PM if interested.
PRICE: $180 per box plus shipping (estimate $50-$75 within the lower 48). I would like to sell these by the box.
I have available four boxes of qty 120 Samsung ICR18650-26F cells. These cells are unused and have never been removed from the box. All four boxes are from the same production date and batch, something very desirable for integrating into a large format battery.
I pulled out 8 samples and took OCV measurements. All read 3762 mV +/- 0.5 mV
PRICE: $180 per box plus shipping (estimate $50-$75 within the lower 48). I would like to sell these by the box.
I have available four boxes of qty 120 Samsung ICR18650-26F cells. These cells are unused and have never been removed from the box. All four boxes are from the same production date and batch, something very desirable for integrating into a large format battery.
I pulled out 8 samples and took OCV measurements. All read 3762 mV +/- 0.5 mV