so my shaft wear is getting worse over time so i gotta do something about it asap. been mulling over a few options:
1) weld the sprocket :lol:
2) build up the splines w/ MIG. high heat settings and 0.6mm wire should deposit some tiny little drops of weld. shouldn't be too hard to shape them w/ a dremel. but i don't have hardfacing wire so it'll probably wear out fast.
3) stack 2 sprockets (welded together) to interface w/ as much splines as possible. then plug weld a washer over the shaft to hold the sprocket in.
any other bright ideas?