New Original LG 21700 5000mAh Cells

Place for dealers to post items for sale.
Post Reply
bibo164   10 µW

10 µW
Posts: 6
Joined: Jan 24 2015 8:38am

New Original LG 21700 5000mAh Cells

Post by bibo164 » Jan 14 2021 8:32am

Hello,

I have a source for BRAND NEW LG INR21700 M50T Cells. They are factory new and have never been used.

I am using them myself and would like to understand if you are also interesten in them? For that please write me a pm or comment how many cells you would order and where you live. From this I can figure out how much demand there is and how I could best sell them to you. Please only write me if you seriously consider buying them.
I live in central Germany and would ship to the EU for now. The price may vary depending on interest/quantity.

The cells are immediately available to me, so once there is enough interest I could start shipping.
These are NOT 18650 Cells, they are slightly bigger 21mm x 700mm!

LG INR21700-M50T 5000mAH / 7,5 A continuous / 15 A peak
3,99€/cell + shipping
>100 cells 3,89€/cell + shipping
a5fdeb89-a822-49f6-9fe2-87424242cdd0.jpg
a5fdeb89-a822-49f6-9fe2-87424242cdd0.jpg (280.31 KiB) Viewed 1008 times
1bdc320a-241c-4b11-878d-dd5885084acc.jpg
1bdc320a-241c-4b11-878d-dd5885084acc.jpg (344.48 KiB) Viewed 1008 times
Max. cont. charge current:
0 ~ 25°C 0.3C (1,455mAh)
25 ~ 45°C 0.7C (3,395mAh)

Max. cont. discharge current:
-20 ~ 10°C 0.5C (2,425mAh)
10 ~ 25°C 3.0C (14,550mAh)
25 ~ 55°C 1.5C (7,275mAh)
Last edited by bibo164 on Feb 12 2021 8:17am, edited 2 times in total.

john61ct   100 GW

100 GW
Posts: 7461
Joined: Dec 18 2018 2:06pm

Re: New Original LG 21700 5000mAh Cells

Post by john61ct » Jan 14 2021 11:47am

What assurance that they are genuine?

Have you run your own cap tests?

bibo164   10 µW

10 µW
Posts: 6
Joined: Jan 24 2015 8:38am

Re: New Original LG 21700 5000mAh Cells

Post by bibo164 » Jan 14 2021 1:17pm

I will do proper capacity tests over the weekend and share the results.

There is in fact no guarantee that they are genuine but all the infos I have add up.

I can send send you a couple of cells at a discount for testing and confirming their quality. Please let me know if you are interested.

User avatar
Merlin   10 MW

10 MW
Posts: 2136
Joined: Jan 29 2013 10:00am
Location: europe

Re: New Original LG 21700 5000mAh Cells

Post by Merlin » Jan 14 2021 5:36pm

but....beside no heatshrinks and me wondering why they circle around when they are "genuine"...this is the NKON price from a well known international seller company with tax and invoice.

....i mean. you are selling ....private.

if you have a source of 20700 sanyos.....well...than iam in :D

bibo164   10 µW

10 µW
Posts: 6
Joined: Jan 24 2015 8:38am

Re: New Original LG 21700 5000mAh Cells

Post by bibo164 » Jan 15 2021 3:42am

You are right, so I adjusted the offer with prices for the expected quantities and made a special offer for anyone who wants to check out those cells and give some feedback. Cap tests will follow over the weekend.

User avatar
Merlin   10 MW

10 MW
Posts: 2136
Joined: Jan 29 2013 10:00am
Location: europe

Re: New Original LG 21700 5000mAh Cells

Post by Merlin » Jan 15 2021 8:15am

capacity test is nice but what counts is internal resistance. thats the only thing that says something about in relation to capacity.

you can squeeze out maybe 5Ah out of it using just 0.5a current.
but if you have "grade C" cells and discharge them with 7.5A continue they may have only 4Ah.

bibo164   10 µW

10 µW
Posts: 6
Joined: Jan 24 2015 8:38am

Re: New Original LG 21700 5000mAh Cells

Post by bibo164 » Jan 18 2021 5:43am

Hello,

so here some more infos on the cells:
cell spec.jpg
cell spec.jpg (691.17 KiB) Viewed 792 times
The cells were supposed to end up in these 13S1P packs for a german OEM. Because for whatever reason this project was scrapped so they had to get rid of the already manufactured packs and the rest of the cells. Unfortunately the fully equipped packs were discharged to 0V so they can only be scrapped.
I took one pack apart and equipped it with new cells but the BMS does not come on. If someone thinks he can reverse engineer this BMS please contact me.
13S1P Packs.jpg
13S1P Packs.jpg (5.12 MiB) Viewed 788 times
so I did several Tests with the cells:
1. Internal resistance test: I never measured any value above 60mOhms
[youtube]Gjfki-W6uVU[/youtube]

2. 5-7A Discharge (maxed out my charger) Result: 4790mAh
[youtube]onBMhaVWftA[/youtube]

3. I configured a 13s1p pack and discharged it through an inverter with 7.5A to 3.35V per cell (inverter cut-off) - Result: 2.52Ah
[youtube]R2BnkjFNHuY[/youtube]

john61ct   100 GW

100 GW
Posts: 7461
Joined: Dec 18 2018 2:06pm

Re: New Original LG 21700 5000mAh Cells

Post by john61ct » Jan 18 2021 1:31pm

The problem is, very difficult to get a "standard" consistent measure of ESIR, without tightly specifying a dozen different conditions.

A pure cap test is always done at super low current rates, 0.01C would be the highest if trying to confirm against the nameplate rating.

This is no verification of "A" vs "B" production runs, that really depends on the reputation of the supply chain.

But assuming they are not counterfeit, at least verifies they are new or at least in good shape, not worn second-hand.

If you start testing for high C-rates without too much voltage drop or heat build-up

that is no longer a cap test, more like the "real C" tests we see members perform to rate brand quality, like ESIR requiring lots of variables to be spec'd and held constant and beyond what most sellers would allow before purchase.
Merlin wrote:capacity test is nice but what counts is internal resistance.

lesta   1 µW

1 µW
Posts: 2
Joined: Apr 16 2019 5:59am

Re: New Original LG 21700 5000mAh Cells

Post by lesta » Jan 28 2021 11:28am

Pm sent

User avatar
Cheburator   100 mW

100 mW
Posts: 43
Joined: May 02 2018 3:48pm

Re: New Original LG 21700 5000mAh Cells

Post by Cheburator » Feb 12 2021 2:44am

Cells received, thank you!
I have tested 3 cells to check the consistency of parameters.
Each cell weights 68.6g, are at 3.58V and my YR1035 shows internal resistance of 22 mOhms. Cells come completely naked without any signs of use. I have added top insulation sticker and shrink wrap for extra safety.
Image Image
Image

Capacity test at 1A showed about 5Ah.
Image
https://i.postimg.cc/L68h52YL/P2080274.jpg
https://i.postimg.cc/50J2VVWH/P2100276.jpg

Capacity test at 7.5A showed about 4.8Ah.

[youtube]www.youtube.com/watch?v=u4zRYvkYTz0[/youtube]
[youtube]https://youtu.be/pXVEqKn1t80[/youtube]
[youtube]https://youtu.be/LZYLJYLt0n8[/youtube]

After all tests internal resistance have not changed.
So I can say that these cells are genuine and new, all parameters correspond to datasheet.

john61ct   100 GW

100 GW
Posts: 7461
Joined: Dec 18 2018 2:06pm

Re: New Original LG 21700 5000mAh Cells

Post by john61ct » Feb 12 2021 3:17am

Very nice results!

Fact that capacity drops so little going from 0.2C to 1.5C a great sign.

What was your LVC on those tests?

USD $270 per kWh

OP please quote for 50 units, with shipping to NYC, slow is fine but tracked of course

User avatar
Cheburator   100 mW

100 mW
Posts: 43
Joined: May 02 2018 3:48pm

Re: New Original LG 21700 5000mAh Cells

Post by Cheburator » Feb 12 2021 3:56am

What was your LVC on those tests?
I discharged to 2.5V as I tried to follow the datasheet instructions as good as I can.
Image

john61ct   100 GW

100 GW
Posts: 7461
Joined: Dec 18 2018 2:06pm

Re: New Original LG 21700 5000mAh Cells

Post by john61ct » Feb 12 2021 8:27am

Yep that is right for benchmarking, but not something to do routinely 8-)

The vendor test for nameplate rating was likely half an amp or even the 20-hour rate

Post Reply