the rest of the motor outside when painting the magnet. I used the paper disk to protect the magnet from dust and magnetic particle while waiting to receive my gaussmeter.

Doc
CURRENT PROJECT: 2WD duo MXUS/Max-E ebike 32kW
http://endless-sphere.com/forums/viewtopic.php?f=3&t=65764
-Fastest speed record 117 km/h on flat
-Fastest 1/4 mile@ 114km/h on flat and 16.316 sec
-Succeded to haul a 19200 pounds schoolbus!
113kmh Gianthttp://www.evalbum.com/3406
Mongoosehttp://www.evalbum.com/1947
YOUTUBE---https://m.youtube.com/user/Doctorbasss
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 8139
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: QS motor magnet max temp before demag ?

Postby madin88 » Fri Apr 21, 2017 3:28 am

I wonder if iron saturation can be measured with such gaussmeter?

About the magnetic field i always was the meaning it is strongest above the middle of the magnets, since between the magnets the fields are canceling out and doing not much (or nothing?) in view of torque.
Thats why weight optimized motors have a gap between the magents.
- Votec V-FR frame / MXUS 3T / 17" Mitas MC11 / Adaptto Max-E / 20s12p 25R -> approved as L1e moped and fully road legal in EU :)
- Vector white / MXUS 4T / 24" Hookworms / Adaptto Max-E / 22s11p 25R
- KTM Hardtail Pedelec / eZee V2 6T / 27,5" / Kelly KBSX @ 1,5kW / Torque PAS / CA-V3 / 13s4p Sanyo GA in Shark case
User avatar
madin88
10 MW
10 MW
 
Posts: 2110
Joined: Mon May 27, 2013 2:02 am
Location: Austria

Re: QS motor magnet max temp before demag ?

Postby spinningmagnets » Fri Apr 21, 2017 5:06 am

Doc, you have tried several coatings inside the motor to protect from rust. what brand of coating do you use now as the best?
User avatar
spinningmagnets
100 GW
100 GW
 
Posts: 10195
Joined: Fri Dec 21, 2007 10:27 pm
Location: Ft Riley, NE Kansas

Re: QS motor magnet max temp before demag ?

Postby DasDouble » Fri Apr 21, 2017 5:16 am

spinningmagnets wrote:Doc, you have tried several coatings inside the motor to protect from rust. what brand of coating do you use now as the best?

Really good question. +1 Im interested too
Highpower Ebike enthusiast.
-Built own ebike: ✔
-Built own high quality 3.2kWh LiIon battery: ✔
-Overtake Porsche with own Ebike: ✔
-Take off with ebike: ✖

~14kW, 3.2kWh LiIon, QS 205 8ml ff
User avatar
DasDouble
10 kW
10 kW
 
Posts: 954
Joined: Sun Jul 12, 2015 1:35 pm
Location: GERMANIA :D

Re: QS motor magnet max temp before demag ?

Postby Doctorbass » Fri Apr 21, 2017 9:02 am

madin88 wrote:I wonder if iron saturation can be measured with such gaussmeter?

About the magnetic field i always was the meaning it is strongest above the middle of the magnets, since between the magnets the fields are canceling out and doing not much (or nothing?) in view of torque.
Thats why weight optimized motors have a gap between the magents.



That's a good point!

In fact i have remeasured the mag field and it appear that if i place the probe 90 degree ( perpendicular) to the magnet exactly while between at the intersection of two consecutive magnets, the magnetic field reach 5000 gauss.
That's the closer point where the magnet field lines ( WITHOUT being affected by the stator witch is absent) are the most dense since this is the point where N and S are the closest. However when the stator is present the core make the mag filed to modify their path and from now i have no way to measure it as the room between rotor and stator is too thin. But if you look at this drawing you can see that the fied seem to have a better distribution than the 3400Gauss to 5000 gauss i measure on the rotor only.

Image

Doc
CURRENT PROJECT: 2WD duo MXUS/Max-E ebike 32kW
http://endless-sphere.com/forums/viewtopic.php?f=3&t=65764
-Fastest speed record 117 km/h on flat
-Fastest 1/4 mile@ 114km/h on flat and 16.316 sec
-Succeded to haul a 19200 pounds schoolbus!
113kmh Gianthttp://www.evalbum.com/3406
Mongoosehttp://www.evalbum.com/1947
YOUTUBE---https://m.youtube.com/user/Doctorbasss
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 8139
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: QS motor magnet max temp before demag ?

Postby Doctorbass » Fri Apr 21, 2017 9:19 am

DasDouble wrote:
spinningmagnets wrote:Doc, you have tried several coatings inside the motor to protect from rust. what brand of coating do you use now as the best?

Really good question. +1 Im interested too



I only use one brand as this is the most popular and professional product i have acces to. It is SPECIALY made for that purpose and is specialy formuled to wistand the worst environment. In Canada we develop and produce alot of motor and transformer in different brands and the Sprayon is the product the most availlable/popular. The actual version i use is the EL601. It is a epoxy based coating.



Dielectritic Strength: 2,600VPM

Dielectric Strength: 2,600 Volts per Meter

NEMA & UL Temperature Class

310°F / 155°C

National Electrical Manufacturers Association (NEMA) & Underwriters Laboratories (UL) Temperature Class: F (310°F / 155°C) Maximum Hot Spot Temperature Allowed

Color: Red

Nozzle Type: EZ-Touch™ for superior coverage and control with a conical spray

HMIS Rating: 2,4,0

Hazardous Materials Identification System (HMIS) Rating: Health - 2, Flammability - 4, Reactivity - 0


At a Glance

•Air dries In 10 minutes
•Meets NEMA & UL Class F Requirements
Resists oil, moisture, acids and alkalis
Meets performance requirements of ASTM D115-07 4.2



Uses :
Small field and magnet coils, motor windings, field coils, transformers, armatures, commutator ends, stator windings, ring and frames, bus bars, sealing electrical, switchboard parts and electronic components.

% Solids = 0.228%
% VOC = 0.5517%
Base Type = Phenolic Epoxy
Color = Red
Consistency = Liquid
Dielectric Strength = 2600Volts
Evaporation Rate = Fast
Film Type = Semi-Solid
Flammable = Yes
Flashpoint = <0°F
HMIS Rating = 2,4,0
Plastic Safe = No
Propellant = Hydrocarbon
Sheen = Semi-Gloss
Specific Gravity = 0.79
Spray Pattern = Danvern
Temp High = 400°F
Temp Low = 310°F
Temperature Class = Class F (155°C / 310°)
See more at: https://www.sprayon.com/product-categor ... ncnEB.dpuf

https://www.sprayon.com/product-categories/electrical-and-electronic-cleaners-and-degreasers/red-insulating-varnish-aerosol-el601

Doc
CURRENT PROJECT: 2WD duo MXUS/Max-E ebike 32kW
http://endless-sphere.com/forums/viewtopic.php?f=3&t=65764
-Fastest speed record 117 km/h on flat
-Fastest 1/4 mile@ 114km/h on flat and 16.316 sec
-Succeded to haul a 19200 pounds schoolbus!
113kmh Gianthttp://www.evalbum.com/3406
Mongoosehttp://www.evalbum.com/1947
YOUTUBE---https://m.youtube.com/user/Doctorbasss
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 8139
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: QS motor magnet max temp before demag ?

Postby DasDouble » Fri Apr 21, 2017 11:03 am

Thanks a lot! As always, really detailed information about that spray. I wonder where I could get that in Germany.... :roll:
Highpower Ebike enthusiast.
-Built own ebike: ✔
-Built own high quality 3.2kWh LiIon battery: ✔
-Overtake Porsche with own Ebike: ✔
-Take off with ebike: ✖

~14kW, 3.2kWh LiIon, QS 205 8ml ff
User avatar
DasDouble
10 kW
10 kW
 
Posts: 954
Joined: Sun Jul 12, 2015 1:35 pm
Location: GERMANIA :D

Next

Return to Motor Technology

Who is online

Users browsing this forum: No registered users and 8 guests