MXUS copper wire coating damaged

Electric Motors and Controllers
Post Reply
User avatar
shorza   1 kW

1 kW
Posts: 488
Joined: Oct 13 2010 11:29pm
Location: Melbourne, Australia

MXUS copper wire coating damaged

Post by shorza » Jan 02 2018 6:46am

I opened my MXUS v3 and noticed a small scrape on the varnish of the copper wire. I tested the continuity with my multimeter and it shows a short to my phase wires.

I'm not sure how it happened, it doesn't seem raised enough to be touching the side plate.

Is this a major problem or will this cause an issue?

20180102_220927-768x1024.jpg
20180102_220927-768x1024.jpg (230.12 KiB) Viewed 806 times
20180102_222210-600x1067.jpg
20180102_222210-600x1067.jpg (205.62 KiB) Viewed 806 times
Edit: changed the wording.
Last edited by shorza on Jan 02 2018 3:50pm, edited 1 time in total.

major   10 kW

10 kW
Posts: 832
Joined: Mar 10 2013 10:12am
Location: NW Ohio, USA

Re: MXUS lamination coating damaged

Post by major » Jan 02 2018 11:50am

It appears, from photos, that you refer to a scrape or bare spot on the wire, not a damaged lamination. Laminations are thin steel plates stacked together to make the core. Coils of wire are wound or inserted onto or into slots in the laminated core. The coil wire is copper with a coating or film of insulating varnish or resin. A small bare spot like that on a single wire that does not come in contact with anything else is inconsequential although to be on the safe side, I'd recommend to repair by applying a drop or two of high temperature epoxy or 'super' glue.

major

User avatar
fechter   100 GW

100 GW
Posts: 15182
Joined: Dec 31 2006 3:23pm
Location: California Bay Area, USA

Re: MXUS lamination coating damaged

Post by fechter » Jan 02 2018 3:26pm

Yes, epoxy will fix that, but you should not have any continuity between the phase wires and the laminations. You may have another problem somewhere.
"One test is worth a thousand opinions"

User avatar
shorza   1 kW

1 kW
Posts: 488
Joined: Oct 13 2010 11:29pm
Location: Melbourne, Australia

Re: MXUS copper wire coating damaged

Post by shorza » Jan 02 2018 3:54pm

Thanks guys. I've edited the original post to amend the incorrect term.

The laminations are not damaged, it's the coating on the copper wire that is damaged. I'll put a small dab of super glue over it like major suggested.

User avatar
sn0wchyld   1 MW

1 MW
Posts: 1802
Joined: Mar 18 2011 8:27pm
Location: South Aus.

Re: MXUS copper wire coating damaged

Post by sn0wchyld » Jan 03 2018 5:52pm

just make sure its rated for higher temperatures - super glue can start to break down at ~80C - your wires may get much hotter than that.